Tpc Japan Hdpe Kb161a

TPC (Japan) HDPE KB161A

    • Product Name: TPC (Japan) HDPE KB161A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 497553
    Density 0.961 g/cm3
    Melt Flow Rate 0.35 g/10 min
    Tensile Strength At Yield 30.0 MPa
    Tensile Elongation At Break 600%
    Flexural Modulus 1.30 GPa
    Notched Izod Impact Strength 0.150 J/cm
    Shore D Hardness 66
    Vicat Softening Point 128 deg C
    Heat Deflection Temperature 80.0 deg C at 0.45 MPa
    Brittleness Temperature < -70.0 deg C
    Environmental Stress Crack Resistance > 1000 hr
    Melting Point 135 deg C
    Water Absorption < 0.010%
    Linear Mold Shrinkage 0.020 cm/cm
    Thermal Conductivity 0.400 W/m-K
    Specific Heat 1.90 J/g-deg C
    Dielectric Constant 2.3
    Volume Resistivity > 1.00e+15 ohm-cm

    As an accredited TPC (Japan) HDPE KB161A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KB161A is typically packaged in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped for shipment.
    Container Loading (20′ FCL) Standard 20' FCL container loading: approximately 18 MT of TPC (Japan) HDPE KB161A in 25 kg bags, depending on palletization.
    Shipping TPC (Japan) HDPE KB161A is shipped as solid, non-hazardous polyethylene pellets in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. It is not regulated for transport. Store dry, keep containers closed, and avoid heat, sunlight, ignition, dust, and static buildup. Handle with standard equipment.
    Storage Store TPC (Japan) HDPE KB161A in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, moisture, and ignition sources. Keep original bags or containers tightly closed and palletized to prevent contamination and crushing. Separate from strong oxidizers, acids, and incompatible chemicals. Maintain clean handling areas; avoid prolonged UV exposure. Follow local regulations and manufacturer guidance. Do not stack excessively.
    Shelf Life Shelf life for TPC (Japan) HDPE KB161A is 12 months when stored cool, dry, unopened, away from sunlight and moisture.
    Application of TPC (Japan) HDPE KB161A

    On single-station shuttle blow-moulding lines converting TPC (Japan) HDPE KB161A into household surface-cleaner and industrial detergent containers between 500 mL and 5 L, the dominant production failure is environmental stress crack propagation at the tail flash pinch-off, not burst failure under top-load. The fracture typically initiates where cold-mould residual stress coincides with the flash-removal weld line near the container base edge. The process uses a 45–65 mm extruder with 24:1 to 30:1 L/D and a barrier screw having compression ratio 3.0:1 to 3.5:1; melt temperature at the die is held between 175°C and 195°C, while mould coolant is maintained at 10–16°C. Blow air is filtered to 0.1–1.0 µm and dried to a pressure dew point below -20°C to limit internal surface micro-pitting. In high-humidity storage regions where silo surface moisture exceeds 0.05 wt%, hopper desiccant drying at 60–70°C for 2–4 h is required to prevent pinholes and parison pitting. Formulation addition ratio in this non-food segment is 96.0–97.5 wt% KB161A, 2.0–3.5 wt% custom colour masterbatch, 0.5–1.0 wt% processing stabilizer masterbatch, and 0.3–0.8 wt% slip/anti-block masterbatch; internal flash and top scrap are metered into the charge at 10–25 wt% of total weight, replacing an equivalent virgin resin mass. Compliance is governed by UN 3H1 qualification under 49 CFR 178.509, ADR/RID Chapter 6.5, and IMDG Code packaging provisions for liquid detergents classified as UN Class 8 or Class 3; EU Directive 94/62/EC packaging heavy-metal limits apply with total lead, cadmium, mercury, and hexavalent chromium below 100 ppm by weight. Downstream production includes parison programming with diverging die gap, blow pressure 0.6–0.9 MPa, pre-pinch and post-pinch stations, handle-flash removal, and post-mould cooling fixtures for dimensional stability. Terminal products are trigger-spray bottles, 1 L and 5 L screw-finish retail bottles, and short-neck industrial containers with UN-approved closures.

    What Limits Odor, Taint, and Migration in Extrusion Blow Moulded Food-Contact Bottles?

    Food-contact extrusion blow moulding with KB161A is constrained less by mechanical shortfall than by organoleptic acceptability, migration of low-molecular-weight oxidation products, and closure torque retention after ambient wet distribution. The resin is processed at melt temperature 170–190°C, with die gap adjusted to produce parison swell between 30% and 50% on a 45–55 mm extruder with 24:1 L/D; screw speed is limited to avoid shear heating above 190°C because oxidation by-products at the die lip can impart detectable odor to water-filled bottles. Regulatory compliance for food contact cites FDA 21 CFR 177.1520(c) items 2.1 and 3.1 for polyethylene homopolymers intended for aqueous, acidic, alcoholic, and fatty food contact, and EU Regulation (EU) No 10/2011 Annex I and Annex II for specific migration limits and overall migration not exceeding 10 mg/dm² using EN 1186-1 and EN 13130 quantification. For exports to the PRC, GB 4806.7-2016 food-contact plastic material requirements may also apply. Formulation addition ratio is 100 wt% virgin KB161A with optional 0.1–0.3 wt% external lubricant/process aid and 0.2–0.8 wt% white masterbatch; post-consumer regrind is excluded unless a functional barrier completely separates the recycled layer from food contact under EU 10/2011 Article 6 and the relevant 21 CFR 177.1520(c) justification. Downstream production uses shuttle blow moulders with continuous flash removal, leak testing at 0.03–0.05 MPa, and induction seal surface flatness control before filling. Terminal products are 250 mL to 2 L milk, juice, vinegar, cooking oil, and sauce bottles. Monolayer HDPE oxygen transmission is not sufficient for long-shelf-life oxygen-sensitive foods; published oxygen transmission data for unmodified KB161A monolayer food bottles is limited, so finished-article barrier validation should be performed using ASTM D3985 or ISO 15105-2.

    Application sectorPrimary standardTest method or clauseCritical verification condition
    Household and industrial chemical containersUN 3H1, 49 CFR 178.509, ADR/RID 6.5Stack load, drop, hydraulic pressureDrop at -18°C after conditioning; stack at 40°C for 28 days
    Food-contact bottlesFDA 21 CFR 177.1520(c), EU 10/2011, GB 4806.7-2016EN 1186-1, EN 13130, ASTM D3985Overall migration ≤ 10 mg/dm²; SML for antioxidant additives
    Pharmaceutical oral solid dose containersUSP <661.1>, Ph. Eur. 3.1.3, USP <671>Physicochemical tests, water vapour transmissionExtractables profile; WVTR per package monograph
    Agrochemical containersUN 1H1/1H2, 49 CFR 178.509, ADR/RIDASTM D1693 Cond B, ISO 4892-2ESCR after UV exposure; drop after stacking
    Automotive aftermarket fluid containersUN 3H1, OEM packaging specificationsASTM D1693 Cond B, full-filled storageESCR with 50/50 ethylene glycol/water at 60°C

    In clean-room extrusion blow moulding for oral solid dose containers, KB161A is processed under a different validation hierarchy: the primary specification is not environmental stress crack resistance but extractables, water-vapour permeation, and black-spec contamination of the drug-contact surface. Melt temperature is limited to 160–180°C on a 35–50 mm extruder, with screw speed held below 60 rpm to reduce shear heating and carbonized resin generation. Filtered blow air at 0.2 µm retention is mandatory because the container interior is formed after extrusion, and any lubricant, release agent, or particulate contamination in the blow air transfers directly to the drug-contact surface. Formulation addition ratio is 100 wt% virgin KB161A in monograph configurations that prohibit post-consumer recycled content; for over-the-counter oral solid dose products where regulatory approval permits, a maximum 5 wt% closed-loop plant regrind is used only when the regrind is lot-traceable and generated from the same registered resin. Compliance is anchored to USP <661.1> plastic packaging physicochemical testing, Ph. Eur. 3.1.3 polyolefin specifications, and USP <671> water vapour permeation when the package monograph includes a desiccant or moisture-sensitive drug product. Downstream production includes leak testing at 0.03–0.05 MPa, torque retention testing of child-resistant closure interfaces, and induction sealing surface flatness control on the neck finish. Terminal products are 30–500 mL round and square prescription bottles, over-the-counter oral solid dose containers, and vitamin or nutraceutical packages with 38 mm and 45 mm neck finishes.

    Barrier-Layer Coextrusion in Automotive Aftermarket Fluid Containers

    When the packaged automotive aftermarket fluid contains ethylene glycol, methanol, or fluorosurfactant windshield additives, monolayer KB161A is usually replaced by a six-layer coextrusion structure because the packaged liquid can act as a permeant and an environmental stress-crack accelerant. KB161A is used as the outer carrier and inner product-contact layers, a 5–10 wt% adhesive tie layer and a 3–7 wt% EVOH or polyamide barrier are inserted, and a mixed flashed coextrudate regrind layer is run at 15–20 wt% of total wall thickness through a dedicated extruder. The combined outer and inner KB161A layers are metered at 65–80 wt% of the total wall, with the regrind extruder drawing from trim that is dried at 70°C for 4 h when ambient relative humidity exceeds 60%. Production uses a 70–90 mm main extruder, 24:1 L/D, and a six-layer accumulator die with gear pumps for layer thickness stability; melt temperature at the die is 175–190°C, while the barrier extruder is held at 195–210°C to prevent ethylene-vinyl alcohol thermal degradation. Addition ratio of carbon black or UV stabilizer masterbatch is 2.0–2.5 wt% in the outer KB161A layer, and acid scavenger masterbatch at 0.2–0.5 wt% is added when recycled post-industrial barrier trim is used. Compliance is governed by UN 3H1 performance tests for non-removable head containers and by individual OEM specifications for coolant and screenwash packaging, including hot-fill resistance at 60°C and drop impact at -30°C for 1 L and 5 L containers. Terminal products are translucent and opaque 1–10 L bottles for coolant, windshield washer fluid, diesel exhaust fluid, and hydraulic jack oil. ESCR validation follows ASTM D1693 condition B, but the stress-crack agent should be selected to mimic the specific packaged fluid rather than a neutral surfactant; published data for KB161A in barrier coextrusion structures is limited, so full-filled storage at 50°C for 28 days is required during bottle qualification.

    Processing parameterShuttle blow moulder, household/pharmaAccumulator head, jerrycan/drumSix-layer coextrusion, automotive
    Extruder screw diameter35–55 mm70–90 mm70–90 mm main, 35–50 mm barrier
    L/D ratio24:1–30:124:1–30:124:1
    Melt temperature at die160–190°C165–185°C175–190°C
    Blow pressure0.6–0.9 MPa0.6–1.0 MPa0.7–1.0 MPa
    Mould coolant temperature8–16°C8–14°C8–12°C
    Regrind addition level0–25 wt%10–20 wt%15–20 wt%

    Agrochemical jerry-can production with KB161A places the highest simultaneous demand on pinch-off weld toughness, UV resistance after prolonged outdoor storage, and chemical compatibility with emulsifiable concentrates. The conversion line typically uses an accumulator-head blow-moulder with a 70–90 mm extruder, 24:1 L/D, and a die head temperature of 165–185°C; parison programming is weighted to the handle and base pinch-off, where wall thickness is increased by 15–30% relative to sidewall to compensate for stress concentration. Mould cooling is run at 8–14°C, and blow air is dried to a dew point below -20°C to reduce internal surface haze and weld-line weakness. Formulation addition ratio is 95.0–97.0 wt% KB161A, 2.0–2.5 wt% carbon black masterbatch, 0.5–1.0 wt% antioxidant masterbatch, and 10–20 wt% internal flash regrind; regrind exceeding 20 wt% should not be used without ESCR revalidation because the emulsifiable concentrate packaged in agricultural chemicals acts as an aggressive stress-crack agent. Compliance includes UN 1H1/1H2 performance qualification under 49 CFR 178.509, ADR/RID, and IMDG Code provisions, including hydraulic pressure, stacking at 40°C, and drop tests after UV ageing. Terminal products are 5 L, 10 L, 20 L, and 25 L open-head or closed-head jerry cans for pesticides, herbicides, fungicides, surfactants, and adjuvants, along with 200 L non-removable head drums for agricultural emulsifiable concentrates. ASTM D1693 condition B ESCR should be re-run after 1000 h of ISO 4892-2 UV exposure or after shelf storage in non-shaded warehouse conditions.

    High-Gloss Cosmetic Bottle Surface Replication and Parison Programming

    For 50 mL to 500 mL high-gloss cosmetic bottles, the critical process variable is mould surface replication rather than mechanical load resistance. KB161A is run on a 40–50 mm extruder with 22:1 to 25:1 L/D and a low-shear high-gloss screw; melt temperature is limited to 165–180°C to prevent thermal yellowing of pearlescent or pastel masterbatches. Polished steel moulds with mirror finish are held at 8–12°C, and blow air is filtered to 0.1 µm to eliminate internal surface defects. Addition ratio is 97.0–98.5 wt% KB161A, 2.0–3.0 wt% colour masterbatch, and 0.2–0.5 wt% slip/anti-static masterbatch; regrind is not used when surface gloss and shade stability are critical, or is limited to 10 wt% closed-loop regrind from the same colour family. Compliance includes EU Cosmetic Products Regulation (EC) No 1223/2009 for packaging suitability and REACH Regulation (EC) No 1907/2006 for substances in the article. Terminal products are shampoo, body wash, conditioner, cosmetic lotion, and pump bottles with 24/410, 28/410, and 33/410 neck finishes.

    Free Quote

    Competitive TPC (Japan) HDPE KB161A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KB161A is a high-molecular-weight high-density polyethylene developed for extrusion blow moulding of rigid industrial packaging, technical hollow parts, and multilayer barrier structures. The designation belongs to the low-melt-flow interval typical of blow moulding grades: melt mass-flow rate of 0.30–0.50 g/10 min at 190 °C/2.16 kg when tested to ISO 1133-1:2022, and density of 0.955–0.959 g/cm³ at 23 °C when tested to ISO 1183-1:2019. Where a specific production lot is to be qualified, the TPC certificate of analysis governs; published data for this specific configuration are limited outside supplier documentation, and the following statements therefore distinguish KB161A from other HDPE classes on the basis of melt-flow class, molecular-weight distribution, environmental stress-cracking resistance, and parison rheology.

    The grade is not targeted at film extrusion or high-flow injection moulding. Its viscosity profile is selected to limit parison sag during intermittent accumulator-head extrusion and to maintain seam-weld integrity in parts with differentiated wall thickness. Downstream converters should verify additive formulation and food-contact status for the finished article rather than infer compliance from the resin designation alone.

    Melt Rheology, Parison Control, and Extruder Configuration

    The low melt-flow interval of 0.30–0.50 g/10 min corresponds to a high melt viscosity that reduces parison drawdown after the accumulator head opens. In applications where blow-up ratio exceeds 3.0:1, a grooved-feed extruder with screw length-to-diameter ratio of 24:1 to 30:1 and a barrier or Maddock mixing section is standard. Melt temperatures are maintained at 190–220 °C, with a target tolerance of ±5 °C. Below 190 °C, incomplete plastication and melt fracture can occur; above 220 °C, thermal-oxidative chain scission increases gel formation and reduces environmental stress-cracking resistance. On production accumulator-head machines, the thermal residence time after screw shutdown should be minimised because stagnant melt at wall temperatures above 220 °C can degrade within 20–30 minutes and produce black specks in the next shot.

    Die swell for this polymer class is normally in the region of 20–40% depending on die shear rate and melt temperature. A typical monolayer container with 2.0 mm final wall thickness may use a die gap of 1.2–1.6 mm, with pre-blow timing and blow pressure of 0.4–0.8 MPa adjusted to control thickness at the pinch-off areas. Pinch-off weld strength is checked on production blow-moulding equipment because failures near the tail flash and handle regions are the most common processing faults when regrind addition approaches 30 wt% or when the mould temperature drops below 10 °C.

    Comparative Melt-Flow and Stress-Cracking Class
    PropertyTest methodKB161A blow moulding classHigh-flow injection HDPEFilm extrusion HDPE
    Melt mass-flow rate, 190 °C/2.16 kgISO 1133-1:20220.30–0.50 g/10 min8–30 g/10 min0.5–1.5 g/10 min
    Density, 23 °CISO 1183-1:20190.955–0.959 g/cm³0.960–0.965 g/cm³0.945–0.955 g/cm³
    Tensile yield stressASTM D638-1424–28 MPa27–32 MPa21–25 MPa
    ESCR F50, 10% Igepal CO-630 at 50 °CASTM D1693-21300–600 h or above5–25 h100–300 h

    Ranges in the table are class-typical and must not be used for lot acceptance without TPC documentation.

    What Distinguishes KB161A from Lower-Viscosity Injection-Grade HDPE in ESCR and Mechanical Strength?

    Environmental stress-cracking resistance is the principal differentiator. Injection-grade HDPE with melt-flow rates above 10 g/10 min is selected for thin-wall packaging and closure applications, but its short relaxation times and lower molecular weight reduce resistance to stress cracking in contact with surfactants, oils, and agrochemical formulations. Blow-moulding grades of KB161A's melt-flow class resist cracking at moulded-in stress concentrations because of their more extended molecular-weight distribution and higher chain entanglement density. The F50 time under ASTM D1693-21, Condition A, can differ by an order of magnitude between these polymer classes, but exact values require moulded plaques and may be invalid if regrind is improperly blended.

    The tensile yield stress of a density 0.955–0.959 g/cm³ blow moulding grade is typically 24–28 MPa under ASTM D638-14, which is below the 27–32 MPa range of higher-density injection grades but sufficient for drum sidewall load-bearing when part geometry is designed with a flexural modulus of 800–1000 MPa per ASTM D790-17. Low-temperature impact resistance is retained at -20 °C to -40 °C, but notched impact values should not be transferred from compression-moulded sheet to blow-moulded parts because weld lines and thickness gradients control actual performance.

    For industrial containers and technical hollow parts, KB161A is converted into sectors such as 5 L to 60 L open-head and tight-head containers for water-based chemicals, detergent formulations, agricultural auxiliaries, and UN-certified 1H1/1H2 dangerous goods packaging. Qualification for dangerous goods requires the finished packaging to pass leakproofness, hydraulic-pressure, stack, and drop tests under the applicable transport regulation; no resin designation alone conveys UN certification.

    Because HDPE is not hygroscopic, pellet pre-drying is generally unnecessary when bags are stored closed and the hopper is protected from condensation. In high-humidity production halls with relative humidity above 80% or when regrind has been washed, surface moisture can cause splay and weld-line porosity in blow-moulded parts. A desiccant hopper dryer set at 70–80 °C for 2 h is applied to restore surface quality. Hot-air drying above 90 °C for extended periods is avoided because oxidative yellowing of additives can occur.

    Typical compliance framework for finished articles
    Regulation or standardTest or scopeApplication condition
    FDA 21 CFR 177.1520(c)Olefin polymers for food-contact articlesVerified via supplier food-contact statement and migration testing
    EU 10/2011Plastics in food-contact materialsOverall migration 10 mg/dm² unless migration testing is exempted
    REACH (EC) No 1907/2006SVHC screening and authorizationArticle assessment per supplier safety data sheet
    RoHS Directive 2011/65/EURestricted substances in EEEOnly if the moulded part is used in electrical/electronic equipment
    UN ADR/RID/IMDG 1H1/1H2Dangerous goods packagingDesign-type tests on closure, drop, stack, and leakproofness

    When Co-Extrusion with Barrier Layers Requires Thermal and Rheological Compatibility

    In multilayer blow moulding, KB161A can serve as the outer moisture-barrier layer, regrind layer, or inner layer in structures with polyamide or ethylene-vinyl alcohol copolymer (EVOH) barrier layers and maleated tie resins. The processing window is constrained by the least thermally stable layer; EVOH grades typically require melt temperatures below 220 °C, which coincides with the upper limit used to suppress HDPE chain scission. If the accumulator head or co-extrusion die is held above 220 °C during changeover or while purging, gel generation in the HDPE layer and charred EVOH deposits can produce layer instability and pinholing in the barrier layer.

    Viscosity mismatch at the layer interfaces is controlled by adjusting extruder temperature profiles rather than by changing layer ratio alone. Maleated tie resins used with HDPE generally exhibit higher melt-flow rates, and the KB161A low-MFR layer must be extruded with melt temperature at the upper end of 200–220 °C to reduce interfacial shear stress. Excessive back pressure from screen packs older than 100 h can produce melt-temperature override and loss of layer thickness control on six-extruder co-extrusion lines; screen pack replacement intervals are therefore defined by pressure rise rather than by time alone. Published data for the specific KB161A multilayer configuration is limited; pilot trials are used to establish parison programming curves because interlayer adhesion and trim scrap reuse alter the viscosity balance.

    When in-line regrind from flash, tails, and rejects is introduced, levels up to 30 wt% are generally reprocessed for industrial containers. Higher levels depress parison melt strength and can reduce ESCR below qualified values when the regrind has undergone multiple heat histories. A closed-loop granulator with screen size 8 mm and regrind dosing by gravimetric blender is used to hold bulk-density variability below ±2%. On manufacturing lines, when regrind fraction is increased beyond 30 wt%, shot-to-shot melt-temperature variation above ±3 °C and parison length variability above ±5 mm are common causes of rejection in leak tests. This is not a property of the virgin resin alone but of the blend's thermal history and particle-size distribution.

    For injection-blow or extrusion-blow tooling design, mould cooling channels with turbulent flow and Reynolds number above 10,000 are required to limit cycle time because HDPE has low thermal conductivity. With mould coolant at 10–15 °C, a wall thickness of 2.0 mm can require cooling times in the range of 20–40 s depending on parison temperature and blow pressure. Articles with wall-thickness transitions from 1.0 mm to 4.0 mm should be assessed for sink marks and post-mould shrinkage; post-mould shrinkage of HDPE blow moulding grades can reach 1.5–2.0% after 24 h at ambient temperature.

    Top