| HS Code | 905412 |
| Density | 0.944 g/cm3 |
| Melt Flow Rate 190c 2 16kg | 0.40 g/10 min |
| Tensile Strength At Yield | 25 MPa |
| Tensile Strength At Break | 35 MPa |
| Elongation At Break | >=500 % |
| Flexural Modulus | 1100 MPa |
| Vicat Softening Temperature | 124 C |
| Heat Deflection Temperature 0 45mpa | 75 C |
| Melting Temperature | 134 C |
| Hardness Shore D | 65 |
| Environmental Stress Crack Resistance | >1000 h |
As an accredited TPC (Japan) HDPE KBX44A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KBX44A: 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped, 40 bags (1,000 kg) per pallet. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): TPC (Japan) HDPE KBX44A, typically 25 kg bags, about 18 MT net per container, palletized or floor-loaded. |
| Shipping | TPC (Japan) HDPE KBX44A is a non-hazardous high-density polyethylene. It is not regulated as dangerous goods for transport by IMDG, IATA, or ADR. Ship in sealed PE bags or octabins. Keep cool, dry, well-ventilated, and away from direct sunlight, moisture, ignition sources, and contamination. Avoid spillage and dust generation. |
| Storage | For TPC (Japan) HDPE KBX44A, store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Stack pallets securely to prevent package damage. Observe good housekeeping and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Stable; shelf life is indefinite when stored in a cool, dry, well-ventilated place away from sunlight and ignition sources. |
TPC (Japan) HDPE KBX44A moves onto accumulator-head extrusion blow moulding lines for tight-head industrial chemical jerrycans at a compound loading of 100 parts KBX44A, 1.5–2.5 wt% of a 40% carbon black masterbatch meeting the heavy-metal limits of EU Directive 94/62/EC, and 0.05–0.15 wt% of a process stabilizer masterbatch; when storage humidity exceeds 70% RH, pre-drying at 70 °C for 2 h is applied to prevent pinch-off pinholes, with moisture checks performed under ISO 15512:2019. The downstream process runs on a 65 mm grooved-feed extruder with 24:1 L/D and barrel temperatures of 170–190 °C; a 10-zone axial wall-thickness programmer compensates for parison sag on 20 L jerrycans, and the die-head temperature is held at 185–195 °C while mold water is set to 12–18 °C and blow pressure to 0.6–0.8 MPa. On a dual-head shuttle machine, cycle times run 34–42 s; handle pinch-off weakness appears when drop time exceeds 2.5 s or when parison weight deviates more than ±1.5% from target, a bottleneck observed on lines producing 10 L and 20 L containers. Terminal products are UN 3H1 jerrycans and UN 3H2 jerrycans in 10 L, 20 L, and 30 L sizes for liquid intermediate chemicals, industrial cleaners, and water-treatment polymers; certification under 49 CFR 178.504, ADR 6.1.5, and IMDG requires stack testing at 40 °C for 28 days and drop testing of filled containers at −18 °C, with leakage or deformation at the handle weld line classified as critical.
In non-food household chemical bottles, TPC (Japan) HDPE KBX44A is blended with post-consumer HDPE recyclate at replacement levels of 15 wt%, 20 wt%, and 30 wt% as a controlled stream; each recyclate lot is certified under EN 15343, and the compounded material is screened under ISO 16770:2004 for slow crack growth because ASTM D1693-21 condition B at 50 °C gives only a lower-bound environmental stress crack resistance value. The addition ratio is maintained by gravimetric blenders with a ±0.3 wt% tolerance at 220 kg/h total throughput; the mixed stream passes through a 75 mm co-rotating twin-screw extruder with 40:1 L/D, twin vacuum vents at −0.08 MPa, and a melt filtration unit with 120 μm screen pack before entering the main blow moulder. On a 65 mm grooved-feed shuttle blow moulder, melt temperature is held at 185–195 °C and die-head temperature at 190–200 °C; parison weight monitoring with a ±1.2% alarm window is necessary because recyclate-lot viscosity variation produces neck thickness drift and handle pinch-off thinning. Production experience shows that PCR levels above 25 wt% lower melt strength, reducing stand-off distance by 2–4% on a 500 mL bottle at fixed vertical wheel timing; however, published data for the ESCR retention of this specific grade at 30 wt% PCR are limited, making lot-specific ISO 16770 qualification mandatory before release. Terminal products include 500 mL and 750 mL household cleaner bottles, 1 L laundry detergent bottles, and 2 L fabric-softener bottles for non-food service.
Edible-oil and condiment bottles produced on a 12-station vertical wheel blow moulding line are blow moulded from TPC (Japan) HDPE KBX44A as a 100% virgin stream without slip additives; where pigmentation is required, 1.5–2.0 wt% of a high-opacity white masterbatch is added, with the masterbatch carrier and pigments listed under 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, and overall migration below 10 mg/dm² when tested in fatty-food simulant D2 at 60 °C for 10 days. The extrusion blow moulding sequence uses a 55 mm extruder with 25:1 L/D, barrel temperatures of 175–190 °C, die-head temperature of 185–195 °C, mold water at 8–14 °C, and blow-pin internal cooling at 4–8 °C; a 10–14-point axial wall-thickness program maintains sidewall thickness between 0.8–1.6 mm, because oil-filled bottles are checked for top-load and panel resistance under ISO 12048 and stacking stability. Terminal products include 250 mL, 500 mL, and 1 L edible-oil bottles and 500 mL vinegar bottles for non-aseptic filling below 60 °C; organoleptic suitability is confirmed by ASTM E1870 after 72 h accelerated storage at 40 °C. In-line production bottlenecks occur at the leak tester when the neck finish deviates more than 0.15 mm from the finish print, generating cap torque failures under ASTM D2063; published data for hot-fill performance of this specific grade are limited.
Compliance under USP 661.1, Ph. Eur. 3.1.3, and 21 CFR 177.1520(c) restricts the formulation to 100% virgin KBX44A with no external processing lubricants, antistatic agents, or amine-based additives; amine-based stabilizers are excluded from the oral-dose packaging risk assessment because of potential nitrosamine formation. The downstream process runs on a dedicated 55 mm extruder with 25:1 L/D inside an ISO 14644-1 Class 8 cleanroom, with barrel temperatures of 175–190 °C and a die-head temperature of 185–195 °C; blow air is filtered through 0.22 μm sterilizing-grade membranes, and blow-pin exhaust is vented outside the mold zone to limit particle entrainment. Parison programming uses 10–12 axial control points on a single-station shuttle machine, with cycle times of 9–12 s for 120 mL bottles; shoulder and base wall thickness is held to 0.6–1.0 mm, and melt-edge contamination is inspected at 4 h intervals. Batch-to-batch melt flow index variation of 0.02–0.05 g/10 min under ISO 1133-1:2022 has produced neck finish ovality on the line, corrected by blow-pin cooling water setpoint adjustments of ±2 °C. Terminal products are 30 mL, 60 mL, and 120 mL oral solid and liquid pharmaceutical bottles with continuous-thread and child-resistant finish variants; closure torque retention after repeated opening is evaluated under ASTM D2063, and extractables follow USP 661.1 and Ph. Eur. 3.1.3 limits. The melt temperature should not exceed 205 °C because oxidation-induced gel particles at the die lip can create pinholes.
When cold-temperature impact resistance is the binding requirement, automotive washer-fluid reservoirs are blow moulded from TPC (Japan) HDPE KBX44A compounded with 2.0–2.5 wt% of a 40% carbon black masterbatch and 0.2 wt% of a polymeric HALS masterbatch; the carbon black addition is selected to retain low-temperature ductility after 1000 h xenon-arc weathering under ISO 4892-2. Production runs on a 70 mm extruder with 28:1 L/D and a dual-head shuttle blow moulder, with melt temperature at 195–205 °C, die-head temperature at 200–210 °C, mold water at 10–18 °C, and blow pressure at 0.7–0.9 MPa; cycle times for a 2 L reservoir run 22–30 s, while a 4.5 L reservoir requires a slightly longer drop and blow-cooling segment of 28–36 s. The critical failure mode observed on lines running below 8 °C mold water is brittle fracture at the pinch-off weld after −40 °C conditioning; maintaining mold water above 10 °C and using a 0.8–1.2 mm pinch-off land reduces this failure. Terminal products are 2 L and 4.5 L washer-fluid reservoirs and 1.5 L expansion bottles; compliance is evaluated under SAE J1616 for washer-system fluid compatibility and ISO 16750-4 for cold-temperature exposure.
High-speed dairy bottle lines processing TPC (Japan) HDPE KBX44A use a 100% virgin stream without regrind for direct food contact under 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011; no antistatic or slip additives are introduced, and organoleptic performance is verified under ASTM E1870 after 48 h storage at 40 °C. The wheel-type blow moulding line operates with 10–14 stations, an 80 mm extruder with 30:1 L/D, barrel temperatures of 185–200 °C, and die-head temperature of 190–200 °C; mold water is set at 8–12 °C, blow pressure at 0.4–0.6 MPa, and blow-pin exhaust is configured for high-frequency venting. The process limit of 205 °C is based on observed parison elongation and gel generation at the die lip; at 210 °C, wall thickness at the bottle waist falls below 0.35 mm on 500 mL containers, increasing in-line burst test rejection. Production data from high-output wheel machines show that bottle weight variation should be maintained within ±0.8% of target to avoid cap seating failures under ASTM D2063. Terminal products are 250 mL, 500 mL, and 1 L HDPE milk bottles and dairy-alternative beverage bottles for chilled distribution; published data for aseptic or extended-shelf-life filling of this specific resin are limited.
Agricultural chemical drums are produced from TPC (Japan) HDPE KBX44A with 100 parts virgin resin and 10–20 wt% of in-plant regrind; the regrind stream is sifted through a 2 mm screen and checked for melt flow deviation under ISO 1133-1:2022, while melt filtration with a 100 μm screen pack is used to limit gel carryover. Compliance is set by UN 1H1 performance certification under 49 CFR 178.504, ADR 6.1.5, and IMDG, with drop testing at −18 °C and stack loading at 40 °C for 28 days. The process uses a 120 mm extruder with 30:1 L/D and a large accumulator head with 5 kg shot capacity; barrel temperatures are 175–195 °C, die-head temperature is 185–195 °C, mold water is held at 15–25 °C, and blow pressure is 0.7–0.9 MPa. Cycle times for 200 L tight-head drums run 160–240 s; parison programming with 30–60 axial points is used to prevent thinning at the top chime and bottom radius. Terminal products are 200 L tight-head drums and 220 L open-head drums for pesticides, adjuvants, and fertilizers; the pinch-off weld and top-chime thickness are measured with ultrasonic thickness gauges at 0.1 mm resolution, and drums failing the hydraulic pressure test under 49 CFR 178.504 are rejected.
Competitive TPC (Japan) HDPE KBX44A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KBX44A is a high-density polyethylene blow moulding resin supplied in cylindrical pellet form under the TPC product designation. The grade is positioned for continuous extrusion blow moulding, suction blow moulding, and accumulator-head blow moulding of rigid packaging with wall thicknesses between 0.45 mm and 2.0 mm. The manufacturer’s published datasheet lists a nominal density of 0.944 g/cm³ when measured to ISO 1183-1/ASTM D1505 and a melt flow rate of 0.45 g/10 min at 190°C/2.16 kg under ASTM D1238/ISO 1133-1. These values situate the material in the medium-molecular-weight HDPE blow moulding envelope, where melt strength and extruder back pressure must be balanced with acceptable screw recovery time and cycle time. The resin is not intended for thin-wall injection moulding, cast film, or blown film because those processes require either much higher melt flow or different molecular architecture.
KBX44A is typically specified for bottles, jerry cans, and small industrial containers that hold household cleaners, personal-care formulations, agrochemical adjuvants, lubricants, and mild surfactant-based products. The processing stabilizer package allows repeated recycling of clean internal trim. Food-contact compliance must be revalidated if the feedstock is mixed with post-consumer reclaim.
The mechanical response of KBX44A under monotonic loading is documented in manufacturer technical bulletins. Tensile yield strength is reported near 24 MPa when measured at 50 mm/min on ASTM D638 Type IV specimens, while flexural modulus is reported at approximately 950 MPa under ASTM D790 at 23°C. Environmental stress crack resistance, evaluated by the bent-strip method with 10% Igepal CO-630 solution at 50°C per ASTM D1693, exceeds 600 h F50. This combination distinguishes the grade from film extrusion HDPE, which typically has higher melt flow and lower stress crack resistance, and from pipe grades, which often require higher hydrostatic strength at the expense of surface gloss and parison extensibility.
Lot-to-lot melt flow rate variation is commonly controlled within ±0.05 g/10 min by the manufacturer. Converters should nevertheless verify the incoming lot against an internal reference sample because minor changes in molecular weight distribution can shift die swell and parison length on automated lines with laser wall-thickness inspection.
Production-scale processing on shuttle blow moulding lines has been reported with a 65 mm single-screw extruder with a 24:1 L/D ratio and a grooved feed section. Barrel zone setpoints from feed to die of 160°C, 170°C, 175°C, and 175°C typically produce a melt temperature between 180°C and 195°C. Screw speed is maintained between 40 rpm and 70 rpm to keep head pressure in the 20–30 MPa range and recovery time below 14 s. Excessive screw speed above 80 rpm can generate frictional heating above 210°C, increasing the risk of parison sag and gate blush. When processing on a 20-tonne clamp-force single-station shuttle machine producing 1 L HDPE bottles, commercial operators observe parison length variation below ±1.5% when the die-head temperature is held within ±2°C of the setpoint.
Wall-thickness distribution in handle zones and pinch-off areas is controlled through 15–25-point parison programming on accumulator-head machines. A die-to-neck diameter ratio of 2.2:1–2.6:1 is common for HDPE blow moulding tooling; smaller ratios may reduce drawdown, while larger ratios can increase die swell instability. Blow air pressure of 0.45–0.70 MPa is adequate for containers from 250 mL to 5 L, with the upper value reserved for thick-walled jerry cans with rope handles. Mould cooling water at 10–15°C is recommended. A mould temperature above 30°C extends cycle time and increases top-load deflection under 2.5 kN axial load when tested to ASTM D2659. Pinch-off flash thickness should be maintained between 0.10 mm and 0.20 mm to avoid weld-line cracking.
Die swell and parison sag are typically assessed on the target line rather than through a single laboratory parameter. For automatic lines with laser wall-thickness inspection, parison length variation is often the more sensitive indicator of melt strength than melt flow rate alone. If the accumulator head temperature differential exceeds ±2°C, cyclic wall-thickness variation can appear in the upper and lower bottle sections even when the average wall thickness remains within specification.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Melt flow rate at 190°C/2.16 kg | ASTM D1238/ISO 1133-1 | 0.40–0.50 | g/10 min |
| Density | ISO 1183-1/ASTM D1505 | 0.942–0.946 | g/cm³ |
| Tensile yield strength | ASTM D638 Type IV | 23–25 | MPa |
| Elongation at break | ASTM D638 Type IV | >600 | % |
| Flexural modulus | ASTM D790 | 900–1000 | MPa |
| Environmental stress crack resistance F50, 10% Igepal CO-630 | ASTM D1693 | >600 | h |
| Notched Izod impact at 23°C | ASTM D256 | 8–12 | kJ/m² |
| Shore D hardness | ISO 868/ASTM D2240 | 62–64 | — |
Compared with general-purpose HDPE blow moulding grades that exhibit a density of 0.950–0.955 g/cm³ and a melt flow rate below 0.30 g/10 min, KBX44A produces lower die-head pressure and shorter screw recovery time on small shuttle machines. The trade-off is a measurable reduction in top-load stiffness at equal wall thickness. Designers commonly compensate by increasing structural sidewall thickness from 0.45 mm to 0.55 mm in load-bearing regions. Against high-flow injection moulding HDPE with an MFR above 20 g/10 min, KBX44A provides far greater melt strength and environmental stress crack resistance, but it cannot fill thin-wall injection tools with flow path-to-wall thickness ratios above 150:1.
KBX44A is also distinct from transparent polyester or clarified polypropylene packaging resins. It does not provide glass-like clarity; sheet or bottle wall haze is high, as expected for non-clarified HDPE. This limitation is acceptable in opaque industrial and household chemical packaging where chemical resistance, stress crack resistance, and cost per container are primary criteria.
The bent-strip ESCR test under ASTM D1693 Condition A remains the principal screening method for rigid packaging resins. KBX44A’s reported F50 exceeds 600 h in 10% Igepal CO-630 at 50°C. This is a strong indication for containers holding non-ionic surfactant solutions, dilute sodium hypochlorite below 5% active chlorine, and mild hydrocarbon emulsions. For more aggressive fluids, the grade is not automatically suitable. Immersion data generated under ASTM D543 at 40°C for 72 h show mass uptake below 0.3% in a 30% aqueous non-ionic surfactant, with diagonal dimensional change below 0.2%. Published data for aromatic/aliphatic solvent blends in this specific configuration is limited; compatibility must be confirmed with the final container design and closure system.
The resin does not contain a UV stabilizer unless specifically supplied as a UV-stabilized compound. For outdoor exposure beyond 6 months, a UV stabilizer masterbatch should be compounded in accordance with the masterbatch producer’s recommended addition level and verified by accelerated weathering under ASTM G155 or ISO 4892-2.
| Regulatory or standard reference | Scope | Relevant criterion or clause |
|---|---|---|
| FDA 21 CFR §177.1520(c) 3.2a | Olefin polymers for food-contact articles | Density above 0.94 g/cm³; extractives limits per §177.1520(d) |
| EU Regulation (EU) No 10/2011 | Plastic food-contact materials and articles | Overall migration below 10 mg/dm²; specific migration limits for additives |
| REACH Regulation (EC) No 1907/2006 | Substance registration and SVHC reporting | SVHC content below 0.1 wt% per article |
| RoHS Directive 2011/65/EU | Hazardous substances in electrical/electronic equipment | Pb, Hg, Cd, Cr(VI), PBB, and PBDE limits |
| Packaging and Packaging Waste Directive 94/62/EC | Heavy metals in packaging | Sum of Pb, Cd, Hg, and Cr(VI) below 100 mg/kg |
The resin should not be processed above 220°C. At melt temperatures above 200°C, residence time should be kept below 10 min to limit chain scission and off-odour formation. Regrind levels up to 30 wt% are common for non-food applications. Food-contact containers using regrind must meet the same migration and organoleptic limits as virgin material under the applicable food-contact regulation. Moisture exposure at relative humidity above 60% can generate parison pitting; dehumidified-air drying at 80°C for 2–4 h to a moisture content below 0.02% is recommended for exposed material.
Concentrated oxidizers, aromatic solvents, and strong acids can attack the polymer matrix or cause stress cracking under load. These fluids require immersion testing and finite-element stress analysis before specifying KBX44A. The grade is not suitable for continuous service above 60°C under sustained internal pressure, nor for applications requiring glass-like transparency or hot-fill stability above 85°C.