Tpc Japan Hdpe Ke016a

TPC (Japan) HDPE KE016A

    • Product Name: TPC (Japan) HDPE KE016A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 295321
    Density 0.956 g/cm³
    Melt Flow Rate 0.16 g/10 min (190°C, 2.16 kg)
    Tensile Strength At Yield 28 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 600%
    Flexural Modulus 1200 MPa
    Izod Notched Impact Strength 0.20 J/cm
    Vicat Softening Point 124°C
    Brittleness Temperature -70°C
    Hardness Shore D 66
    Melting Point 134°C
    Environmental Stress Crack Resistance >1000 h
    Water Absorption <0.01%
    Thermal Conductivity 0.44 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Dielectric Constant 2.3
    Volume Resistivity >10^16 ohm·cm
    Mold Shrinkage 2-4%

    As an accredited TPC (Japan) HDPE KE016A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KE016A comes in 25 kg net paper bags, stacked on pallets and wrapped in stretch film.
    Container Loading (20′ FCL) TPC (Japan) HDPE KE016A loaded in a 20′ FCL container, 25 kg bags, palletized, shrink-wrapped, and secured for ocean freight.
    Shipping TPC (Japan) HDPE KE016A is a non-hazardous high-density polyethylene resin. It is not regulated for transport by DOT, IMDG, or IATA; no UN number, hazard class, or placard is required. Typically shipped in 25 kg bags, palletized and shrink-wrapped, keeping dry.
    Storage Store TPC (Japan) HDPE KE016A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, and ignition sources. Keep original bags or containers closed and palletized to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers and incompatible chemicals. Maintain stable ambient temperature, stack securely, and follow the manufacturer’s SDS and local regulations.
    Shelf Life TPC (Japan) HDPE KE016A typically has a 24-month shelf life when stored cool, dry, and in its unopened original packaging.
    Application of TPC (Japan) HDPE KE016A

    When TPC (Japan) HDPE KE016A is converted on an accumulator-head blow moulding machine at a nominal melt flow specification of 0.16 g/10 min at 190 °C/2.16 kg and density in the 0.950–0.956 g/cm³ range, the primary process variable is parison sag at shot weights above 8 kg. Large tight-head and open-top drums from 30 L to 220 L are produced with screw diameters of 80–120 mm and 24:1–30:1 L/D grooved-feed sections. Barrel set points run from 160 °C in the feed zone to 195 °C in the metering zone, while melt temperature is maintained at 190–205 °C. The die head is set at 195–205 °C and the die land ratio is kept at 15:1–20:1 to limit sharkskin at shear rates below 100 s⁻¹ while retaining die swell of 30–50%. For drums above 120 L, a parison programmer with 100-point axial wall control is required because gravitational sag thins the upper wall by more than 10% when shot weight exceeds 12 kg. Blow air pressure is typically 0.7–0.9 MPa, mould water temperature is 12–25 °C, and clamp force for a 200 L drum set is 3500–5000 kN. Cycle times range from 90 s to 180 s for wall thicknesses of 2.5–5.0 mm. Finished tight-head drums are type-tested under UN RTDG Chapter 6.1, including drop testing at -18 °C for liquid dangerous goods and internal hydraulic pressure retention. Food-contact drums may be specified under FDA 21 CFR 177.1520 for olefin polymers when the polymerisation stabiliser and antioxidant package meet extraction limits. The observed production failure modes are pinch-off weld thinning at the bottom seam, weight variation beyond ±3.0% caused by fluctuating regrind feed, and odour generation when melt temperature remains above 210 °C for extended residence time. Regrind stored at relative humidity above 60% may carry surface moisture above 0.05 wt%, producing pinholes unless the feed system is vented or pre-dried. Melt flow verification is performed to ISO 1133-1:2022.

    What Controls Interlayer Adhesion in Three-Layer HDPE/EVOH/HDPE Coextruded Containers?

    In a six-layer structure — outer HDPE, regrind, adhesive tie, EVOH, adhesive tie, inner HDPE — the layer distribution is regulated by independent gear pumps. Typical 5–20 L agrochemical jerrycan configurations use 3–6 wt% EVOH, 1–2 wt% tie resin on each side, and up to 35 wt% in-house regrind in the HDPE layers. Melt temperatures are maintained at 200–210 °C for the HDPE streams, 210–230 °C for EVOH, and 205–220 °C for the adhesive tie layer. The tie-layer processing window is the narrowest boundary; excursions above the upper limit by more than 5 °C cause gel formation and reduce peel adhesion below 1 N/15 mm when measured in a T-peel test under ISO 11339:2022. The HDPE extruders use 25:1–30:1 L/D screws and melt filtration at 200–250 µm to remove agglomerates that would create barrier defects. Die head temperature is controlled at 195–205 °C, and the blow-up ratio is restricted to 2.0:1–2.8:1 to maintain EVOH layer continuity. The finished containers are used for pesticide, solvent-based wood treatment, and UV-curable ink intermediates. Oxygen transmission below 0.5 cm³/(m²·day·MPa) at 23 °C/50% RH is achievable only if the EVOH layer remains continuous through the pinch-off and handle weld zones. The pinch-off is the main process conflict because folded EVOH thins by up to 50% near the bottom weld, lowering local barrier performance unless parison programming reduces wall thickness before the weld point. Dangerous goods packaging must also pass UN RTDG Chapter 6.1 and the relevant ADR/RID packing instruction. Published data for KE016A in this exact barrier structure is limited; qualification should include peel adhesion, barrier decay after drop impact, and 90-day storage at 40 °C with the target solvent system.

    Extruded Sheet Roll Temperatures and Deep-Draw Sag Boundaries

    Flat-die extrusion of 0.5–4.0 mm HDPE sheet is run on 90–120 mm single-screw machines with 30:1–35:1 L/D. Melt temperature at the die is kept at 200–220 °C, and the flex-lip die gap is set from 1.5 mm to 5.0 mm before the sheet enters a three-roll polishing stack at 75–95 °C for the upper and middle rolls and 65–85 °C for the lower roll. Sheet gauge variation above ±2.0% across the web is corrected only by flex-lip bolts; melt temperature changes are too slow for gauge control. Plug-assisted thermoforming heats the sheet surface to 165–185 °C with oven dwell of 30–90 s. Deep-draw parts with draw ratios up to 5:1 are formed in aluminium female moulds at 90–100 °C with plug temperatures at 110–130 °C. Sag is the critical process conflict: at sheet surface temperatures above 185 °C, the melt strength of this density class drops sufficiently to reduce corner wall thickness below 60% of nominal. Edge trim and skeletal scrap are closed-loop reground and reincorporated up to 35 wt%; above that level haze increases and pinholes appear during deep-draw because low-molecular-weight degradation products migrate to the sheet surface. Terminal products include industrial trays, dunnage, and inner liners. Food-contact forms are assessed under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, with overall migration below 10 mg/dm². Tensile yield is tested to ASTM D638-14 or ISO 527-2:2012; density and melt flow are verified under ISO 1183-1:2019 and ISO 1133-1:2022.

    In heavy-duty blown film conversion, the 0.16 g/10 min melt flow fraction is blended with 10–30 wt% LDPE or LLDPE to stabilise the bubble at blow-up ratios from 3.0:1 to 4.5:1. The die gap is set at 1.2–2.0 mm, die diameter between 250 mm and 400 mm, and frost-line height at 6–10 die diameters. Film gauge is controlled from 70 µm to 200 µm; below 70 µm on low-MI HDPE-rich formulations, bubble instability appears as gauge variation above ±5%. Heavy-duty industrial sacks, construction-site liners, temporary landfill covers, and agricultural silage films are the principal terminal products. Dart impact is tested under ASTM D1709-16a, tensile under ASTM D882-18 or ISO 527-3:2018, and Elmendorf tear under ASTM D1922-22. For direct food-contact sacks, EU Regulation (EU) No 10/2011 applies with specific migration limits for the antioxidant system; processing above 210 °C increases low-molecular-weight volatile species and may affect organoleptic performance. The low melt flow contributes high melt strength and high machine-direction tensile properties, but the narrow die gap raises head pressure to 25–35 MPa on 65 mm extruders. Screen packs above 100 µm are not recommended unless the die-clamp pressure limit is verified.

    When Heat Welding of HDPE Geomembrane Seams Must Satisfy Minimum Peel Strength

    Geomembrane sheet in the 1.5–3.0 mm thickness range is converted from HDPE with density of 0.948–0.956 g/cm³, melt flow between 0.12 g/10 min and 0.25 g/10 min, and carbon black content of 2.0–3.0 wt% for ultraviolet resistance. KE016A falls within this viscosity window, but published notched constant tensile load data for this specific grade in geomembrane service is limited; specification requires confirmation under ASTM D5397-12 before long-term design. The sheet is extruded at melt temperatures of 200–230 °C through a coat-hanger die, then embossed or textured on a roll stack at 70–90 °C. Seam welding is performed with hot-wedge equipment at 420–450 °C, wheel pressure of 0.5–0.8 MPa, and travel speed of 1.5–3.0 m/min. Destructive peel testing under ASTM D6392 should yield seam peel strength above 80% of the unsealed sheet yield strength, typically above 70 N/25 mm for a 2.0 mm sheet. Sheet tensile properties are measured to ASTM D6693-20, puncture resistance to ASTM D4833-07, and stress cracking to ASTM D5397-12. The main process boundary is oxidation: repeated weld fusing above 230 °C or air exposure longer than 30 s at the weld root depletes the antioxidant package. Oxidation induction time measured to ISO 11357-6:2018 may then fall below 20 min at 200 °C, which is not acceptable for exposed liner service beyond 10 years.

    Extruded high-tenacity strapping from this melt flow class is run on 45–65 mm vented single-screw extruders at melt temperatures of 200–220 °C. The extrudate enters a water quench bath at 30–40 °C followed by hot-air orientation at 100–130 °C. First-stage draw ratio is 4:1–7:1, second-stage draw ratio is 1.5:1–2.0:1, and total draw ratio is 8:1–12:1. Line speeds above 150 m/min require closed-loop tension control because draw resonance above ±0.5% speed variation creates thickness bands and reduced strap elongation. Terminal products include polyester-strapping substitutes, rope yarns, and binder twines for press-baled agricultural fibre. Tensile break stress is measured to ASTM D3950; for 12 mm × 0.6 mm strapping, break stress above 300 MPa is common. Processing above 12:1 total draw ratio leads to edge fibrillation, and die lips must be radiused to 0.2–0.5 mm to prevent slit-film splitting.

    Free Quote

    Competitive TPC (Japan) HDPE KE016A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KE016A is a high-density polyethylene extrusion blow moulding grade supplied as pellet stock. The resin is positioned for rigid packaging applications—detergent, cosmetic, personal-care, and small industrial fluid containers—where melt strength, stiffness, and resistance to environmental stress cracking must be balanced. Lot-specific melt flow rate is determined under ISO 1133-1:2022 at 190 °C under 2.16 kg or under ASTM D1238 Procedure A; the certificate of analysis from TPC Japan controls for density reported under ISO 1183-1:2019 or ASTM D1505-18. Published multi-lot property windows for KE016A are distributed through TPC Japan’s technical service and customer portal, and some public grade-specific data are limited; the ranges cited in this document are class-typical for low-flow HDPE blow moulding resins and are not a substitute for the CoA. The polymer is not formulated for film tensile draw or for high-melt-length injection moulding.

    What Limits Parison Stability in Low-Flow Blow Moulding Grades?

    Parison stability in KE016A processing is governed by two competing phenomena: extrudate swell and gravitational sag. Swell in blow moulding heads is determined mainly by die land length, die gap, draw-down ratio, and melt temperature. For low-flow HDPE with a melt flow rate below 0.8 g/10 min, free-hanging parison swell is often 20–45% when measured as the difference between parison diameter and die diameter. A land length to die gap ratio below 10:1 increases swell but makes parison weight hypersensitive to melt-temperature variation; a melt-temperature drift of ±3 °C at the die can shift parison length by 4–6% on a continuous shuttle machine. Sag is controlled by zero-shear viscosity, melt density, and parison length. Parison programming on shuttle machines alters die gap geometry during extrusion, but it cannot restore radial thickness uniformity after severe sag has occurred.

    On a 60 mm barrier screw extruder with L/D 26:1, throughput of 60–90 kg/h is typical for HDPE bottle output. Head pressures from the accumulator to the die commonly range between 25 MPa and 35 MPa, with melt temperature maintained between 180 °C and 195 °C at the die. Barrel set temperatures are often flat or reverse profile from 170 °C in Zone 1 to 180 °C in Zone 3, while the adapter and head are held at 185–195 °C to reduce melt fracture. Screw cooling is not usually required unless process temperatures exceed 205 °C; if a melt pump is present, the pump discharge pressure should maintain at least 5 MPa above die pressure to limit shot-weight variation.

    Pinch-off weld quality in extrusion blow moulding is a leading source of field failures not captured by sidewall tensile data. When the mold closes at clamp speeds below 0.8 m/s, melt fronts cool before intimate contact; above 1.2 m/s, flash lands can entrap air and create voids. A flash land angle of 30–45° and a pinch line depth of 0.2–0.5 mm are common starting values for HDPE bottles. Weld-line ESCR under ASTM D1693 or ISO 22088-3 can be 30–50% lower than that of the adjacent sidewall, so drop impact at 0 °C should be performed on bottles filled with 5% surfactant solution. Closed-loop chilled water at 7–10 °C through 8–10 mm channels in aluminum 7075 tooling removes heat more rapidly from the pinch area than from the sidewall, but can generate condensation when plant relative humidity exceeds 60%. For a 500 mL monolayer bottle with a nominal sidewall thickness of 1.2 mm, forced cooling times in the range of 8–14 s are typical; demolding surface temperature should be below 76 °C to avoid handle distortion. Blowing air pressure follows a two-stage profile: 0.5–0.7 MPa pre-blow to distribute the parison, then 0.8–1.0 MPa final calibration.

    Head-Pressure Control and Thermal Stabilization in Continuous Extrusion

    Head-pressure control is more sensitive for low-flow molecular-weight distributions than for high-MFR grades because the shear-thinning exponent is lower. Pressure transducers installed after the breaker plate and at the die land allow separation of screen-pack loading from die-gap changes. With a 60/80/100 mesh pack, initial differential pressure is commonly 2–4 MPa; an increase beyond 5 MPa over 200 h indicates screen fouling, color masterbatch residue, or degraded gel accumulation. Melt pumps are generally avoided in blow moulding because parison memory of pump pulsations can produce visible thickness bands; where used, the pump discharge pressure must hold a constant 5 MPa differential above die pressure. Thermal stabilizers in the base resin permit short-term operation near 200 °C, but residence time beyond 10 min at 205 °C increases gel formation and risk of odor at the container mouth. Shutdown purges should transition to a low-MFR, high-viscosity HDPE; a metallocene LLDPE purge can cause melt elasticity mismatch and long shot-weight recovery periods.

    Suggested process envelope for KE016A-type extrusion blow moulding
    ParameterTypical conditionRelevance
    Barrel Zone 1170–180 °Csolid conveying
    Barrel Zones 2–3180–190 °Cplastication
    Adapter/head185–195 °Cmelt temperature control
    Die melt195–205 °Cmaximum residence before gel risk
    Mold coolant7–12 °Ccycle time and condensation control
    Pre-blow pressure0.5–0.7 MPaparison expansion
    Final blow pressure0.8–1.0 MPawall conformity
    Regrind levelup to 30 wt%only after process validation

    Material selection between KE016A and adjacent HDPE blow moulding grades is driven by top-load stiffness, ESCR, and bottle drop profile. High-stiffness unimodal homopolymer grades may show 10–18% higher flexural modulus but fail earlier in surfactant ESCR tests, whereas high-ESCR copolymer grades may sacrifice 15–20% top-load strength. KE016A is positioned as a mid-stiffness grade for containers holding detergents, disinfectants, and personal-care formulations; its density remains above 0.94 g/cm³, which is the threshold for olefin polymers in some food-contact frameworks. The difference from high-MFR injection moulding HDPE is fundamental: injection grades with MFR above 10 g/10 min have insufficient melt strength for parison hang and produce insufficient die swell. The difference from bimodal film HDPE is also material: film grades are optimized for axial tear and dart impact at thicknesses below 0.1 mm, while KE016A-type blow moulding resins are optimized for 0.5–2.0 mm wall sections and closure thread geometry.

    Class-typical property windows for KE016A-type HDPE and adjacent blow moulding resin families
    PropertyTest standardKE016A class windowHigh-stiffness unimodal HDPEHigh-ESCR copolymer HDPE
    Melt flow rate, g/10 minISO 1133-1:20220.55–0.700.30–0.550.50–0.80
    Density, g/cm³ISO 1183-1:20190.955–0.9590.960–0.9650.948–0.953
    Tensile yield strength, MPaISO 527-226–3030–3422–26
    Flexural modulus, MPaISO 1781200–14001500–1800900–1100
    ESCR, hASTM D1693 Condition B>405–15>100
    Vicat softening point, °CISO 306 A50124–128127–131120–124

    These are class-typical ranges for a low-flow blow moulding HDPE of the KE016A type, not CoA values.

    When Mold Cooling Becomes the Cycle-Time Bottleneck

    Cycle time in extrusion blow moulding is often set by the cooling side, not by plastication. The heat removed from a 22 g HDPE bottle is approximately Q = m cp ΔT + m ΔHf. With a heat capacity of 2.2 kJ/(kg·K), a temperature drop from 190 °C to 40 °C, and an enthalpy of fusion of 190 kJ/kg, the total heat load is about 8.1 kJ. If the mold/chiller interface removes 1.0 kW, the theoretical minimum cooling time is 8.1 s; industrial cycle times are longer because of contact resistance, mold heat diffusion, and demolding temperature limits. Heat transfer across the polymer-mold interface controls cooling, so raising water flow above 0.03 kg/s per circuit does not linearly shorten cycle once channel Reynolds number exceeds 10,000. Separate circuits for the pinch-off and flash pockets at 5 °C can reduce weld-line annealing time by 15–20% but raise condensation risk above the plant dew point. Blow molds made from aluminum 7075 require hard-anodized cavity surfaces to avoid wear from flash and to maintain release at demolding surface temperatures below 76 °C. Cooling channel spacing should be no more than 2.5 times channel diameter to reduce wall-thickness variation from uneven crystallization.

    Regulatory compliance for KE016A must be evaluated at the finished article level; bulk resin declarations do not cover colorants, processing aids, or recycled content. In the European Union, plastic materials and articles intended for food contact are regulated under Regulation (EU) No 10/2011; HDPE produced from authorized monomers and additives may require migration testing under final article migration conditions. In the United States, olefin polymers may be covered by 21 CFR 177.1520(c) if density, extractables, and end use meet specified conditions. For pharmaceutical packaging, current USP <661.1> or ICH Q3D risk assessment may apply for plastic packaging systems. The supplier’s REACH and RoHS declarations typically confirm absence of intentionally added lead, mercury, hexavalent chromium, cadmium, and polybrominated biphenyls above regulatory thresholds; however, upstream catalysts and process aids should be documented. No specific food-contact approval should be assumed for regrind except when the converter validates that the proportion and source of regrind do not alter migration.

    On a single-station shuttle machine producing 1 L detergent bottles with a 25–27 g shot weight, a typical validation protocol for KE016A monitors shot-to-shot mass standard deviation below 0.15 g, sidewall thickness distribution within ±0.15 mm, and closure torque at 1.5 N·m to ensure the finish does not crack. Drop impact is measured at -18 °C after 24 h conditioning; bottles filled with 5% nonionic surfactant solution are dropped from 1.0 m onto concrete. Storage in 10% sodium hydroxide solution at 40 °C for 14 days stresses the pinch-off weld; if cracks appear, the corrective action is usually to reduce clamp speed at pinch contact below 0.8 m/s, lower flash land angle to 30°, or increase weld-line cooling. The grade is also run on continuous rotary blow moulding machines, but parison programmer parameters and head tooling pressure settings differ from shuttle machines. Published data for KE016A on specific rotary wheel configurations is limited; converters typically run on-site trials with TPC Japan technical service.

    Top