| HS Code | 990372 |
| Density | 0.960 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.05 g/10 min |
| Tensile Strength At Yield | 28 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 500% |
| Flexural Modulus | 1200 MPa |
| Charpy Notched Impact Strength | 10 kJ/m² |
| Shore D Hardness | 66 |
| Vicat Softening Temperature | 125°C |
| Melting Temperature | 132°C |
| Brittleness Temperature | -70°C |
| Environmental Stress Crack Resistance | >1000 h |
| Water Absorption | 0.01% |
| Volume Resistivity | 1E16 ohm·cm |
| Dielectric Constant | 2.3 |
| Dielectric Strength | 20 kV/mm |
| Coefficient Of Linear Thermal Expansion | 1.2E-4 /°C |
| Thermal Conductivity | 0.44 W/m·K |
| Specific Heat Capacity | 1.9 kJ/kg·K |
As an accredited TPC (Japan) HDPE KC980A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KC980A comes in 25 kg polyethylene-lined woven bags, palletized at 40 bags (1,000 kg) per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loading for TPC (Japan) HDPE KC980A: 25kg bags, palletized, shrink-wrapped, and safely secured for ocean export. |
| Shipping | TPC (Japan) HDPE KC980A is a non-hazardous high-density polyethylene resin. It is shipped in 25 kg bags or 1000 kg jumbo bags, palletized and stretch-wrapped, in clean, dry containers or trucks. Store away from moisture, direct sunlight, and heat. No special dangerous-goods requirements apply. |
| Storage | Store TPC (Japan) HDPE KC980A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging sealed to prevent moisture, dust, and contamination. Use pallets, avoid excessive stacking, and follow FIFO stock rotation. Maintain stable temperatures and avoid prolonged UV exposure. Ground handling equipment to control static. Ensure good ventilation and no ignition sources. |
| Shelf Life | Shelf life is about 24 months when stored cool, dry, ventilated, away from direct sunlight, moisture, and contamination. |
Extrusion blow molding of 200 L tight-head chemical drums from HDPE KC980A is predicated on a parison mass exceeding 8.5 kg and a melt strength sufficient to prevent sag-induced wall thinning before mold closure. The accumulator head is paired with a grooved-feed extruder having an L/D ratio between 24:1 and 30:1; barrel temperature settings from feed throat to metering zone typically span 180°C to 210°C, while the die head is held at 190°C to 210°C to avoid surface melt fracture at the die lips. Clean regrind from trimmed pinch-off material can be re-introduced at 5 wt% to 10 wt% without compromising UN 1H1 drop performance; higher regrind ratios require full ESCR and impact revalidation because residual stabilizer concentration and melt strength can shift. Parison programming applies a wall-thickness profile of 2.5 mm to 4.0 mm across the cylindrical body, increasing to 4.0 mm to 6.0 mm around the closure boss and top chime. Blow air at 0.65 MPa to 0.80 MPa expands the parison against a mold chilled to 10°C to 25°C, with a total cycle time of 150 s to 240 s on single-head rotary shuttle machines. After trimming, each lot is subjected to UN 1H1 hazardous chemical packaging tests, including the 1.2 m drop at -18°C for Packing Group II liquids; environmental stress crack resistance is evaluated on compression-molded plaques under ASTM D1693 Condition B, with industrial drum grades commonly positioned at an F50 value above 100 h. Density and melt flow rate are controlled under ISO 1183-1 and ISO 1133-1:2022, respectively, and monomer/additive compliance is documented under REACH (EC) No 1907/2006 and EU 10/2011 where food contact is specified. The finished drum is used for industrial lubricant, solvent, and solid chemical packaging requiring UN certification and high stack-load performance. Published data for this specific configuration is limited; pre-production trials on the target line are required to correlate mold cooling geometry with wall-thickness distribution.
In 20 L to 30 L open-head pail tooling, the dominant failure mode is localized thinning at the top bead and handle undercut, not mid-body sag. The die gap must therefore be increased to 2.0 to 2.5 times the nominal body wall thickness at the handle station; with KC980A at a body wall of 1.5 mm to 2.0 mm, the corresponding undercut gap reaches 3.0 mm to 5.0 mm. Mold water is controlled at 8°C to 15°C to stabilize the bead, and blow-air pressure is held at 0.50 MPa to 0.70 MPa. Clean post-industrial regrind from the same pail line may be introduced at 10 wt% to 20 wt%; beyond this range, some lines observe a measurable decrease in ASTM D1693 Condition B F50 and an increase in handle-weld splits during drop tests. Moisture on regrind is removed if ambient relative humidity exceeds 60%, using a hot-air hopper dryer set at 80°C for 2 h to 4 h. Finished pails are commonly used for paints, greases, water-based emulsions, and fine powders; lids and gaskets are tested separately for closure integrity under ISO 16101 or an equivalent transport standard. The process window for the parison programmer is narrow; a deviation of 5°C in the die head can change parison length enough to increase scrap rate by 2% to 5% on high-speed single-station machines.
Agricultural chemical container production shifts from simple monolayer shell construction to a six-layer coextruded structure when the packaged liquid contains emulsifiable concentrates, aromatic solvents, or ester-based penetrants that reduce HDPE environmental stress crack resistance. HDPE KC980A is used as the outer virgin layer, inner virgin layer, and regrind core in a sequence with tie resins and an ethylene-vinyl alcohol copolymer barrier layer. The table below lists a typical layer distribution used in high-barrier agrochemical containers from 1 L to 20 L.
| Layer sequence | Function | Mass distribution | Governing standard or control method |
|---|---|---|---|
| Outer virgin HDPE | Shell strength, surface finish, UV protection | 15–20% | ISO 527-2 tensile yield |
| Regrind HDPE | Structural core, scrap reuse | 35–45% | Internal filtration 0.5–1.0 mm |
| Tie adhesive | Adhesion to EVOH | 2–3% | ASTM F904-16 bond strength |
| EVOH | Solvent barrier | 1.5–3.0% | ASTM D3985 oxygen transmission |
| Tie adhesive | Adhesion to regrind | 2–3% | ASTM F904-16 bond strength |
| Inner virgin HDPE | Product contact | 20–25% | FDA 21 CFR 177.1520, EU 10/2011 |
Extrusion is performed on a coextrusion blow molding line with six extruders feeding a multi-manifold die. The die temperature must be kept within ±5°C of the set point because EVOH is thermally sensitive and small temperature variations alter its viscosity relative to the HDPE layers, producing layer-thickness nonuniformity. Regrind containing EVOH must be dried to 0.1% moisture or lower; if ambient relative humidity exceeds 60%, a vacuum dryer with a dew point of -30°C is required because EVOH regrind absorbs atmospheric moisture and can generate voids. The terminal bottles are subjected to ESCR testing under ASTM D1693 Condition B, drop testing under UN 1H1, and barrier testing by ASTM D3985 for oxygen transmission. Aromatic hydrocarbon and ketone-containing formulations may require fluorination of the inner surface; published data for this specific configuration is limited, so fluorination exposure time and gas concentration must be validated on the actual bottle geometry.
For a 1,000 L intermediate bulk container inner bottle, the extrusion blow molding operation deals with a shot mass between 60 kg and 70 kg and a parison length greater than 1.5 m. The accumulator head must be sized for a shot capacity no less than 1.2 times the maximum shot mass to maintain consistent parison ejection; die-gap profiling across 50 to 100 circumferential points is used to hold wall thickness from 4.0 mm to 6.5 mm at the bottom corner and top neck. The product-contact layer is 100% virgin HDPE KC980A; regrind, if used, is confined to a middle structural layer. Cooling water at 8°C to 12°C is directed through beryllium-copper pinch-off inserts, which must remain engaged until the weld line reaches 20°C to 30°C below the resin’s Vicat softening point; premature clamp release produces pinch-line splits under the UN 31H1 composite IBC drop test from 1.2 m. The finished bottle is fitted into a steel cage, and the composite unit is tested under UN 31H1 for drop, stack load, and leakproofness. Oxidizing or aggressive liquids may require surface fluorination of the inner HDPE layer; published data for this specific configuration is limited, and production-scale fluorination trials must correlate fluorine concentration with permeation reduction for the target liquid class. The terminal application is bulk liquid and solid chemical transport in reusable or single-trip composite IBCs, including food ingredient handling where the inner layer meets EU 10/2011 or FDA 21 CFR 177.1520.
Fuel tank manufacturing is a restrictive downstream segment for HDPE KC980A; no OEM approval should be inferred from base resin specification alone. Six-layer coextrusion blow molding lines use a horizontally fed accumulator die or oscillating die to create a wall structure consisting of outer virgin HDPE, regrind core, two tie layers, EVOH barrier, and inner virgin HDPE. The regrind core may reach 35% to 45% of the wall because trimmed tank flashing contains all previously coextruded layers; the EVOH layer is maintained at 1.5% to 3.0% of the total wall thickness, and each tie layer typically occupies 1.0% to 2.0%. Die temperature must be held within ±5°C of the target to prevent viscosity mismatch between the EVOH and HDPE streams; viscosity mismatch across the die manifests as layer thickness variation in the pinch-line region, which is the primary weld location for tank failure. Blow air at 0.60 MPa to 0.80 MPa expands the parison against an aluminum mold cooled to 10°C to 20°C, and the tank is trimmed, welded with filler neck and sender flange, and leak-tested under internal pressure. Evaporative emission compliance is validated according to regional standards such as US CARB EVAP regulations and UN ECE R34; long-term permeation is a function of EVOH layer continuity and tank wall thickness. KC980A is not formulated as a conductive HDPE; therefore, if electrostatic dissipation is required for the tank shell or filler neck, a separate conductive carbon-black filled layer or external grounding path must be incorporated. Terminal products include 50 L to 90 L spark-ignition engine fuel tanks for passenger cars and light trucks, although vehicle-specific approval and validation on the OEM’s line are mandatory.
Because marine float shells are subject to impact loads at sub-zero temperatures, blow molding conditions for KC980A are biased toward high dart impact strength at the expense of surface gloss. Cylindrical and spherical floats with diameters from 0.5 m to 1.2 m are blown with wall thicknesses of 5 mm to 10 mm on large accumulator machines; blow-air pressures of 0.70 MPa to 0.90 MPa and mold temperatures of 5°C to 15°C are used to stabilize the pinch-off weld. The finished float shell is tested under ISO 6603-2 multiaxial impact at -20°C, with weld-line failure treated as a reject criterion. UV stabilization is introduced via hindered amine light stabilizer and carbon black masterbatch at the feed throat at a let-down ratio specified by the masterbatch producer; incorrect dosing leads to visible surface chalking within 12 months of outdoor service. Terminal applications include dredging pipeline floats, aquaculture buoyancy units, and cable marker shells; continuous submerged service is not recommended without a hydrostatic integrity test at 2.0 bar to 3.0 bar internal air pressure after molding.
Strongly oxidizing acids above 40°C, aromatic hydrocarbons, and ketone solvents place HDPE KC980A outside its recommended service envelope without a validated permeation and chemical resistance program. Oxidizing acids attack the polyethylene chain at elevated temperature, while aromatics and ketones can swell the matrix and reduce ASTM D1693 Condition B F50 below the release criterion in less than 100 h. Long-term outdoor exposure requires a UV stabilization package; unstabilized KC980A should not be used for multi-year sunlight storage. No post-molding crosslinking or compatibilization is assumed for this grade; if impact modification or conductive performance is required, those properties must be achieved by blending with a qualifying masterbatch under the producer’s guidance and validated on the target blow molding line. This restriction applies to all downstream segments above; packaged liquid classes outside the original application envelope require full permeation testing under ASTM D2684 or equivalent.
Competitive TPC (Japan) HDPE KC980A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KC980A is a high-density polyethylene injection-moulding grade distributed for rigid packaging and industrial logistics applications. The KC980A designation identifies a controlled melt-mass-flow range and a density window that place the material between low-flow blow-moulding high-density polyethylene and very high-flow thin-wall packaging resins. Users should obtain the manufacturer’s certificate of analysis for batch-specific values because published distributor data may be normalised rather than absolute. The following tables and processing thresholds are derived from standardised testing methods and, where distributor-specific data are incomplete, from equivalent medium-flow HDPE copolymer grades with the same nominal design envelope.
The resin is produced by low-pressure catalytic polymerisation of ethylene with a minor α-olefin comonomer, typically 1-butene or 1-hexene. The comonomer insertion reduces lamellar thickness and crystallinity; the resulting density is therefore below 0.960 g/cm³, whereas a homopolymer HDPE grade commonly exceeds 0.960 g/cm³ when measured by ISO 1183-1:2019. Published data for this specific configuration are limited, but the density window of 0.952–0.958 g/cm³ is characteristic of a copolymer HDPE with sufficient crystallinity for load-bearing service and enough chain branching for crack resistance.
The molecular weight distribution is moderate to narrow. A narrow distribution improves warpage consistency in injection moulding and reduces the tendency to shear-burn at gate velocities above 150 mm/s. The melt-mass-flow rate, measured at 190 °C under 2.16 kg per ISO 1133-1:2022, is reported in the range 8.0–10.0 g/10 min. That range places KC980A in the medium-flow injection-moulding class rather than the high-flow class of 20–60 g/10 min used for disposable thin-wall containers.
The high-load melt-flow index at 21.6 kg is a shear-thinning indicator. For KC980A, the ratio of 21.6 kg melt-flow index to 2.16 kg melt-flow index typically falls between 15:1 and 25:1. This ratio is used to anticipate filling behaviour in long, thin rib sections and to compare batch-to-batch lot consistency on a production line.
| Property | Test method | Reported window |
|---|---|---|
| Melt mass-flow rate, 190 °C/2.16 kg | ISO 1133-1:2022 / ASTM D1238 | 8.0–10.0 g/10 min |
| Density | ISO 1183-1:2019 / ASTM D1505 | 0.952–0.958 g/cm³ |
| Tensile yield stress | ISO 527-2:2012 / ASTM D638 | 24–28 MPa |
| Tensile elongation at break | ISO 527-2:2012 / ASTM D638 | > 300 % |
| Flexural modulus | ISO 178:2019 / ASTM D790 | 900–1050 MPa |
| Izod notched impact, 23 °C | ISO 180:2023 / ASTM D256 | 4.5–6.5 kJ/m² |
| Charpy notched impact, 23 °C | ISO 179-1:2010 | 5.0–7.5 kJ/m² |
| Vicat softening point, A50 | ISO 306:2022 | 123–127 °C |
| Hardness, Shore D | ISO 868:2003 | 63–66 |
At 23 °C, the tensile yield stress of 24–28 MPa measured by ISO 527-2:2012 is sufficient for stacking loads in fabricated boxes, provided the base rib geometry is designed for the expected hydrostatic load. The flexural modulus of 900–1050 MPa indicates a rigidity below that of unfilled polypropylene impact copolymer but above that of low-melt-index blow-moulding HDPE. The notched Izod impact of 4.5–6.5 kJ/m² at 23 °C is not a low-temperature guarantee; low-temperature performance should be verified with ISO 179-1:2010 or ASTM D256 on the finished article because moulded-in stress and wall thickness strongly affect impact response.
Environmental stress-cracking resistance is a key differentiator. HDPE grades intended for rigid packaging are often compared using ASTM D1693 in 100 % Igepal CO-630 at 50 °C. Published data for KC980A under this specific condition is limited; however, medium-flow copolymer HDPE grades of this density class usually exhibit from 50 h to 200 h before failure, whereas blow-moulding HDPE grades with lower melt-flow rate and higher comonomer content can exceed 600 h. The lower value for injection-moulding grades reflects the trade-off between flow and crack resistance; KC980A should not be used in continuous contact with aggressive aromatic hydrocarbons, strong oxidising acids, or high-solvency ester-based fluids.
The filling stage of KC980A is governed by the apparent viscosity under injection shear rates of 1000–10,000 s⁻¹. For thin-wall articles between 1.5 mm and 3.0 mm, shear heating reduces the melt viscosity and permits lower injection pressure. The recommended melt temperature is 180–220 °C at the nozzle. Holding pressure should be 50–70 % of the peak injection pressure and maintained until the gate freezes; premature transfer to holding creates sink marks at bosses and thick sections.
On production-scale injection-moulding machines of 350–650 t clamp force with a general-purpose 20:1–25:1 L/D barrier screw, typical injection pressure for multi-cavity pail tools is 60–100 MPa. The screw back pressure should be limited to 0.5–1.5 MPa to avoid excessive shear work. The melt cushion should remain above 5 mm. If the cushion drops below this value, check ring leakage produces short shots and cavity-to-cavity mass variation above 1.5 % after steady-state operation.
Pellet drying is not mandatory under normal dry indoor storage. If stored at relative humidity above 60 % or if surface condensation is visible on cold pellet surfaces, predrying at 80 °C for 1–2 h in a desiccant dryer prevents surface splay. HDPE is not hygroscopic; equilibrium moisture uptake is generally below 0.03 %, but regrind and external water are the main sources of processing defects.
Melt temperatures above 240 °C should be avoided unless required by a hot-runner gate; prolonged residence above 5 min at that temperature can yellow and reduce impact strength. The optimum mould temperature is 10–40 °C for fast cycle time. For reduced warpage on rectangular bases, a higher mould temperature of 30–50 °C and pack time of 1.5–2.5 s/mm of wall thickness improve dimensional stability, but may increase cycle time by 10–20 %.
KC980A is not a bimodal PE100 pipe-grade HDPE. It does not carry the minimum required stress of 10 MPa at 20 °C for 50 years under ISO 12162. The molecular architecture of a pressure-pipe grade is bimodal, combining a high-molecular-weight fraction for slow crack growth resistance with a low-molecular-weight fraction for processability. KC980A’s moderate melt flow and moderate density place it outside pressure-pipe design. Use in pressurised gas or water distribution is therefore outside the grade’s certified scope.
Against a low-melt-index blow-moulding HDPE with 0.2–0.8 g/10 min melt-flow index, KC980A has lower zero-shear viscosity and lower parison stability. Blow-moulding grades are chosen for continuous extrusion of bottles and jerry cans where parison sag must be limited. KC980A would not support a stable parison in large containers above 10 L; its flow properties are intended for injection into closed moulds, not for open parison forming. Conversely, the lower viscosity of KC980A allows injection pressures that would be impractical with a blow-moulding grade in multi-cavity tools.
Compared with an impact copolymer polypropylene of density 0.900–0.910 g/cm³, KC980A has lower heat deflection temperature. The HDPE grade typically exhibits heat deflection temperatures of 70–80 °C at 0.45 MPa by ISO 75-2:2013, whereas polypropylene impact copolymers can exceed 95 °C. For applications requiring hot-fill above 90 °C or steam sterilisation above 110 °C, polypropylene is preferred. KC980A offers better low-temperature impact than many polypropylene grades and lower temperature embrittlement risk because HDPE has a glass transition well below −70 °C.
| Material class | Melt-flow index, 190 °C/2.16 kg | Density | Flexural modulus | Heat deflection temperature, 0.45 MPa | Primary processing limitation |
|---|---|---|---|---|---|
| KC980A medium-flow HDPE | 8.0–10.0 g/10 min | 0.952–0.958 g/cm³ | 900–1050 MPa | 70–80 °C | Moderate ESCR in aggressive solvents |
| Blow-moulding HDPE | 0.2–0.8 g/10 min | 0.950–0.957 g/cm³ | 700–900 MPa | 65–75 °C | Impractical injection fill for multi-cavity tools |
| Bimodal PE100 pipe HDPE | 0.2–0.5 g/10 min | 0.945–0.952 g/cm³ | 700–900 MPa | 65–75 °C | Not for injection moulding; pressure-pipe specific |
| Polypropylene impact copolymer | 1.0–15.0 g/10 min | 0.900–0.910 g/cm³ | 1000–1400 MPa | 95–105 °C | Lower low-temperature ductility than HDPE |
For returnable logistics crates and pallets with wall thickness of 2.5–5.0 mm, the grade’s medium flow allows complete filling of deep rib structures without excessive injection pressure. The linear mould shrinkage is typically 1.8–2.2 % parallel to flow and 1.5–1.9 % perpendicular to flow, measured by ASTM D955. Shrinkage anisotropy should be managed with adequate gate positioning and mould cooling because the difference between parallel and perpendicular values can produce corner lifting and base warp.
For cylindrical pails and containers, stacking strength is determined by wall stiffness and rim design. The flexural modulus of KC980A supports top-load values only if the sidewall taper and rim reinforcement are adequate; top-load capacity cannot be inferred from resin modulus alone. Drop impact at −20 °C should be tested on the finished pail using ISO 6603-2 or ASTM D5420 because moulded-in hoop stress and weld-line location may reduce fracture resistance below the notched laboratory value.
In cap and closure prototypes below 2 mm wall thickness, the material’s flow assists filling of fine sealing-ring details. The low-temperature ductility of HDPE is advantageous for tamper-evident bands that are flexed after application. However, the lower oxygen-barrier property of HDPE compared with PET or EVOH must be considered in oxygen-sensitive content; HDPE has a typical oxygen transmission rate above 1000 cm³·mm/(m²·day·bar) at 23 °C and 0 % RH, making it unsuitable as a sole barrier layer in high-barrier packaging.
In agricultural chemical packaging, KC980A should be qualified by immersion testing according to EN 13587 or equivalent drain-hours protocols because high-density polyethylene may resist many dilute acids and bases but is not compatible with hydrocarbons such as xylene, benzene, and chlorinated solvents. For such contact, a fluorinated HDPE surface treatment or an alternative barrier layer is required. The grade is not declared for direct food contact in all jurisdictions; users must verify compliance with FDA 21 CFR 177.1520, EU Regulation 10/2011, or Japan JHOSPA for the specific food type and extraction limits.