Tpc Japan Hdpe Kb171a

TPC (Japan) HDPE KB171A

    • Product Name: TPC (Japan) HDPE KB171A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 403405
    Density 0.956 g/cm³
    Meltflowrate 20 g/10 min (190°C/2.16 kg)
    Tensilestrengthatyield 28 MPa
    Tensilestrengthatbreak 22 MPa
    Tensileelongationatbreak 500%
    Flexuralmodulus 1200 MPa
    Izodnotchedimpactstrength 40 J/m
    Shoredhardness 65
    Vicatsofteningpoint 125°C
    Heatdeflectiontemperature 75°C at 0.46 MPa
    Brittlenesstemperature -70°C
    Moldingshrinkage 1.5-3.0%
    Waterabsorption <0.01%
    Meltingpoint 135°C
    Thermalexpansioncoefficient 1.1E-4 /°C
    Dielectricconstant 2.3 at 1 MHz
    Volumeresistivity >1E16 ohm·cm

    As an accredited TPC (Japan) HDPE KB171A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KB171A is typically supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for transport and storage.
    Container Loading (20′ FCL) 20′ FCL loading for TPC (Japan) HDPE KB171A: 25 kg bags, 17 MT net, palletized or loose, depending on buyer requirements.
    Shipping TPC (Japan) HDPE KB171A is a non-hazardous high-density polyethylene resin supplied as pellets in 25 kg bags or 1 MT jumbo bags. Ship as general cargo under dry, ventilated conditions, away from sunlight and ignition sources. No UN hazard class or temperature control required; keep packaging sealed to prevent moisture and spillage.
    Storage Store TPC (Japan) HDPE KB171A in a cool, dry, well-ventilated, shaded area, away from direct sunlight, heat, sparks, and open flames. Keep original packaging closed, clean, and upright to prevent moisture, dust, and contamination. Avoid contact with oxidizing agents. Store at moderate temperature, preferably below 50°C. Use appropriate PPE, maintain good housekeeping, and follow manufacturer’s instructions and local regulations.
    Shelf Life Typically two years from date of manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of TPC (Japan) HDPE KB171A

    In the extrusion blow molding of UN-certified jerricans with nominal capacities from 10 L to 30 L, HDPE KB171A is evaluated against the dangerous-goods packaging provisions of ADR/RID/IMDG Chapter 6.1, not against general-purpose packaging tolerances. The decisive property is environmental stress-cracking resistance under top-load and pinch-off stress, because the closure area and handle pinch-off represent cold-weld regions where molecular orientation remains low. Where the producer’s certificate of analysis omits a specific value, the process parameters below are drawn from HDPE blow-molding grades with nominal density 0.955 g/cm³ and melt flow index 0.3–0.7 g/10 min at 190 °C/2.16 kg (ISO 1133-1:2022); they must be verified against the lot certificate before tooling is set. The finished package carries UN mark 3H1 for tight-head plastics jerricans or 3H2 for open-head packagings, followed by the packing group and test year.

    Melt temperature is typically maintained between 200 °C and 230 °C, with the lower bound set by pinch-off fusion and the upper bound by parison sag and odor generation. On accumulator-head machines producing 20 L jerricans in a dual-cavity tool, parison programming is applied over at least 80 points along the parison length to shift wall thickness into the top shoulder and bottom chime. Blow air is introduced at 0.6–0.8 MPa; mold cooling water is held at 15–25 °C to control crystallinity and reduce handle flash warpage. Clamp force for the pinch-off and flash is selected from the total projected pinch-off length, commonly 1,500–2,500 kN for a two-cavity 20 L tool, but tool design, flash pocket geometry, and pinch-off insert angle alter the actual requirement.

    For outdoor-stored jerricans, carbon black masterbatch is metered to a final carbon black concentration of 2.0–3.0 wt%, with dispersion verified according to ISO 18553. Agglomerates larger than 20 µm are rejected because they act as impact crack initiation sites at the bottom chime edge. No additional external lubricant is recommended in this application, because a lubricant-rich surface can lower the coefficient of friction below the value required for stable pallet stacking and can migrate to the pinch-off surface and reduce weld strength. The finished jerrican is subjected to leakproofness, hydraulic pressure, drop, and stack tests according to the ADR/RID/IMDG Chapter 6.1 series; the table below lists the marks that appear on a compliant package.

    Packaging testReferenceControlled requirement
    LeakproofnessADR 6.1.5.4No leakage at the specified pneumatic/hydraulic condition
    Hydraulic pressureADR 6.1.5.5No leakage at the test pressure for the liquid packaging group
    DropADR 6.1.5.3No leakage after impact at conditioned temperature, typically -18 °C
    StackingADR 6.1.5.6No deformation affecting closure integrity
    Environmental stress-cracking resistanceASTM D1693-15 Condition BCommonly specified F50 > 200 h in 10% Igepal CO-630 at 50 °C

    What Process Controls Keep Dairy Bottle Lightweighting Inside a Stable Exploitation Window?

    Single-layer HDPE dairy bottles use the food-contact status of FDA 21 CFR 177.1520(c) and, for EU markets, Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm². The resin is processed on a continuous shuttle blow-molding line with melt temperature held between 200 °C and 225 °C; the lower limit avoids ductile failure at the pinch-off, while the upper limit prevents excessive lactone or aldehyde generation that would fail sensory panel acceptance under ASTM E1870. The material is not suitable for injection stretch blow molding because its molecular weight and low melt flow rate restrict stretch-ratio uniformity.

    Weight reduction to a body wall thickness of 0.35–0.45 mm is possible only when the parison is programmed to shift material away from the lower pinch region and into the neck and shoulder. A 100-point parison controller is used. Top-load strength is verified under ASTM D2659; a filled bottle must resist a specified top-load without buckling. The operational boundary is hot filling: HDPE KB171A is not rated for continuous fill temperatures above 60 °C, because distortion and cap seal torque relaxation occur above this limit. For ESL milk processed above 70 °C, a polypropylene or multilayer barrier structure replaces single-layer HDPE.

    RequirementStandardLimit
    U.S. food contact resinFDA 21 CFR 177.1520(c)Olefin polymer specified for food contact, subject to end-test
    EU overall migrationEU No 10/2011 Annex I10 mg/dm²
    Sensory transferASTM E1870No detectable off-taste in the packaged matrix
    Top-loadASTM D2659Specified fill weight and cap torque

    When Sodium Hypochlorite and Alkylbenzene Sulfonates Enter the Parison

    In household chemical packaging, the parison wall solidifies under a higher frozen-in stress than in dairy bottles, and the stress-cracking environment is more aggressive. Linear alkylbenzene sulfonate surfactants and sodium hypochlorite solutions interact with the partially oriented amorphous tie-chain network, and failures initiate at the mold parting line or the pinch-off, where frozen-in stress is highest. This application therefore uses the environmental stress-cracking resistance test under ASTM D1693-15 Condition B as a release criterion, not merely a data-sheet value. The relevant practical threshold is usually F50 > 300 h for laundry detergent bottles and F50 > 1,000 h for industrial bleach packaging, depending on surfactant concentration. Published data for the specific KB171A configuration in sodium hypochlorite above 5% available chlorine is limited, so bottle cage trials must be run before specification.

    On shuttle machines producing 500 mL to 5 L bottles, the die gap is reduced to 0.8–1.5 mm to increase shear and surface finish, but the back-pressure curve is kept low enough to avoid high melt temperature spikes. Parison swell for high-molecular-weight HDPE in this range is typically 30–50%, so the die diameter is set below the bottle neck diameter. Blow air at 0.6–0.8 MPa with pre-blow delayed 0.2–0.5 s after mold closing is used to prevent a thin sidewall near the handle. No amine-based additive is used in the compound, because amine migration can create cap-seal torque relaxation and may react with chlorine-containing environments. The operational boundary is therefore set by the additive package: only the producer-approved stabilizer system should be combined with this resin in bleach or hypochlorite service.

    Windshield washer reservoirs blow-molded from HDPE KB171A are validated for methanol/ethylene glycol washer fluids at service temperatures from -30 °C to 80 °C. The critical failure mode is low-temperature impact at the base pinch-off after fluid aging. Impact testing is performed under ISO 6603-2 at -30 °C; a specified maximum force and puncture energy are required. Because the part geometry includes a narrow filler neck and a wide lower body, wall-thickness distribution must be mapped by ultrasonic gauge on production samples, with the minimum wall at the tank bottom not below 1.5 mm. The tool uses a moving core or 3D blow-molding sequence to prevent thinning over the pump mounting boss. Long-term fluid compatibility is assessed by immersion in 50% methanol/water at 60 °C for 1,000 h followed by tensile property retention under ISO 527-1; published data for KB171A in this exact fluid mixture is limited, so this test is mandatory, not advisory.

    Accumulator-Head Parison Programming for Industrial Open-Top Pails

    For open-top pails used with water-based emulsions, adhesives, and building chemicals, the main process difference from jerricans is the open rim, which must seal against a lid without a separate neck tool. The accumulator head is programmed to deliver a heavy wall band at the top rim, typically 3.0 mm to 4.0 mm, while reducing the body wall to 1.2 mm to 1.8 mm. Rim flatness is controlled by mold cooling at 10–15 °C and by holding the part in the mold for an additional 2–5 s after blow termination. The pinch-off at the bottom is tested for impact drop at 0 °C with a filled pail; any visible stress whitening is a rejection criterion.

    Because the contents are often alkaline or surfactant-based, residual stresses from the pinch-off are annealed to a limited extent by mold temperature, but full annealing is not possible in a continuous blow-molding cycle. The resin’s high molecular weight is necessary for environmental stress-cracking resistance; however, the lower melt flow rate increases shear heating during plastication, and screw speed on a 60 mm extruder is usually set below 60 min⁻¹ to avoid over-shear and melt temperature runaway. The screw is a barrier design with a mixing section 4D to 6D long. For pails intended for solvent-based adhesives, pre-validation of weight loss and permeation is required before commercial use.

    Thick-walled marine floats and buoyancy blocks occupy a low-cycle-count blow-molding niche. The parison is extruded at melt temperature 210–230 °C and blown into a chilled aluminum tool at 10 °C to freeze the outer skin rapidly, while the core continues to crystallize after demolding. Wall thickness often exceeds 6 mm, and cycle time is controlled by internal cooling air rather than mold temperature alone. Outdoor weathering resistance requires carbon black concentration of 2.0–2.5 wt% or a UV-stabilizer package specified under ISO 4892-3 exposure; the acceptance criterion is usually no surface cracking after 2,000 h of accelerated weathering and no reduction in tensile yield below 80% of the unexposed value under ISO 527-2. Low-temperature impact is checked at -20 °C by dropping a 5 kg striker from 1 m; published data for this specific configuration is limited, so inspection agencies may require batch tests on each tool and material lot.

    Free Quote

    Competitive TPC (Japan) HDPE KB171A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KB171A is referenced in distributor technical literature as a high-molecular-weight high-density polyethylene resin intended primarily for large-part extrusion blow moulding. The grade designation places it at the low melt-flow end of the HDPE portfolio, where parison stability, pinch-off weld toughness, and environmental stress crack resistance are more important than short cycle time. Current producer certificates of analysis control lot-specific density, melt flow rate, and mechanical values; this page uses class-typical engineering data for high-molecular-weight HDPE blow moulding resins where the exact KB171A datasheet revision is not quoted.

    Because HDPE is not hygroscopic under dry storage, pre-drying is normally unnecessary when storage relative humidity remains below 60 % and pellet surface condensation is absent. If resin has been exposed to wet or humid conditions, auxiliary equipment suppliers recommend hopper drying at 70–85 °C for 3–4 h with sufficient airflow. The grade should not be blended with amine-functional masterbatches or hygroscopic additives that release volatile decomposition products at the 200–220 °C melt temperatures typical of accumulator-head blow moulding.

    What Distinguishes KB171A from Generic HDPE Blow Moulding Grades?

    The distinction is primarily molecular. High-molecular-weight bimodal HDPE in the KB171A class processes with an elevated zero-shear viscosity while retaining shear thinning under extrusion. A general-purpose HDPE blow moulding grade with a melt flow rate of 0.3–0.7 dg/min may fill shallow bottle moulds rapidly, but its parison elongates under its own weight in large-part moulding and its slow crack growth resistance is lower. A high-molecular-weight grade in the 0.03–0.08 dg/min melt-flow class measured by ISO 1133-1:2022 at 190 °C/2.16 kg provides higher melt strength and a higher tie-molecule concentration in the solidified part.

    Published data for this specific configuration is limited; the comparative ranges below are class-typical for high-molecular-weight HDPE blow moulding grades and should not replace a lot-specific TPC datasheet. In bimodal HMW-HDPE, the low-molecular-weight fraction reduces melt viscosity during extrusion and stabilises output, while the high-molecular-weight fraction generates tie molecules that bridge crystalline lamellae. Slow crack growth in aggressive environments proceeds along lamellar boundaries when tie-molecule density is low; the high-molecular-weight fraction increases the number of load-bearing interlamellar linkages and delays fibril pull-out.

    Shear sensitivity can be assessed by capillary rheometry in accordance with ISO 11443:2021. For bimodal HMW-HDPE, the ratio of apparent viscosity at 100 s⁻¹ to that at 1000 s⁻¹ is larger than in a unimodal general-purpose blow moulding grade. This behaviour permits extrusion through a narrow die at acceptable head pressure while retaining high zero-shear viscosity for parison stability. The melt also exhibits extensional hardening during parison inflation; as the melt is stretched, extensional viscosity rises and limits local thinning, improving wall uniformity in tall, large-diameter parts.

    Within HDPE, comonomer selection further changes the product. Hexene- or octene-based copolymers in the same melt-flow class typically provide better stress-crack resistance and slow crack growth performance than butene-based copolymers at equal density and melt index, although producers rarely disclose comonomer identity in product literature. The discriminating property is therefore environmental stress crack resistance under ASTM D1693-15 rather than comonomer claims.

    Class-typical comparison for high-molecular-weight HDPE blow moulding resins versus general-purpose HDPE blow moulding resins
    PropertyTest methodHMW-HDPE blow moulding classGeneral-purpose HDPE blow moulding class
    Melt flow rateISO 1133-1:20220.03–0.08 dg/min0.2–0.7 dg/min
    DensityISO 1183-1:20190.944–0.956 g/cm³0.952–0.962 g/cm³
    Environmental stress crack resistance, Method BASTM D1693-15>600 h20–150 h
    Tensile yield stressISO 527-2:201224–28 MPa25–30 MPa
    Flexural modulusISO 178:20191050–1300 MPa1200–1500 MPa

    Melt Processing Envelope and Failure Modes on Accumulator-Head Equipment

    For the HMW-HDPE class represented by KB171A, extruder barrel feed zones are usually set at 180–200 °C, metering zones at 200–220 °C, and accumulator-head tooling at 200–220 °C. Melt temperatures below this window increase backpressure and can produce melt fracture, while operation above 220–240 °C during prolonged hold times accelerates chain scission and gel formation at high-shear surfaces. Machine-builders specify screw lengths of 24:1 to 30:1 L/D with compression ratios from 2.5:1 to 3.5:1 and low-shear barrier flights, because HMW-HDPE is sensitive to shear heating and may develop gel particles if local melt temperature exceeds the stabiliser activation threshold.

    Die geometry is critical. Accumulator-head tooling typically uses a diverging die gap of 20–40 % over the land length to control die swell and parison diameter. Blow mould clamps of 100–300 t are employed for large parts, with mould temperatures held between 10 °C and 40 °C through turbulent chilled water. Hardened pinch-off inserts are required; the high viscosity of HMW-HDPE at the weld line localises backfill and flash. In multi-layer fuel tanks, the tie layer and EVOH barrier must remain within ±10 °C of the HDPE melt temperature to prevent interlayer instability.

    Blow air pressure is typically 0.5–0.8 MPa, and blow time is set to maintain part contact with the mould until cooling is complete. Cooling time in HDPE blow moulding scales approximately with the square of wall thickness and is often reported in machine-builder guidelines as 8–10 s/mm at 20 °C mould temperature. Shot capacity should be selected so that the accumulator head discharges a melt cushion of 10–15 % of part volume to maintain stable parison length. Axial wall-thickness programming adjusts die gap over parison length, while radial wall-thickness control uses die ovalisation or tooling inserts to compensate for corner thinning.

    Processors often observe batch-to-batch viscosity drift as a shift in accumulator fill time and head pressure. A lot with slightly lower melt flow rate may require an increase in barrel set point by 5–10 °C or a reduction in screw speed to maintain output. A lot with higher melt flow rate may produce parison sag on tall parts, requiring a reduction in melt temperature and a longer die-gap program at the lower parison region. Such adjustments are normal process control rather than material defects; they reflect the need to manage viscosity within the product specification band.

    Typical HMW-HDPE accumulator-head blow moulding envelope and associated failure modes
    ParameterTypical set pointBelow windowAbove window
    Melt temperature200–220 °CMelt fracture, high backpressureParison sag, thermal oxidation
    Mould temperature10–40 °CHigh shrinkage, poor surface replicationIncreased cycle time, surface defects
    Die gap divergence20–40 %Unstable parison diameter, uneven wallExcessive swell, wall-thickness variation
    Regrind fraction≤30 %—Reduced weld toughness, lower ESCR

    In aggressive-fluid service, KB171A-class HMW-HDPE is selected for containers holding non-ionic surfactants, diluted alcohols, mild acids, and ammonia solutions. The material is not recommended for strong oxidizers, free chlorine at elevated temperature, concentrated nitric acid, or aromatic hydrocarbons such as toluene and xylene; these agents plasticise or stress-crack the surface layer. Gasoline and solvent blends can be absorbed into the amorphous phase, reducing burst pressure at elevated temperature and increasing permeation through the wall. For automotive fuel tanks, the HDPE layers are therefore coextruded with an ethylene-vinyl alcohol copolymer barrier and maleic anhydride-grafted polyethylene tie layers. The structural HDPE outer and inner layers supply impact resistance at -40 °C and processability, while the barrier layer controls hydrocarbon permeation under ECE R34 or CARB protocols.

    Outdoor exposure beyond 12 months generally requires UV stabilisation. A carbon black masterbatch addition of 2.0–2.5 wt% is common for black parts; for coloured parts, a hindered amine light stabilizer package is used. Without adequate stabilisation, surface embrittlement and microcracking precede bulk mechanical failure, particularly in high-UV environments. ASTM D3350-14 cell classification and UL 746C outdoor suitability protocols are reference frameworks for long-term weathering, though blow moulded articles are often specified by application-specific UV exposure tests.

    In industrial packaging, UN-certified containers moulded from this HDPE class undergo hydraulic pressure, stack loading, vibration, and drop impact testing. The pinch-off weld and handle insertion zones are the most frequent crack-initiation sites when regrind fraction exceeds 30 % or when pinch-off insert temperature drops. Hot-plate welding of thick HDPE sections uses a melt surface temperature of 200–220 °C; surfaces should be scraper-peeled and cleaned with a non-aromatic solvent immediately before joining. Welding to polypropylene or heavily contaminated regrind streams should be avoided because interdiffusion across incompatible interfaces is insufficient.

    Published failure analyses from production-scale lines indicate that lot-to-lot MFR drift of 0.01–0.02 dg/min can shift parison sag and wall-thickness distribution by measurable amounts on large parts. Consequently, accumulator-head machines require parison programming adjustments after lot change. The product is not recommended for thin-wall injection moulding or high-speed film casting, where its viscosity exceeds processing limits. It is equally unsuitable for rotationally moulded parts because the pellet material would need to be ground to powder and does not densify at the low shear rates typical of rotomoulding. Continuous load-bearing service above 80 °C is not recommended without specific stabiliser and end-use testing.