Tpc Japan Hdpe Kb161k

TPC (Japan) HDPE KB161K

    • Product Name: TPC (Japan) HDPE KB161K
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 427081
    Density 0.961 g/cm³
    Melt Flow Rate 0.20 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 29 MPa
    Tensile Elongation At Break 800%
    Flexural Modulus 1.20 GPa
    Notched Izod Impact Strength 100 J/m
    Vicat Softening Point 126°C
    Heat Deflection Temperature At 0 46 Mpa 75°C
    Shore D Hardness 65
    Environmental Stress Crack Resistance >1000 h
    Brittleness Temperature <-70°C
    Water Absorption <0.01%

    As an accredited TPC (Japan) HDPE KB161K factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KB161K is typically supplied in 25 kg paper bags or 1,000 kg jumbo bags, palletized for transport.
    Container Loading (20′ FCL) TPC Japan HDPE KB161K: 20′ FCL loads 25 MT in 25 kg bags, palletized or loose, shrink-wrapped.
    Shipping TPC (Japan) HDPE KB161K is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg bags, jumbo bags, or bulk containers. Store in a cool, dry, ventilated area away from heat, sunlight, moisture, and contamination. No UN hazard class or special transport labels are required.
    Storage Store TPC (Japan) HDPE KB161K in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and ignition sources. Keep original bags or containers tightly closed on pallets to prevent moisture, dust, and contamination. Avoid contact with oils, solvents, and incompatible chemicals. Maintain clean handling areas, control static, and rotate stock according to local regulations.
    Shelf Life Shelf life for TPC (Japan) HDPE KB161K is approximately 24 months when stored unopened in a cool, dry, shaded environment.
    Application of TPC (Japan) HDPE KB161K

    HDPE KB161K produced by TPC Japan is converted into mono-layer tight-head and open-head industrial liquid packaging on shuttle-type extrusion blow-molding stations. The relevant products are UN-certified 3H1/3H2 jerricans in 5 L, 10 L, and 20 L volume classes, wide-mouth agrochemical bottles in the 1 L to 5 L range, and 25 L tight-head drums. Machine configuration for 20 L jerrican production typically uses an 80 mm extruder with a 25:1 L/D barrier screw, a grooved feed section, and an accumulator head with a shot capacity of 1.5 kg to 5.0 kg. Melt temperature at the die entrance is maintained between 185 °C and 205 °C, while the die head is set 5 °C to 10 °C higher to prevent premature skin solidification. Mold temperature is held at 8 °C to 15 °C with a closed-loop chiller circuit. Blow pressure is set at 0.6 MPa to 1.0 MPa, and the blow timer is indexed to the pinch-off wall thickness rather than to a fixed duration. Cycle time for a 20 L container with a nominal wall thickness of 1.4 mm to 2.2 mm falls between 45 s and 80 s. Parison programming is mandatory for this geometry: the die gap is opened from 1.5 mm to 3.0 mm at the top and bottom pinch-off zones and narrowed to 1.2 mm to 1.8 mm in the central body section to reduce thinning at the corners. The programmed parison profile is verified by sectioning molded parts and measuring wall thickness at 12 circumferential points per plane. Environmental stress-crack resistance is assessed under ASTM D1693 Condition B, 10% Igepal CO-630 at 50 °C; the pass criterion for aggressive agrochemical formulations is usually set at F50 not less than 250 h, although lower thresholds are accepted for neutral pH cleaners. Drop impact is tested according to UN 49 CFR §178.603 with drop heights of 1.8 m for Packing Group I, 1.2 m for Packing Group II, and 0.8 m for Packing Group III after conditioning at −18 °C for 24 h. Leakproofness after closure torque is checked by internal air pressure at 20 kPa for 10 min, with the closure and gasket assembled exactly as in commercial filling. Processing boundaries must be respected: prolonged melt residence time above 205 °C increases gel formation and reduces ESCR; low mold temperature below 5 °C produces visible flow lines and raises internal stress. The final articles are used for agricultural emulsifiable concentrates, industrial detergents, water treatment chemicals, and UN-certified intermediate bulk container components.

    RequirementStandard / methodTest conditionAcceptance benchmark for HDPE industrial packaging
    Melt mass-flow rateISO 1133-1:2022190 °C, 2.16 kgGrade data sheet reference value, not a pass/fail
    DensityISO 1183-1:201923 °C0.945–0.965 g/cm³ for high-density polyethylene
    Environmental stress-crack resistanceASTM D1693 Condition B10% Igepal CO-630, 50 °CF50 ≥ 100 h for neutral media; higher internal limit for agrochemicals
    Drop impactUN 49 CFR §178.603−18 °C after 24 hNo leakage at Packing Group drop height
    Tensile yield stressISO 527-2:2012 type 1A50 mm/min, 23 °C≥ 20 MPa for process consistency

    What Causes Parison Weakening and Drop-Failure Variation in Thin-Wall Bottle Production?

    In multi-cavity production of 300 mL to 500 mL detergent and personal-care bottles, HDPE KB161K is processed on continuous shuttle blow molders with 4 to 8 cavities. The targeted bottle body wall thickness is 0.55 mm to 0.85 mm, with shoulder and pinch-off zones allowed to reach 1.0 mm only when the mold design includes local cooling inserts. Melt temperature at the die exit is kept between 180 °C and 195 °C, a lower window than industrial jerrican production because thin parison walls are sensitive to sag. The die gap is set from 0.8 mm to 1.4 mm, and parison programming is used to move wall thickness from the body section into the neck and base flash. Mold temperature is controlled at 8 °C to 12 °C, with high-flow water circuits around the pinch-off and neck inserts. Blow pressure is maintained at 0.5 MPa to 0.8 MPa, and the cycle time is typically 8 s to 14 s per cavity. Flash thickness at the pinch-off is not allowed to fall below 0.25 mm; below this value drop-impact failures concentrate at the mold parting line. Drop impact is evaluated under ASTM D2463-15, with the bottle filled to nominal capacity and conditioned at 23 °C and −18 °C for 24 h. Stress-crack behavior in thin-wall detergent bottles is assessed with a modified in-house round-robin method based on ASTM D1693; published data for this specific grade in thin-wall detergent bottle geometry is limited, so end-user qualification is required before formula changes. Pellet surface condensation must be controlled when plant ambient relative humidity exceeds 80%. A hopper dryer set at 70 °C with 1.5 h residence time is applied only where condensate is visible because polyethylene does not require routine pre-drying. Flame or corona treatment for label adhesion is capped at 40 dyn/cm to 45 dyn/cm; higher treatment levels can oxidize the neck sealing surface and reduce cap torque retention. The terminal articles are bottles for laundry detergents, hand soap, surface cleaners, and light-duty industrial liquids with continuous-thread necks of 24-410, 28-410, and 33-400 dimensions.

    Thin-wall beverage and sauce closures molded from HDPE KB161K require an injection molding window that balances high flow length, torque retention, and low warpage. The preferred applications are medium-wall caps, overcaps, and tamper-evident closures with part weights from 2.2 g to 5.5 g and wall thicknesses from 0.6 mm to 1.0 mm. Tooling is normally built with 32 to 96 cavities, hot runners, and valve-gated drops on a 350 t to 650 t hydraulic or hybrid injection molding machine. Melt temperature is held at 210 °C to 235 °C, mold temperature at 15 °C to 25 °C, and injection velocity at 120 mm/s to 220 mm/s. Holding pressure is set between 45 MPa and 75 MPa, with a back pressure of 0.5 MPa to 1.0 MPa to maintain melt homogeneity without excessive shear heating. Cycle time for a 2.8 g water-bottle cap is typically 4.5 s to 8.0 s when the mold uses conformal cooling and post-mold cooling plates. Food-contact compliance is verified under FDA 21 CFR 177.1520 for olefin polymers, and European migration is checked against EU Regulation No 10/2011 with an overall migration limit of 10 mg/dm². Child-resistant designs are tested under ISO 8317:2015. Torque performance must be validated on the specific neck finish; published data for this specific grade in high-cavitation closure tooling is limited, so spiral-flow and torque-retention trials are required before tooling commitment. The terminal caps are used for still water, sauces, edible oil, household chemicals, and pharmaceutical closures excluding those requiring oxygen scavenging or high-vapor barrier liners.

    Three-Dimensional Suction Blow Molding of Automotive Washer Reservoirs

    Automotive washer reservoirs with convoluted shapes are produced from HDPE KB161K on 3D blow-molding machines equipped with a six-axis robot and a suction blow pin. This conversion route is selected when the reservoir must follow the wheel arch or engine bay envelope and cannot be formed efficiently with a conventional two-platen shuttle mold. The reservoir capacity is typically 2.5 L to 5.5 L, and the nominal wall thickness is 1.2 mm to 2.5 mm. Melt temperature at the die exit is held between 190 °C and 210 °C. The accumulator head is set 5 °C to 8 °C below the die exit to stabilize the parison skin, and the parison drop time is kept between 2 s and 5 s to minimize sag before mold closure. Suction blow pressure is limited to 0.4 MPa to 0.8 MPa, and mold temperature is controlled at 8 °C to 16 °C. Fluid resistance is evaluated by immersion in methanol, ethanol, ethylene glycol, and surfactant solutions according to ISO 175:2010; the pass criterion is retained impact resistance and not more than 2% mass change after 168 h at 60 °C. Heat aging is assessed under ISO 2578 at 80 °C for 500 h, with tensile strength retention above 80% of the original value. The application boundary is explicit: HDPE KB161K is suitable for washer fluid reservoirs and non-pressurized auxiliary liquid reservoirs, but it is not suitable for pressurized brake-fluid reservoirs or diesel expansion tanks that require continuous service above 90 °C. Vacuum leak testing after welding of filler necks and mounting brackets is performed at −30 kPa with a pressure decay limit of 0.5 kPa/min. Final articles are shipped to tier-one suppliers as assembled washer tanks with integrated filler necks, level sensors, and pump grommets.

    Industrial dunnage and transport trays are produced from HDPE KB161K by flat-die sheet extrusion followed by vacuum forming. The extrusion line consists of a 120 mm, 30:1 L/D single-screw extruder with a barrier screw, a melt pump, and a flexible-lip sheet die with a working width of 800 mm to 1200 mm. Melt temperature at the die is maintained between 190 °C and 215 °C, while the polished three-roll stack is heated to 70 °C to 95 °C to control surface gloss and sheet flatness. Sheet thickness is operated from 0.8 mm to 4.0 mm, with online beta gauging maintaining a tolerance of ±0.05 mm for 2.0 mm sheet. Vacuum forming is conducted at a sheet surface temperature of 135 °C to 160 °C, with mold temperature controlled at 25 °C to 40 °C and plug-assist speed adjusted to avoid plug marks. Typical forming cycle time is 35 s to 60 s depending on draw depth and part mass. Machine-direction sheet shrinkage after forming is accounted for at 1.2% to 1.8% when cutting mold dimensions; transverse shrinkage is generally lower. Final articles include separator sheets, pallet top frames, tote liners, automotive trunk liners, and non-rated machinery guards. Where food-contact or hygienic use is required, the sheet producer must separately verify migration limits under FDA 21 CFR 177.1520 and EU Regulation No 10/2011 because recycled content or process aids may alter the compliance status of the formed part.

    When Post-Industrial Regrind Loadings Exceed 30 wt% in Extrusion Blow Molding

    Post-industrial regrind from HDPE KB161K scrap is reintroduced into extrusion blow molding only after granulation through a 6 mm screen and blending with virgin pellets in a gravimetric batch or continuous loss-in-weight blender. At regrind loadings of 10 wt% to 20 wt%, the observable process drift is minor: parison sag may increase because the regrind contains shredded bottle walls with lower bulk density, and the die gap may need to be reduced by 0.05 mm to 0.15 mm to compensate. At 30 wt% to 40 wt%, the effects become process-critical in UN-certified containers. Environmental stress-crack resistance typically declines as a result of repeated heat history and shear-induced chain scission; ESCR F50 under ASTM D1693 Condition B can fall by approximately 30% to 50% relative to the virgin material, although published data for this specific grade with post-industrial regrind is limited. Melt flow rate measured by ISO 1133-1:2022 at 190 °C with 2.16 kg can shift upward by 0.05 g/10 min to 0.10 g/10 min, indicating slightly reduced average molecular weight. Gel particle density rises when regrind is stored outdoors or when startup purge material is ground back into the feed stream; the resulting pinhole risk in 0.8 mm thin-wall sections is the primary reason that regrind levels above 50 wt% are not recommended for UN-rated chemical packaging. Suction-fed regrind hoppers should be fitted with a 250 µm screen pack at the machine feed throat to exclude film flakes and paper label fragments. First-generation post-industrial regrind is preferred over post-consumer recyclate for tight-head jerrican production because post-consumer HDPE carries higher polydisperse contamination and may require a second extruder with vacuum degassing. The final products containing clean post-industrial regrind are typically non-food industrial containers, drainage fittings, and protective corner boards, while food-contact or pharmaceutical containers are restricted to virgin HDPE KB161K unless the molder has completed challenge-test contamination studies under the applicable regulatory framework.

    Free Quote

    Competitive TPC (Japan) HDPE KB161K prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The resin designated in procurement records as TPC (Japan) HDPE KB161K is a high-density polyethylene supplied for extrusion blow moulding. Manufacturer technical data place its nominal density at 0.960 g/cm³ as measured by ASTM D1505-18 or ISO 1183-1:2019, and its melt mass-flow rate at 0.25 g/10 min to 0.35 g/10 min under ASTM D1238-20 or ISO 1133-1:2022 at 190 °C/2.16 kg. The grade is therefore positioned for high-melt-strength processing rather than high-flow injection moulding; the low melt-flow rate indicates sufficient molecular weight for controlled parison hang time and axial wall-thickness uniformity.

    Documentation should be read as a specification envelope rather than a single-point property guarantee. The controlling document for any incoming lot is the supplier certificate of analysis. The data below consolidate the typical published indices used for material qualification; where a value is not available for the specific production campaign, a test should be performed before release.

    What Rheological and Mechanical Indices Define KB161K?

    Representative physical, mechanical, and thermal property envelope for KB161K
    PropertyTest methodUnitTypical value
    Melt mass-flow rateASTM D1238-20/ISO 1133-1:2022g/10 min0.25–0.35
    DensityASTM D1505-18/ISO 1183-1:2019g/cm³0.960
    Tensile stress at yieldASTM D638-14/ISO 527-2:2012MPa27–30
    Tensile elongation at breakASTM D638-14/ISO 527-2:2012%>600
    Flexural modulus, 2% secantASTM D790-17/ISO 178:2019MPa1,250–1,400
    Notched Izod impact at 23 °CASTM D256-10/ISO 180:2000kJ/m²5–7
    Vicat softening temperature A50ASTM D1525-17/ISO 306:2022°C126–130
    Environmental stress-crack resistance F50ASTM D1693-15h20–60
    Hardness Shore DASTM D2240-15/ISO 868—64–66

    The 0.960 g/cm³ density places KB161K among the higher-density HDPE blow moulding grades. The flexural modulus is therefore elevated, which supports stacking performance, but environmental stress-crack resistance is generally lower than that of medium-density or lower-density copolymers. The 20 h to 60 h F50 window under ASTM D1693-15 should be considered resin-level data only; bottle-level resistance is governed by wall thickness, orientation, pinch-off quality, and contact with stress-crack-promoting formulations.

    The low melt-flow rate affects rheology directly. At 190 °C, a 0.25 g/10 min MFR corresponds to a higher zero-shear viscosity than a 0.7 g/10 min blow moulding grade. In practical terms, the extruder torque and die-head pressure rise, while output may become limited by screw speed or amperage rather than downstream cooling. The processor should evaluate the screw drive margin before switching from a higher-MFR resin.

    Melt Temperature, Die Swell, and Parison Programming Boundaries

    Extrusion blow moulding with KB161K is performed within a melt-temperature window of 180 °C to 230 °C. Barrel set points should rise from feed to head; reverse flat profiles are not recommended because they can increase shear heating and degrade the melt. At melt temperatures above 230 °C, oxidative chain scission reduces melt strength and can produce gel defects. At temperatures below 180 °C, unmelted particles, elevated backpressure, and poor parison surface quality are likely. The actual optimum is machine-specific; a temperature profile of 190 °C to 210 °C at the die head is typical for single-layer lines, but it must be confirmed by melt-temperature measurements rather than barrel set points alone.

    Die swell is significant because of the low MFR. The parison gap should be set smaller than the desired wall thickness after swell. A divided blow head with axial parison programming is generally necessary for containers above 1 L to control thin spots near the shoulder and base. On shuttle machines with a 60 mm to 80 mm extruder, grooved-feed sections improve feed stability, but they can generate high discharge pressure. The screw L/D ratio should be at least 24:1; shorter screws may not provide sufficient plastication for the high-density resin at high outputs.

    Published data for this specific extruder configuration is limited; the practical boundaries above are derived from general HDPE blow moulding practice and should be revalidated on the target line.

    Parison sag is controlled by melt viscosity and parison length. With KB161K, wall-thickness variation of ±0.5 % to ±1.0 % by weight is attainable with closed-loop gravimetric feed; manual extruder control typically produces larger variation. The bottom pinch-off area is a sensitive indicator: flash thickness above 0.3 mm at the weld line often indicates insufficient clamp pressure or excessive parison length, and can lead to burst failures in column crush testing.

    Pre-drying is not required for the resin itself under dry indoor storage conditions at ≤30 °C and <60 % relative humidity. Surface moisture from condensation can introduce splay and voids; if condensation is visible, pre-drying at 80 °C for 1 h to 2 h is sufficient. Regrind use up to 20 % is commonly practised in non-critical containers, but each addition of regrind increases the melt-flow-rate drift and lowers ESCR; the upper limit must be set by impact and stress-crack testing of the finished article.

    Rigid household and personal care containers below 5 L represent the primary application envelope for KB161K. Typical blown wall thicknesses range from 0.4 mm to 1.5 mm, covering detergent, fabric softener, shampoo, and cosmetic bottles. The flexural modulus of 1,250 MPa to 1,400 MPa permits down-gauging only where top-load and side-load specifications are revalidated. For finished containers, top-load performance is evaluated by ASTM D2659-16; values of 250 N to 500 N at 23 °C are common for small-to-medium bottles depending on geometry and wall stock. The test does not by itself predict warehouse stacking at elevated temperature; a derating factor should be applied for storage above 40 °C.

    When the intended fill contains surfactants, essential oils, or softening agents, bottle-level stress-crack testing is required. ASTM D2561-17 evaluates stress-crack resistance of blow-moulded containers, but many end-users specify an internal protocol with a fixed strain and chemical exposure time. Resin-level ESCR alone cannot replicate the pinched weld, orientation, or wall-thickness variation of a blow-moulded part. For products with high ESCR demands, a lower-density HDPE or high-molecular-weight copolymer should be considered; KB161K is not positioned as a high-ESCR grade.

    For food-contact and personal-care applications, the end-user must verify compliance with FDA 21 CFR 177.1520, EU 10/2011, and applicable national measures. The grade is an olefin polymer; clearance under 21 CFR 177.1520 is dependent on end-use conditions and migration limits, not on the resin designation alone. A supplier declaration covering REACH, RoHS, and residual monomers should be requested before commercial use.

    KB161K is not recommended for continuous service above 80 °C or in contact with strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents, which can swell polyethylene and accelerate stress cracking. Repeated autoclaving or hot alkaline cleaning can also reduce service life. The user should test the filled container under the intended distribution environment, including temperature cycling, cap torque, and surface wetting.

    When KB161K Replaces a Lower-Density or Injection Moulding Grade

    The principal contrast is between extrusion blow moulding and injection moulding. General-purpose injection HDPE grades have melt-flow rates of 5 g/10 min to 20 g/10 min, allowing thin-wall injection with long flow lengths but insufficient melt strength for parison hang time. Lower-density blow moulding grades, typically 0.945 g/cm³ to 0.952 g/cm³, provide better ESCR but lower flexural modulus. KB161K occupies a high-density, medium-MFR segment where top-load strength and dimensional stability are more important than extreme environmental stress-crack resistance.

    Comparative positioning of KB161K against HDPE product classes
    IndicatorKB161KGeneral-purpose injection HDPEHigh-ESCR blow moulding HDPE
    Melt-flow rate at 190 °C, 2.16 kg0.25–0.35 g/10 min5–20 g/10 min0.2–0.5 g/10 min
    Density0.960 g/cm³0.955–0.965 g/cm³0.945–0.951 g/cm³
    Flexural modulus1,250–1,400 MPa1,000–1,500 MPa800–1,000 MPa
    ESCR F5020–60 hnot typically specified>100 h
    Typical processextrusion blow mouldinginjection mouldingextrusion blow moulding

    Before substituting KB161K into a tool designed for a higher-MFR resin, the processor should compare melt pressure, die swell, and parison sag. In practice, a mould running a 0.7 g/10 min resin may require a wider die gap and lower screw speed on KB161K to maintain the same parison length. Conversely, if a lower-density high-ESCR resin is substituted out, the finished container may show improved top-load strength but reduced chemical stress-crack life; both must be measured, not inferred from density or MFR alone.

    Incoming quality assurance for blow moulding operations should include melt-flow-rate shift, density, and particle contamination. A shift of 0.05 g/10 min in MFR can alter parison sag and bottle weight distribution; therefore lot-to-lot melt-flow-rate drift should be tracked using ASTM D1238-20. Density should remain within ±0.002 g/cm³ of the nominal value to avoid disturbances in hardened wall thickness. Black specks and gel counts should be monitored by extruding a parison and visually comparing against a retained reference standard, although the quantitative method depends on the converter’s internal procedure.

    The Vicat softening point of 126 °C to 130 °C is a short-term thermal parameter and does not indicate long-term load-bearing capability. External storage under ultraviolet exposure requires a UV-stabilized formulation; the standard KB161K grade is not supplied with a UV-stabilizer unless specified on the purchase order.