| HS Code | 544716 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate | 5.0 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 28 MPa |
| Tensile Strength At Break | 20 MPa |
| Elongation At Break | 1000% |
| Flexural Modulus | 1100 MPa |
| Notched Izod Impact Strength | 50 J/m |
| Unnotched Izod Impact Strength | 1000 J/m |
| Shore D Hardness | 65 |
| Vicat Softening Point | 124°C |
| Heat Deflection Temperature | 70°C at 0.45 MPa |
| Melting Point | 130°C |
| Coefficient Of Linear Thermal Expansion | 1.2E-4 1/°C |
| Thermal Conductivity | 0.40 W/m·K |
| Electrical Resistivity | 1E16 ohm·cm |
| Dielectric Constant | 2.3 |
| Dielectric Strength | 20 kV/mm |
| Water Absorption | 0.01% |
As an accredited TPC (Japan) HDPE KF051A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KF051A is packaged in 25 kg PE-lined bags, 40 bags per pallet, totaling 1,000 kg. |
| Container Loading (20′ FCL) | 20′ FCL container loading: TPC (Japan) HDPE KF051A resin in 25 kg bags, palletized, shrink-wrapped, securely stowed for ocean export. |
| Shipping | TPC (Japan) HDPE KF051A is shipped as non-hazardous high-density polyethylene resin pellets, typically in 25 kg bags or 1000 kg jumbo bags, palletized and wrapped. Transport in clean, dry containers or trucks. Store away from moisture, heat, sunlight, and contamination. Not classified as dangerous goods. |
| Storage | Store TPC (Japan) HDPE KF051A in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, heat, and ignition sources. Keep original packaging sealed and palletized to prevent moisture, dust, and contamination. Avoid contact with oils, acids, alkalis, and strong oxidizers. Protect from UV and mechanical damage. Stack safely, rotate stock FIFO, and maintain clean handling conditions. |
| Shelf Life | TPC (Japan) HDPE KF051A typically has a 24-month shelf life when stored dry, cool, ventilated, and protected from sunlight and moisture. |
TPC (Japan) HDPE KF051A is converted into direct food-contact liner and bag stock as a 100 wt% virgin pellet feed, with food-contact-approved white masterbatch charged at 1.0–2.0 wt% and a slip/antiblock concentrate at 0.5–1.5 wt% to control blocking on wound rolls. The sector’s regulatory anchor is FDA 21 CFR 177.1520(c) for olefin polymers used in contact with food; parallel compliance under EU Regulation No 10/2011 requires overall migration below 10 mg/dm², and shipments into China fall under GB 4806.7-2023. Because food-contact clearance is lot-specific rather than universally conferred by resin grade, converters must obtain declarations for each batch. The film is produced on single-screw blown film equipment with a barrier screw at L/D 24:1–30:1, die gap 1.2–1.6 mm, melt temperature 190–220 °C, blow-up ratio 2.5:1–4.0:1, and frost-line height of 6–9 die diameters. At plant ambient relative humidity above 60%, surface condensation on pellets can create slit-seal micro-voids; hopper dryers set to 70–80 °C for 1–2 h are used where seal strength is release-critical. Zinc stearate or similar metal soap lubricants above 800 ppm are avoided because of die-lip plate-out and reduced seal consistency. Terminal outputs include bread bags, cereal liner pouches, frozen food bags, and produce roll bags.
Down-gauging of KF051A-based carrier film from 25 µm to 10–12 µm shifts failure mode from tensile yield to puncture and dart propagation, making ASTM D1709-22 Method A and ISO 7765-1:2017 the controlling release tests. The formulation uses 70–85 wt% KF051A with 15–30 wt% C4- or C6-LLDPE to restore dart drop energy and seal initiation; a higher-α-olefin copolymer may replace up to 5 wt% of the LLDPE when gauge falls below 12 µm. Additive loading is 1–2 wt% carbon black or white masterbatch and 0.5–1.0 wt% slip/antiblock. Lot release screening under ASTM D1238-20 at 190 °C and 2.16 kg is used to detect abnormal melt viscosity before the line runs. Extrusion is continuous high-stalk bubble geometry; if die gap is reduced below 0.8 mm at constant output, shear stress at the die lip can cross the critical melt fracture threshold and produce sharkskin on the outer film surface, while melt temperatures below 180 °C produce the same defect as frost-line height drops under 4 die diameters. The stable production window for this construction is melt temperature 190–225 °C, blow-up ratio 3:1–4.5:1, and frost-line height 6–8 die diameters. Scrap regrind can be re-introduced at up to 15 wt% without failing dart impact if it is dried to 0.05% moisture or lower. Terminal products are T-shirt bags, die-cut handle sacks, and produce roll bags used in high-speed dispensers.
| Parameter | Lower boundary | Upper boundary | Failure mode outside boundary |
|---|---|---|---|
| Die gap | 0.8 mm | 1.6 mm | Sharkskin and gauge variation |
| Melt temperature | 180 °C | 225 °C | Melt fracture below; oxidative gel above |
| Blow-up ratio | 2.5:1 | 4.5:1 | Bubble flutter above; low transverse orientation below |
| Frost-line height | 4 die diameters | 9 die diameters | Puncture loss below; stalk sag above |
Heavy-duty industrial sack conversion runs KF051A at 80–90 wt% with 10–20 wt% high-ESCR HDPE or C8-LLDPE, and 2.0–3.0 wt% carbon black masterbatch where ultraviolet exposure during outdoor storage is specified. The governing standards are ASTM D4976-12a for polyethylene materials, ISO 527-3:2018 for film tensile properties, and ASTM D1693-21 Condition B for environmental stress-cracking resistance of filled sacks. The blown film line uses a high-stalk bubble with film thickness 80–180 µm, gusseted tube formation, and in-line flexographic printing; bottom seams are formed by hot-air or impulse sealing. Extruder back pressure is maintained between 25–35 MPa, and the gusseted tube is collapsed at 2.5–3.0 times die diameter before winding. Terminal products are fertilizer sacks, pet food bags, resin shipping sacks, and liners for FIBCs. Published ESCR data for KF051A under aggressive lye-filled storage conditions is limited, so filled-drop performance must be confirmed on the converter’s own line.
High-output refuse sack lines operate with KF051A at 60–80 wt% and 20–40 wt% LLDPE or LDPE to raise dart impact and tear propagation resistance; carbon black masterbatch is charged at 2–4 wt% for opacity and cost dilution. Release criteria are EN 13592:2017 for refuse sacks, ASTM D1709-22 dart impact, and ASTM D1922-15 for Elmendorf tear. Blown film equipment with internal bubble cooling and capacitive thickness scanning maintains gauge variability below ±5% in the flatwidth; perforation blades are specified with 25–30 teeth per 100 mm and cut depth of 0.5–0.8 mm to permit easy strip separation without premature splitting. The film is post-gusseted and perforated in-line at high winder speeds, with back pressure controlled between 25–35 MPa and screen packs changed when pressure exceeds 40 MPa. Terminal products are household refuse sacks, institutional can liners, and industrial disposal bags.
| Downstream sector | Standard or regulation | Test method designation | Control value or condition |
|---|---|---|---|
| Food-contact liners | FDA 21 CFR 177.1520(c), EU No 10/2011, GB 4806.7-2023 | Overall migration | 10 mg/dm² |
| Retail carrier bags | ASTM D1709-22, ISO 7765-1:2017 | Dart impact F50 | Converter release specification |
| Heavy-duty sacks | ASTM D4976-12a, ISO 527-3:2018, ASTM D1693-21 | Tensile elongation, ESCR Condition B | Filled-drop and stack pass |
| Refuse sacks | EN 13592:2017, ASTM D1709-22, ASTM D1922-15 | Drop, impact, tear | No splitting at perforation |
| Coextruded barrier | FDA 21 CFR 175.105, EU No 10/2011 | Adhesive migration, overall migration | 10 mg/dm² |
| Powdered product packaging | REACH, UN 6.1.5 | SVHC screening, stacking flexibility | None detected above threshold |
In multi-layer barrier film, KF051A is used as a stiff cap or substructure layer at 20–40 wt% of total structure; tie resins are dosed at 10–15 wt% and barrier polymers such as EVOH or polyamide at 5–10 wt%. The relevant adhesives and food-contact plies must comply with FDA 21 CFR 175.105 and EU No 10/2011 when the laminate is intended for direct food use. The coextrusion line operates with die gap 1.2–2.0 mm, blow-up ratio 2.0:1–3.5:1, and separate melt channels to keep apparent shear viscosity mismatch below 30% at the die wall. The KF051A-containing cap layer is often corona treated to 40–44 mN/m before lamination; if EVOH is present, melt temperature must not exceed 230 °C to avoid degradation. Terminal products include dry-food laminate webs, medical device pouches, and flow-wrap films where stiffness and dead-fold are required.
Pouch film for powdered detergents and mineral-based formulations uses KF051A at 85–100 wt%, with 0–15 wt% LDPE added where lower seal initiation is required. Compliance is verified under ISO 527-3:2018 for tensile properties, ASTM D882-18 for thin-film tensile, and REACH SVHC screening; if the package is used for UN-certified dangerous goods, UN 6.1.5 flexibility and stacking tests may govern. The film is converted on blown film lines with film thickness 50–120 µm, melt temperature 190–220 °C, die gap 1.0–1.5 mm, and blow-up ratio 2.5:1–3.5:1. Seal initiation temperature is checked by heat-seal testing at 0.5 MPa and 0.5 s dwell; if seal initiation exceeds 125 °C, LDPE is increased within the stated range. Terminal products are detergent pouches, mineral filler sacks, and powdered chemical bags.
Competitive TPC (Japan) HDPE KF051A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KF051A is a pelletized high-density polyethylene extrusion resin intended for blown film conversion. The grade is supplied as a high-molecular-weight film resin in which melt strength, bubble stability, and thin-gauge stiffness govern downstream performance. Melt flow rate is measured under ISO 1133-1:2022 at 190 °C and 2.16 kg; density is measured under ISO 1183-1:2019. Published producer data for KF051A should be obtained from the TPC technical bulletin, because public documentation for this specific designation is limited. The resin is used in carrier bag film, produce bag film, and industrial liner stock where high-density polyethylene provides higher modulus and lower moisture transmission than linear low-density polyethylene under ASTM F1249-20. KF051A is not described as an injection molding grade or as a pipe extrusion grade.
On high-stalk blown film lines, KF051A is processed through a grooved-feed extruder with a barrel length of 25:1 to 30:1 L/D. Barrel temperature profiles typically run from 180 °C at the feed section to 220 °C at the adapter, with die zones maintained at 220 °C to 230 °C. Melt fracture initiates when shear stress at the die lip exceeds the critical shear stress of the high-molecular-weight fraction; this condition is more likely below 200 °C melt temperature or with a die gap below 0.8 mm. The die gap is generally held at 0.8 mm to 1.8 mm. A narrower gap raises shear rate and machine-direction orientation, increasing tensile yield but reducing tear resistance. Bubble stability depends on the relationship between blow-up ratio, frost line height, and stalk diameter. For high-density film resin of this class, blow-up ratios between 3.0 and 5.0 and frost line heights of 6 to 10 die diameters are common. Published data for KF051A in a specific die set is limited; startup trials should begin at the lower end of the melt-temperature range and raise output only after gauge variation is below ±5%.
Because film-grade KF051A has lower melt flow than high-flow injection grades, melt index alone is an insufficient indicator of processability. The relevant difference appears in elongational flow at the die exit, where high-molecular-weight polyethylene resists neck-in and stabilizes the stalk. Processors characterize tensile properties under ISO 527-3:2018 or ASTM D882-18. Dart impact is measured according to ASTM D1709-16a, and Elmendorf tear under ASTM D1922-15a. The test methods are gauge-specific; a 25 μm film cannot be compared directly with a 50 μm film because dart impact scales nonlinearly with thickness in high-density polyethylene. Melt-pressure monitoring at the screen changer is also used. A rise above 350 bar at constant screw speed indicates screen blockage or a cold melt, while a declining pressure at constant output suggests feed bridging in the grooved feed section.
Dart impact resistance in KF051A film is governed by film gauge, orientation balance, and molecular architecture. The free-falling dart method under ASTM D1709-16a reports the mass at which 50% of specimens fail; reported values therefore depend on film thickness, conditioning, and test temperature. Elmendorf tear measured under ASTM D1922-15a is anisotropic because HDPE film orientation follows stalk height and blow-up ratio. A low blow-up ratio and high frost line generally increase machine-direction orientation; machine-direction tear declines while machine-direction tensile modulus rises. Tensile yield and elongation are measured under ASTM D882-18 or ISO 527-3:2018. For a high-density film grade of this class at 50 μm gauge, tensile yield is commonly reported between 20 MPa and 30 MPa, but the KF051A-specific producer bulletin should be consulted for exact lot limits. Because high-molecular-weight HDPE retains orientation, processors sometimes blend with LLDPE to increase dart impact and tear while reducing stiffness.
Film properties also depend on crystalline orientation. HDPE film made with a high stalk process develops row-nucleated lamellar morphology. The extent of orientation is measurable by birefringence or by the ratio of machine-direction to transverse-direction tear. This ratio is not a standard specification for KF051A but is used in production laboratories to monitor bubble symmetry. A tear ratio above 3.0 often indicates excessive machine-direction orientation and predicts field failures in bag handles. Thermal behavior is characterized by differential scanning calorimetry under ISO 11357-3:2018. For high-density polyethylene film resins of this class, the crystallization peak commonly occurs near 117 °C, and the melting peak near 132 °C. The exact values for KF051A should be obtained from the producer certificate of analysis, because comonomer distribution and molecular weight affect lamellar thickness. Faster cooling from the melt creates thinner lamellae and lower crystallinity, reducing modulus and barrier while improving impact. In blown film cooling, frost line height therefore functions as a crystallinity control in addition to a bubble stability control.
Comparative polyethylene classes are summarized in the following matrix. The ranges are class-typical data and do not replace producer lot limits for KF051A.
| Resin class | Melt flow rate range (ISO 1133-1:2022) | Density range (ISO 1183-1:2019) | Primary film property test |
|---|---|---|---|
| HDPE film grade KF051A class | 0.3 g/10 min to 1.0 g/10 min | 0.958 g/cm³ to 0.964 g/cm³ | Dart impact ASTM D1709-16a |
| HDPE blow molding class | 0.2 g/10 min to 0.7 g/10 min | 0.954 g/cm³ to 0.962 g/cm³ | Drop impact ASTM D2463-15 |
| HDPE injection molding class | 4 g/10 min to 30 g/10 min | 0.952 g/cm³ to 0.965 g/cm³ | Flexural modulus ISO 178:2019 |
| LLDPE film class | 0.5 g/10 min to 2.0 g/10 min | 0.916 g/cm³ to 0.940 g/cm³ | Dart impact ASTM D1709-16a |
Substitution of LLDPE by KF051A in carrier bag film is evaluated when film stiffness, tensile yield, or moisture barrier must be increased without raising gauge. High-density polyethylene provides higher density and crystallinity than linear low-density polyethylene; tensile modulus rises while moisture vapor transmission declines. Moisture vapor transmission rate is measured under ASTM F1249-20, and oxygen transmission rate under ASTM D3985-24. The density difference is the primary driver: HDPE film grades at 0.958 g/cm³ to 0.964 g/cm³ yield higher crystallinity than LLDPE film grades at 0.916 g/cm³ to 0.940 g/cm³. The trade-off is lower dart impact and lower tear resistance. Published data for KF051A substitution ratios in specific carrier bag constructions is limited, but class-typical HDPE film shows lower Elmendorf tear than LLDPE at equal gauge. Low-temperature impact also decreases; freezer service below -20 °C may require blending with LLDPE to reduce film fracture during drop loading.
For food-contact applications, KF051A must be verified against the supplier’s current regulatory statement. High-density polyethylene olefin polymers intended for food contact are assessed under 21 CFR 177.1520 in the United States and Regulation (EU) No 10/2011 in the European Union. The EU regulation specifies an overall migration limit of 10 mg/dm² for plastic food-contact materials under Annex I. Compliance with Directive 2011/65/EU (RoHS) is assessed for lead, cadmium, mercury, hexavalent chromium, and selected phthalates. REACH obligations are defined under Regulation (EC) No 1907/2006. The matrix below identifies the principal instruments but does not replace producer certification.
| Regulatory instrument | Test or status | Application boundary |
|---|---|---|
| 21 CFR 177.1520 | Olefin polymer food-contact clearance | US food-contact film, subject to end-use conditions |
| Regulation (EU) No 10/2011 | Overall migration limit 10 mg/dm² | EU food-contact plastic material |
| Directive 2011/65/EU | RoHS restricted substance screening | Electrical/electronic packaging where applicable |
| Regulation (EC) No 1907/2006 | REACH SVHC and registration status | EU supply chain |
When KF051A is stored in cold environments or exposed to relative humidity above 60%, surface condensation can introduce moisture into the feed throat and cause die lines or bubble pinholes. Pre-drying at 80 °C for 1 h in a desiccant or hot-air hopper dryer is used only when surface moisture is present; HDPE does not require drying under normal dry storage. Melt temperature should remain below 240 °C during continuous runs to limit oxidative chain scission and gel formation. Prolonged residence time above 240 °C can shift molecular weight distribution and reduce bubble stability. Use of abrasive masterbatches or flame-retardant additives containing free halogens can increase die lip deposit and gauge bands unless the formulation is evaluated for compatibility. On coextrusion lines, KF051A is generally placed in the core or skin layers where its high modulus contributes to film stiffness; the tie-layer and sealant layers are selected from LLDPE or LDPE to preserve seal strength and dart impact.
Production-scale observation on high-stalk HMW-HDPE lines shows that bubble instability is frequently misdiagnosed as melt fracture when the actual cause is frost-line drift after cooling-air temperature changes. On a 150 mm die, a 2 °C shift in cooling air can move the frost line by more than 50 mm, altering gauge and tear balance. Operators should monitor bubble diameter, frost line height, and melt pressure simultaneously. The high melt strength of KF051A allows a tall stalk, but excessive stalk height increases machine-direction orientation and lowers Elmendorf tear. The operating boundary is therefore a balance between bubble stability and tear retention.
Oxidative degradation under processing conditions is evaluated by melt flow stability and gel count. A significant increase in melt flow after multiple extrusion passes indicates chain scission; a significant decrease indicates crosslinking or gel formation. For high-molecular-weight film grades, gel particles above 200 μm create film defects in 25 μm gauge. Screen packs of 40/60/80 mesh are used to remove agglomerates, but excessive back pressure can increase melt temperature and degrade the resin. Output on a 50 mm grooved-feed extruder running HDPE film of this class is typically limited by bubble cooling rather than screw capacity. Specific energy consumption is commonly in the range of 0.25 kWh/kg to 0.35 kWh/kg, depending on screw design and back pressure. In internal bubble cooling systems, higher output can be achieved before bubble instability, but the frost line must be controlled by infrared thermometer or ultrasonic gauge.
Compared with a high-flow HDPE injection molding grade, KF051A has lower melt index and higher melt strength, so it is unsuitable for thin-wall injection molds with long flow paths. Compared with a high-density blow molding grade, KF051A has melt rheology and additive package tuned for film surface quality and die lip deposit control rather than parison swell control. The die swell behavior of KF051A is therefore not specified for accumulation-head blow molding machinery. Published data for the additive package in KF051A is limited. If the resin is supplied as a natural film grade, anti-block and slip masterbatch may be required at the converter. The type and level should be determined by coefficient of friction testing under ISO 8295:1995 and blocking tests under ASTM D3354-15. Organoleptic testing under DIN 10955:2004 may be required for sensitive dairy or coffee packaging because food-contact clearance does not guarantee taste and odor neutrality.