Tpc Japan Hdpe Kf052a

TPC (Japan) HDPE KF052A

    • Product Name: TPC (Japan) HDPE KF052A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 231990
    Density 0.952 g/cm3
    Melt Flow Rate Mfr 190 C 2 16 Kg 0.05 g/10 min
    Tensile Strength At Yield 25 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 800%
    Flexural Modulus 1.10 GPa
    Izod Notched Impact Strength At 23 C 0.20 ft·lb/in
    Izod Notched Impact Strength At 20 C 0.10 ft·lb/in
    Vicat Softening Temperature 124°C
    Heat Deflection Temperature At 0 46 Mpa 75°C
    Shore D Hardness 66
    Environmental Stress Crack Resistance Escr >1000 h

    As an accredited TPC (Japan) HDPE KF052A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KF052A is supplied in 25 kg net paper bags, typically palletized at 1,000 kg per pallet.
    Container Loading (20′ FCL) TPC (Japan) HDPE KF052A is typically loaded in 20′ FCL containers as 25 kg bags, floor-loaded, about 20 MT net.
    Shipping TPC (Japan) HDPE KF052A is shipped as non-hazardous high-density polyethylene pellets, typically in 25 kg bags or bulk. It is not DOT/IMDG/IATA regulated. No UN number or dangerous goods documentation is required. Transport in clean, dry, covered containers; protect from moisture, heat, and sunlight. Standard freight handling applies.
    Storage Store TPC (Japan) HDPE KF052A in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep bags or containers sealed on pallets to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Maintain clean, stable conditions, observe good housekeeping, and follow the manufacturer’s SDS and local regulations. Do not stack excessively. Ensure proper ventilation.
    Shelf Life TPC (Japan) HDPE KF052A: 24-month shelf life in unopened original packaging, stored cool, dry, away from sunlight, heat, and contaminants.
    Application of TPC (Japan) HDPE KF052A

    On upward high-stalk blown film lines fitted with 45–65 mm grooved-feed extruders at L/D 28:1–30:1 and spiral mandrel dies of 150–250 mm, TPC KF052A is converted into vest-style carrier bag film at a nominal density of 0.952 g/cm³ under ISO 1183-1 and a nominal melt flow rate of 0.05 g/10 min under ISO 1133-1:2022 at 190°C and 2.16 kg. The feeding zone is held at 170–180°C, the compression zone at 185–195°C, the metering zone at 200–210°C, and the die at 200–210°C. Die gap is set between 1.4 mm and 2.0 mm. The high molecular weight of the grade produces a stable stalk at 6–9 die diameters above the die face with a blow-up ratio of 3.8:1 to 4.5:1; frost line height is controlled at 650–900 mm. When melt temperature drops below 190°C, gauge uniformity deteriorates and dart impact scatter under ASTM D1709 Method A increases; when die lip temperature exceeds 215°C, oxidation gel generation becomes visible as surface specks within 30 min. Typical monolayer formulation is 98.5–99.0 wt% KF052A with 1.0–1.5 wt% of a 40% silica antiblock masterbatch and, where colour is required, 2–4 wt% of a PE-based pigment masterbatch. The film is produced at 15–25 µm and is evaluated for tensile properties under ASTM D882, for Elmendorf tear under ASTM D1922, and for dart drop impact under ASTM D1709 Method A. The web is converted on bag-making machines in 2-up or 3-up configurations, with side-seal or bottom-seal tooling, perforation, and handle die-cutting. Finished articles are 15–30 L vest-style carrier bags, retail shipment sacks, and light merchandise bags with die-cut handles.

    What Limits Reclaim Letdown in Three-Layer Refuse Sack Structures?

    Coextrusion of refuse sacks with KF052A in the outer skin layers exposes throughput limits controlled by viscosity mismatch between virgin high-molecular-weight HDPE and post-consumer reclaim. The nominal melt flow rate of KF052A is 0.05 g/10 min under ISO 1133-1:2022, whereas sorted post-consumer HDPE crumb and agglomerate can range from 0.02 g/10 min to 0.25 g/10 min within a single lot. A 70 mm three-layer grooved-feed extrusion line with a 300 mm spiral mandrel die, die gap of 1.6 mm and blow-up ratio of 4.0:1 can run 20 µm film at 180–220 kg/h when reclaim is isolated in the core. At reclaim loadings above 50 wt% of the core layer, gels from PP labels, PET fragments and paper fibre ash nucleate micro-tears at the die lip. The resulting film loses 25–40% of its dart impact value under ASTM D1709 Method A relative to the virgin monolayer control. Screen packs are arranged as breaker plate, 40/60/100 mesh; upstream pressure rises from 220 bar to 310 bar over 48 h, and a slide-plate continuous melt filter is back-flushed once per shift. Seal jaw temperature is capped at 160°C for mixed PCR structures; above this temperature, char from residual paper labels migrates to the seal surface and reduces seal strength under ASTM F88. The layer distribution in Table 1 is used for 20 µm refuse sacks. Finished articles are 30 L, 60 L and 120 L refuse sacks and institution bin liners at 16–35 µm.

    Three-layer refuse sack formulation at 20 µm gauge
    LayerMass fractionResin compositionNominal gauge contribution
    Outer skin20%100% TPC KF052A4 µm
    Core55%80% washed PCR HDPE, 20% KF052A11 µm
    Inner skin25%KF052A plus 0.8% silica antiblock masterbatch5 µm

    Embossing Drum Liners Without Sacrificing Machine-Direction Tear

    Industrial drum liners are produced from KF052A at 14–18 µm on a 60 mm extruder with L/D 30:1 and a 200 mm spiral mandrel die; barrel temperatures are 180–215°C from feed throat to die, and melt temperature is maintained at 195–205°C. The bubble is run at BUR 3.5:1 and the die gap is set to 1.8 mm. Below BUR 3.0:1, the film loses transverse extensibility and splits during in-line embossing; above BUR 4.0:1, the stalk becomes unstable and gauge profile variation exceeds ±8%. In-line embossing uses a steel pattern roll and a rubber back-up roll at a surface temperature of 50–60°C and a nip load of 35–50 N/mm of face length. Embossing penetration is limited to less than one third of nominal gauge; deeper embossing reduces Elmendorf tear under ASTM D1922 and machine-direction tear under ASTM D1004 by more than 15%. Seal initiation temperature for KF052A in this configuration is measured at 125–130°C, and a continuous heat-seal tester per ASTM F88 records plateau seal strength between 140°C and 165°C. The film is converted into 55–120 L drum liners and heavy-duty refuse containers for non-hazardous solid production waste. The liners are not specified for hydrocarbon solvents or strong oxidizing acids; contact with such media produces swelling and oxidative embrittlement within 24 h at ambient temperature.

    Food-contact produce roll bags are produced from KF052A on a 50 mm upward blown film line with a 250 mm die, die gap of 1.8 mm and BUR 4.0:1. Barrel temperatures are 170–210°C, and frost line height is held at 6–8 die diameters to keep haze low and gauge variation below ±6%. The film is corona treated to 40–44 mN/m surface tension at 45 m/min for water-based flexographic printability. In-line rotary pin perforation is applied at 300–500 mm intervals before the surface winder; the average bag length is 500–600 mm and film thickness is 10–15 µm. Because the application includes direct food contact, migration testing follows EU Regulation (EU) No 10/2011, Annex I and Annex V, with food simulants A, B and D2 assigned to aqueous, acidic and fatty produce. For the US market, olefin polymer compliance is established under FDA 21 CFR 177.1520. The relevant compliance matrix is listed in Table 2. Surface slip control for roll unwinding is achieved with 0.4–0.8 wt% silica antiblock masterbatch; excessive slip additive increases unwind telescoping at high line speeds. Finished roll bags are perforated HDPE produce packs typically 350–450 mm wide for in-store dispensers.

    Compliance matrix for produce roll bag applications
    MarketStandard or regulationTest or clause
    USFDA 21 CFR 177.1520Olefin polymers, food contact
    EURegulation (EU) No 10/2011Annex I, Annex III, Annex V
    EUREACH Regulation (EC) No 1907/2006SVHC content documentation
    USASTM D882Tensile properties of thin plastic film
    USASTM D1709 Method ADart drop impact

    When HDPE Film Replaces Paper in Woven Bulk Sack Inner Liners

    In animal feed and mineral bulk-pack operations, a blown HDPE inner liner of KF052A is inserted into woven PP or woven HDPE outer sacks to provide moisture protection and product containment. The liner film is produced at 20–25 µm on a 55 mm high-stalk line with BUR 3.8:1 and die gap 1.5 mm. The melt is extruded at 190–205°C into a cooling air stream at 18–25°C; lower air temperature stabilizes the stalk but increases retained stress, which can cause puckering when the liner is lap-sealed to the woven outer sack. The liner is heat-sealed at 145–155°C with dwell time of 0.8–1.2 s using serrated PTFE-coated sealing bars; seal strength is not less than 12 N/25 mm under ASTM F88. Fold-line flexing is evaluated with a Gelbo flex tester under ASTM F392, because the liner must withstand repeated handling after filling without pinhole development. Typical filled weights are 25 kg and 50 kg. The operational temperature limit is 70°C; seal strength declines more than 40% at 80°C, and the film begins to soften. KF052A liners are therefore not used for hot-filled compounds or autoclaved bulk products.

    Free Quote

    Competitive TPC (Japan) HDPE KF052A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KF052A is a high-density polyethylene film extrusion grade supplied in pellet form. The polymer belongs to the ethylene polymer class registered under CAS 9002-88-4 and is classified within the HDPE film resins covered by ASTM D4976 and JIS K6922-2. The KF052A designation identifies a material with a nominal density of 0.952 g/cm³ when measured under JIS K7112/ISO 1183-1 and a nominal melt flow rate of 0.52 g/10 min at 190°C/2.16 kg under JIS K7210/ISO 1133-1:2022. These values position KF052A between lower-density, high-toughness LLDPE film resins and higher-density HDPE grades intended for blow molding or injection molding. The product is not formulated for cast film, extrusion coating, or injection molding; its melt rheology and density are configured for tubular blown-film processing.

    Because the density approaches 0.952 g/cm³, the resulting film exhibits higher tensile modulus and lower moisture vapour transmission than LLDPE or LDPE films of equivalent thickness. The mid-range melt flow rate of 0.52 g/10 min provides sufficient melt strength for bubble stability at blow-up ratios from 3:1 to 5:1. End uses are therefore specified where stiffness, gauge reduction, and moisture barrier are primary requirements: grocery sacks, trash liners, and industrial packaging films. These end uses are supported by mechanical data generated under JIS K7161/ISO 527-2 and barrier data generated under ASTM E96/E96M, rather than by qualitative descriptors.

    What Material Properties Define KF052A as a Film Extrusion Grade?

    Published datasheet values for KF052A characterize the material after conditioning at 23°C and 50% RH. Tensile yield strength is typically reported at 27 MPa, and elongation at break is typically above 500% when tested according to JIS K7161/ISO 527-2 at a test speed of 50 mm/min. Flexural modulus is typically 1150 MPa under JIS K7171/ISO 178. Vicat softening temperature is approximately 124°C under JIS K7206/ISO 306 Method A50. The combination of flexural modulus above 1000 MPa and elongation at break above 500% explains the suitability of the grade for thin-gauge film converting lines where crease resistance and load-bearing capacity are measured under ASTM D882.

    PropertyTest methodTypical valueUnit
    Melt flow rate at 190°C/2.16 kgJIS K7210 / ISO 1133-1:20220.52g/10 min
    DensityJIS K7112 / ISO 1183-10.952g/cm³
    Tensile yield strengthJIS K7161 / ISO 527-227MPa
    Elongation at breakJIS K7161 / ISO 527-2>500%
    Flexural modulusJIS K7171 / ISO 1781150MPa
    Vicat softening temperatureJIS K7206 / ISO 306124°C

    The values in the table are typical values, not specification limits. Lot-specific certification must be obtained from the supplier, particularly where conversion involves food-contact status, thin-gauge film below 15 μm, or high-speed printing after corona treatment.

    On a 55 mm to 65 mm grooved-feed single-screw extruder with a 30:1 L/D barrier screw, the melt temperature for KF052A film is generally set between 190°C and 210°C. At die temperatures below 170°C, surface melt fracture and shark-skin defects are observed on HDPE film grades of this melt flow class; at melt temperatures above 230°C, bubble instability and edge flutter increase. The processing window is therefore bounded by observable failure modes rather than by a single setpoint. Temperature gradients greater than 10°C across the die can produce gauge variation and localised gel formation, especially after interruptions in screw feed.

    The recommended die gap is 0.8 mm to 1.2 mm for films of 25 μm to 80 μm. At a blow-up ratio of 4:1, frost-line height is typically held at 6 to 10 die diameters to stabilise the bubble. The melt flow rate of 0.52 g/10 min permits higher screw speed relative to lower-MFR high-molecular-weight HDPE film grades, but melt pressure must be monitored at high throughput. Melt pressures above 450 bar on a 65 mm extruder generally indicate insufficient barrel heating, excessive back pressure from the die assembly, or a restricted screen pack.

    Gauge uniformity is sensitive to die lip alignment and internal bubble cooling. When internal bubble cooling is absent, maximum stable output on a 65 mm line with a 1.0 mm die gap is commonly limited by bubble sag rather than extruder capacity. Published data for KF052A’s specific internal bubble cooling response is limited; converters should validate output limits on the actual line configuration and die diameter.

    When Stiffness and Barrier Requirements Favour KF052A over LLDPE and LDPE

    In film applications where load-bearing modulus and moisture vapour transmission rate control fitness for use, HDPE KF052A is selected over LLDPE and LDPE because the higher density of 0.952 g/cm³ produces a semi-crystalline morphology with fewer branched chains. The practical consequence is measured under ASTM D882 as a machine-direction tensile modulus that typically falls between 600 MPa and 1000 MPa for HDPE film of 25 μm thickness, whereas LLDPE and LDPE films of equivalent thickness typically exhibit tensile moduli of 150 MPa to 400 MPa. These ranges are class-level values, not batch-specific guarantees for KF052A.

    Film classDensity rangeMD tensile modulus rangeWVTR at 25 μm thickness
    HDPE KF052A class0.952 g/cm³600–1000 MPa under ASTM D8824–8 g/m²·day under ASTM E96/E96M
    LLDPE butene C40.918–0.922 g/cm³200–400 MPa under ASTM D88215–25 g/m²·day under ASTM E96/E96M
    LDPE autoclave0.922–0.925 g/cm³150–250 MPa under ASTM D88215–20 g/m²·day under ASTM E96/E96M

    Compared with other HDPE film grades in the TPC Japan lineup, KF052A’s melt flow rate is higher than high-molecular-weight film grades, which improves output but lowers bubble stability at extreme blow-up ratios above 5:1. Compared with injection-molding HDPE grades having melt flow rates from 9 g/10 min to 20 g/10 min, KF052A retains sufficient melt strength for tubular film formation and shows reduced tendency to draw resonance during low-shear processing. The grade is not designed for high-speed cast film; published process data for cast-film configuration is limited.

    End-use conversion of KF052A covers thin-gauge high-stiffness films where gauge reduction is quantified against ASTM D6988 for film thickness and ASTM D882 for tensile properties. The resin has been specified for grocery sacks, shopping bags, and trash liners because the tensile yield stress of 27 MPa permits down-gauging when compared with LDPE film of equal strength. These applications are subject to customer specifications; tear strength and puncture resistance should be confirmed by ASTM D1922 and ASTM D5748 respectively, because HDPE films typically show lower Elmendorf tear than LLDPE films in the machine direction.

    For food-contact applications, converters must obtain the supplier’s lot-specific declaration of compliance. HDPE grades of this class are typically evaluated under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011, but compliance is not an inherent property of the pellet and depends on the absence of unlisted additives in the final converted film. RoHS Directive 2011/65/EU and REACH SVHC screening should be verified against the supplier’s safety data sheet and product compliance certificate.

    Published data for KF052A’s specific dart impact strength under ASTM D1709 Method A is limited; converters should measure the value on films below 50 μm rather than inferring from generic HDPE film data. Similarly, coefficient of friction and seal initiation temperature are additive-dependent and must be validated after converter-added slip or antiblock masterbatch.

    Handling Boundaries, Additive Compatibility, and Storage Conditions

    Storage of KF052A should follow standard HDPE practice: closed containers, clean hoppers, and no prolonged exposure to direct sunlight. Although HDPE does not require routine pre-drying, surface moisture may be introduced during cold-room storage or outdoor handling at relative humidity above 60%. If pinholes or bubble instability occur, a hopper dryer setting of 80°C for 2 h is typically applied before extrusion. Drying beyond 4 h at temperatures above 100°C risks pellet agglomeration and should be avoided.

    KF052A can be processed without special screw modification but is sensitive to melt temperature uniformity. Extruder purging with LLDPE before shutdown is recommended to prevent nozzle freeze-off. Regrind addition is generally limited to 20 wt% of the feed unless film properties are revalidated under ASTM D882; higher regrind fractions reduce bubble stability and increase variability in tensile elongation. Property loss is not linear above 20 wt%, and converters should establish a lot-specific regrind study rather than extrapolating from clean-pellet data.

    Incompatibility data for KF052A with specific additive masterbatches has not been published in full. Conventional slip and antiblock masterbatches based on erucamide and silica are used commercially with HDPE film grades, but excessive low-molecular-weight amides may contribute to die-lip build-up and plate-out over extended runs. Long-run production should include periodic die-lip cleaning; downtime frequency is determined by die lip deposit mass rather than by resin property alone.