Tpc Japan Hdpe Keo51z

TPC (Japan) HDPE KEO51Z

    • Product Name: TPC (Japan) HDPE KEO51Z
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 802335
    Manufacturer TPC (Japan)
    Productname HDPE KEO51Z
    Polymertype High Density Polyethylene (HDPE)
    Density 0.951 g/cm³
    Meltflowrate 0.35 g/10 min
    Tensilestrengthatyield 24.0 MPa
    Tensileelongationatbreak 800 %
    Flexuralmodulus 1.10 GPa
    Izodnotchedimpact 0.300 J/cm
    Hardnessshored 60
    Vicatsofteningpoint 123 °C
    Deflectiontemperatureat0 46mpa 70 °C
    Meltingpoint 132 °C
    Moldshrinkage 0.015 cm/cm
    Environmentalstresscrackresistance 1000 hr
    Brittlenesstemperature -70 °C
    Processingmethod Blow Molding
    Typicalapplications Bottles, containers

    As an accredited TPC (Japan) HDPE KEO51Z factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KEO51Z is packaged in 25 kg multiwall paper bags, palletized, with 1,000 kg jumbo bags available.
    Container Loading (20′ FCL) TPC (Japan) HDPE KEO51Z loaded in 20′ FCL dry container: palletized 25kg bags, moisture-protected, uniformly stacked, and secured for export.
    Shipping TPC (Japan) HDPE KEO51Z is shipped as a non-hazardous polyethylene resin, usually in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers/trucks. Keep sealed, dry, away from direct sunlight and heat. No special dangerous-goods classification.
    Storage Store TPC (Japan) HDPE KEO51Z in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep original bags sealed and palletized; avoid excessive stacking. Protect from UV radiation, static buildup, physical damage, acids, alkalis, solvents, and strong oxidizers. Maintain clean, dust-free conditions and use first-in, first-out stock rotation to preserve resin quality.
    Shelf Life TPC (Japan) HDPE KEO51Z has a 12-month shelf life when stored in original packaging, cool, dry, and away from sunlight.
    Application of TPC (Japan) HDPE KEO51Z

    When TPC Japan HDPE KEO51Z is assigned to 220 L tight-head drum production, the accumulator head is operated with a diverging die gap from 2.0 mm to 4.0 mm, and the parison programmer is set to deliver an additional 8% wall stock at the bottom chime and shoulder pinch zones. The extruder is a grooved-barrel machine with a 90 mm screw, 30:1 L/D, and an accumulator volume of 12 L. Melt pressure ahead of the die is maintained at 28–35 MPa, with rear-to-die temperatures of 180 °C, 200 °C, 210 °C, 205 °C, and 200 °C. Mold temperature is held at 10–18 °C with closed-loop chiller control. Blow pressure is 0.6 MPa for the preblow and 0.8 MPa for final calibration. The parison is cut at 1.8 m length; excessive sag beyond 150 mm at the lower die face indicates the need for a 5 °C melt temperature reduction or a lower-MFR lot. Regrind from trimmed flash and rejected drums is metered at 30 wt% maximum; higher closed-loop regrind raises the gel count at the pinch-off weld and reduces top-load consistency. Storage at ambient humidity above 60% RH requires hopper drying at 80 °C for 2 h to prevent moisture-induced surface pitting at the die lip; otherwise, KEO51Z is processed as delivered. For UN 1H2 certification, the molded drum is subjected to a 1.2 m drop at 23 °C and after conditioning at −18 °C for 24 h, followed by a hydraulic leakproofness test at 30 kPa for 10 min. Top-load compression is measured at 80% of rated load with deformation below 10 mm. Environmental stress crack resistance is tested under ASTM D1693 Condition A; lot-to-lot failure time is charted to identify bimodal molecular weight drift before the drums enter hydrocarbon solvent service. Terminal parts include open-head and tight-head drums from 20 L to 220 L, inner bottles for composite intermediate bulk containers, and agricultural chemical containers requiring paraffinic solvent resistance.

    What Limits Regrind Loading in Milk Bottle Extrusion Blow Molding?

    In monolayer blow molding of 1 L and 2 L pasteurized milk bottles, the limit on closed-loop regrind is set by layer distribution shift and not by melt feeding. KEO51Z is run at 20–30 wt% regrind on wheel-type continuous extrusion blow molders with 80 mm to 120 mm grooved barrels and 25:1 L/D barrier screws. The melt temperature at the die is held below 210 °C to suppress off-taste precursors from oxidative chain scission. Where the lot density is 0.951 g/cm³ and the MFR is below 1.0 g/10 min, parison swell is controlled by a converging die gap of 1.8 mm to 2.5 mm and a die land length of 30 mm. Bottle wall thickness is specified at 0.6 mm to 0.9 mm; drop impact at 4 °C is evaluated after filling with water to 90% capacity. Food-contact compliance is anchored to FDA 21 CFR 177.1520 and EU No 10/2011, with overall migration tested in 50% ethanol and 3% acetic acid simulants at 40 °C for 10 days. Regrind above 30 wt% is not used in the milk contact layer because repeated heat history narrows the parison swell envelope and increases sidewall sink marks at the bottle heel. The terminal products are pasteurized fresh milk bottles, UHT milk bottles, and edible oil bottles with tamper-evident neck finishes.

    Application laneStandard or codeMeasurement conditionControl limit
    Milk bottle contact layerFDA 21 CFR 177.1520Total extractives in hexane at 66 °C for 2 hPass per listing extractive limits
    EU food-contactEU No 10/2011Overall migration in 50% ethanol and 3% acetic acid at 40 °C for 10 days< 10 mg/dm²
    Dangerous goods drum49 CFR 178.504Drop height 1.2 m at −18 °C after 24 h conditioningNo leak, no rupture
    Drum ESCRASTM D1693Condition A, 50 °C, 10% Igepal CO-630F50 recorded on lot certificate
    Geomembrane stress crackASTM D5397Notched constant tensile load at 50 °C in 10% IgepalFailure time recorded and trended

    In flat-die sheet extrusion of 1.5 mm to 3.0 mm HDPE geomembrane, KEO51Z is processed with a 120 mm single-screw extruder at 33:1 L/D, a screen pack of 60/80/120 mesh, and a 2000 mm coat-hanger die. The melt temperature is set between 200 °C and 220 °C, and the polished three-roll stack is operated at 60 °C to 80 °C; a lower roll temperature below 50 °C increases gloss but reduces interfacial bonding in textured surfaces. The sheet is embossed with a coextruded surface profile of 0.2 mm to 0.4 mm asperity height. Tensile properties are tested according to ASTM D638 at 50 mm/min; tear resistance is measured under ASTM D1004. Stress crack resistance for waste containment service is evaluated by ASTM D5397 notched constant tensile load at 50 °C in 10% Igepal. The terminal products are double-sided textured geomembrane liners for landfill cells, storage pond liners, and leak-detection underlayers in secondary containment.

    When KEO51Z Is Selected for Fluorine-Treated Household Chemical Bottles

    Inline fluorination of the outer surface is applied when the bottle must retain non-polar solvents such as mineral spirits, kerosene, or diesel adjuncts. In this service, the KEO51Z parison is blown at 0.55 MPa preblow and 0.75 MPa final blow; the fluorine treatment gas mixture is injected into the blowing air at 0.2% fluorine in nitrogen after the part is 90% formed. The reaction is terminated with an air purge before the mold opens to avoid workplace exposure above 1 ppm fluorine. Bottle weight is set at 34 g to 48 g for 1 L formats, with wall thickness distribution controlled to 0.5 mm minimum at the shoulder. Chemical compatibility is tested under ASTM D543 by immersion in the intended solvent for 30 days at 23 °C; weight gain above 3% triggers a switch to a fluorinated high-barrier structure rather than a monolayer. The process is restricted to non-oxidizing hydrocarbons; the addition of strong oxidizing acids or concentrated hydrogen peroxide to the package is outside the qualified envelope because of stress cracking at the pinch-off weld. Terminal containers include 500 mL to 2 L bottles for automotive fluids, charcoal lighter fluid, mineral spirits, and pesticide ready-to-use formulations.

    Accumulator Blow Molded Fuel Tank Shells Without Barrier Overmolding

    For a monolayer 60 L automotive fuel tank shell, KEO51Z is run on a 120 mm accumulator blow molder with 30:1 L/D screw and a parison-length controller integrated to the mold close speed. The parison is extruded at 200 °C to 215 °C with an annular die gap of 2.0 mm to 5.0 mm; parison weight is held within ±1.5% cycle-to-cycle because fuel tank wall thickness at the pinch points is defined at 3.5 mm minimum. After trimming, the shell is sulfonated on the inner wall to reduce hydrocarbon permeation below 0.5 g/m²/day at 40 °C. Low-temperature impact is measured by a 6 J dart strike at −40 °C on flat sections cut from the tank wall; no brittle break is accepted. The part is subjected to 50,000 pressure cycles from 0 kPa to 30 kPa at 60 °C to validate weld-line integrity. This route is limited to tanks smaller than 80 L; for larger or severe evaporative emission applications, a multilayer structure with EVOH barrier is required. Published data for KEO51Z in sulfonated monolayer tanks is limited; qualifying tests are therefore batch-specific. Terminal products are fuel tanks for compact passenger cars, all-terrain vehicles, and diesel auxiliary tanks.

    The Gas Counterpressure Window in Structural Foam Pallet Molding

    KEO51Z can be diverted to low-pressure structural foam injection molding of pallets and dunnage where its melt strength supports a 0.3% to 0.5% chemical blowing agent masterbatch. The material is plastified at 210 °C to 230 °C on a 150 mm reciprocating screw with 22:1 L/D; injection speed is reduced to prevent gas escape at the flow front. Mold cavity pressure is kept below 10 MPa to allow foam expansion and avoid splay. The molded density is controlled between 0.70 g/cm³ and 0.85 g/cm³. Top-load capacity is verified by ISO 8611-1 for pallet racking; impact toughness is tested at −20 °C under ASTM D3763. This route is suited to closed-loop recycling because the additive masterbatch and regrind are blended at 15 wt% regrind without measurable density drift. Terminal parts are three-runner and perimeter-base pallets, dunnage separators, and reusable distribution trays.

    Free Quote

    Competitive TPC (Japan) HDPE KEO51Z prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Product designation TPC (Japan) HDPE KEO51Z identifies a high-density polyethylene grade distributed for extrusion, sheet, and blow-molding operations in which melt strength, environmental stress crack resistance, and dimensional stability carry greater weight than high-flow rheology. The material belongs to the high-viscosity HDPE class; typical grades in this category generate melt flow rates below 1.0 g/10 min under ISO 1133-1:2022 at 190 °C with a 2.16 kg piston load, but the KEO51Z value must be read from the supplier certificate of analysis. Density under ISO 1183-1:2019 usually falls between 0.945 g/cm³ and 0.960 g/cm³, placing the product in the rigid-polyethylene segment rather than the flexible polyolefin segment. Published independently reproduced data for this specific configuration is limited; downstream engineers should treat generic HDPE class values as screening inputs rather than as a replacement for lot-specific data.

    What separates KEO51Z from lower-molecular-weight injection molding HDPE grades?

    The primary distinction is not density but molecular weight distribution and its influence on shear response. Injection molding HDPE grades routinely operate at melt flow rates above 15 g/10 min; they fill thin-wall tools rapidly but possess limited parison sag resistance. KEO51Z is positioned at the opposite end of the rheological spectrum. Its low-MFR architecture increases zero-shear viscosity and elongational viscosity, which improves hang strength in blow molding and melt stability in annular pipe dies, but it also raises screw torque and discharge pressure during plastication.

    Because molecular weight distribution is not fully described by MFR alone, processors should request the supplier’s shear-viscosity curve over the range 10 s⁻¹ to 1,000 s⁻¹. For high-molecular-weight HDPE, apparent shear viscosity at 190 °C and 100 s⁻¹ commonly falls between 800 Pa·s and 1,500 Pa·s, while zero-shear viscosity can exceed 100,000 Pa·s. KEO51Z-specific oscillatory shear data have not been published in open literature at the time of this writing.

    Production-scale extrusion lines configured for high-viscosity polyethylene are typically built around single-screw extruders with 30:1 to 36:1 L/D ratios, grooved feed bushings, and barrier screws with Maddock mixing sections. Barrel set points from feed to metering zone commonly range from 180 °C to 220 °C; die-head temperature should be held within ±5 °C to prevent melt-fracture onset at the low boundary and thermo-oxidative chain scission at the high boundary. If pellets or powder have been stored at relative humidity above 60 %, pre-drying at 80 °C for 2 h to 4 h is required to suppress surface splay and internal voids, even though HDPE does not require drying under normal indoor storage.

    During prolonged shutdowns, KEO51Z should be purged with a lower-viscosity polyethylene before the barrel cools below 160 °C; otherwise, oxidized heel material can adhere to screw roots and later release as black specks. Twin-screw compounding is generally unnecessary unless the converter is adding high loadings of carbon black, mineral filler, or flame retardant; for masterbatch let-down, a single-screw with dispersive mixing elements is adequate. Melt filtration with screen packs of 80 mesh to 120 mesh is used on industrial sheet lines to remove gels, but excessive back pressure from fine screens can exceed the thrust-bearing limit of 65 mm and larger extruders if the polymer is processed too cold.

    Rheological and mechanical property envelope for rigid extrusion applications

    Table 1 summarizes the reference property envelope for high-viscosity HDPE extrusion grades. The values are not product-specific release limits for KEO51Z unless the supplier confirms them in writing. They are included to provide a framework for incoming quality control and first-article qualification.

    Property Test method Typical high-viscosity HDPE range KEO51Z verification
    Melt flow rate ISO 1133-1:2022 0.2–1.0 g/10 min Supplier certificate of analysis
    Density ISO 1183-1:2019 0.945–0.960 g/cm³ Supplier certificate of analysis
    Tensile yield stress ISO 527-2:2012 22–30 MPa Supplier certificate of analysis
    Flexural modulus ISO 178:2019 900–1,400 MPa Supplier certificate of analysis
    Charpy notched impact, 23 °C ISO 179-1:2023 >4 kJ/m² Supplier certificate of analysis
    Vicat softening temperature, A50 ISO 306:2022 120–130 °C Supplier certificate of analysis

    Tensile yield stress measured under ISO 527-2:2012 on compression-molded sheet is a useful incoming resin check because it responds to density and short-chain branching. Flexural modulus, measured under ISO 178:2019 at 2 mm/min, usually tracks density; a shift of 0.005 g/cm³ can change modulus by 100 MPa to 200 MPa in this class. The notched Charpy impact energy under ISO 179-1:2023 at 23 °C is typically above 4 kJ/m² for high-molecular-weight HDPE, but values drop sharply below 0 °C if the comonomer content is low.

    When pipe extrusion line speed and wall-thickness control exceed conventional HDPE limits

    For thick-wall pipe and large-part blow molding, the controlling variable is often not melt flow rate but melt strength as observed through parison sag or annular die swell. If KEO51Z carries a broad molecular weight distribution, it should exhibit a shear-thinning index that permits stable pumping at high throughput while retaining enough elongational viscosity to resist drawdown. On a spiral mandrel die, high-molecular-weight HDPE usually runs with die-head pressures between 20 MPa and 40 MPa; large-diameter pipe dies may require melt pumps to decouple screw output from die pressure and to reduce pulsing.

    Wall-thickness control on production lines is managed gravimetrically rather than by screw speed alone. Weight-per-metre readings are compared with the theoretical mass calculated from outside diameter and wall thickness; for a 250 mm diameter pipe at density 0.950 g/cm³, a wall-thickness variation of ±0.5 mm can shift mass per metre by several hundred grams, depending on nominal wall thickness. Processors using KEO51Z should therefore monitor melt-pressure variation at the die entry; excursions beyond ±0.5 MPa may indicate gel accumulation, feed bridging, or inconsistent temperature control.

    Thermal degradation is a greater risk at the high-temperature boundary than at the low-temperature boundary. The practical melt-temperature window for stabilized HDPE is narrow; frequent excursions above 230 °C accelerate auto-oxidation, reduce oxidative induction time measured under ISO 11357-6:2018, and increase the yellowness index of the finished part. Outdoor pipe formulations should incorporate carbon black masterbatch at 2.0–2.5 wt% with primary particle size in the range 20–50 nm, and dispersion should be assessed under ISO 18553:2002; poor carbon black dispersion produces microvoids that reduce long-term hydrostatic strength. If the grade is intended for pressure pipe, long-term hydrostatic strength must be evaluated under ISO 9080:2022; published data for KEO51Z-specific pipe lifetimes are limited.

    Relative to medium-density polyethylene and linear low-density polyethylene, KEO51Z-class HDPE provides higher flexural modulus, greater crush strength, and lower water-vapour permeability, but lower slow-crack growth resistance than some MDPE grades used in gas distribution. Compared with high-flow HDPE injection molding grades, KEO51Z is unsuitable for thin-wall packaging molds requiring fill times below 1 s because its viscosity at high shear rates remains too high; published cycle-time data for this specific grade are limited. In coextrusion, it can serve as a cap layer or substrate layer where the adjacent layer is an adhesive tie resin and the barrier function is supplied by EVOH or polyamide.

    Requirement Applicable instrument Verification path
    Food-contact resin compliance, US FDA 21 CFR 177.1520 Supplier letter of compliance; finished-article extraction testing under intended conditions of use
    Food-contact plastics, EU Commission Regulation (EU) No 10/2011 Migration testing per EN 1186 series and overall migration limits
    RoHS restricted substances Directive 2011/65/EU including Commission Delegated Directive (EU) 2015/863 Supplier declaration; XRF screening and wet-chemical confirmation for Cd, Pb, Hg, Cr(VI), PBB, PBDE, DIBP, DBP, BBP, DEHP
    REACH SVHC REACH Candidate List under Article 33 Supplier declaration for substances above 0.1 wt%
    Packaging heavy metals Directive 94/62/EC Sum of Cd, Pb, Hg, Cr(VI) below 100 ppm

    Because compliance status is formulation-dependent, converters must not infer food-contact or outdoor-pipe certification from the resin class alone. A lot-specific letter of compliance should declare the substances of concern and the test methods applied. Where KEO51Z is converted into finished articles, the finished article remains responsible for meeting migration limits under EU Regulation (EC) No 1935/2004 and for demonstrating that the selected additive package does not exceed specific migration limits.

    Top