Tpc Japan Hdpe Kbz81z

TPC (Japan) HDPE KBZ81Z

    • Product Name: TPC (Japan) HDPE KBZ81Z
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 575368
    Density 0.952 g/cm³
    Melt Flow Rate 0.25 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 25 MPa
    Tensile Elongation At Break 500%
    Flexural Modulus 1100 MPa
    Shore D Hardness 62
    Vicat Softening Point 124°C
    Heat Deflection Temperature At 0 45 Mpa 73°C
    Brittleness Temperature -70°C
    Environmental Stress Crack Resistance >1000 h
    Melting Point 130°C
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Thermal Conductivity 0.44 W/m·K
    Specific Heat Capacity 1.9 J/g·°C
    Dielectric Constant 2.3
    Volume Resistivity 1E15 Ω·cm
    Flammability HB

    As an accredited TPC (Japan) HDPE KBZ81Z factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KBZ81Z comes in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for secure transport.
    Container Loading (20′ FCL) 20′ FCL container loading for TPC (Japan) HDPE KBZ81Z: palletized 25 kg bags, stretch-wrapped, strapped, and secured for ocean freight.
    Shipping TPC (Japan) HDPE KBZ81Z is a non-hazardous high-density polyethylene resin supplied as pellets. It is typically packed in 25 kg bags or jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers away from moisture, heat, and direct sunlight. No dangerous-goods classification applies.
    Storage Store TPC (Japan) HDPE KBZ81Z in original, closed packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, strong oxidizers, and incompatible materials. Avoid excessive stacking; ensure stable pallets. Maintain ambient temperature, low humidity, and first-in, first-out inventory. Do not store outdoors or near open flames. Follow manufacturer SDS and local regulations.
    Shelf Life TPC (Japan) HDPE KBZ81Z shelf life is typically 24 months when stored cool, dry, and unopened in original packaging.
    Application of TPC (Japan) HDPE KBZ81Z

    Accumulator-head blow moulding of UN-rated large-volume containers

    Extrusion blow moulding of HDPE KBZ81Z into tight-head drums, open-top drums and IBC inner bottles requires a parison with sufficient melt strength to resist sag over vertical drop lengths exceeding 1200 mm on accumulator-head machines with shot capacities from 2.5 kg to 7.5 kg. In production-scale accumulator-head machines with extruder length-to-diameter ratios of 25:1 to 30:1, barrel zone settings are typically staged from 170 °C to 205 °C, with the die head held at 190 °C to 210 °C and the die gap set between 1.5 mm and 3.0 mm. The grade-specific melt flow rate of HDPE KBZ81Z should be verified against the certificate of analysis; large-part blow moulding HDPE grades commonly fall within 0.25 g/10 min to 0.45 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022, and if the actual MFR exceeds 0.50 g/10 min, the parison programmer must be recalibrated to reduce draw-down. The addition ratio for the container compound is based on 100 parts by weight of HDPE KBZ81Z: colour masterbatch at 1.0 wt% to 3.0 wt%, UV stabiliser masterbatch based on hindered amine light stabilisers at 0.10 wt% to 0.35 wt%, fluoropolymer processing aid at 0.02 wt% to 0.06 wt% to suppress die build-up, and antistatic additive at 0.05 wt% to 0.15 wt% where the container is used for solvent or powder transfer. Blow air pressure is maintained at 0.6 MPa to 0.9 MPa, mould temperature is held at 10 °C to 35 °C, and cooling time is controlled by wall thickness at 2.5 mm to 4.0 mm; the process is not tolerant of melt temperatures above 220 °C, where oxidation generates gel particles in the parison and reduces drop-impact performance, nor of die temperatures below 170 °C, where shark-skin melt fracture appears on the inner and outer wall. Compliance anchors for this application include ADR 2025 Chapter 6.1 for UN marking, IMDG Code 40-20 for maritime shipments, FDA 21 CFR 177.1520 for food-contact containers, EU Regulation (EU) No 10/2011 and EU Directive 94/62/EC for packaging, ASTM D2463-15 for drop impact, ASTM D1693-21 for environmental stress crack resistance in 10 % and 100 % Igepal CO-630, ISO 1183-1:2019 for density, and ISO 527-2:2012 for tensile yield. Terminal finished product types include UN-rated 20 L, 25 L and 30 L jerrycans, 120 L to 220 L tight-head and open-top drums, and 1000 L IBC inner bottles.

    Compliance propertyStandard designationTest condition or acceptance basis
    Melt flow rateISO 1133-1:2022190 °C, 2.16 kg
    DensityISO 1183-1:2019Grade certificate basis
    Tensile yield stressISO 527-2:2012Grade certificate basis
    Drop impactASTM D2463-15No brittle failure at -20 °C
    ESCRASTM D1693-2110 % and 100 % Igepal CO-630

    In high-cavitation injection moulding of beverage and dairy closures, the limiting variable is the residence time distribution across a high-cavitation tool, because the melt must be injected through gates of 0.5 mm to 1.2 mm without shear-induced discolouration or gate-vestige variation. A formulation based on 100 parts by weight of HDPE KBZ81Z with a nucleating agent at 0.05 wt% to 0.20 wt%, a slip agent such as erucamide or oleamide at 0.05 wt% to 0.15 wt%, a phenolic-phosphite antioxidant package at 0.03 wt% to 0.08 wt%, and colour masterbatch at 1.0 wt% to 3.0 wt% is applied in high-speed cap lines. Processing on a hydraulic or all-electric injection moulding machine with screw L/D of 20:1 to 24:1 and compression ratio 2.0:1 to 2.5:1 uses a melt temperature of 210 °C to 250 °C, injection speeds of 100 mm/s to 250 mm/s, holding pressure of 40 MPa to 70 MPa, back pressure of 5 bar to 15 bar, and chilled mould temperature of 5 °C to 15 °C to achieve cycle times of 5 s to 9 s. The main failure modes on production scale are gate freeze-off when the mould temperature falls below 5 °C, warpage from non-uniform cooling when the closure thickness varies by more than 0.15 mm, and splay or silver streaking if surface moisture is not removed; pre-drying at 80 °C for 2 h to 4 h is therefore applied when storage relative humidity exceeds 60 %. Published data for HDPE KBZ81Z in high-cavitation closure moulding is limited, and the grade-specific melt flow rate must be confirmed before converting a mould designed for a conventional injection-grade HDPE. Compliance for the finished closures includes FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011, EU Directive 94/62/EC, RoHS 2011/65/EU, CONEG Model Legislation for heavy metals, ISO 1133-1:2022 for melt flow rate, ASTM D638-22 for tensile strength, and ASTM D256-23 for notched Izod impact. Terminal finished product types include 28 mm and 29/25 mm carbonated soft drink closures, 38 mm aseptic dairy closures, and 30/25 mm water and juice closures.

    Which blown film parameters govern heavy-gauge liner puncture resistance?

    For heavy-gauge industrial liners converted from HDPE KBZ81Z, blown film performance is dominated by bubble cooling, stalk height, and blow-up ratio rather than by melt temperature alone. On grooved-feed extruders with L/D of 30:1 and die diameters from 150 mm to 250 mm, the melt temperature is maintained between 180 °C and 220 °C, the die gap is set at 1.2 mm to 2.0 mm, and the blow-up ratio is held between 2.0:1 and 4.0:1, with a frost line height of 6 to 12 die diameters. Bubble stability is the operational boundary: a blow-up ratio above 4.0:1 introduces lateral oscillation and gauge variation above ±8 %, while a die temperature below 170 °C increases melt pressure beyond 30 MPa and triggers melt fracture at the die lip. The compound is based on 100 parts by weight of HDPE KBZ81Z with slip agent at 0.03 wt% to 0.10 wt%, antiblock additive at 0.05 wt% to 0.20 wt%, fluoropolymer processing aid at 0.02 wt% to 0.05 wt%, and antioxidant at 0.02 wt% to 0.08 wt%; the slip/antiblock balance is not adjusted upward without puncture resistance testing because additive migration to the film surface can reduce heat-seal strength. Compliance testing for this downstream route includes ASTM D1709-16a for dart drop, ASTM D1922-15 for Elmendorf tear, ISO 527-3:2018 for tensile properties of film, ISO 1183-1:2019 for density, FDA 21 CFR 177.1520 for food-contact liners, and EU Regulation (EU) No 10/2011 for specific migration limits. Terminal finished product types include 25 kg to 120 kg form-fill-seal industrial liners, heavy-duty refuse sacks, agricultural silage films, and temporary containment sheeting.

    When monolayer sheet is calendered through a three-roll stack prior to vacuum forming, the dimensional stability of HDPE KBZ81Z sheet must be established before the sheet enters a trim station, otherwise post-trim shrinkage produces out-of-specification cut-edges on downstream filling lines. In sheet lines with extruder L/D of 28:1 to 32:1 and die widths from 800 mm to 1500 mm, the melt temperature at the die is held between 200 °C and 230 °C, the roll stack temperature is set at 60 °C to 90 °C, and sheet thickness is controlled from 0.3 mm to 1.5 mm with a tolerance of ±0.05 mm. The formulation based on 100 parts by weight of HDPE KBZ81Z includes nucleating agent at 0.03 wt% to 0.10 wt% to increase crystallisation rate and reduce post-forming shrinkage, antioxidant at 0.03 wt% to 0.08 wt%, and colour concentrate at 2.0 wt% to 4.0 wt%; a sheet containing more than 4.0 wt% of mineral-filled masterbatch is not recommended for vacuum forming because it reduces draw ratio and causes corner thinning. Thermoforming ovens apply surface temperatures of 170 °C to 190 °C with mould temperatures of 20 °C to 40 °C and vacuum levels of 0.3 bar to 0.6 bar; plug-assist tooling is required for draw ratios above 1.5:1. Compliance for the sheet and formed articles includes FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011, EU Directive 94/62/EC, ISO 1183-1:2019, ASTM D638-22, and ASTM D648-18 for deflection temperature under load. Terminal finished product types include retail bakery trays, deli containers, portion cups, insert trays for confectionery, and medical device packaging trays where sterility is introduced downstream by ethylene oxide or gamma irradiation.

    When extrusion blow moulding of pharmaceutical bottles requires organoleptic neutrality

    Pharmaceutical and personal care bottles made from HDPE KBZ81Z on shuttle blow moulding machines must combine low odour, low taint and consistent part weight in multi-cavity tools. The process window is narrower than in industrial container blow moulding because wall thickness is typically 0.4 mm to 1.2 mm and drop impact must be retained at -10 °C without increasing density beyond the grade specification. Shuttle machines with 1 to 8 cavities and screw L/D of 20:1 to 24:1 are operated with melt temperatures of 170 °C to 210 °C, die head temperatures of 175 °C to 200 °C, blow air pressure of 0.5 MPa to 0.8 MPa, and mould temperatures of 10 °C to 30 °C; cycle times for 100 mL to 500 mL bottles are typically 8 s to 20 s. The addition ratio is structured around 100 parts by weight of HDPE KBZ81Z with antioxidant at 0.02 wt% to 0.05 wt%, slip agent at 0.03 wt% to 0.08 wt%, and white or coloured masterbatch at 0.5 wt% to 2.0 wt%; the use of amine-based processing additives is excluded unless the additive supplier certifies absence of reaction with the polymer at melt temperatures above 200 °C, because degradation by-products can alter organoleptic performance. Compliance requirements include USP <661.1> for plastic packaging systems, Ph. Eur. 3.1.5 for polyethylene with additives for containers for oral preparations, FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011, and ISO 10993-5 for cytotoxicity when the bottle is used in medical device packaging. Terminal finished product types include 30 mL to 500 mL oral liquid syrup bottles, tablet desiccant bottles, ophthalmic dropper bottles, and cosmetic lotion bottles.

    On corrugator lines producing non-pressure drainage conduit and cable duct, the melt strength of HDPE KBZ81Z is used to maintain corrugation profile after the forming blocks close, and the limiting defect is valley-thinning when melt temperature is too low or when carbon black dispersion is non-uniform. In corrugator lines with extruder L/D of 24:1 to 30:1, melt temperatures from 190 °C to 230 °C, and forming block temperatures of 15 °C to 50 °C, the outer wall is drawn into the corrugator under vacuum and the inner wall is cooled by compressed air; line speed is adjusted from 2 m/min to 8 m/min depending on diameter and wall thickness. The compound is based on 100 parts by weight of HDPE KBZ81Z with carbon black masterbatch at 2.0 wt% to 3.0 wt% for UV resistance, antioxidant at 0.05 wt% to 0.10 wt%, and processing aid at 0.02 wt% to 0.05 wt%; carbon black dispersion must be verified by particle count or pressure-rise test to avoid micro-voids in thin corrugation valleys. Compliance standards for this downstream route include ISO 9969:2016 for ring stiffness, ISO 9967:2016 for creep ratio, ASTM D2412-21 for ring stiffness of thermoplastic pipe, EN 61386-24 for underground conduit, and ISO 1183-1:2019 for density. Terminal finished product types include DN 50 to DN 200 non-pressure drainage pipes, corrugated land drainage pipes, cable protection ducts, and electrical conduit.

    Free Quote

    Competitive TPC (Japan) HDPE KBZ81Z prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KBZ81Z is a high-molecular-weight high-density polyethylene copolymer supplied for extrusion blow moulding and thick-wall container manufacture. Melt flow rate under ISO 1133-1:2022 at 190 °C/2.16 kg is reported by the supplier in the range 0.30–0.45 g/10 min; density under ISO 1183-1 is typically 0.954–0.958 g/cm³. Those figures locate the grade in the high melt strength segment used for large-part blow moulding, where parison sag, weld-line integrity, and environmental stress crack resistance are controlled by molecular weight distribution. On accumulator-head blow moulding lines with die diameters between 80 mm and 120 mm, barrel temperatures are maintained at 180–210 °C and head temperatures at 190–205 °C. Melt temperature measured at the die exit should not exceed 215 °C, because oxidative chain scission accelerates and parison surface haze increases.

    Capillary rheometry at 190 °C through a 1 mm die with L/D=30 places the apparent shear viscosity of this molecular weight class near 1500–2500 Pa·s at 100 s⁻¹ and 300–500 Pa·s at 1000 s⁻¹. The melt flow ratio under ISO 1133-1:2022 at 21.6 kg divided by the 2.16 kg value is typically 15–25. A higher ratio indicates broader molecular weight distribution and improves parison stability, but can reduce surface gloss. Over-shearing the melt in grooved-feed extruders above 120 rpm can shift the melt flow ratio upward and degrade environmental stress crack resistance.

    Product Designation and Pellet-State Properties

    The product is delivered as translucent white pellets with an average pellet size of 2–4 mm. Bulk density ranges from 0.56 g/cm³ to 0.60 g/cm³ depending on pellet geometry and fines content. The table below presents representative values for the high-molecular-weight HDPE sub-family represented by KBZ81Z; certified lot-level values must be taken from the supplier’s certificate of analysis.

    PropertyTest methodRepresentative rangeProcessing relevance
    Melt flow rateISO 1133-1:20220.30–0.45 g/10 minControls parison sag, die pressure, and extruder torque
    DensityISO 1183-1:20190.954–0.958 g/cm³Sets stiffness, chemical resistance, and barrier baseline
    Tensile stress at yieldISO 527-2:201226–30 MPaPredicts hoop strength in pressurised containers
    Flexural modulusISO 178:20191050–1350 MPaInfluences top-load strength and panel stiffness
    Charpy notched impact at 23 °CISO 179-1:202020–35 kJ/m²Relates to low-temperature drop resistance after moulding
    ESCR F50, 10% Igepal CO-630ASTM D1693>500 hCritical for chemical containers and detergent packaging
    Vicat softening temperature A50ISO 306:2022124–128 °CDefines upper service temperature margin

    Because the grade is not hygroscopic in the manner of polyamide or polyester, drying is not required when pellet surface moisture is below 0.05 wt%. Condensation on cold pellets transferred from outdoor silos to a heated mezzanine introduces feed-throat moisture. A desiccant dryer at 80 °C for 2–4 h with dew point below −30 °C removes surface condensation. Failure to dry condensate-loaded pellets produces surface splay, melt froth, intermittent gas locking in grooved-feed extruders, and local density reduction in weld zones.

    Extruder screw geometry for KBZ81Z should use a barrier flight section and a mixing element with moderate shear heating; compression ratios between 2.5:1 and 3.5:1 are typical. Screw speeds of 80–100 rpm on grooved-feed extruders avoid melt-temperature overshoot above 210 °C. Parison programming through 100-point electronic controllers is required for containers with width-to-height ratios below 0.6. At shot weights from 5 kg to 25 kg, die gap openings of 5–12 mm and accumulator discharge rates of 0.2–0.5 m/s maintain uniform wall thickness. Blow air pressure of 0.6 MPa on a projected area of 0.4 m² produces a theoretical mould-opening force of 240 kN; clamp force of at least 300–350 kN is specified to avoid flash and pinch-off weld deformation.

    How Does KBZ81Z Differ from Higher-Melt-Flow HDPE Blow-Moulding Resins?

    Relative to general-purpose blow moulding HDPE grades with melt flow rates between 0.7 g/10 min and 1.2 g/10 min, the lower melt flow rate of KBZ81Z increases extensional viscosity and reduces gravity-driven parison thinning. In an accumulator-head tool with a 150 mm die, a 2 m parison remains stable for 8–15 s before necking, while higher-MFR resins develop fold-over or wall-thickness variation in the same interval. The trade-off is a narrower high-shear processing window; excessive screw speed raises melt temperature and degrades the high-molecular-weight fraction. Compared with PE100 pipe compounds having density above 0.958 g/cm³, KBZ81Z shows lower flexural modulus but higher ESCR-failure times under ASTM D1693 Condition A, making it more suitable for containers that must withstand chemical stress and less suitable for pressure-pipe applications requiring long-term hydrostatic strength at 20 °C and 10 MPa hoop stress.

    The grade’s performance envelope also differs from injection-moulding HDPE in the same density class. Injection-moulding high-density polyethylene with MFR above 20 g/10 min fills thin-wall moulds but lacks the melt strength required for a stable parison above 1 kg shot weight. KBZ81Z is not suitable for thin-wall injection moulding below 2 mm part thickness because flow length is limited and mould filling pressures exceed 80 MPa at conventional processing temperatures.

    KBZ81Z is evaluated for contact with non-oxidising mineral acids, sodium hydroxide solutions, and aqueous salt solutions. Stress-crack testing under ASTM D1693 Condition A in 10% Igepal CO-630 at 50 °C typically yields F50 values above 500 h for this molecular weight class. Strong oxidising acids such as nitric acid above 20% concentration and halogenated solvents are not recommended for continuous service. The resin should not be dry blended with peroxide masterbatches or amine-based antistatic additives above 0.1 wt%, because residual radical species accelerate branching and amine additives can reduce long-term ESCR.

    Compliance declarations for the grade must be verified through the supplier’s certification and do not transfer automatically to a finished moulded article. The following matrix identifies the governing standard areas for HDPE packaging and the required evidence.

    Regulatory areaStandard or directiveRequired evidence for KBZ81Z
    Food contact material frameworkEU 10/2011Specific migration limit verification for finished article, if relevant
    Olefin polymer food contactFDA 21 CFR 177.1520Supplier letter for resin; end-use extraction testing by converter
    Hazardous goods packagingUN Recommendations, Chapter 6.1Design type test on moulded container; drop and stack tests
    Heavy metals and hazardous substancesIEC 62321 / RoHS Directive 2011/65/EUMaterial declaration, XRF screening of lot samples
    Biological and physical safetyISO 22000:2018Process controls in moulding facility, not resin property
    Environmental complianceREACH / SVHCArticle 33 declaration from supplier; lot traceability

    When Wall Thickness Exceeds 6 mm in Industrial Container Moulding

    Cooling time scales approximately with the square of wall thickness. For a 6 mm HDPE wall at mould temperature 12 °C and melt temperature 200 °C, cooling times between 240 s and 420 s are observed on single-station shuttle blow moulding machines. Reducing wall thickness to 3 mm shortens cooling time to 60–120 s. Internal cooling air at 0.3–0.5 MPa and post-mould recirculated air at 10–15 °C reduce cycle time by 15–25%. Excess internal pressure before freeze-off causes doming at the bottom pinch-off, while premature blow-pin retraction before the inner surface cools below 90 °C generates sink marks adjacent to the flash zone.

    The pinch-off weld is the highest-risk region in thick-wall containers. Lower melt temperature at the pinch-off or insufficient clamp force reduces weld strength and can cause drop-impact failure at −18 °C during UN package qualification. Container drop tests for hazardous goods are typically conducted at −18 °C after conditioning for 24 h, following UN Recommendations on the Transport of Dangerous Goods, Chapter 6.1. Thick-walled high-molecular-weight HDPE containers generally meet the 2.0 m drop height at gross mass above 10 kg only when pinch-off welds are fully fused and wall distribution does not fall below 60% of nominal thickness.

    Evaluating Environmental Stress Crack Resistance after Acetic Acid Exposure

    ESCR specimens are compression moulded according to ASTM D4703-16, notched with a razor blade to a depth of 0.3–0.5 mm, bent in a channel, and immersed in 10% Igepal CO-630 at 50 °C. F50 failure time is recorded when 50% of ten specimens exhibit visible cracks. For acetic acid service, the resin can be pre-exposed in 5% acetic acid at 40 °C for 30 days before ESCR testing to detect additive extraction and surface oxidation. Published data for this specific configuration is limited; converters should run comparative coupons against an incumbent resin under the same conditioning protocol. Results below 200 h after acid pre-exposure indicate that the moulding thermal profile has degraded the high-molecular-weight fraction or that recycled regrind level has exceeded the supplier’s recommended limit.

    Incoming inspection of KBZ81Z should record melt flow ratio under ISO 1133-1:2022 at 5.0 kg and 21.6 kg. A shear sensitivity ratio outside the supplier’s control band indicates a change in molecular weight distribution and requires adjustment of head temperature or screw speed. Pellet size distribution is also monitored; fines smaller than 0.5 mm should remain below 0.5 wt% to avoid feed-throat bridging and melt starvation. Regrind addition above 20 wt% reduces parison melt strength and ESCR; if recycled material is used, it must be dried, screened through a 2 mm mesh, and blended gravimetrically to maintain lot traceability.

    The grade is used for intermediate bulk containers, open-top drums, automotive fluid reservoirs, water tanks, and industrial packaging requiring environmental stress crack resistance. On single-station and two-station shuttle machines, shot sizes range from 5 kg to 60 kg; on accumulator-head machines, larger parts exceed 150 kg. Moulds are typically aluminium or kirksite for prototypes and steel for production runs above 100,000 cycles. Mould temperature is maintained with circulating water at 8–15 °C; mould release is not normally required for rigid HDPE, but external mould release agents containing silicones should be avoided because they interfere with printing and adhesive bonding.

    Post-moulding surface treatment for labelling or adhesive assembly uses corona discharge at 40–48 mN/m for HDPE. Flame treatment may be used on large flat surfaces, with a surface energy target of 50 mN/m. Compression-moulded test plaques from the resin class show tensile stress at yield between 26 MPa and 30 MPa under ISO 527-2:2012, elongation at break above 600%, and notched Charpy impact at 23 °C between 20 kJ/m² and 35 kJ/m². At −30 °C, notched impact values fall to 5–10 kJ/m², so low-temperature drop tests of thick-walled containers are more discriminating than ambient tensile tests.