Tpc Japan Hdpe Kb165a

TPC (Japan) HDPE KB165A

    • Product Name: TPC (Japan) HDPE KB165A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 728126
    Density 0.965 g/cm3
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 29 MPa
    Elongation At Break 1000%
    Flexural Modulus 1200 MPa
    Izod Impact Strength Notched 50 J/m
    Hardness Shore D 65
    Vicat Softening Temperature 125°C
    Heat Deflection Temperature 0 46 Mpa 75°C
    Melting Point 130°C
    Water Absorption 0.01%
    Linear Mold Shrinkage 2.0%
    Thermal Conductivity 0.40 W/m·K
    Volume Resistivity 1.0e16 Ω·cm
    Dielectric Constant 2.3
    Dielectric Strength 20 kV/mm

    As an accredited TPC (Japan) HDPE KB165A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KB165A is packaged in 25 kg net paper bags, palletized at 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL loading for TPC (Japan) HDPE KB165A: typically 25kg bags, 25MT net, palletized, shrink-wrapped, securely containerized for export shipping.
    Shipping TPC (Japan) HDPE KB165A is a non-hazardous high-density polyethylene resin supplied as pellets. Ship in moisture-proof 25 kg bags or 1,000 kg jumbo bags on pallets, stretch-wrapped. No UN/DG classification required. Keep dry, cool, and away from direct sunlight; handle as general cargo.
    Storage Store TPC (Japan) HDPE KB165A in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original packaging closed to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Use clean handling equipment, protect from static discharge, and follow local regulations and manufacturer recommendations. Do not store near food, feed, or drinking water.
    Shelf Life TPC (Japan) HDPE KB165A: 24 months shelf life when stored in original unopened packaging, dry, cool, away from direct sunlight.
    Application of TPC (Japan) HDPE KB165A

    A shuttle-type extrusion blow moulding cell processing HDPE KB165A for UN-certified 5–60 L jerricans typically runs a 65 mm grooved-barrel extruder with L/D of 30:1 and a barrier mixing screw, holding melt temperature at 190–210°C and die head temperature at 195–215°C. The accumulator or continuous parison die gap is set between 1.0 mm and 3.0 mm, with axial parison programming used to increase wall thickness in the handle and pinch-off zones. Blow air pressure in the range of 0.6–0.9 MPa and mould temperature of 10–25°C control sidewall crystallinity and drop-impact behaviour. The finished containers fall under UN design type 3H1 or 3H2, depending on neck design, and are tested to drop heights of 1.2 m for Packing Group II and 0.8 m for Packing Group III after conditioning at -18°C for 24 h per UN Chapter 6.1. Leakproofness is verified at 30 kPa internal air pressure. Density measured per ASTM D1505-18 influences barrier and chemical resistance, while environmental stress crack resistance, measured per ASTM D1693-21 condition B in 10% Igepal CO-630, is the primary quality gate for lubricant and solvent packagings. Colour masterbatch addition is held between 0.5 wt% and 3.0 wt%; higher loadings can reduce ESCR by creating low-molecular-weight carrier resin concentrations at the weld line. Post-industrial regrind should be dried to surface moisture below 0.03 wt% when pellets have moved from cold storage to a humid processing hall. Scrap rates rise when die swell drops below 10% or when melt temperature exceeds 225°C, because the high-molecular-weight tail in the resin starts thermo-oxidative chain scission. A conservative barrel-temperature profile from feed to die is 180–200–210–215–215°C; each zone is trimmed by no more than 5°C per 10 min to avoid surging. The end products are 5 L, 10 L, 20 L, 25 L, and 60 L containers for hydrocarbon-based lubricants, glycols, agricultural adjuvants, and cleaning concentrates.

    TestConditionPG II requirementPG III requirement
    Drop test-18°C / 24 h conditioning1.2 m0.8 m
    LeakproofnessInternal air pressure30 kPa30 kPa

    Once shot mass exceeds 2 kg, what limits parison sag in 200 L tight-head drum production?

    Once shot mass exceeds 2 kg and hang time extends beyond 12 s, parison sag in 200 L tight-head drum production becomes measurable and can produce sidewall thinning below the 2.0 mm minimum required for UN PG II certification. On a 90 mm accumulator blow moulder with L/D 30:1, the HDPE KB165A melt is typically held at 200–220°C at the die, but the upper value is only acceptable for hang times below 8 s. The accumulator head delivers the shot into the open mould within 2–5 s; any hang-time extension beyond 12 s produces measurable thinning in the middle of the parison and increases the risk of uneven wall distribution. Wall-thickness programming is set with 5–10 extrusion points; the top chime and bottom chime are programmed to 2.5–3.0 mm, while the sidewall is programmed to 1.8–2.2 mm. Mould clamp force on a typical line is 800–1500 kN, and blow air is supplied at 0.8–1.0 MPa with pre-blow delay of 0.3–0.8 s. The drum body is tested for drop resistance after conditioning at -18°C for 24 h and for leakproofness at 30 kPa. Because this HDPE grade is a high-molecular-weight blow moulding resin, continuous extrusion can cause melt fracture at die gaps below 1.0 mm; therefore, die gaps below 1.0 mm are avoided in full-size drum tooling. Published data for this specific configuration is limited, but production-scale experience shows that sag-related wall non-uniformity is the dominant cause of hydraulic burst rejection before reaching the 100 kPa internal pressure requirement used for certain bulk packagings. The end product is a 200 L or 220 L closed-head or open-top drum for export hazardous liquids, food ingredients, and high-density intermediates.

    In 20 L agricultural chemical packagings, stress cracking at the pinch-off weld is the primary field-failure mode, not burst strength. Active ingredients formulated as emulsifiable concentrates introduce aromatic solvent systems that plasticise the amorphous tie chains in the HDPE sidewall. Therefore, the standard processing route combines extrusion blow moulding with inline fluorination of the inner surface, using 0.1–1.0 vol% fluorine in nitrogen for 10–60 s immediately after mould opening. The fluorination forms a fluorocarbon barrier layer by replacing surface hydrogen atoms, reducing permeation of xylene, cyclohexanone, and naphthalene-based carriers. The outer wall remains unfluorinated to preserve weld strength. UN certification follows design type 3H1 for non-removable head containers, and drop testing is performed with the actual liquid or a standard substitute at Packing Group II or III heights. The pinch-off weld thickness is programmed to 2.5–3.0 mm to compensate for molecular orientation loss at the parting line. Mould temperature is held at 15–25°C to avoid residual thermal stress that accelerates environmental stress cracking. Post-flushing with compressed air for 30–60 s removes free fluorine from the vessel before hydrostatic leak testing at 30 kPa. Because no monolayer HDPE structure can meet the permeation limits for highly volatile fumigants, the grade is limited to products classified as non-fumigant agricultural chemicals. The end products are 10 L, 20 L, and 25 L pesticide and adjuvant packagings with UN 3H1 markings and ADR/RID authorised transport.

    When post-industrial regrind exceeds 20 wt%, what changes in pinch-off weld integrity?

    When post-industrial regrind from flash, start-up purges, and rejected containers is added back at levels beyond 20 wt%, the ESCR of the finished sidewall can shift non-linearly because each extrusion heat history consumes antioxidant and shortens the high-molecular-weight fraction. The pinch-off weld is the most sensitive zone: oxidised regrind particles create localised low-melt-strength domains that reduce the effective entanglement density at the weld line. Published data for this specific configuration is limited; however, industrial experience with similar high-load melt index HDPE grades indicates that virgin HDPE KB165A weld line ESCR is generally sufficient for PG II hydrocarbon fill at room temperature, but the same formulation with 40 wt% regrind can shift failure time significantly when tested per ASTM D1693-21 condition B. Therefore, production controls set regrind inclusion at 10–15 wt% for hazardous-liquid containers and allow up to 25 wt% only for non-hazardous detergent or aqueous products. The regrind stream is passed through a 40-mesh screen pack and blended offline at 100–200 rpm in a gravimetric batch mixer before being reintroduced to the extruder throat. Pre-drying is required only when pellets or regrind show visible surface condensation from moving between cold storage and a humid processing hall. The same limitation applies to colour masterbatch carriers: high-flow LDPE carrier resins act as stress concentrators at weld lines. For high-gloss consumer containers, the addition of 1.0–2.0 wt% of a high-density PE-based colour masterbatch is preferred over a low-density or EVA carrier because EVA can increase interfacial weakness at the weld. End products are 10–60 L containers with controlled recycled content, but not food-contact or pharmaceutical containers unless a separate food-grade recycling validation is completed.

    For outdoor water storage tanks and aquaculture floats, blow-moulded halves or single-piece containers are produced in the 100–5000 L range. On a 120 mm accumulator blow moulder with an L/D of 26:1 to 32:1, HDPE KB165A is processed at melt temperature of 195–215°C and die head temperature of 200–220°C. The grade is not suitable for rotational moulding because its molar mass distribution is optimised for parison extrusion rather than low-shear sintering. Blow-moulded tank halves are joined by butt fusion at 210–225°C with a heating plate pressure of 0.15–0.25 MPa, producing a weld that retains the sidewall’s chemical resistance. For outdoor exposure, 1.0–2.5 wt% of a PE-based carbon black masterbatch is added to achieve a carbon-black dispersion level of 2.0–2.5%, which provides UV stabilisation under ISO 4892-2 accelerated weathering; the actual outdoor service life depends on wall thickness and climate. Because wall thickness in large tanks is often 4–8 mm, cooling time in the mould is set between 180 s and 600 s to avoid post-mould warpage and sink marks. Blow air is supplied at 0.6–0.8 MPa, and mould temperature is kept at 8–20°C. The resulting products are vertical or horizontal water reserve tanks, rainwater harvesting vessels, and fish transport totes. A key limitation is that the material should not be used for potable-water tanks that require long-term chlorine dioxide disinfection at greater than 1 ppm residual unless the tank manufacturer has completed migration testing under the applicable national standard, because chlorine exposure can accelerate oxidative degradation in high-stress hopper transitions. Published data for this specific configuration is limited, but fabricators report better wall-thickness uniformity when the accumulator shot size is kept below 70% of maximum capacity to reduce melt hold-up time.

    Free Quote

    Competitive TPC (Japan) HDPE KB165A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KB165A is a high-density polyethylene resin positioned for extrusion blow moulding of rigid hollow articles where parison melt strength, environmental stress cracking resistance, and wall-thickness uniformity are the dominant process variables. The designation KB165A falls within the polyolefin food-contact class when supplied with appropriate conformity documentation, but grade-specific property values are not fully described in public datasheets and should be verified against the manufacturer’s certificate of analysis. Density is normally characterized in the HDPE range of 0.945–0.960 g/cm³ using ISO 1183-1 or ASTM D1505, and melt-flow properties are evaluated at 190 °C under both 2.16 kg and 21.6 kg loads according to ISO 1133-1 or ASTM D1238. Because this grade is intended for blow moulding rather than injection moulding, the interpretation of melt-flow data must focus on sag resistance and die swell rather than spiral-flow length.

    What Processing Window Applies to KB165A in Continuous Extrusion Blow Moulding?

    On continuous shuttle blow moulding machines with general-purpose polyolefin screws of 24:1 to 30:1 L/D, barrel temperatures for unmodified HDPE are commonly set between 160 °C and 200 °C, with the die head maintained at 190–210 °C to control parison gloss and weld-line strength. These values are starting points, not grade-specific process guarantees; publication of exact KB165A processing data is limited. The die gap must be adjusted to the parison diameter and target wall thickness, because excessive die land shear can initiate melt fracture at the outer parison surface. Accumulator-head machines require additional attention to shot-to-shot temperature uniformity. Melt temperature measured at the die exit should be stable within ±3 °C; larger swings produce visible parison length variation and pinch-off thickness drift. Blow pressure is normally in the range of 0.6–1.0 MPa for high-density polyethylene, and mould temperatures between 10 °C and 40 °C are used to balance cooling rate against surface replication. Higher mould temperatures reduce cooling-induced internal stress but extend cycle time. Since published data for this specific configuration is limited, process development should begin with a design of experiments that varies die gap, melt temperature, and blow pressure while measuring part mass and top-load capacity.

    Because high-density polyethylene is a semi-crystalline polymer, the cooling rate in the mould controls crystallinity gradients and shrinkage anisotropy. On production-scale equipment, uneven mould cooling channels produce differential crystallinity across the part, which can deform the pinch-off weld or reduce drop-impact resistance. The melt must retain sufficient elastic recovery at the die exit to prevent parison sag during the open-mould transfer. Parison sag is routinely assessed by measuring the length of a freely extruded parison under a fixed time and temperature; a high-molecular-weight blow moulding grade will exhibit a lower sag velocity than a general-purpose injection grade. The ratio of high-load melt index at 21.6 kg to standard melt index at 2.16 kg is a useful rheological indicator; an elevated ratio is associated with strong shear thinning and better parison hang time. Published data for the specific ratio of KB165A is limited, but the grade’s blow moulding designation implies that the resin is formulated for controlled melt elasticity. Weld-line integrity at the pinch-off is a separate failure mode that depends on melt temperature, mould temperature, and the pinch-off land geometry. Inadequate pinch-off compression can produce a weak weld line that fails in drop testing, while excessive compression can displace material and create thick internal flash. Operators should monitor part weight, pinch-off flash thickness, and drop-impact results from ASTM D2463 or customer-specific drum tests.

    Comparative Melt Strength and Environmental Stress Cracking Resistance

    The technical distinction between KB165A and standard low-molecular-weight HDPE injection moulding grades is expressed primarily through melt viscosity and environmental stress cracking resistance. Injection moulding grades are typically characterized by higher melt-flow rates and shorter cycle times, but their low-melt-strength response is unsuitable for large hollow parts with long parison hang times. Blow moulding grades such as KB165A are positioned in the low melt-flow-rate region, where the high-load melt index is more diagnostically relevant than the 2.16 kg value. Environmental stress cracking resistance is assessed by ASTM D1693 or ISO 22088, which place a notched specimen under a controlled strain in a surfactant environment. High-molecular-weight HDPE grades generally show longer failure times than lower molecular weight grades, but the exact value for KB165A must be confirmed from the supplier’s certificate of analysis. Compared with unimodal blow moulding grades, bimodal or broad molecular weight distribution resins can improve the balance between stiffness and ESCR, because the high-molecular-weight fraction increases tie-molecule concentration while the low-molecular-weight fraction maintains melt processability. If KB165A is supplied with a bimodal reactor architecture, the improvement in ESCR relative to conventional unimodal grades of equal density is measurable through longer time-to-failure in ASTM D1693 and through higher notched Charpy impact at −30 °C under ISO 179-1. However, published data for this specific configuration is limited, and such comparisons should be made only on specimens moulded under identical thermal history. Differences from HDPE pipe grades are equally important: pipe resins are optimized for long-term hydrostatic strength under ISO 9080, while blow moulding resins are optimized for parison stability and pinch-off weld performance. The two performance envelopes are not interchangeable.

    Property equivalence should not be inferred solely from density and melt-flow data. Two HDPE resins with identical density and high-load MFR can differ in comonomer type and placement; butene, hexene, and octene copolymers display different tie-molecule formation and ESCR at equal density. Incoming quality control should therefore include not only density and MFR but also a notched ESCR test under ASTM D1693. Without this data, a resin substitution can pass routine melt-flow checks and still fail in field container stress-cracking.

    Regulatory compliance for food-contact and industrial packaging applications is not a single property but a matrix of chemical migration, compositional, and processing requirements.

    Regulation or standard Test method or clause Typical HDPE requirement
    US FDA 21 CFR 177.1520 Olefin polymer compliance with extractable fraction limits
    EU plastics regulation Regulation (EU) 10/2011 Overall migration 10 mg/dm² for food-contact articles
    Japan Food Sanitation Act Positive list for polyolefins Supplier conformity declaration required
    REACH EC 1907/2006 SVHC declaration and 0.1 % w/w communication threshold
    RoHS Directive 2011/65/EU Pb 1000 ppm, Hg 1000 ppm, Cd 100 ppm, CrVI 1000 ppm
    Density ISO 1183-1 or ASTM D1505 HDPE range 0.945–0.960 g/cm³
    Melt-flow rate ISO 1133-1 or ASTM D1238 Low MFR for blow moulding; high-load MFR typically specified
    Tensile properties ISO 527-1 or ASTM D638 Tensile yield stress in HDPE range, depending on density
    ESCR ASTM D1693 Time to failure in surfactant; grade-dependent

    The table is a compliance checklist rather than a product-specific data sheet. Each production lot should be verified against the supplier’s certificate of analysis, because additive package and catalyst residues influence food-contact status and organoleptic performance.

    When Moisture Control Becomes Process-Critical in Humid Storage Conditions

    HDPE is generally non-hydroscopic, and pre-drying is not normally required for pellets stored in closed containers at ambient humidity. However, surface moisture from condensation can be introduced when cold pellets are moved into a warm, humid production hall. If the pellet surface moisture exceeds 0.05 % by weight, steam bubbles and splay can appear at the die exit. In such cases, a desiccant hopper dryer operating at 70–80 °C for 1–2 h is a conservative start-up measure, but extended drying above 90 °C can oxidize the polymer and shift the melt-flow curve. The resin should not be stored in direct sunlight or in open silos adjacent to amine-based additives or volatile organic liquids, because polyethylene can absorb low-molecular-weight species that later migrate to the surface. Storage temperature above 40 °C in unventilated silos can cause pellet agglomeration in warm climates, particularly if the pellet surface retains waxes or residual monomers. Lot-to-lot moisture variability is a minor contributor compared to temperature instability in the extruder, but moisture checks using a thermogravimetric moisture balance are inexpensive and should be recorded with each incoming lot.

    On accumulator-head blow moulding lines used for large industrial containers, the parison is extruded quickly and then inflated inside a closed mould. The critical processing failure is not short shot but parison fold-over or uneven wall thickness caused by inadequate melt strength. The extruder head must be purged with a compatible HDPE of similar viscosity before any colour or additive change; contamination by polypropylene, acetal, or incompatible pigments can reduce melt strength and create delamination at the pinch-off weld. Screw recovery time should be stable within ±0.5 s on a 60 mm extruder; larger fluctuations indicate bridging in the feed throat or worn screw elements. The die head is normally set to a converging land geometry to suppress flow lines, but excessive convergence can introduce melt fracture. Die tooling should be checked for chromium plating wear, because exposed steel increases wall slip variability and surface roughness. Top-load capacity and drop-impact testing at low temperature are more useful quality indicators for blow moulded containers than tensile tests on compression-moulded plaques, because they capture the integrated effect of parison programming, weld-line strength, and cooling-rate-induced crystallinity.

    Chemical resistance of HDPE is not uniform across all hydrocarbons. The grade may be suitable for aqueous acids, alkalis, and many polar solvents, but prolonged contact with strong oxidizers, chlorinated solvents, or low-molecular-weight hydrocarbons can reduce ESCR or cause swelling. For exact service, testing under ASTM D543 or ISO 175 with the actual chemical at the maximum service temperature is required. Published data for this specific configuration is limited, and no blanket chemical compatibility claim should be inferred solely from the HDPE density class. This limitation is particularly relevant for industrial containers holding mixtures that include surfactants, because stress cracking is accelerated by the combined effect of stress and a surface-active environment.

    Equipment Configuration Limits for Accumulator-Head Lines

    Accumulator-head machines impose a practical upper limit on melt residence time. For HDPE blow moulding, total residence time above 220 °C should not exceed 30 min; longer exposure can increase gel formation and reduce ESCR. The extruder screw should provide a barrier mixing section with a compression ratio between 2.5:1 and 3.5:1 for high-density polyethylene, although screw geometry should be confirmed by the equipment supplier. The melt pump, if installed, must be operated within the manufacturer’s suction-pressure limits; cavitation at the melt pump inlet can introduce gas bubbles that weaken the parison. Blow mould cooling circuits should be balanced so that the temperature difference between inlet and outlet does not exceed 3 °C; larger differences produce non-uniform part shrinkage and may cause the pinch-off weld to curl inward. Mould venting is also critical: insufficient venting traps air between the parison and cavity, creating local thinning and surface defects. These operational limits are not unique to KB165A but are amplified when running high-molecular-weight blow moulding grades because the high melt viscosity reduces the tolerance for low-temperature processing.