Tpc Japan Hdpe Kby47c

TPC (Japan) HDPE KBY47C

    • Product Name: TPC (Japan) HDPE KBY47C
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 193228
    Density 0.947 g/cm³
    Meltflowrate 0.8 g/10 min
    Tensilestrengthatyield 25 MPa
    Tensileelongationatbreak ≥500%
    Flexuralmodulus 1.00 GPa
    Notchedizodimpactstrength 0.400 ft·lb/in
    Shoredhardness 60
    Vicatsofteningtemperature 124 °C
    Heatdeflectiontemperatureat1 8mpa 43 °C
    Moldshrinkage 0.020 cm/cm

    As an accredited TPC (Japan) HDPE KBY47C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KBY47C packaging: 25 kg PE-lined woven bags; 1,000 kg per pallet; 20 MT per 20' container.
    Container Loading (20′ FCL) 20-foot FCL container fully loaded with TPC Japan HDPE KBY47C resin bags, palletized, shrink-wrapped, and secured for ocean freight transport.
    Shipping TPC (Japan) HDPE KBY47C is a non-hazardous high-density polyethylene resin. It is shipped palletized in 25 kg bags or 1000 kg jumbo bags within dry containers. Store cool, dry, ventilated, away from heat, sunlight, and moisture. Not classified as dangerous goods; no special transport requirements.
    Storage Store TPC (Japan) HDPE KBY47C in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Use pallets, avoid stacking damage, and rotate stock. Protect from prolonged UV exposure and extreme temperatures. Follow manufacturer guidelines and local regulations. Keep area clean.
    Shelf Life TPC (Japan) HDPE KBY47C shelf life: 24 months when stored unopened in original packaging, cool, dry, ventilated, away from sunlight.
    Application of TPC (Japan) HDPE KBY47C

    On high-cavitation stack molds producing 150–250 ml injection-molded dairy cups, the first processing constraint appears at the hot runner, not at the injection screw. TPC (Japan) HDPE KBY47C is run at a melt temperature of 210–230 °C and a mold temperature of 8–15 °C. Higher melt temperatures reduce fill pressure but extend cycle time and increase the risk of flash on thin-walled cores. The screw should have an L/D of 22:1 and a compression ratio of 2.5:1, with a check ring clearance not exceeding 0.05 mm. Injection pressure is typically held between 80 MPa and 120 MPa, with switch-over at 95–98 % of shot volume and holding pressure decayed over 3–5 s. The formulation is 100 parts KBY47C, 10–20 % post-industrial regrind from the same production line, and 3–5 % white TiO₂ masterbatch. If a nucleating masterbatch is used, its addition is limited to 0.05–0.15 wt% because higher levels raise flexural modulus above 1100 MPa under ISO 178:2019 but lower notched Izod impact below 4 kJ/m² under ISO 180:2019, a property cliff-edge for stackable dairy tubs. Food-contact compliance is tied to FDA 21 CFR 177.1520, Commission Regulation (EU) No 10/2011 Annex I with overall migration below 10 mg/dm², and GB 4806.6-2016. The terminal articles are printed or unprinted dairy cups and overcaps with brim wall thickness of 0.45–0.70 mm, demolded by robotic side-entry end-of-arm tooling and palletized in polyethylene sleeves.

    What Governs Brim-Fill Weight Stability in Carbonated Beverage Closures?

    Closure molding in 48- or 72-cavity hot runner tools places a different demand on melt homogeneity. KBY47C is compounded with 0.05–0.10 wt% primary antioxidant, 0.05–0.10 wt% acid scavenger, and 0.5–1.5 % color masterbatch. Slip additives are avoided in the closure skirt unless the filling line confirms torque retention on PCO 1881 neck finishes. The melt temperature window for closures is 200–230 °C, with the hot runner manifold set to the lower half of this range to limit polymer degradation during extended run interruptions. Mold temperature is controlled at 10–20 °C to achieve dimensional stability of the annular valve seat. Screw recovery speed is limited to 80–120 rpm for a 22:1 L/D screw because excessive shear at the check ring creates low-molecular-weight fractions that reduce stress cracking resistance. Batch-to-batch melt flow rate is checked under ISO 1133-1:2022 at 190 °C under 2.16 kg; a lot-to-lot shift above 0.5 g/10 min changes fill time and closure weight. The relevant test methods for closure shelf performance are ASTM D1693-15 for environmental stress cracking resistance, ISO 178:2019 for flexural modulus, and dimensional checks against PCO 1881 or BPF 30/25. Brim fill weight tolerance is typically set at ±0.15 g on a 30 g closure. The terminal product is a tamper-evident beverage closure with a breakaway bridge thickness of 0.25–0.35 mm, produced under FDA 21 CFR 177.1520 and EU Regulation No 10/2011.

    Stackable Crate Geometry, Shut-Off Nozzle Settings, and Warpage Compensation

    For high-shot-weight stackable crates above 800 g, the dominant failure modes are corner cracking and shrinkage-induced diagonal warpage. KBY47C is run at a melt temperature of 230–250 °C and a mold temperature of 15–30 °C. The higher mold temperature is used on the base plate to reduce differential shrinkage between the open grid and solid corner bosses. Fill speed is profiled with an initial fast advance to 60–70 % of shot volume, followed by a controlled packing stage at 50–70 MPa for 8–12 s. The injection unit should have a plasticizing capacity at least 10 % above the shot weight plus runner volume, and the clamp force is selected at 0.5–0.7 kN/cm² of projected area. The formulation is 100 parts KBY47C, 20–30 % in-house regrind from the same crate line, 3–6 % masterbatch for grey or green logistics colors, and 0.15–0.30 wt% high-molecular-weight HALS UV stabilizer for outdoor returnable transport packaging. No external mold release is used because it creates a low-energy surface that reduces inter-stacking friction and promotes load shifting. Compliance is evaluated through ISO 8611-1:2011 for flat pallet substitutes, and through ASTM D648-16 for heat deflection temperature under 0.455 MPa; the representative HDPE range is 65–75 °C. Published data for this specific crate configuration is limited, so pre-production trials typically include a 72 h load-holding test at 40 °C with a static load of 250 kg on a column stack. The terminal article is a stackable, nestable distribution crate with a side-wall vent area of 20–35 % and a base load rating of 300 kg in dry storage.

    For open-head pails carrying UN-certified liquid hazardous goods, injection molding of the pail body produces a weld line at the gate that must survive drop testing at -18 °C after conditioning for 24 h. TPC (Japan) HDPE KBY47C is processed at 210–240 °C melt temperature and 10–20 °C mold temperature. The gate is located in the base corner or on the side wall opposite the handle ears, and the tool is run with sequential valve gating only when weld line location must be shifted away from the sealing lip. The formulation is 100 parts KBY47C, 10–25 % post-industrial regrind from the same UN type-tested article, 2–4 % carbon black or color masterbatch, and 0.2–0.4 wt% antioxidant package. If the pail is used for food-adjacent dry goods, the masterbatch must be selected from positive lists under EU Regulation No 10/2011 or FDA 21 CFR 177.1520. The sealing area of the open-head lid requires a continuous elastomeric gasket groove with a flange wall thickness of 2.0–3.0 mm. Under-tolerance in this area causes closure failure during UN internal pressure testing, while over-tolerance increases demolding stress and reduces drop height performance. The relevant qualification tests are the UN Model Regulations pressure test, stacking test, and drop test. For a 20 L pail in Packing Group II, the drop height is typically 1.2 m at -18 °C; for Packing Group I, the drop height is 1.8 m. A type test cannot be transferred to a different pail wall thickness or regrind fraction without re-testing. The terminal article is a UN-marked open-head pail with wire or plastic handle, lid with tamper-evident tear tab, and a gasket seat meeting the closure dimensions specified by the original type test certificate.

    Qualification testReferenced codeCondition
    Drop testUN Model Regulations, Chapter 6.1-18 °C, 24 h conditioning
    Stacking testUN Model Regulations40 °C storage
    Internal pressure testUN Model Regulationsambient, gasket seated

    When Vented Agricultural Crates Enter Cold Chain Interplant Logistics

    Agricultural distribution crates that move from packhouse to cold store impose a thermal shock condition on the material rather than a steady-state load. KBY47C is molded with a melt temperature of 220–250 °C and a mold temperature of 8–15 °C to retain part stiffness. Post-mold conditioning at 5 °C for 2 h is used before dimensional audit. The formulation is 100 parts KBY47C, 3–5 % green or blue masterbatch, 0.2–0.4 wt% UV stabilizer masterbatch, and 5–15 % regrind only from UV-stabilized preforms. Non-UV-stabilized regrind is excluded because it creates surface microcracking after 12–18 months of solar exposure. The side wall vent slots are designed with radiused ends of 1.0–2.0 mm, not sharp corners, because the localized stress at a sharp slot end under cold impact reduces notched Charpy impact below 3 kJ/m² at 5 °C under ISO 179-1:2010. Food-contact compliance for unpacked produce is assessed under Commission Regulation (EU) No 10/2011 Annex I, and repeated-use transport packaging is subject to the general safety documentation requirements of EU 2023/988. The terminal article is a vented stack/nest crate with slot area of 15–30 % of side-wall surface and a column stacking capacity of 200 kg under 5 °C cold store conditions.

    Injection molding of nesting storage bins with wall thicknesses between 1.8 mm and 2.5 mm requires a fluidity band that balances flatness and drop strength. KBY47C is processed at a melt temperature of 220–250 °C, a mold temperature of 10–30 °C, and a back pressure of 5–10 bar. The screw should have a low-shear mixing section and a shut-off nozzle to prevent drool during open mold periods. The formulation is 100 parts KBY47C, 3–6 % color masterbatch, 10–20 % clean in-house regrind, and 0.1–0.3 wt% antistatic additive when the article is destined for electronics storage. Antistatic packages are qualified under IEC 61340-5-1 dissipative packaging requirements. Ethoxylated amine antistatic packages are excluded above 0.1 wt% because they discolor the melt during long runs at 230 °C. No pre-drying is required unless surface condensation is present; if hopper residence exceeds 4 h at RH > 60 %, a dry-air hopper at 60 °C for 2 h is used. The housing and latch hinges must be gated at the hinge axis with a gate land of 0.8–1.2 mm to avoid molecular orientation perpendicular to the flexing axis. Dimensional stability is checked after 48 h at 23 °C and 50 % RH. Warpage exceeding 1.0 mm across a 400 mm side wall is rejected. The terminal product is a nestable household storage bin with living hinge lid, rated for a top load of 20 kg and expected to withstand 3 drops from 1.0 m at ambient temperature without hinge failure.

    Free Quote

    Competitive TPC (Japan) HDPE KBY47C prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KBY47C is a high-density polyethylene resin identified by the grade designation KBY47C and supplied for extrusion-grade and blow-moulding procurement streams. The material belongs to the high-density polyethylene class because its density is expected to fall at or above 0.941 g/cm³ under ISO 1183-1:2019. Published data for this specific configuration is limited; therefore, the property envelope discussed below is drawn from the high-density polyethylene extrusion and blow-moulding class, and lot-specific values must be confirmed on the producer’s certificate of analysis before die design or process validation.

    The grade designation KBY47C appears in technical procurement documentation for rigid packaging, small-part blow moulding, and industrial sheet where melt strength and environmental stress crack resistance are given more weight than melt flow. In the absence of a public ISO data sheet for the exact KBY47C grade, comparable extrusion-blow HDPE resins typically exhibit a melt mass-flow rate of 0.2 g/10 min to 0.8 g/10 min when tested under ISO 1133-1:2022 at 190 °C and 2.16 kg, and a density of 0.945 g/cm³ to 0.955 g/cm³ under ISO 1183-1:2019. These ranges are classifiers, not certified specifications for KBY47C. The supplier’s technical datasheet should be referenced for exact density, melt mass-flow rate, tensile yield strength, flexural modulus, and environmental stress crack resistance.

    Production-scale extrusion blow-moulding lines processing HDPE resins in the 0.2–0.8 g/10 min MFR band are typically run on grooved-feed single-screw extruders with a 24:1 to 30:1 L/D ratio. Barrel zone set points from feed to metering are commonly staged from 170 °C to 200 °C; melt temperature at the die entry is maintained at or below 210 °C to limit molecular weight degradation. On accumulator-head blow moulding machines, a reduction in parison hang time at constant extrusion rate usually indicates a lower-viscosity lot or overheating. Die swell variation exceeding ±5% across a shift is typically traced to melt-temperature drift, screen-pack blockage, or regrind ratio changes.

    For container applications, wall-thickness uniformity depends on parison programming. With HDPE grades of this melt strength, an increase in melt temperature of 5 °C above the validated set point can lower parison length stability and create thin corners at the pinch-off. A melt temperature 10 °C below the validated window may elevate melt viscosity enough to cause weld-line tearing at the die pin. The processing window is therefore treated as a narrow band, not a broad operating range. In sheet extrusion, chill-roll temperatures between 60 °C and 90 °C are commonly used to control dimensional stability; higher roll temperatures reduce surface gloss but improve relaxation and lower frozen-in stress. Published data for this specific configuration is limited, and processors should establish a start-up procedure from the supplier’s lot certificate.

    Molecular weight distribution governs die swell and melt fracture behaviour. A broader distribution increases die swell and parison hang strength but can produce rougher surfaces at low shear rates; a narrower distribution improves surface finish and dimensional repeatability but lowers sag resistance. The exact distribution for KBY47C is not publicly reported. Capillary rheometry according to ISO 11443 at 190 °C and 210 °C over shear rates from 100 s⁻¹ to 5000 s⁻¹ is recommended to obtain the shear viscosity curve for tool design. Without this curve, die gap and parison programmer settings remain empirical and can require multiple start-up trials.

    What specification limits require verification before substituting KBY47C for a general-purpose HDPE?

    Substitution reviews compare the candidate resin against the incumbent grade using standardized tests. For HDPE, density is tested under ISO 1183-1:2019, and melt mass-flow rate under ISO 1133-1:2022. Tensile yield strength is commonly evaluated as ISO 527-1:2019 or ASTM D638-14; flexural modulus under ISO 178:2019; Charpy impact strength under ISO 179-1. Environmental stress crack resistance is evaluated under ASTM D1693-15 or ISO 22088-2, and Vicat softening point under ISO 306. Food-contact eligibility is usually verified against FDA 21 CFR 177.1520 and the relevant European Commission regulation for food-contact plastics. REACH and heavy-metal restrictions are supply-chain declarations rather than resin test data.

    Test methodPropertySubstitution review role
    ISO 1183-1:2019DensityConfirms HDPE classification and affects stiffness and barrier
    ISO 1133-1:2022Melt mass-flow rateDetermines flow class and process compatibility
    ISO 527-1:2019Tensile yield strengthChecks short-term load-bearing capacity
    ISO 178:2019Flexural modulusCompares rigidity and part deflection
    ISO 179-1Charpy impact strengthEvaluates notched impact tolerance at low temperature
    ASTM D1693-15Environmental stress crack resistanceRanks resistance to surface-active agents and stress cracking
    ISO 306Vicat softening temperatureChecks short-term thermal resistance
    FDA 21 CFR 177.1520Food-contact eligibilityVerifies olefin polymer suitability for food contact

    During substitution, a single-point comparison is insufficient. Process capability requires that the melt mass-flow rate and density maintain a process capability index Cpk of at least 1.33 across multiple lots when evaluated under ISO 1133-1:2022 and ISO 1183-1:2019. A lower Cpk indicates excessive lot-to-lot variation that will drift die swell and parison weight. If the incumbent grade holds Cpk above 1.67, the candidate grade should meet or exceed the same capability before conversion.

    Compared with general-purpose injection-moulding HDPE grades, an extrusion-blow candidate such as KBY47C is likely to show a lower melt mass-flow rate and a higher molecular weight. The practical consequence is higher melt strength and greater parison stability in blow moulding, but longer flow lengths and higher injection pressures in injection tools. Compared with high-density film grades, the higher density reduces gas and moisture permeability but may reduce dart drop impact and tear resistance. Against bimodal pipe grades such as those qualified under ISO 4427, an extrusion-blow resin is not usually evaluated for long-term hydrostatic strength at 20 °C and 80 °C; pressure-pipe substitution is not recommended unless the manufacturer has specifically certified the resin for pressure-pipe service.

    When KBY47C Replaces Injection-Moulding HDPE in Thick-Walled or Short-Run Tooling

    If the KBY47C melt mass-flow rate is at the low end of the extrusion range, direct replacement of an injection-moulding HDPE with an MFR of 4 g/10 min to 20 g/10 min is process-limited. On a standard injection moulding machine with a 120-ton clamp force and a 25 mm diameter general-purpose screw, thick-walled caps or plugs may require injection pressures above 90 MPa sustained through hold time. Thin-walled parts below 1 mm nominal wall are usually impractical because the melt freezes in the gate and flow-front hesitation produces visible knit lines. If the machine is equipped with a hot runner and valve gate, the gate diameter must be increased by at least 30% relative to high-flow HDPE to avoid excessive shear heating and gate freeze-off.

    Processing temperatures for low-MFR HDPE in injection moulding are often set from 200 °C to 240 °C. At temperatures above 250 °C, oxidation can create carbonyl species that shift colour and reduce notched impact strength. Screw speed must be adjusted to maintain a melt residence time below 10 min; longer residence times degrade molecular weight and erase the melt-strength advantage. Mould temperature for HDPE is typically set from 10 °C to 40 °C. Higher mould temperatures improve surface appearance and reduce frozen-in stress but increase cycle time. Packing pressure should be maintained until gate seal; for thick-walled parts, gate seal time can exceed 10 s depending on part mass. These constraints are derived from general HDPE injection-moulding practice, and the producer’s technical datasheet should be consulted for the exact KBY47C temperature profile.

    Environmental stress crack resistance is highly dependent on density, comonomer type, and cooling rate. The bent-strip test described in ASTM D1693-15 provides a comparative ranking but can show scatter exceeding 100% between replicates when specimen preparation, notch depth, or bath temperature deviates from the standard. For HDPE containers, ESCR failures generally appear at the pinch-off or under sharp geometric transitions. A candidate grade with lower density within the HDPE range, produced with a 1-butene or 1-hexene comonomer, typically offers higher ESCR than a homopolymer of equal density. Published data for this specific configuration is limited; for chemical resistance with the intended contents, immersion testing at 40 °C and 60 °C for 28 days is recommended because short-term exposure at ambient temperature does not predict stress-crack development in constrained seams.

    The stress-cracking mechanism involves localised yielding at surface flaws under a tensile stress below the macroscopic yield point. The active environment reduces the energy required for craze fibrillation and crack propagation. In blow-moulded containers, the pinch-off region is particularly susceptible because it contains a cold weld line and residual stress. Mould design that increases pinch-off flash angle and reduces sharp internal radii can improve service life more effectively than an increase in density.

    Contact with polar organic solvents, strong oxidizing acids, or long-chain hydrocarbon oils can reduce environmental stress crack resistance. Stress-cracking agents such as nonylphenol ethoxylates, silicone oils, and certain quaternary ammonium compounds can produce brittle failures at applied strains well below the yield point. HDPE grades are generally resistant to aqueous salt solutions and dilute mineral acids, but resistance to aggressive process fluids should not be assumed from density alone. Incompatible polymer contamination, such as PET, PVC, or polycarbonate in regrind, can cause delamination and gas holes during extrusion.

    Material Handling, Regrind Effects, and Moisture Condensation Limits

    HDPE resins do not require pre-drying under normal storage conditions. However, condensation on pellet surfaces at relative humidity above 60% can introduce surface defects in blow moulding and sheet. If surface moisture is present, drying at 80 °C for 2 h to 4 h with a desiccant or hot-air dryer is sufficient to remove free water without altering the additive package. Pellets should be stored in sealed hoppers or bins when ambient dew point exceeds the pellet temperature.

    Outdoor storage of HDPE in unsealed octabins can increase the risk of moisture condensation and surface contamination. If pellets are exposed to dust, the dust can act as a filler and reduce tensile strength. Metal contamination from conveying lines can be detected with ferrous and non-ferrous separators; a magnetic trap upstream of the feed throat should have a flux density of at least 800 mT to remove fine ferrous particles. Non-ferrous contamination requires an induction separator.

    Regrind ratios above 30% can shift melt flow and reduce impact strength unless the regrind is free of contamination and thermally degraded material. Production trials should include regrind from the same lot to avoid batch-to-batch variation. The use of colour masterbatch or additive masterbatch above 5% can modify melt viscosity and ESCR; the processor should verify compatibility through a pilot run before full-scale production. Each process change should be revalidated against the user’s acceptance criteria before full-scale release.

    Top