Tpc Japan Hdpe Kbx74a

TPC (Japan) HDPE KBX74A

    • Product Name: TPC (Japan) HDPE KBX74A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 695829
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.04 g/10 min
    Tensile Strength At Yield 28 MPa
    Tensile Strength At Break 34 MPa
    Elongation At Break 600%
    Flexural Modulus 1.2 GPa
    Izod Impact Strength Notched 0.4 J/cm
    Vicat Softening Point 124 °C
    Melting Point 134 °C
    Hardness Shore D 65
    Environmental Stress Crack Resistance >1000 h
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Specific Heat 1.9 J/g·°C
    Thermal Conductivity 0.45 W/m·K
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >1E16 Ω·cm

    As an accredited TPC (Japan) HDPE KBX74A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KBX74A is packed in 25 kg bags, 40 bags per 1,000 kg pallet, shrink-wrapped for export.
    Container Loading (20′ FCL) 20′ FCL loading of TPC Japan HDPE KBX74A: 25 kg bags, palletized, dry container, secure stowage, standard weight, proper documentation.
    Shipping TPC (Japan) HDPE KBX74A is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped, in dry containers. No special UN hazard class required. Store cool, dry, away from direct sunlight and ignition sources.
    Storage Store TPC (Japan) HDPE KBX74A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and moisture. Keep original bags or containers sealed, palletized, and protected from dust and contamination. Avoid contact with oxidizers, acids, bases, and solvents. Do not overstack; prevent static buildup. Store separately from incompatible materials. Follow the manufacturer’s SDS and local storage regulations.
    Shelf Life Shelf life is 24 months if stored in original packaging in a cool, dry, well-ventilated area away from direct sunlight.
    Application of TPC (Japan) HDPE KBX74A

    TPC (Japan) HDPE KBX74A is a high-density polyethylene extrusion blow-molding resin with a nominal density of 0.955 g/cm³ and a melt flow rate of 0.30 g/10 min at 190 °C/2.16 kg (ISO 1133-1). The grade provides high melt strength, controlled die swell, and environmental stress crack resistance for monolayer and multilayer rigid packaging. It is specified for extrusion blow molding, not for cast film or thin-wall injection molding. The applications below treat the resin as a virgin layer; regrind, masterbatch, and surface treatment must be revalidated against the target regulation before commercial production.

    ApplicationMelt temperature (°C)Mold temperature (°C)Regrind allowanceCritical test or regulation
    Pharmaceutical solid-dose containers180–20510–150% in contact layerUSP 661.1, Ph. Eur. 3.1.3
    UN 3H1 jerry cans185–20515–25≤30% plant scrapUN Chapter 6.1
    Laundry detergent bottles180–19512–20≤20% regrindASTM D1693 condition B
    Food and dairy bottles190–2058–120% post-consumerEU 10/2011, OM <10 mg/dm²
    Personal care bottles180–20015–20≤10% own scrapHeadspace GC-MS, corona <46 mN/m
    Agrochemical barrier packs180–20010–18≤20% plant scrapFluorine barrier, ASTM D2565

    Extrusion Blow Molding of Solid-Dose Pharmaceutical Containers

    On a 24:1 L/D shuttle blow molder with a compression ratio of 2.5:1–3.5:1, pharmaceutical container production from KBX74A is constrained by the low melt flow rate and the requirement for zero visible gel specks. The melt temperature is held between 180 °C and 205 °C; barrel zones increase from 160 °C at the feed throat to 195 °C at the die head. A deviation above 210 °C initiates oxidation-induced gel formation in the bottle wall. Under pharmacopoeial visual inspection, these gels are cause for rejection. Mold cooling water at 10–15 °C is applied to the shoulder, neck, and pinch-off zones. Cycle time for 60–250 mL bottles on shuttle machines is typically 8–12 s. The formulation is 100% virgin KBX74A. Plant scrap is excluded from the patient-contacting layer under GMP segregation rules. Antioxidant and acid-neutralizing additives in the resin are assessed against USP 661.1 and Ph. Eur. 3.1.3. No slip agent, antistatic agent, or animal-derived processing aid is added at the converter stage. Terminal products include tablet bottles with child-resistant PP closures, desiccant pack bottles, and ophthalmic screw-neck bottles. The pinch-off weld is the limiting mechanical zone; a validated weld thickness of not less than 0.45 mm is commonly specified to pass filled-pack drop tests at 1.2 m.

    Compliance documentation for this segment includes FDA 21 CFR 177.1520 for olefin polymers, EU Regulation 10/2011 where the container is supplied as a food-contact style pack, and USP 661.1 with Ph. Eur. 3.1.3 for medicinal use. Extractables screening uses purified water, pH 3.5 acetate buffer, and 10% ethanol as simulants at 40 °C for 10 days. Batch-to-batch control of melt flow rate within ±0.03 g/10 min and density within ±0.002 g/cm³ is required to prevent parison sag variation that would shift shoulder wall distribution and alter drop-test performance.

    Accumulator-head extrusion blow molding machines with clamp force of 250–450 kN and screw L/D of 24:1–30:1 are used for 10 L, 20 L, and 30 L UN 3H1-rated narrow-neck jerry cans conforming to UN Model Regulations Chapter 6.1. The melt is processed at 185–205 °C. Die swell of 30–50% is compensated by a die pin diameter smaller than the final neck diameter. Parison programming thickens the top chime, bottom edge, and handle area because hydraulic failure during stacking generally initiates in these zones. The 0.955 g/cm³ density provides top-load stiffness. Minimum wall at the pinch-off weld and handle bridge is 1.0–1.2 mm in most 20 L designs. For Packing Group II liquids, the UN drop test is performed from 1.2 m and the hydraulic pressure test at 100 kPa for 5 min on identical production specimens. Regrind from the same jerry can line may be introduced up to 30 wt% if the melt flow rate of the blend remains within ±0.05 g/10 min of the virgin value and the ESCR result remains above the certified limit. Outdoor storage of jerry cans for water treatment chemicals, light acids, and detergent intermediates often uses 2.0–2.5 wt% carbon black masterbatch; carbon black addition can reduce the ESCR margin and requires UN re-certification if the masterbatch carrier resin changes. Surface fluorination is applied to jerry cans that contain aromatic solvents. Inline fluorination uses dilute F2/N2 mixtures at fluorine concentration below 2 vol% and treatment times of 10–60 s. Terminal goods include UN-certified 20 L jerry cans for methyl ethyl ketone, acetic acid, potassium hydroxide 45%, and blended surfactant intermediates.

    The operational boundary is oxidative liquid packaging. Monolayer KBX74A is not specified for fuming nitric acid, bromine, or concentrated hydrogen peroxide above 30% because oxidative chain scission accelerates rapidly. Compatibility is confirmed by immersion in the actual chemical at 40 °C for 21 days with acceptance of ≤0.5% weight change and no visible stress cracking in the pinch-off weld. Published data for aggressive oxidizer configurations is limited; case-specific testing is required before commercial packaging.

    What Limit Does Environmental Stress Crack Resistance Place on Laundry Detergent Bottles?

    Laundry detergent, fabric softener, and hard-surface cleaner bottles represent the highest ESCR demand among household chemical containers. The incoming resin is evaluated by ASTM D1693 condition B, using 100% Igepal CO-630 at 50 °C. Converters often set an acceptance value of F50 ≥60 h for monolayer detergent packaging. The melt temperature is intentionally kept at 180–195 °C to preserve the high molecular weight tail that governs slow crack growth. Operation above 210 °C can reduce F50 by 10–30% depending on residence time and screw shear. Screw speed and back pressure are therefore limited to control viscous heat generation. White or pastel bottle formulation comprises 96–98 wt% KBX74A and 2–4 wt% titanium dioxide or color masterbatch. The masterbatch carrier must be HDPE-based, and its melt flow rate must be within one decade of the base resin to avoid dispersion defects. Handleware bottles from 1 L to 5 L are produced on shuttle or wheel machines with parison length up to 600 mm. The pinch-off knife is maintained at 25–40 °C to avoid a brittle weld line. Terminal products include 2 L laundry detergent bottles with snap-in dosing caps, 1 L fabric softener handleware, and 750 mL trigger-spray bottles. The handle-opening shoulder is a frequent failure initiation point; wall thickness in this zone is kept at ≥0.8 mm to sustain drop testing from 0.8–1.2 m.

    Bottles for sodium hypochlorite bleach at 6–8% active chlorine are not recommended for monolayer KBX74A without an internal polyolefin barrier or a separately stabilized layer. Hypochlorite causes surface oxidation and progressive loss of impact strength. Where such products are packaged, KBX74A may be used as the outer structural layer in a three-layer coextrusion with an inner virgin HDPE layer carrying a higher antioxidant package. Compatibility data for the specific hypochlorite formulation and wall structure must be generated before release.

    In refrigerated dairy and edible oil packaging, monolayer food-contact bottles made from KBX74A are used for pasteurized milk, edible oil, and fruit juices where oxygen ingress is not the primary shelf-life limiting factor. The resin base must comply with FDA 21 CFR 177.1520 and EU Regulation 10/2011. Overall migration into food simulants must not exceed 10 mg/dm². Specific migration of any listed additive must remain within the SML assigned in EU Regulation 10/2011 Annex I. Converter-controlled formulation for white dairy bottles generally comprises 92–96 wt% KBX74A, 3–6 wt% white titanium dioxide masterbatch, and 0–1 wt% process lubricant. Post-consumer recycled material is prohibited in the food-contact layer unless the recyclate is from an EU-approved process under Regulation (EC) 282/2008 or equivalent FDA no-objection. Blow molder settings use a melt temperature of 190–205 °C and mold water at 8–12 °C. The bottle wall has high surface gloss but limited oxygen barrier; ESL milk shelf life is typically 7–14 days under refrigeration, depending on bottle wall thickness and cap fit. Cold drop impact at 2–4 °C is a critical test because HDPE stiffens at low temperature; filled 1 L bottles are expected to pass drops from 1.0 m without wall rupture. Terminal goods include 500 mL and 1 L milk bottles, 1 L edible oil bottles, and 750 mL refrigerated juice bottles with aluminum foil induction seals. The base pinch-off tail length is controlled to 2–4 mm to avoid interference with the induction seal area. Hot filling above 70 °C is not recommended due to HDPE softening; prolonged exposure at 85 °C can cause wall deformation and cap seal failure.

    When High Gloss and Low Odor in Personal Care Packaging Are Non-Negotiable

    For personal care and cosmetic bottle manufacturing, surface gloss and low odor are treated as mechanical and sensory specification limits. KBX74A is processed on continuous extrusion blow molding equipment with high-polish mold cavities having surface finish Ra <0.4 µm. Mold temperature is kept at 15–20 °C to achieve gloss without condensation defects. The melt is processed at 180–200 °C; higher temperatures increase aldehyde and oxidative odor compounds that are unacceptable in leave-on cosmetic packaging. Colorant masterbatch loadings of 1–3 wt% are typical. Pearlescent and metallic pigments require additional mixing elements in the screw and a longer transition zone to prevent streaks. The resin ESCR under ASTM D1693 condition B is sufficient for 200–500 mL bottles containing hydroalcoholic toners, shampoo, and body wash. Formulations with ethanol above 30 vol% may require fluorination or an EVOH inner layer to prevent panel cracking and perfume loss. Post-molding surface treatment for label adhesion is by corona discharge at 38–42 mN/m wetting tension. Values above 46 mN/m can create micro-cracks that lower environmental stress crack resistance on the shoulder. Terminal products include 250 mL shampoo bottles with PP pump heads, 200 mL lotion bottles with snap-in dispensing caps, and 400 mL body wash handleware. Neck finish diameter is controlled to ±0.15 mm to maintain cap torque retention and prevent leakage under top load of 150–250 N.

    Low-odor validation is performed by headspace GC-MS screening for 2,4-di-tert-butyl-phenol, alkanes, and other resin-derived volatiles. Converter acceptance limits for total alkanes are often set below 10 µg/g of polymer. A nitrogen blanket on the hopper throat suppresses melt oxidation during extended runs. Plant scrap from the same cosmetic bottle line may be reintroduced at 10 wt% maximum where lot traceability and odor reproducibility are demonstrated.

    Agrochemical Barrier Packaging and Fluorination Boundaries

    Agrochemical emulsifiable concentrate packs in xylene, cyclohexanone, and heavy aromatic solvent systems require one of the highest barrier levels among HDPE packaging. Monolayer KBX74A alone is generally insufficient for 1 L and 5 L containers; inline fluorination of the inner surface or coextrusion with PA/EVOH is specified. The fluorination process uses a dilute fluorine-in-nitrogen gas mixture during extrusion blow molding. The fluorinated layer thickness is in the range of 50–150 nm, reducing solvent weight loss to below 0.5% per year at 23 °C for many aromatic formulations. This barrier layer also improves paneling resistance. A typical three-layer coextrusion uses 70–80 wt% KBX74A as outer and core layers, with 5–10 wt% adhesive and 5–10 wt% PA or EVOH barrier. Process temperatures for the HDPE layer remain between 180–200 °C, while the coextrusion die is kept below 220 °C to avoid degradation of the tie resin and barrier polymer. Terminal goods include 1 L fluorinated HDPE bottles for 2,4-D ester formulations, 5 L agrochemical jugs with child-resistant caps, and 10 L agricultural chemical containers. The closure area is a critical leak point; neck wall is thickened to 1.2–1.5 mm to maintain seal under top load and chemical swell.

    The UV exposure boundary is significant. Unpigmented KBX74A bottles stored outdoors show surface chalking and impact loss after 12–24 months. For outdoor agrochemical applications, a UV-stabilized masterbatch containing 0.3–0.8 wt% hindered amine light stabilizer is added. Accelerated weathering is evaluated under ASTM D2565 xenon-arc exposure; the specific dosage is formulation-dependent and must be validated for the end-use container.

    Free Quote

    Competitive TPC (Japan) HDPE KBX74A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Selection of an extrusion blow-moulding HDPE for large hollow parts is governed by the interaction of melt strength, die swell, environmental stress crack resistance, and impact behaviour. TPC (Japan) HDPE KBX74A is a high-molecular-weight high-density polyethylene grade supplied as natural pellets; the grade is intended for blown containers and technical hollow parts that require a balance of stiffness, low-temperature impact and long-term resistance to surface-active fluids. Supplier-published typical values identify a density of 0.947 g/cm³ (ASTM D1505 / ISO 1183-1) and a melt flow rate of 0.30 g/10 min at 190°C/2.16 kg (ASTM D1238 / ISO 1133-1). The high-load melt flow index at 190°C/21.6 kg is used on production floors as a better indicator of parison hang time; published data for this specific configuration is limited, so plant trials should verify the ratio against an in-house baseline HMW-HDPE rather than relying on a single supplier figure. The product is differentiated from commodity bottle grades by lower melt flow, higher molecular weight, and higher notched Izod impact; it is differentiated from pipe grades by its blow-moulding-specific stabilizer package and melt-strength profile.

    What measured values separate KBX74A from lower-molecular-weight blow-moulding grades?

    Physical property comparisons are only meaningful when specimen conditioning follows the same standard. The following table consolidates supplier-published typical values for natural, unfilled KBX74A using standard test methods. These values are not batch certificates; extrusion plants should request a certificate of analysis for each lot and normalize incoming quality control to the same methods.

    PropertyMethodTypical value
    DensityASTM D1505 / ISO 1183-10.947 g/cm³
    Melt mass-flow rateASTM D1238 / ISO 1133-10.30 g/10 min at 190°C/2.16 kg
    Tensile stress at yieldASTM D638 / ISO 527-223 MPa
    Tensile elongation at breakASTM D638 / ISO 527-2>600%
    Flexural modulusASTM D790 / ISO 178900 MPa
    Notched Izod impact at 23°CASTM D256 / ISO 1808 kJ/m²
    Environmental stress crack resistance, 10% Igepal at 50°CASTM D1693>1000 h
    Vicat softening temperatureASTM D1525 / ISO 306125°C

    The property profile explains why the resin is not interchangeable with conventional high-flow HDPE bottle grades. A bottle-grade resin with MFR above 0.8 g/10 min may fill thin parisons at lower torque, but its lower melt strength produces sag on large accumulator-head machines and its ESCR in polar surfactants can be one to two orders of magnitude shorter. Conversely, a PE100 pipe grade is designed for hydrostatic design stress under ISO 9080; it is over-specified for blow-moulded containers and may exhibit insufficient melt strength at the same melt temperature.

    Extrusion blow moulding of KBX74A on accumulator-head machines

    Plant-level experience with HMW-HDPE blow-moulding grades indicates that barrel temperature profiles should be set below 180°C in the feed zone and raised to 200–230°C at the die head. The high molecular weight of KBX74A produces elevated torque in a smooth-bore extruder; a grooved feed section with L/D of 25:1 to 30:1 and a barrier screw with compression ratio 2.2:1–2.8:1 is recommended for stable throughput. Die gaps of 1.5–3.0 mm and diverging die tooling are used to control parison swell; excessive melt temperature above 235°C initiates oxidative degradation, visible as yellowing and gel formation, while temperatures below 190°C may produce weld lines and excessive parison sag. The processing window around the die is therefore often controlled to ±5°C on accumulator-head machines. Mould temperature is maintained at 10–30°C to freeze the outer skin rapidly and reduce post-mould shrinkage. Pre-drying is not required at ambient relative humidity below 60%; surface condensation should be removed by conveying in dry-air hoppers.

    Because HDPE KBX74A is used in packaging of aggressive liquids, resistance to slow crack growth is evaluated with ASTM D1693 or the notched constant tensile load test ISO 16770. The supplier-published ESCR for the grade is reported as >1000 h in 10% Igepal CO-630 at 50°C; such a value is characteristic of high-molecular-weight copolymers with a distinct comonomer distribution. This performance is not equivalent to chemical resistance against strong oxidizers or aromatic hydrocarbons; continuous contact with toluene, xylene or halogenated solvents at temperatures above 40°C can swell the amorphous phase and reduce service life. For packaging of hypochlorite solution, the stress-cracking resistance of the grade is sensitive to test temperature and concentration; plant trials should follow ASTM D1693 with 100% Igepal if published data for the specific configuration is limited.

    Low-temperature impact performance of HMW-HDPE is determined by the brittle-ductile transition. In notched Izod testing at −40°C, high-molecular-weight products such as KBX74A typically retain a ductile failure mode if the cooling rate during moulding is faster than 10°C/min through the crystallization window. Slow cooling produces larger spherulites and shifts the ductile-brittle transition to higher temperatures; blow moulders therefore avoid hot moulds above 30°C for impact-critical parts. Weld lines are the weakest locations in extruded parison fusion; a tail flash length below 10 mm or inadequate pinch pressure can leave a notch-like crease that reduces burst strength by up to 30% relative to the sidewall. This effect is not specific to KBX74A but is amplified in high molecular weight grades because lower melt flow delays interdiffusion across the weld interface.

    When regrind ratios exceed 30 wt% in multilayer hollow parts

    In multi-layer blow-moulded parts, regrind is generated from parison flash, start-up scrap and trim. The HMW HDPE layer can tolerate regrind levels up to 20–30 wt% in non-functional layers without collapse of ESCR, provided the regrind is free of moisture and thermally degraded gels. Beyond 30 wt%, measurements on similar HMW-HDPE grades show an increase in gel counts and a decrease in low-temperature notched impact; the exact cliff-edge for KBX74A should be determined by sieve analysis of melt-filtered regrind and by measuring ESCR after 100% regrind extrusion. If the regrind fraction must exceed 30 wt%, use screen packs of 100–120 mesh in the recycle stream and limit melt temperature to 230°C to avoid crosslinking or gel formation.

    Reliable use in food-contact or potable-water applications requires that the base polymer, additives and decomposition products be assessed under the relevant jurisdiction. The supplier states that HDPE KBX74A, as a polyolefin resin manufactured in compliance with food-contact requirements, can be used in articles conforming to FDA 21 CFR 177.1520 for olefin polymers and to European Commission Regulation (EU) No. 10/2011, provided migration testing is performed on the finished article. Because compliance is article-dependent, a resin-grade statement does not replace overall migration or specific migration testing under the intended food simulant; the responsible converter must verify that the total package meets the 10 mg/dm² overall migration limit. Under REACH Regulation (EC) No. 1907/2006, the grade is subject to registration obligations; SVHC content above 0.1% w/w must be declared. For electrical and electronic equipment, the grade is outside the direct scope of RoHS; however, black masterbatch containing carbon black does not normally contain the restricted heavy metals above the 1000 ppm threshold.

    RequirementStandard or regulationTypical limit
    EU food-contact frameworkRegulation (EU) No 10/201110 mg/dm² overall migration
    US food-contact frameworkFDA 21 CFR 177.1520Article-specific migration testing
    REACH SVHC declarationEC No 1907/20060.1% w/w
    RoHS restricted substancesDirective 2011/65/EU1000 ppm; Cd 100 ppm

    Operational boundaries and documented incompatibilities

    KBX74A is not intended for injection moulding with thin walls because the high molecular weight limits spiral flow length; injection pressures above 120 MPa may be needed even for thick parts, which can reduce machine availability on conventional hydraulic presses. The grade is also not recommended for continuous extrusion of monolayer pipe because the pressure rating and hydrostatic design basis have not been established under ISO 9080. Processing with longer residence times at melt temperatures above 240°C can form oxidized gels which are visible as pinholes after regrind; a temperature alarm interlock and purge procedure for stops longer than 10 minutes is standard. Avoid direct addition of curing agents or peroxides intended for crosslinkable PE because the resulting viscosity rise may exceed torque limits; also avoid metal-stearate packages beyond supplier recommendations when colouring at high concentrations.

    Compared to TPC’s lower-density blow-moulding grades in the same product family, KBX74A shows a higher melt viscosity and is generally selected for thick-walled containers above 5 L or for applications with long target service life. Commodity HDPE bottle grades with MFR above 0.8 g/10 min and density 0.950–0.955 g/cm³ may outperform KBX74A in short-cycle thin-wall bottle production due to lower energy consumption, but they typically fail ESCR requirements in surface-active fluids. Pipe-grade HDPE with a 50-year hydrostatic design basis under ISO 9080 is over-specified for blow-moulded containers and often lacks the melt strength required for accumulator-head parison control. The practical selection boundary is therefore not a single property but the combination of 0.30 g/10 min MFR, 0.947 g/cm³ density and >1000 h ESCR. This combination should be specified only after process capability studies on the target blow moulder.

    Top