| HS Code | 307146 |
| Manufacturer | TPC (Japan) |
| Product | HDPE KBZ61Z |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.961 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Strength At Yield | 30 MPa |
| Tensile Elongation At Break | 600% |
| Flexural Modulus | 1250 MPa |
| Vicat Softening Temperature | 128°C |
| Brittleness Temperature | -70°C |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Shore D Hardness | 65 |
As an accredited TPC (Japan) HDPE KBZ61Z factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KBZ61Z is supplied in 25 kg multiwall paper bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): TPC Japan HDPE KBZ61Z, 25 kg bags palletized, shrink-wrapped, securely stowed and lashed for ocean shipment. |
| Shipping | TPC (Japan) HDPE KBZ61Z is a non-hazardous high-density polyethylene resin. It is shipped in 25 kg bags, jumbo bags, or bulk containers/trucks. Palletized and stretch-wrapped for bag shipments. Keep dry, clean, and away from heat, direct sunlight, and ignition sources. Standard handling with PPE; no dangerous goods classification required. |
| Storage | Store TPC (Japan) HDPE KBZ61Z in a cool, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Stack pallets securely to prevent deformation or bursting. Protect from physical damage. Follow the manufacturer’s safety data sheet and local regulations. |
| Shelf Life | TPC (Japan) HDPE KBZ61Z has a shelf life of approximately 24 months if stored cool, dry, sealed, and away from sunlight. |
On accumulator-head extrusion blow moulding lines producing 10–30 L tight-head jerrycans for dangerous goods, melt temperature control at the die exit is the primary variable governing parison wall thickness uniformity. The resin is compounded at 100 phr with carbon black masterbatch at 1.5–2.5 wt% and antioxidant masterbatch at 0.1–0.3 wt%; regrind from flash and rejected parison trim is incorporated at 10–25 wt%, provided the regrind fraction passes a melt flow rate deviation check under ISO 1133-1:2022 and does not exceed 25 wt% of the total charge. Crosshead and accumulator temperature settings are maintained between 185 °C and 210 °C, with the extruder barrel profile from 170 °C near the feed zone to 195 °C at the metering zone; die gap is adjusted from 0.8 mm to 1.5 mm depending on part weight. Blow pressure is set at 0.6–0.8 MPa, and mould temperature is held at 12–20 °C to balance surface finish and cycle time. Terminal products are UN type 3H1 tight-head jerrycans of 10 L, 20 L, 25 L, and 30 L capacity for packing group II/III liquid chemicals. Certification is conducted under the UN Model Regulations via ADR/RID/IMDG Code, with stack compression testing at 40 °C for 28 days, drop testing at -18 °C, and leakproofness testing at 30 kPa internal air pressure. Food-contact variants are moulded only when the base resin is supported by FDA 21 CFR §177.1520(c) 2.1 and EU Regulation (EU) No 10/2011 with overall migration below 10 mg/dm².
Environmental stress crack resistance in agrochemical packaging is evaluated under ASTM D1693-15, condition B, in a 10% Igepal CO-630 solution at 50 °C; for jerrycans holding emulsifiable concentrates, xylene-based solvents, or ester-functional actives, the failure criterion is no visible crazing beyond 48 h in 12 replicate specimens. Formulations for 1–5 L narrow-neck bottles use 100 phr KBZ61Z in the outer and inner skins, with a polyamide or EVOH barrier layer at 1.5–3.0 wt% of total wall thickness and maleic anhydride-grafted polyethylene tie resin at 1–2 wt%; in monolayer 10 L crop-protection containers, a carbon black concentrate is added at 2.0–3.5 wt% to achieve minimum light transmission below 0.1% across 290–450 nm. The extrusion blow moulding process operates with a barrier screw of L/D 24:1–30:1, a grooved feed section, and an accumulator head delivering 2.0–4.5 kg parison weight; parison programming uses 30–50 points to account for pinch-off zones at the handle and base. Bottles are top/tail trimmed, leak tested at 25 kPa, and weighed to a tolerance of ±1.0 g for 1 L and ±2.5 g for 5 L. Terminal types are UN 3H1 5 L and 10 L agrochemical packagings, 1 L and 2 L ready-to-use containers, and closed-loop refillable containers under FAO/WHO guidelines when the design passes 30 repeated immersion cycles. Drying is not normally required for the base resin, but regrind exposed to relative humidity above 60% should be dried at 80 °C for 2 h before compounding to avoid surface splay at the die lip.
Underhood reservoirs produced from this HDPE grade are evaluated for thermal loading under ISO 16750-4 and for vibration under ISO 16750-3, with resonance dwell from 10–1000 Hz and pressure cycling from 0 kPa to 150 kPa for at least 250,000 cycles at 80 °C. The typical formulation is 100 phr resin with a UV/thermal stabilizer masterbatch at 0.3–0.8 wt% and a carbon black concentrate at 0.5–1.5 wt% for black parts; white or natural reservoirs use hindered phenolic/phosphite systems at 0.2–0.5 wt% and a light-stable pigment masterbatch at 1.0–2.0 wt%. Process temperatures are kept at 195–215 °C melt temperature, with die gap set to 1.0–2.0 mm for 2–5 L parts, and the shuttle or single-station blow moulding machine clamp force is typically limited to 150–250 kN for a flat flash area below 0.15 m². Mould cooling circuits are balanced to maintain 8–15 °C surface temperature to prevent warpage at the mounting bosses. Terminal components are windshield washer tanks of 2.5–5.5 L, coolant surge tanks of 0.8–2.0 L, and urea solution reservoirs for selective catalytic reduction systems up to 15 L. Parts that fail validation typically exhibit stress whitening at the pinch weld, which is alleviated by increasing the parison die gap by 0.2 mm and reducing regrind to 15 wt% maximum. Avoid combining the base resin with unknown zinc stearate-based processing aids from recycled streams, because inconsistent stearate migration can reduce weld line strength after thermal cycling.
When the same polymer is converted on single-station shuttle blow moulding machines for pharmaceutical-grade oral liquid bottles, the limiting factor shifts from mould temperature to die lip cleanliness and traceability of batch-specific additive composition. The base resin is used at 100 phr without recycled content; a masterbatch based on the same HDPE carrier is added at 0.5–1.5 wt% for colour, and slip/antiblock additives are restricted to 0.05–0.10 wt% to avoid exceeding compendial extractables thresholds. Extrusion blow moulding equipment is configured with a 25:1 L/D barrier screw, feed zone at 165 °C, transition at 180 °C, and die head at 195–205 °C; parison drop time is maintained below 1.8 s to avoid neck-down in 100–250 mL bottle formats. Moulds are polished to Ra 0.8 µm and cooled at 10–15 °C; bottles are trimmed with a hot-knife unit and purged with filtered air at 0.2 MPa before closure. Terminal products are high-density polyethylene oral liquid bottles of 100 mL, 150 mL, 200 mL, and 250 mL, ophthalmic bottles, and cosmetic lotion bottles from 50 mL to 500 mL. Compliance is demonstrated under FDA 21 CFR §177.1520(c) 2.1, EU Regulation (EU) No 10/2011, USP <31> and <661.1>, and Ph.Eur. 3.1.3; extractables testing is conducted in ethanol/water and acidic conditions according to ISO 10993-18 when the bottle is intended for orally administered liquids. Published grade-specific extractables data for this exact KBZ61Z configuration is limited; therefore, lot-specific validation is required for each colour masterbatch and process temperature combination.
Multi-layer bottles for methyl ethyl ketone, mineral spirits, and methylene chloride-free paint stripper formulations are moulded with KBZ61Z as the structural outer and inner layers, an EVOH or polyamide barrier layer, and maleic anhydride-grafted tie resin. The outer and inner HDPE skins are formulated at 100 phr each with a colour masterbatch at 1.0–2.0 wt% and process stabilizer at 0.1–0.3 wt%; the tie resin is metered at 1.5–2.5 wt% of total wall thickness and the barrier layer at 1.0–2.5 wt%. Six-layer continuous blow moulding systems with five extruders are used, with extruder diameters of 65 mm for the outer skin, 50 mm for the inner skin, 35 mm for the barrier layer, and 25 mm for the tie layers; all extruders have L/D 24:1. Melt temperatures are maintained at 200–215 °C for HDPE and 190–210 °C for EVOH; die gap is set at 0.7–1.5 mm, blow pressure at 0.5–0.7 MPa, and mould temperature at 10–15 °C. Terminal products are 0.5 L, 1 L, and 2 L bottles for household degreasers, paint solvents, and adhesive cleanup solvents. Chemical resistance is assessed by immersion under ASTM D543-21, and vapour permeation is measured according to ASTM D2684/D2684M-15. Barrier layer drop-out must be monitored by layer-thickness scanning at the pinch weld; a deviation greater than 0.3 mm in barrier thickness at the sidewall is grounds for rejecting the batch because pinhole formation elevates permeation rate above the formulation-specific target.
Portable fuel cans for gasoline, kerosene, and diesel are moulded as monolayer HDPE containers and subsequently fluorinated to reduce hydrocarbon vapour loss. The pre-fluorination compound is 100 phr KBZ61Z with carbon black concentrate at 1.5–2.5 wt%, antioxidant masterbatch at 0.2–0.5 wt%, and no recycled fraction when the container is intended for CARB-compliant gasoline service. Extrusion blow moulding is performed at melt temperatures of 190–210 °C, blow pressure 0.6–0.8 MPa, mould temperature 10–18 °C, and clamp force sufficient for a projected flash area up to 0.20 m² on high-output shuttle equipment. After trimming and cooling to 25–40 °C, containers are placed in a fluorination chamber with a dilute fluorine/nitrogen blend at 0.5–2.0 vol% fluorine; surface fluorine uptake is controlled at 0.5–2.0 atomic% and verified by X-ray photoelectron spectroscopy. The treatment window must begin within 24 h of moulding and before any exposure to high ambient humidity; containers stored above 60% RH require pre-drying at 50 °C for 1 h to avoid hydrogen fluoride formation at the surface. Terminal products are portable fuel cans from 5 L to 20 L certified under ASTM F852/F852M-20, US EPA 40 CFR Part 59, and CARB portable fuel container provisions; permeation testing is conducted according to the applicable regulatory method for gasoline at 28–40 °C. Operational boundaries include avoiding post-fluorination reheating above 60 °C before filling, because rapid desorption of residual fluorination gases can create odour complaints and reduce barrier performance in the sealing area.
| Application zone | Primary regulatory or performance standard | Key test designation or clause | Critical measured parameter |
|---|---|---|---|
| Dangerous goods jerrycans | UN Model Regulations, ADR/RID/IMDG Code | UN type 3H1 | Drop at -18 °C, stack at 40 °C for 28 days, leakproof at 30 kPa |
| Agrochemical containers | FAO/WHO guidelines, UN packaging requirements | ASTM D1693-15 | No crazing beyond 48 h in 10% Igepal CO-630 at 50 °C |
| Automotive underhood reservoirs | OEM thermal/vibration specifications | ISO 16750-3, ISO 16750-4 | Pressure cycling 0–150 kPa, 250,000 cycles at 80 °C |
| Pharmaceutical oral liquid bottles | USP, Ph.Eur., food-contact regulations | USP <661.1>, Ph.Eur. 3.1.3, FDA 21 CFR §177.1520 | Extractables below compendial threshold |
| Household chemical barrier bottles | Chemical resistance and permeation standards | ASTM D543-21, ASTM D2684/D2684M-15 | Barrier thickness deviation < 0.3 mm at sidewall |
| Portable fuel cans | US EPA, CARB, ASTM container specification | ASTM F852/F852M-20, 40 CFR Part 59 | Gasoline permeation limit at 28–40 °C |
Competitive TPC (Japan) HDPE KBZ61Z prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KBZ61Z is a high-density polyethylene grade identified in supplier literature as KBZ61Z and supplied in pellet form for extrusion and extrusion blow moulding. The material belongs to the PE-HD class under ISO 1043-1 and is released to converters rather than as a finished article. The producer’s technical documentation positions the grade where melt strength, environmental stress crack resistance, and stiffness after cooling are required. The values below are representative properties from supplier documentation, not release-specification minima or maxima. Acceptance should be based on the lot-specific certificate of analysis.
Typical physical and mechanical properties reported for the grade are compiled in Table 1. Test specimens are conditioned at 23 °C and 50% RH before measurement unless a different condition is specified by the relevant test method.
| Property | Typical value | Test method |
|---|---|---|
| Melt flow rate, 190 °C/2.16 kg | 0.60 g/10 min | ISO 1133-1 |
| Density at 23 °C | 0.961 g/cm³ | ISO 1183-1 |
| Tensile stress at yield | 29.0 MPa | ISO 527-2 |
| Elongation at break | >600% | ISO 527-2 |
| Flexural modulus | 1350 MPa | ISO 178 |
| Shore D hardness | 64 | ISO 868 |
| Vicat softening temperature, A120 | 127 °C | ISO 306 |
| Charpy notched impact strength, 23 °C | 38 kJ/m² | ISO 179-1/1eA |
| Environmental stress crack resistance, F50 | >1000 h | ASTM D1693/B, 100% Igepal CO-630 |
| Brittleness temperature | -76 °C | ASTM D746 |
The property set indicates a stiffness-driven grade with an ESCR reserve that is not typical of low-viscosity commodity HDPE. A flexural modulus of 1350 MPa permits wall-thickness reduction when compared with a lower-density HDPE at 0.952 g/cm³, but the stiffness gain is not linear with density. The notched Charpy value of 38 kJ/m² is a laboratory ranking and does not predict drop-impact performance of a filled transport container at −20 °C. Full-scale article testing remains necessary for UN-certified packaging.
Process behaviour is governed by the viscosity associated with a melt flow rate of 0.60 g/10 min and by the sensitivity of HDPE to oxidation at the upper end of the working temperature range. On a grooved-feed single-screw extruder with L/D ratio 30:1 to 36:1, barrel temperature settings from 200 °C to 240 °C are used from feed to metering zone, with adapter and die zones set at 220 °C to 250 °C. Melt temperature measured at the die entry should be maintained between 230 °C and 260 °C. Sustained excursions above 270 °C for more than 10 min increase carbonyl species formation and can produce oxidised gel particles that appear as surface defects on blow-moulded parts. A screen pack of 60/80/60 mesh is common; finer screens increase melt pressure and residence time. If head pressure exceeds 35 MPa, screw rpm and temperature profile should be re-evaluated before surface finish deteriorates.
For blow moulding of containers between 20 L and 60 L, accumulator-head machines are preferred because the high molecular weight of the grade produces a stable parison with limited sag at typical cycle times. Blow moulds are cooled at 10 °C to 30 °C, and blow pressure of 0.6 MPa to 1.0 MPa is common. The parison thickness control window at the die lip is narrow at ±5 °C when compared with higher-flow HDPE grades. The lower viscosity of KBZ61Z relative to a 0.30 g/10 min high-molecular-weight HDPE reduces screw motor load, but the grade still requires more torque than a 6 g/10 min injection grade.
When HDPE containers are filled with agricultural adjuvants, industrial surfactants, or hypochlorite-based cleaners, failure is usually dominated by slow crack propagation from stressed weld lines, scratch zones, or moulded-in residual stress. The quoted ESCR value of >1000 h under ASTM D1693 condition B with 100% Igepal CO-630 indicates resistance to brittle fracture in a highly wetting environment, but the value is comparative only. Laboratory ESCR cannot be substituted for full-scale container testing under transport-of-dangerous-goods rules such as UN 6.1. In pipe applications, slow crack growth resistance should be assessed by ISO 13479 rather than inferred from D1693 results.
The grade’s density of 0.961 g/cm³ is high enough to provide a flexural modulus of 1350 MPa, while the molecular architecture is intended to preserve an interconnected tie-molecule population. Slow crack growth in polyethylene is controlled in part by tie-molecule disentanglement between crystalline lamellae. A broader molecular weight distribution can maintain that tie-molecule network at a given density better than a narrow-distribution metallocene-catalysed HDPE. The improvement appears in notched ESCR tests, but the magnitude depends on wetting agent, notch depth, moulded-in orientation, and processing history. Published data for this specific configuration is limited for full-scale bottle drop impact after filling with oxidising fluids; only article-level testing on the converted container can establish fitness for those service conditions.
Extrusion blow moulding of intermediate bulk container liners, 20–60 L jerry cans, agricultural chemical bottles, and extruded profile or conduit are among the conversion routes implied by the melt strength and ESCR of KBZ61Z. Sheet extrusion can be run with barrel temperatures of 200–230 °C, die temperature of 230–245 °C, and cooling-roll temperatures of 60–90 °C. Lower roll temperatures increase crystallinity and short-term modulus but may increase frozen-in stress and reduce ESCR. For thin-wall articles below 0.8 mm, the low melt flow rate restricts drawdown; a higher-flow HDPE should be selected if the design cannot be adjusted to tolerate shorter parison extensions. Injection moulding of large structural parts is possible only with generous gate dimensions and sufficient clamp force, because the grade does not flow like a conventional high-flow injection resin.
Substituting KBZ61Z into tooling designed for a high-flow HDPE requires re-validation of feed system, gate freeze time, wall thickness, and injection pressure. The melt flow rate of 0.60 g/10 min is outside the typical 4–10 g/10 min injection HDPE window, and spiral flow will be shorter under identical melt temperature and injection speed. Table 2 compares KBZ61Z with a generic unimodal HDPE reference class; the reference is not a specification for any single commercial product.
| Property | HDPE KBZ61Z | Generic unimodal HDPE reference |
|---|---|---|
| Melt flow rate, 190 °C/2.16 kg | 0.60 g/10 min | 5.0 g/10 min |
| Density | 0.961 g/cm³ | 0.958 g/cm³ |
| Flexural modulus | 1350 MPa | 1200 MPa |
| ESCR, ASTM D1693/B, F50 | >1000 h | 30 h |
| Vicat softening temperature, A120 | 127 °C | 124 °C |
The comparison indicates that KBZ61Z should be selected when ESCR and stiffness dominate the design, not when cycle time or thin-wall fill is the primary constraint. The difference in melt flow rate also means that colour dispersion and additive mixing require more attention. If masterbatches are added above 2 wt%, dispersion should be checked by cross-section microscopy because agglomerates can act as stress concentrators and reduce ESCR. For continuous production, batch-to-batch variation in melt flow rate is typically narrower than ±0.05 g/10 min when pellets are stored in unopened packaging, but converters should still record extruder amps and melt pressure per lot.
Storage and compliance boundaries are part of the operational specification. Pellets stored above 60% RH may develop surface condensation. If wet, a dry-air hopper treatment at 70–80 °C with a dew point below −20 °C for 2 h removes moisture before extrusion. The natural grade is not automatically food-contact compliant. Compliance with FDA 21 CFR 177.1520(c), EU Regulation No 10/2011, REACH SVHC restrictions, and RoHS Recast 2011/65/EU must be confirmed from the supplier’s written declaration for the specific additive package and colour masterbatch. Outdoor weatherability is not provided by the base resin unless carbon black or an approved UV stabilizer package is included. Uncontrolled blending with free-radical initiators or peroxide concentrates should be avoided, because peroxide residues can crosslink HDPE and shift melt flow rate, gel content, and surface quality. Purging after shutdown with LLDPE reduces carbonised deposit formation in the die.