Tpc Japan Hdpe Ke041l

TPC (Japan) HDPE KE041L

    • Product Name: TPC (Japan) HDPE KE041L
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 314170
    Density 0.954 g/cm³
    Melt Flow Rate 0.4 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 24 MPa
    Elongation At Break ≥500%
    Flexural Modulus 1000 MPa
    Vicat Softening Point 124°C
    Heat Deflection Temperature 70°C at 0.45 MPa
    Shore D Hardness 60
    Notched Izod Impact Strength 200 J/m
    Environmental Stress Crack Resistance >1000 h
    Brittleness Temperature <-70°C
    Melting Point 130°C
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >1×10^16 Ω·cm
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2×10^-4 1/°C
    Specific Heat 1.9 J/g·°C
    Mold Shrinkage 2.0%

    As an accredited TPC (Japan) HDPE KE041L factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KE041L is packaged in 25 kg multi-wall paper bags, palletized for efficient transport and storage.
    Container Loading (20′ FCL) Container Loading (20′ FCL) for TPC (Japan) HDPE KE041L: 25kg bags, palletized, securely loaded, approx. 17–18 MT per container.
    Shipping TPC (Japan) HDPE KE041L is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg moisture-barrier bags, palletized and stretch-wrapped. Transport as general cargo, not regulated as dangerous goods. Store dry, away from heat and direct sunlight. Handle with standard warehouse practices.
    Storage Store TPC (Japan) HDPE KE041L in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, and ignition sources. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Palletize off the floor, avoid excessive stacking, and separate from strong oxidizers, acids, and solvents. Use clean handling equipment and follow local fire and safety regulations.
    Shelf Life Shelf life: two years if stored in original packaging in a cool, dry, well-ventilated area away from direct sunlight.
    Application of TPC (Japan) HDPE KE041L

    In monolayer food-contact extrusion blow molding with KE041L, the resin is processed at a melt temperature of 180–220 °C on a single-screw extruder with L/D 24:1–30:1 and a barrier screw equipped with a Maddock mixing section. Melt strength sufficient for 15 s parison hang time is verified through high-load melt flow rate under ISO 1133-1 at 21.6 kg; if the value drifts outside the supplier control range, the parison programmer must be adjusted to prevent diameter swell and sag. Compliance for the finished container is governed by EU Regulation (EU) No 10/2011 and its amendments, including the overall migration limit of 10 mg/dm², and by FDA 21 CFR §177.1520(c) for olefin polymers under the relevant conditions of use; the converter must also verify GB 4806.7-2016 when the container enters the China food-contact market. Formulation for this sector typically uses KE041L at 100 parts by weight with food-grade white masterbatch at 2–4 wt%; natural unpigmented formulations use 0 wt% color concentrate, while erucamide slip additive is either omitted or held below 0.1 wt% because migration can alter organoleptic properties of fatty foods. The parison is programmed with 20–50 wall-thickness control points, blow air pressure is maintained at 0.4–0.7 MPa, and mold temperature is controlled at 10–15 °C to balance surface gloss against residual stress. Production-scale failure modes observed on shuttle blow molders include top-load thinning above 5 L capacity when parison hang time exceeds 15 s and insufficient pinch-off compression at the flash line if clamp force is below 200 kN. Finished article types include 200 mL single-serve milk bottles, 1 L edible oil bottles, 3–5 L sauce or vinegar jugs, and dairy containers with tamper-evident neck finishes.

    When UN Certification for Dangerous Goods Packaging Demands Environmental Stress Crack Resistance

    UN certification for dangerous goods packaging imposes drop, leakproofness, hydraulic pressure, and stack test requirements under ADR/RID/IMDG Chapter 6.1 and the UN Model Regulations; a 20 L jerrican must carry the permanent UN stamp marking the packaging group and test year. For HDPE grades used in this sector, environmental stress crack resistance is measured under ASTM D1693-15, Condition B, using 10% Igepal CO-630 at 50 °C, with F50 values commonly specified above 100 h; notched Izod impact is evaluated under ASTM D256-10. The formulation sets KE041L at 100 parts by weight, allows up to 30 wt% clean in-house regrind only when the UN type approval certificate includes that exact regrind fraction, and uses 2–3 wt% carbon black or UV masterbatch for outdoor weather resistance; any increase of regrind above the approved ratio by more than 5 wt% requires re-testing. The downstream blow molding process uses an accumulator head machine with an extruder diameter of 80–120 mm and L/D 30:1, a parison programmer with 50–100 control points, mold temperature 8–15 °C, and post-cooling fixtures to prevent sidewall deflection; leak testing is run at 20–60 kPa internal air pressure. Repeated field failures occur at the pinch-off weld when the parison is too cool or when regrind contains degraded gel particles, which create stress concentrators that fail ESCR after stack loading. Terminal article types include 20 L and 25 L rectangular jerricans, 30 L and 60 L tight-head drums, and inner containers for combination packaging used with liquid agrochemicals and industrial detergents.

    Compliance matrix across downstream application segments
    SegmentStandard / methodClause / designationThreshold or test condition
    Food-contact blow moldingEU Regulation (EU) No 10/2011Overall migration10 mg/dm²
    Food-contact blow moldingFDA 21 CFR §177.1520(c)Olefin polymers for food contactConditions of use A–H as applicable
    Dangerous goods packagingASTM D1693-15ESCR Condition B, 10% Igepal CO-630F50 ≥ 100 h
    Dairy sheet / thermoformingEU Regulation (EU) No 10/2011Specific migrationComponent-specific SML
    Pharmaceutical containersUSP <661.1>Plastic packaging systemsPhysicochemical test panel
    Automotive reservoirsRoHS Directive 2011/65/EUAnnex II restricted substances0.1 wt% per homogeneous material for lead, mercury, hexavalent chromium, PBB, PBDE; 0.01 wt% cadmium

    When dairy cup and tray thermoforming uses blow-molding-grade HDPE such as KE041L, the sheet line must compensate for a melt flow rate below 1.0 g/10 min at 190 °C/2.16 kg, which produces higher shear heating than typical sheet grades and requires flat-die lip adjustments. Regulatory compliance for the final dairy article follows EU Regulation (EU) No 10/2011 with component-specific migration limits, and FDA 21 CFR §177.1520 for the polymer; if the sheet is used for medical packaging, USP <661.1> may also apply. The extrusion formulation is 100 parts by weight KE041L, 2–4 wt% food-grade white or cream masterbatch, up to 0.15 wt% nucleating agent for faster crystallization, and up to 30 wt% in-line skeletal regrind from the same thermoforming line where migration testing is unchanged. Sheet production uses a 75–120 mm single-screw extruder with L/D 28:1–32:1, a flat die with adjustable lip, and a polished three-roll stack at 70–90 °C to control sheet thickness 0.3–1.5 mm; thermoforming then runs at mold temperature 20–40 °C with plug assist for deep-draw yogurt cups. Published data for thermoforming of this specific blow-molding grade below 0.3 mm sheet thickness is limited; converter trials are needed because edge tear and roll-stack chatter can appear at line speeds above 40 m/min if melt temperature drops below 190 °C. Terminal products include 125–250 mL yogurt cups, dairy tubs, deli containers, and disposable food trays.

    Pharmaceutical and Personal Care Container Blow Molding Under Cleanroom Conditions

    In cleanroom blow molding of pharmaceutical and personal care containers, KE041L is converted at melt temperatures of 175–210 °C on 50–80 mm extruders with L/D 24:1–30:1; all parison inflation air is passed through HEPA filtration to prevent airborne contamination. The container material compliance framework includes USP <661.1> for plastic packaging systems, European Pharmacopoeia 3.1.3 for polyolefins, and FDA 21 CFR §177.1520 for food and drug contact; where liquids are ophthalmic, the converter must also verify extractables under ICH Q3D elemental impurity guidance. Formulation is maintained at 100 parts by weight KE041L with 1–3 wt% resin-matched color masterbatch that meets the same pharmacopoeial requirements; phthalates and BPA are excluded from the additive package, and no post-hoc lubricant is added because slip agent migration can alter the container’s extractable profile. The process uses a shuttle or long-stroke blow molder installed in an ISO Class 8 cleanroom, mold temperature 5–12 °C, clamp force sufficient to produce a compressed flash seal, and in-line leak testing at 20–50 kPa with camera vision inspection. A major production-scale bottleneck is the control of gel particles and black specks from residence-time degradation in the head channels; these become critical in clear or light-colored pharmaceutical bottles. Terminal article types include 50–500 mL oral liquid bottles with child-resistant closures, dropper bottles, ophthalmic wash bottles, and cosmetic cream jars.

    Automotive Washer Reservoirs: Why Cold Impact Resistance Limits Low-Temperature Use

    Automotive washer reservoirs manufactured from KE041L require a balance between parison stability in three-dimensional blow molding and impact resistance at -30 °C, which is typically evaluated by Charpy notched impact under ISO 179-1/1eA and by multi-axial puncture testing on production parts. The material must also satisfy RoHS Directive 2011/65/EU Annex II restrictions for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE, and the supplier must provide a REACH SVHC declaration for each batch. The formulation uses 100 parts by weight KE041L, 2.0–2.5 wt% carbon black masterbatch for UV resistance, 0.15–0.30 wt% hindered amine light stabilizer, and no external impact modifier because the base molecular weight supplies low-temperature ductility. Production equipment typically includes an accumulator head capable of parison manipulation for 3D blow molding, an extruder diameter of 80–120 mm, L/D 28:1–32:1, mold temperature 10–15 °C, and post-mold cooling jigs to control warpage; leak testing is performed at 30–50 kPa after welding of filler necks and pump ports. A known limitation is continuous exposure to hot ethylene glycol coolant at 120 °C exceeds the practical continuous-use temperature of HDPE, so this grade is not specified for pressurized engine-side degassing reservoirs. Terminal products include windshield washer reservoirs, headlamp washer fluid bottles, and coolant overflow reservoirs in low-pressure atmospheric configurations.

    Free Quote

    Competitive TPC (Japan) HDPE KE041L prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KE041L is encountered in Asia-Pacific extrusion blow moulding supply chains as a high-molecular-weight high-density polyethylene for large rigid containers, industrial bulk packaging, and fluid reservoirs. The grade is positioned between conventional single-reactor HDPE blow moulding resins and very high molecular weight HDPE used for automotive fuel tanks, with property control normally handled through the supplier certificate of analysis rather than a broadly harmonized public datasheet. Melt mass-flow rate according to ISO 1133-1:2022 and density according to ISO 1183-1:2019 are the primary incoming-quality checks. Because the published grade-specific data for this configuration is limited, acceptance limits should be obtained from the current supplier technical bulletin. Industrial classification places KE041L in the bimodal medium-to-high molecular weight family, where a higher molecular weight fraction is combined with a lower molecular weight fraction to maintain extrudability under the low shear rates encountered in accumulator-head parison formation.

    Typical usage includes extrusion blow moulding of containers in the 5 L to 1,000 L class, industrial jerry cans, agricultural chemical packaging, and automotive reservoirs. The main differentiating claim in this product class is an improved balance between stiffness, impact resistance, and environmental stress crack resistance relative to single-reactor unimodal HDPE of similar density. However, the actual balance depends on comonomer type, molecular weight distribution, regrind quality, and processing history. Incoming material should therefore be evaluated against mechanical and rheological control limits rather than relying on a single nominal datasheet value.

    What separates KE041L from single-reactor HDPE in stress-cracking service?

    Environmental stress crack resistance is the primary property that separates bimodal HMW-HDPE blow moulding grades from conventional unimodal HDPE. In this product class, the high molecular weight fraction contributes tie molecules that bridge adjacent crystalline lamellae. Under constant-strain exposure to non-ionic surfactants such as Igepal CO-630, crack initiation time increases when the weight-average molecular weight and tie-molecule population increase. Unimodal grades of similar density may have a narrower molecular weight distribution and fewer high-molecular-weight tie molecules, therefore the same surface stress in a moulded bottle can produce craze propagation at lower exposure times. The comparative test is normally ASTM D1693-15, Condition B, with notched specimens bent to a controlled radius and immersed in 10% Igepal CO-630 at 50 °C. Because F50 data are geometry-dependent, direct comparisons require identical specimen thickness, notch depth, and conditioning history.

    Rheologically, bimodal HMW-HDPE grades typically exhibit a higher shear-thinning ratio than unimodal resins. The high-load melt flow rate measured at 190 °C/21.6 kg is therefore used as an incoming consistency check for parison melt strength, while the low-load melt flow rate at 190 °C/2.16 kg may be used to detect contamination or degradation. However, no single shear-thinning ratio defines KE041L without supplier data. Quality-control laboratories should compare each lot against the supplier-certified value and against an internal reference resin that has been validated on the intended blow moulding machine. A deviation in high-load melt flow rate of more than ±10% from the reference can alter parison sag, pinch-off weld thickness, and container weight distribution.

    On accumulator-head extrusion blow moulding machines with extruder L/D of 24:1 to 30:1, the barrel temperature profile for HMW-HDPE of this type is normally set between 180 °C and 210 °C, while the die head is held in the 190 °C to 210 °C range. Head pressures in continuous extrusion can exceed 250 bar, and the melt temperature should not exceed 220 °C for extended residence times. Die swell is typically observed at 30% to 50% for high-molecular-weight blow moulding grades; however, actual parison swell depends on die gap, melt temperature, and shear history. Wall-thickness programming must be re-zeroed after each resin lot change because small shifts in viscosity and swell affect the radial thickness distribution in large containers. Batch-to-batch variation in melt flow rate of ±10% relative to the lot-certified value can be enough to alter pinch-off weld thickness on rectangular jerry cans.

    Field observations from large-container production lines indicate that insufficient melt strength causes parison drawdown on tools with a mould height exceeding 400 mm, while excessive melt strength can produce high orientation, uneven wall thickness at the flash line, and incomplete replication of handle features. Pinch-off weld integrity is influenced by resin temperature, mould closing speed, and contamination by low-viscosity polyolefins. On accumulator-head machines, a drop in head pressure during parison extrusion generally indicates a viscosity-reducing contaminant or excessive regrind. The acceptable regrind fraction depends on the container specification; typical internal rework loading is maintained at or below 20 wt% unless weld-line and drop-impact tests demonstrate otherwise.

    Moisture Uptake, Regrind Limits, and Food-Contact Compliance

    HDPE is not hygroscopic in the same manner as polyamide or PET, but surface moisture can create splay and pinholes in parisons if wet flake or cold regrind is introduced into the feed throat at ambient relative humidity above 60%. Pre-drying is generally not required for virgin material stored in sealed packaging; however, hopper dryers set to 70–80 °C for 1–2 h are applied when condensation is visible or when regrind has been stored in unheated external silos. Drying beyond 4 h at temperatures above 90 °C may accelerate additive migration and is not recommended without supplier confirmation.

    For food-contact use in the United States, compliance with 21 CFR 177.1520 is typically claimed by the resin supplier for the base olefin polymer, subject to end-use limitations and migration testing if the container is used with fatty or alcoholic foods. However, the resin itself is not the sole determinant of compliance; pigments, masterbatch carriers, and processing aids must also comply. Under EU practice, EU No 10/2011 governs overall migration, and supporting documentation is required for specific container geometries. For industrial chemical packaging, stress crack resistance under continuous contact with polar solvents or surfactants should be verified at the intended wall thickness, because laboratory ESCR data do not predict every packaged liquid formulation.

    In industrial packaging, contact with strong oxidizers, highly aromatic hydrocarbons, or aggressive chlorinated solvents can reduce service life even when the polymer is classified as chemically resistant. The container design must account for the wall thickness reduction caused by environmental stress cracking rather than assuming that the resin alone will protect the packaged product. If the packaged liquid has a net vapour pressure above atmospheric at storage temperature, the closure and neck strength, not the resin’s tensile yield stress, often determine the maximum safe stacking height.

    When cold-impact specifications fall below 0 °C, how should incoming testing be structured?

    Drop-impact tests on filled containers are not directly comparable to laboratory notched specimens. Containers for agricultural chemicals or industrial fluids may be conditioned at -5 °C or lower for 24 h and dropped from a specified height onto a concrete floor or steel plate. The relevant property is not only resin ductility but also pinch-off weld and handle weld design. Bimodal HMW-HDPE grades of this class generally retain ductile behavior below -20 °C in unnotched Charpy tests, but notched Charpy values fall with decreasing test temperature. Incoming material should be checked using ISO 179-1:2010 or ASTM D256 on notched specimens conditioned to the minimum service temperature, with acceptance limits derived from a reference container that has passed the filled-container drop test.

    Low-temperature impact testing should be accompanied by a visual inspection of the failure mode. Brittle fracture initiating at the flash line or pinch-off weld indicates a processing defect rather than a resin ductility limit. Ductile yielding in the container sidewall, with permanent deformation without fragmentation, generally indicates that the polymer remained above its brittle–ductile transition temperature. For containers with wall thickness below 0.8 mm, cooling rate differences between the mould wall and the inner surface can produce through-thickness crystallinity gradients that reduce impact performance even when the resin lot meets all specification limits.

    If the container is intended for cold-chain or outdoor northern-climate service, notched impact at -30 °C should be compared against a validated production reference. Because a single notched impact value does not fully describe the behavior of a moulded container, the drop height and fill weight should be fixed in the container specification and not altered after resin source changes. When published data for the specific grade are limited, the production facility should maintain an internal reference dataset from qualified containers.

    Table 1 lists a minimum incoming inspection matrix that can be applied when a grade-specific certificate of analysis is unavailable. It is not a replacement for the supplier datasheet.

    Table 1: Minimum incoming inspection matrix for HDPE KE041L class
    StandardPropertyInspection role
    ISO 1183-1:2019DensityDetects regrind contamination and grade substitution
    ISO 1133-1:2022Melt mass-flow rate at 190 °C/21.6 kgConfirms high-load rheology and parison melt strength
    ISO 527-2:2012Tensile yield stressConfirms stiffness baseline of moulded parts
    ISO 179-1:2010Charpy notched impactIndicates low-temperature container impact resistance
    ASTM D1693-15Environmental stress crack resistancePredicts surfactant and chemical stress cracking in service
    ASTM D648Deflection temperature under flexural loadAssists hot-fill and warehouse storage limits

    Relative to high-density film grades used in blown film, KE041L has a distinctly lower melt index and higher melt strength; it is not a film resin. The low-flow architecture increases extrusion head pressure and reduces throughput if processed on a film die, while the high molecular weight fraction resists the high shear conditions required in injection moulding. Compared with specialized very high molecular weight HDPE grades used for automotive fuel tanks, KE041L can be processed at lower head pressures and more predictable parison swell, but published data for the specific grade are limited, so the user should not transfer the processing window from another HMW-HDPE grade without rheological verification.

    Incoming resin lots should be compared with the supplier-certified density and melt flow rate and with the production facility’s internal reference lot. Where containers are subject to UN dangerous goods transport requirements, the moulded article must be certified by performance tests on the finished packaging, not by resin properties alone. The resin selection standard should therefore remain subordinate to the container performance specification, especially when wall thickness, closure, and stacking loads are the primary failure drivers.

    Top