Tpc Japan Hdpe Kf041a

TPC (Japan) HDPE KF041A

    • Product Name: TPC (Japan) HDPE KF041A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 993186
    Density 0.954 g/cm³
    Melt Flow Rate 0.40 g/10 min
    Tensile Strength At Yield 29.0 MPa
    Tensile Elongation At Break 500%
    Flexural Modulus 1.18 GPa
    Izod Impact Strength Notched 0.150 J/cm
    Shore D Hardness 65
    Vicat Softening Point 126 °C
    Heat Deflection Temperature 0 45 Mpa 72 °C
    Environmental Stress Crack Resistance >1000 h
    Brittleness Temperature < -70 °C
    Melting Point 130 °C
    Volume Resistivity >1E15 ohm·cm
    Dielectric Constant 2.3
    Dissipation Factor 0.0003

    As an accredited TPC (Japan) HDPE KF041A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KF041A is supplied in 25 kg paper sacks, 40 sacks per pallet, 1,000 kg net weight.
    Container Loading (20′ FCL) Container Loading (20′ FCL) for TPC (Japan) HDPE KF041A: 25 kg bags, 18–20 MT net, depending on palletization.
    Shipping TPC (Japan) HDPE KF041A is shipped as a non-hazardous HDPE resin, not classified as dangerous goods. Standard packaging includes 25 kg bags, jumbo bags, or bulk. Keep dry, cool, ventilated, away from sunlight/heat. Normal sea, road, and rail freight; no special UN number. Avoid moisture and contamination.
    Storage Store TPC (Japan) HDPE KF041A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags/containers closed, off the floor on pallets, and protect from moisture, dust, and physical damage. Avoid prolonged UV exposure. Maintain good housekeeping and follow local regulations. Ensure containers are labeled and inspect regularly for leaks or damage.
    Shelf Life TPC (Japan) HDPE KF041A shelf life is typically 24 months when stored in original packaging, protected from direct sunlight, heat, and moisture.
    Application of TPC (Japan) HDPE KF041A

    Blown Film Extrusion Through High-Stalk Bubble Geometry for Retail Carrier Film

    KF041A from TPC (Japan) is processed on high-stalk blown film lines equipped with grooved-feed extruders of 65–90 mm screw diameter and 24:1–30:1 L/D ratio, feeding a spiral mandrel die with a gap of 0.8–1.2 mm and a dual-lip air ring. The high-stalk geometry permits separate control of bubble diameter and frost line height; stalk heights of 250–400 mm and blow-up ratios of 3.5:1–4.5:1 are maintained for retail carrier film. The resin is not processed neat on most converting lines: 70–85 wt% KF041A is blended with 15–30 wt% C6 linear low-density polyethylene having a melt index of 0.5–1.0 g/10 min to raise dart impact and transverse direction tear, while 0.5–1.5 wt% antiblock masterbatch and 0.03–0.08 wt% slip masterbatch are added to control blocking and coefficient of friction. Melt temperature is held at 190–210°C at adapter and die; temperatures above 230°C produce oxidative molecular weight loss, increased odor, and occasional pinhole defects. Output rates of 0.8–1.4 kg/h per mm of die circumference are observed on lines with die diameters from 150–350 mm. Residual moisture above 0.03 wt% requires hopper drying at 80°C for 2 h; otherwise, die-lip oxidation specks and surface microgel defects appear. Compliance is verified under FDA 21 CFR 177.1520, EU Regulation 10/2011 Annex I, EU Regulation 1935/2004 Article 3, REACH SVHC screening, and CONEG heavy metal limits. Film tensile properties are tested under ISO 527-3:2018, Elmendorf tear under ISO 6383-2, dart impact under ASTM D1709-16A or ISO 7765-1, melt flow stability under ISO 1133-1:2022, and density under ISO 1183-1:2019. Terminal products include vest carrier bags, produce roll sacks, household refuse sacks, and retail roll bags.

    In T-die cast film lines used for lamination bases, KF041A is blended with 1.0–3.0 wt% masterbatch containing 10 wt% erucamide slip and 15 wt% synthetic silica antiblock, plus 0.05–0.10 wt% phosphite processing stabilizer and 0.05–0.10 wt% hindered phenolic antioxidant. The feed is conditioned to 0.02–0.03 wt% residual moisture; at relative humidity above 60%, edge trim scrap may carry surface moisture into the hopper and generate die-lip oxidation specks. Extruders with barrier screws and 28:1–32:1 L/D ratios feed coat-hanger dies of 1200–2400 mm width with die gaps of 0.4–0.8 mm; melt temperature is maintained at 230–250°C, air gap between die exit and chill roll is 15–30 mm, and the matte chill roll is held at 40–60°C. The molten web is pinned by air knife or electrostatic pinning to a matte chill roll with nip pressure of 2–4 N/mm. Line speed above 120 m/min without optimized chill roll finish produces transverse thickness variation of ±2–4% and increases blocking tendency. Compliance under EU Regulation 10/2011 and EC 2023/2006 GMP applies for lamination substrates intended to remain below overall migration limits; FDA 21 CFR 177.1520 applies to the polyolefin layer when used in finished food-contact structures. The cast film is converted into printed lamination substrates, industrial wrapping, release liner bases, and adhesive tape backings.

    Does rHDPE Loading Shift Melt Fracture Onset and Frost Line Height in Thin-Gauge Bubble Extrusion?

    Post-consumer recyclate loading in KF041A thin-gauge blown film alters melt pressure before the screen changer and shifts the onset of melt fracture. At 20–50 wt% rHDPE, the blend is processed through a recyclate extruder with 36:1 L/D ratio and a vent port maintained at 25–30 mbar vacuum, followed by continuous melt filtration through 60–100 mesh screen packs. The formulation consists of 50–80 wt% KF041A, 20–50 wt% washed rHDPE, 0.5–1.5 wt% fluoropolymer processing aid masterbatch, and 0.05–0.15 wt% antioxidant masterbatch. Melt temperature at the die is kept at 200–220°C because higher temperatures depress melt strength and cause bubble oscillation. Die gap is widened to 1.0–1.5 mm and blow-up ratio is limited to 2.5:1–3.5:1; frost line height is lowered by 50–100 mm relative to virgin film to maintain bubble contact with the stabilizing cage. Recyclate moisture above 0.1 wt% generates gel specks and pinholes, requiring vented extrusion or pre-drying at 80°C for 2–4 h. Melt pressure variance across the screen changer typically increases from 20–35 bar with virgin feed to 35–60 bar at 50 wt% recyclate; replacing screen packs at 8–12 h intervals prevents flow instability. Compliance is evaluated under EN 15342:2007 for recycled plastics characteristics, EU Packaging and Packaging Waste Directive 94/62/EC, REACH Annex XVII, and EU Regulation 10/2011 if the recyclate contains food-use fractions. The converted film is used for refuse sacks, construction film, temporary protective film, and agricultural mulch substrate.

    Three-layer coextruded dry food packaging structures using a KF041A core layer are run at die gaps of 1.0–1.4 mm and blow-up ratios of 2.5:1–3.5:1, with extruder sizes of 45/65/45 mm and melt temperatures of 190–210°C across all zones. The layer distribution is typically 15/70/15 or 20/60/20, where the outer skin is a low-density polyethylene sealant with melt index 1.0–2.0 g/10 min and the core is 60–70 wt% KF041A. Where an EVOH barrier is inserted, the structure becomes five-layer with maleic anhydride grafted tie layers at 10–15 μm; the KF041A layer is not in direct food contact in this configuration. Seal initiation temperature of the LDPE skin is 92–105°C, while the KF041A core retains stiffness at hot-fill temperatures up to 60–70°C. Compliance under EU Regulation 10/2011 Articles 3, 11, 12 and Annex II migration limits, FDA 21 CFR 177.1520(c) with extraction testing under 21 CFR 176.170(c) conditions of use, and EC 2023/2006 applies to the finished structure. Mechanical verification uses ISO 527-3:2018 for tensile properties, ISO 6383-2 for Elmendorf tear, ASTM D1709-16A for dart impact, and ISO 1133-1:2022 for layer melt flow stability. The structure is converted into cereal liners, biscuit pouches, dry soup sachets, and frozen food bags.

    When Machine Direction Orientation Is Applied to High-Density Polyethylene Web Stock

    Machine direction orientation of KF041A web stock requires a short-gap draw ratio between 4:1 and 8:1, preheat roll temperatures of 80–110°C, slow draw roll speeds of 20–40 m/min, fast draw roll speeds of 140–200 m/min, and annealing roll temperatures of 100–120°C. The feed web is cast or blown film with gauge variation below ±3%; above this limit, draw resonance and transverse tearing occur at draw ratios above 6:1. The formulation is 85–95 wt% KF041A and 5–15 wt% PE-based MDO modifier masterbatch, plus 0.05–0.15 wt% antioxidant masterbatch. Upstream melt temperature is held at 210–230°C, and the drawn web is annealed to control shrinkage below 5% at 70°C. Compliance is verified under ASTM D882-18 and ISO 527-3:2018 for tensile modulus and elongation at break, ASTM D1938-19 for trouser tear, and FDA 21 CFR 177.1520 or EU Regulation 10/2011 for food-contact applications. The oriented web is converted into label facestock, perforated pouches, bag-in-box inner liners, and stand-up pouch stiffening layers.

    Heavy-Duty Industrial Sack Film and the Role of KF041A in Load Retention

    Load retention in heavy-duty industrial sacks produced from KF041A is governed by dart impact resistance, creep deformation under sustained load, and transverse tear propagation resistance. The formulation blends 80–90 wt% KF041A with 10–20 wt% medium-density polyethylene or high-molecular-weight HDPE to increase strain hardening and reduce creep at filled bag stacking heights of 5–8 m. Blown film processing uses die gaps of 1.2–1.8 mm, blow-up ratios of 2.0:1–3.0:1, and melt temperatures of 200–220°C. Film gauge is held at 80–150 μm, and output on a 120 mm extruder with 30:1 L/D ratio reaches 200–350 kg/h. Compliance is evaluated under ISO 527-3:2018 for tensile properties, ISO 6383-2 for Elmendorf tear, ASTM D1709-16A for dart impact, and ASTM D2990-17 for tensile creep. The film is converted into valve sacks and open-mouth sacks for polymer pellets, construction mortars, mineral powders, and chemical granules.

    Free Quote

    Competitive TPC (Japan) HDPE KF041A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KF041A is a high-density polyethylene resin identified within the producer’s film-extrusion portfolio. The grade designation contains the melt-flow marker corresponding to a nominal melt flow rate of 0.4 g/10 min when measured at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. Its nominal density is 0.951 g/cm³ when measured by ISO 1183-1:2019, placing it in the medium-density region of high-density polyethylene film resins rather than in the lower-stiffness linear-low-density grades. The resin is intended for blown film extrusion, cast film extrusion, and thin-gauge packaging structures that require stiffness, moisture barrier, and melt strength during bubble formation.

    The material is supplied as free-flowing pellets. Because publicly available technical datasheets for the exact additive package and lot-specific molecular architecture of KF041A are limited, this document distinguishes between producer certificate-of-analysis values and general engineering windows for the density and melt-flow class. The certificate of analysis and safety data sheet remain the normative references for lot approval and specification acceptance.

    What Limits the Processing Window on High-Output Blown Film Lines?

    Processing of HDPE KF041A on high-output blown film equipment is governed by the interaction among melt temperature, die geometry, cooling-air temperature, frost line height, and haul-off speed. The recommended melt temperature envelope is 190–220 °C at the adapter, with die temperature maintained between 200 and 220 °C to avoid die-lip crystallisation while limiting oxidative degradation. A die gap of 1.2–1.8 mm is suitable for tubular film at blow-up ratios of 3.0:1–5.0:1. When the blow-up ratio exceeds 5.0:1, transverse-direction tear strength tends to decline sharply because of anisotropic orientation; below 2.5:1, dart impact may be reduced by machine-direction molecular alignment. Frost line height should be held at 6–10 die diameters to balance bubble stability and quench rate. Cooling air temperature is preferably 10–18 °C; higher temperatures can cause bubble sag and film blocking on the collapsing frame.

    Extruder selection should favour grooved-feed single-screw machines with L/D ratios of 25–30 and screw diameters from 50 to 70 mm for typical conversion lines. A barrier screw with compression ratio 2.5:1–3.5:1 provides sufficient melting without excessive shear heating. Melt pressure at the die should remain below 400 bar. Screen packs should be specified to avoid sharp pressure fluctuations because HDPE melt fracture can appear when wall shear stress exceeds 0.14–0.20 MPa. Melt temperatures below 185 °C may induce surface roughness known as sharkskin, particularly at high line speeds. Melt temperatures above 230 °C may cause gel formation, discolouration, and odour, especially if edge trim is recycled at levels above 15 wt%. The lower processing limit is therefore narrow; a melt-temperature fluctuation exceeding ±5 °C is often sufficient to shift the film from acceptable surface quality to visible defect.

    Where KF041A differs from high-load melt index HDPE blow molding grades becomes apparent in the shear-viscosity response and melt tension. Blow molding HDPE grades with melt flow rates of 0.20–0.35 g/10 min under ISO 1133-1:2022 can generate higher die swell and parison hang strength, but they commonly raise backpressure and reduce thin-gauge drawdown on film lines. The nominal 0.4 g/10 min melt flow of KF041A provides a more moderate viscosity-shear curve, reducing screw torque and allowing higher specific throughput. Compared with injection molding HDPE grades having melt flow rates above 5 g/10 min, KF041A retains sufficient zero-shear viscosity and melt strength for stable bubble formation. It is therefore not an injection molding resin; attempting to use it in injection molding would create short-shot risk at conventional injection pressures and part densities below nominal.

    Compared with metallocene LLDPE, KF041A has higher crystallinity and higher tensile modulus, but lower puncture resistance, lower dart impact, and lower tear propagation resistance in thin film. The stiffness-to-thickness ratio permits down-gauging in non-impact-critical industrial liners and flat-bottom bag structures. However, strength-critical applications requiring high dart impact should remain with LLDPE or HDPE/LLDPE blends. Haze values for HDPE film in this density class typically exceed 15 % under ASTM D1003:2021, so transparent packaging is not a primary target unless orientation and rapid quench are optimised. The heat-seal initiation temperature of HDPE is generally 120–135 °C compared with 90–105 °C for LLDPE; sealing jaws on form-fill-seal equipment must be set accordingly to maintain hermetic seals at commercial line speeds.

    Mechanical, Rheological and Barrier Property Matrix

    The engineering window in Table 1 is derived from high-density polyethylene film grades with nominal melt flow rates of 0.3–0.5 g/10 min and densities of 0.950–0.955 g/cm³. Lot-specific values for KF041A can shift with comonomer type, molecular weight distribution, additive package, and reactor configuration. These values are therefore provisional engineering data; product release values on the certificate of analysis are binding for specification acceptance.

    PropertyTest methodExpected engineering window
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:20220.3–0.5 g/10 min
    Density, 23 °CISO 1183-1:20190.950–0.955 g/cm³
    Tensile yield stress, 50 mm/minISO 527-3:201824–28 MPa
    Tensile strain at break, 50 mm/minISO 527-3:2018600–900 %
    Flexural modulus, 2 mm/minISO 178:20191000–1300 MPa
    Vicat softening temperature, A50ISO 306:2022123–128 °C
    Water vapour transmission rate, 25 µm film, 38 °C/90 % RHISO 15106-1:20193–5 g/(m²·24 h)

    The water vapour transmission rate in Table 1 is measured on oriented film at 25 µm thickness; thicker films reduce transmission approximately proportionally to thickness up to the point where crystallinity gradients at the surface begin to dominate. Flexural modulus is a key property for stiffness-limited downgauging, but it does not replace puncture or tear testing for packaging validation. Published data for the specific additive formulation of KF041A is limited, and any value used for finite-element simulation or barrier modelling should be confirmed with the producer’s technical service group.

    When KF041A Replaces Low-Density Polyethylene in Stiffness-Limited Structures

    Substituting KF041A for a conventional low-density polyethylene in stiffness-limited structures changes bubble geometry, cooling requirements, dart impact, and tear directionality. At equivalent film thickness, high-density polyethylene film of this density class generally provides a flexural modulus roughly 2–3 times that of LDPE. This allows a thickness reduction from 60 µm to 40 µm in some non-critical industrial liners without loss of bending stiffness. However, dart impact measured under ASTM D1709:2022 Method A typically decreases, and tear propagation measured by ISO 6383-2:2022 becomes more orientation-dependent. The processor should increase bubble stability by maintaining a frost line height of 6–10 die diameters and using dual-lip air rings with a chilled air supply below 15 °C.

    Backpressure on single-screw extruders may rise relative to LDPE at the same screw speed because of higher zero-shear viscosity. This rise can be offset by raising barrel zone temperatures from 180 °C to 210 °C while holding the adapter below 220 °C. If the line uses a barrier screw optimised for LDPE, replacement with a screw designed for polyolefins with higher melting point and higher shear-heating sensitivity is required. In addition, edge trim reincorporation above 15 wt% may lead to gel flecks and bubble instability because the recycled material has undergone multiple heat histories. The trim should be dried and blended at controlled ratios or excluded from films used in critical barrier layers.

    Regulatory compliance for TPC (Japan) HDPE KF041A should be confirmed against the specific food-contact and heavy-metal documentation supplied with the lot. HDPE film grades in this density range are typically formulated to comply with EU 10/2011, FDA 21 CFR 177.1520 for olefin polymers, and RoHS Directive 2011/65/EU when not pigmented with restricted substances. The producer’s statement of composition should be requested for REACH SVHC confirmation under Regulation (EC) No 1907/2006. For medical or pharmaceutical packaging, the additive package must be reviewed because slip agents such as erucamide and antiblocking agents such as silica migrate to the film surface. If migration into sensitive product is not acceptable, a non-additive reactor-grade alternative should be evaluated.

    RequirementReference designationTypical documentation position
    EU food contact plasticsEU 10/2011Subject to migration limits; producer statement required
    US FDA olefin polymers21 CFR 177.1520Compliance declared in producer letter for specified use conditions
    REACH SVHCEC 1907/2006Producer statement required; lot-specific confirmation recommended
    RoHS2011/65/EUApplies to unpigmented base resin; pigment and masterbatch must be assessed separately
    Pharmaceutical packaging extractablesUSP <661.1>Additional testing required for final container system

    KF041A should not be processed at melt temperatures above 250 °C, and contact with strong oxidisers, aromatic hydrocarbons, or chlorinated solvents at elevated temperatures may cause swelling, environmental stress cracking, or additive extraction. Drying is not required at ambient relative humidity below 60 %. If pellets have been stored in unheated silos in humid conditions, condensation on cold pellet surfaces can generate surface defects and should be addressed by pre-drying at 70–80 °C for 2–4 hours. The resin should be stored away from direct ultraviolet exposure and in a clean environment to prevent fines accumulation in conveying lines.

    Top