| HS Code | 191823 |
| Manufacturer | TPC (Japan) |
| Grade | KB158Z |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.958 g/cm³ |
| Melt Flow Rate | 0.15 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 29.0 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 1.20 GPa |
| Vicat Softening Point | 128°C |
| Hardness Shore D | 66 |
| Melting Point | 135°C |
| Thermal Expansion Coefficient | 1.20E-4 1/°C |
| Thermal Conductivity | 0.400 W/m·K |
| Electrical Resistivity | 1.00E+16 ohm·cm |
| Dielectric Constant | 2.3 |
| Dielectric Strength | 20 kV/mm |
As an accredited TPC (Japan) HDPE KB158Z factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KB158Z: 25 kg polyethylene-lined paper bags, 40 bags per pallet, 1,000 kg net per pallet. |
| Container Loading (20′ FCL) | TPC (Japan) HDPE KB158Z container loading: 20′ FCL, 25 kg bags, palletized, shrink-wrapped, securely stowed for safe ocean export. |
| Shipping | TPC (Japan) HDPE KB158Z is a non-hazardous high-density polyethylene resin supplied as solid pellets. Standard shipping: 25 kg PE bags on pallets or 1000 kg jumbo bags, stretch-wrapped in sea containers. Keep dry, cool, away from direct sunlight; avoid contamination. Not regulated for transport. |
| Storage | Store TPC (Japan) HDPE KB158Z in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and oxidizing agents. Keep bags or containers sealed on pallets to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain clean handling equipment. Store at ambient temperature. Rotate stock first-in, first-out. Follow supplier safety data sheet and local regulations. |
| Shelf Life | TPC (Japan) HDPE KB158Z has a 24-month shelf life when stored cool, dry, ventilated, in unopened original packaging, protected from sunlight and moisture. |
In monolayer extrusion blow molding of household chemical containers, KB158Z is introduced as the virgin continuous-phase resin that closes the total feed blend to 100 wt%; clean dry process regrind from trimmed flash and defective bottles is metered at 20–30 wt%, and inorganic or organic color masterbatch is added at 2–4 wt%, with the remaining 66–78 wt% being virgin KB158Z. Lot-specific melt flow rate is verified under ASTM D1238-20 at 190 °C with a 2.16 kg piston load, and density under ASTM D792-20; certificate-of-analysis values outside the supplier control band are quarantined before dry-blending. The resin is not predried at ambient storage below 60% RH; if hopper residence exceeds 4 h in humid coastal warehouses, a desiccant or hot-air hopper set to 70–80 °C for 2 h is used to remove surface condensation. Extrusion is performed on a grooved-feed single-screw extruder with 25:1 L/D and barrier flight screw, with barrel zone set points from feed to metering at 170/180/190/200/205 °C, die head temperature at 195–205 °C, and die gap adjusted for a parison wall-thickness profile between 0.8 mm and 1.4 mm. Blow molds are maintained at 10–25 °C with 0.6–0.8 MPa blowing air; cycle time is dominated by flash removal rather than parison extrusion. Compliance for European retail detergent and cleaner containers is documented under REACH Regulation (EC) No 1907/2006, the Packaging and Packaging Waste Directive 94/62/EC, and, where food-contact use is claimed, FDA 21 CFR 177.1520. Terminal finished types include 500 mL–5 L bottles for hypochlorite bleach, neutral detergent, fabric softener, and trigger-spray general-purpose cleaners; containers in this segment are not intended for continuous hot-fill above 60 °C.
Surface gloss in injection blow molded HDPE cosmetic containers is governed by preform melt temperature uniformity, core rod temperature, and mold cooling rate rather than by melt index alone; with KB158Z constituting 97–99 wt% of the metered shot and a high-opacity white masterbatch added at 1–3 wt%, the material is injected through a hot runner maintained at 200–220 °C onto core rods at 90–120 °C, then transferred to blow cavities held at 15–25 °C and blown at 0.8–1.0 MPa air pressure. The injection blow molding process is selected for narrow-neck cosmetics packs with neck finish tolerances below 0.1 mm, and it minimizes pinch-off flash that would otherwise require post-mold facing. Compliance for cosmetic packaging is assessed under Regulation (EC) No 1223/2009 for cosmetic product contact, REACH (EC) No 1907/2006, and FDA 21 CFR 177.1520 for the polyolefin resin. Surface gloss is tested according to ASTM D2457-21 at 60° geometry, with acceptance typically set at a minimum value negotiated between filler and brand owner because published data for this exact grade in rotary injection blow molding platforms is limited. Terminal finished types include 30–500 mL bottles for shampoo, body wash, lotion, serum dropper bottles when fitted with separate closures, and certain cream jars; the material is not recommended for continuous hot-fill above 60 °C or for barrier fragrance packaging unless a surface coating or secondary barrier is added.
Pharmaceutical dry-syrup and effervescent tablet containers require documentation that resin additives do not induce pharmacopoeial extraction failures; KB158Z is therefore processed as neat virgin resin at 100 parts by weight, with 0–2 parts by weight of a drug-master-file-supported white masterbatch added per 100 parts resin, and process regrind is excluded from the primary contact layer. Extrusion blow molding is performed in an ISO 8 cleanroom using a 25:1 L/D single-screw extruder with polished barrel internals, melt temperature at the die entry held to 180–200 °C, and blow mold coolant set to 10–20 °C; in-line leak detection, wall-thickness scanning, and vision inspection are configured on every cavity. Pharmacopoeial compliance is demonstrated against USP <661.2> for plastic packaging systems, European Pharmacopoeia monograph 3.1.3 for polyolefins, and FDA 21 CFR 177.1520; extraction tests use purified water and ethanol 96% under conditions assigned by the dosage form, and any change in masterbatch supplier triggers revalidation. Terminal finished types include 15–500 mL HDPE bottles for dry-syrup powders, effervescent tablets, desiccant capsules, and chewable tablets; this process is not rated for steam sterilization or depyrogenation tunnel exposure above 80 °C without dimensional stability verification.
A three-layer or five-layer coextrusion die does not eliminate permeation risk in agrochemical packaging; it redistributes the barrier function while KB158Z serves as the outer skin at 100 parts, usually with 2–3 parts of UV-stabilized color masterbatch per 100 parts resin, and the inner skin carries 20–30 wt% sorted process regrind from the same production campaign; a typical wall distribution is 25% outer skin, 5% tie, 3% EVOH barrier, 5% tie, and 62% inner skin, though layer percentages are adjusted for each permeant. Melt temperature at the coextrusion die is held at 190–210 °C, blow molds are cooled to 15–25 °C, and parison programming is set to maintain a minimum wall thickness of 0.8 mm in the chime and top-load neck regions. Dangerous goods packaging qualification follows the UN Recommendations on the Transport of Dangerous Goods, Chapter 6.1, and, for U.S. distribution, 49 CFR 178.509; design qualification includes drop testing at -18 °C after filling with water-antifreeze mixtures, hydrostatic pressure testing, and stack compression for 28 days at 40 °C. Terminal finished types include 5–25 L jerry cans for agricultural adjuvants, solvent-borne cleaning concentrates, mineral oil, and windshield washer fluid; direct fluorination, sulfonation, or internal barrier liners are required only after permeation tests demonstrate insufficient solvent retention for the specific molecule.
Cold-fill dairy and beverage lines using shuttle blow molders require wall-thickness distribution and drop-impact performance after chilled distribution; KB158Z is metered as virgin resin that closes the balance to 100 wt% after 20–30 wt% closed-loop regrind from the same food-packaging line and 0–2 wt% color masterbatch are added. Extrusion blow molding is conducted on a 25:1 L/D extruder with a barrier screw at 180–205 °C melt temperature and 10–20 °C mold temperature; bottles are aged for 48 h before drop impact testing according to ASTM D2463-15, because post-mold crystallization continues at ambient temperature and low-temperature ductility changes during the first two days. Food-contact compliance is established under FDA 21 CFR 177.1520 and European Regulation (EU) No 10/2011, with overall migration tested under EN 1186-1 using food simulants assigned to the intended use. Terminal finished types include 200 mL–2 L bottles for pasteurized milk, cold-fill juices, drinkable yogurt, and liquid breakfast drinks; the material is not assigned for hot-fill above 60 °C, retort, or long-term edible oil storage above 40 °C unless migration and sorption data are generated for the exact lot.
Concentrated nonionic and anionic surfactant formulations attack the amorphous tie-chain population in HDPE, and the resulting craze initiation is accelerated by molded-in stress at the pinch-off seam; KB158Z is therefore processed at 98 wt% with antioxidant masterbatch at 2 wt% and fluorine-free polymer processing aid at 0.05–0.1 wt%, with a minor balance adjustment made using neat KB158Z in the gravimetric blender. Monolayer shuttle blow molding is conducted on a 30:1 L/D extruder with melt temperature set to 185–200 °C; the parison is profiled to achieve a wall-thickness gradient from 0.6 mm in side panels to 1.0 mm at corners and seams, and the blow mold temperature is maintained at 15–25 °C. Post-mold trimming, leak testing, and a 24 h room-temperature conditioning step precede ESCR evaluation. Stress-crack resistance is assessed according to ASTM D1693-21 in 50 °C surfactant solutions or 100% Igepal CO-630 as specified in the method, and full-notch creep data generated under ISO 16770:2019 are used to compare virgin and regrind-containing lots; published third-party ESCR data for this exact grade in concentrated surfactant matrices is limited, so production-floor comparator values are generated on a lot-to-lot basis. Terminal finished types include 250 mL–5 L refill bottles for concentrated laundry detergent, hard-surface cleaner refills, and industrial surfactant dispensers; containers in this segment should not be stored above 40 °C for extended periods and should not be filled with oxidizing acids or ketone-containing solvent blends without full stress-crack testing at the actual use concentration.
| Scenario | Mandatory or reference standard | Test designation | Boundary condition |
|---|---|---|---|
| Household chemical monolayer bottles | REACH (EC) No 1907/2006, 94/62/EC | ASTM D1238-20, ASTM D792-20, ASTM D2463-15 | Melt temperature ≤205 °C, wall 0.8–1.4 mm |
| Cosmetic injection blow molded containers | (EC) No 1223/2009, 21 CFR 177.1520 | ASTM D2457-21 | Core rod 90–120 °C, preform melt 200–220 °C |
| Pharmaceutical primary containers | USP <661.2>, Ph.Eur. 3.1.3, 21 CFR 177.1520 | Extraction tests, ASTM D1238-20 | No primary-contact regrind, melt 180–200 °C |
| Agrochemical barrier coextrusion | UN Chapter 6.1, 49 CFR 178.509 | Drop test -18 °C, hydrostatic pressure, stack 28 days at 40 °C | Minimum wall 0.8 mm, barrier layer 3% |
| Cold-fill dairy and beverage bottles | 21 CFR 177.1520, (EU) No 10/2011 | EN 1186-1, ASTM D2463-15 | Aging 48 h before drop test, hot-fill ≤60 °C |
| Concentrated surfactant packaging | ASTM D1693-21, ISO 16770:2019 | Igepal CO-630 ESCR, full-notch creep | Wall profile 0.6–1.0 mm, storage ≤40 °C |
Competitive TPC (Japan) HDPE KB158Z prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KB158Z is specified as a high-density polyethylene blow-moulding resin for rigid hollow articles that require elevated melt strength, controlled parison sag, and resistance to environmental stress cracking. The grade is positioned in the 0.955–0.960 g/cm³ density band associated with high-molecular-weight HDPE blow-moulding polymers. Lot-specific datasheet values for TPC (Japan) HDPE KB158Z are not reproduced in this document; therefore, numerical descriptors are presented as class-typical ranges for this product segment and must be verified against the supplier’s certificate of analysis. The resin is not a direct drop-in replacement for high-flow injection-moulding HDPE grades because its molecular architecture is oriented toward parison stability and wall-thickness control rather than thin-wall filling at high melt-flow rates.
The primary difference between KB158Z and general-purpose HDPE grades lies in molecular weight distribution and melt-flow behaviour under load. Blow-moulding grades in the KB158Z class exhibit a low-load melt-flow rate measured at 190 °C with 5 kg that is typically below 0.5 g/10 min, while the high-load melt-flow index at 21.6 kg provides sufficient flow for extrusion while preserving parison integrity. General-purpose injection-moulding HDPE commonly produces a high-load melt-flow index above 20 g/10 min, which results in reduced melt strength and excessive parison drawdown in large-part blow moulding. The high molecular weight and broader distribution of KB158Z-class resin increase apparent melt viscosity at low shear rates, improving parison hang time and weld-line strength in accumulator-head equipment.
| Property | Class-typical range | Test basis |
|---|---|---|
| Density at 23 °C | 0.955–0.960 g/cm³ | ISO 1183-1:2019 |
| Melt-flow rate, 190 °C/5 kg | 0.15–0.45 g/10 min | ISO 1133-1:2022 |
| High-load melt-flow rate, 190 °C/21.6 kg | 8–18 g/10 min | ISO 1133-1:2022 |
| Tensile yield stress | 24–30 MPa | ISO 527-2:2012 |
| Elongation at break | >600 % | ISO 527-2:2012 |
| Flexural modulus | 900–1,300 MPa | ISO 178:2019 |
| Charpy notched impact strength at 23 °C | >15 kJ/m² | ISO 179-1:2023 |
| Environmental stress-crack resistance, 100 % Igepal, condition B | >100 h | ASTM D1693-15 |
Comparative differentiation from other HDPE products is most pronounced in environmental stress-crack resistance and parison melt strength. Film-grade HDPE with a density near 0.945 g/cm³ may provide higher puncture resistance in thin films, but it does not maintain the modulus and dimensional stability required for large industrial containers. Blow-moulding grades with lower density or narrower molecular weight distribution can exhibit shorter failure times under ASTM D1693-15 conditions and greater die-lip show-through variation on production lines. The molecular design of KB158Z-class resin supports thicker-wall part formation without the high screw-back pressure spikes observed with very high-molecular-weight polyethylene grades having limited melt index.
Processing trials on single-screw extrusion blow-moulding lines with grooved-feed barrels and accumulator heads have shown that melt-temperature control is the critical threshold governing surface quality and impact retention. The recommended melt temperature measured at the die entry is 185–220 °C, with the accumulator head held between 190 °C and 210 °C. Barrel setpoints typically follow a progressive ramp from 160 °C in the feed zone to 200 °C at the metering zone. Extruder length-to-diameter ratios from 24:1 to 30:1 are preferred because lower L/D ratios can produce insufficient homogenisation, resulting in parison thickness variation and weld-line weakness. Screw speed should be limited to 0.2–0.6 m/s peripheral velocity for this molecular weight class; excessive shear can initiate melt fracture and surface shark skin at the die lip.
| Parameter | Working range | Measurement basis |
|---|---|---|
| Feed-throat temperature | 30–50 °C | Contact thermocouple |
| Barrel zone 1 | 160–180 °C | Setpoint controller |
| Barrel zone 2 | 180–200 °C | Setpoint controller |
| Barrel zone 3 / metering zone | 190–210 °C | Setpoint controller |
| Accumulator head | 190–210 °C | Immersion melt probe |
| Die temperature | 180–205 °C | Die lip thermocouple |
| Melt temperature at die entry | 185–220 °C | Melt thermocouple |
| Blow air pressure | 0.6–1.0 MPa | Mould circuit pressure gauge |
| Mould temperature | 15–40 °C | Mould surface thermocouple |
Field data from accumulator-head machines indicate that melt temperatures above 220 °C can produce oxidative chain scission and gel formation during extended residence times. The resulting gel particles appear as surface specks in the final container and reduce Charpy notched impact strength below the 15 kJ/m² class threshold. Conversely, melt temperatures below 185 °C increase melt viscosity to a point where parison ejection becomes irregular and surface melt fracture is more probable. The window between 185 °C and 220 °C is therefore treated as a process boundary rather than a generic guideline. For large containers with gross weight above 5 kg, accumulator shot capacity should be at least 1.3 times the maximum shot weight to avoid parison cooling at the die lip during slow extrusion.
Continuous-shuttle machines and wheel-type blow-moulding lines require different screw profiles than accumulator-head lines. In continuous-shuttle operation, parison sag time is shorter, and melt temperatures at the upper end of the range are sometimes used to improve surface appearance. However, raising melt temperature beyond 215 °C on a wheel system with high screw speed can lower melt strength enough to cause eccentric wall thickness in tall containers. Production-scale trials on shuttle machines with 60 mm screw diameter and 24:1 L/D have shown that a setpoint reduction of 5–10 °C at the die usually reduces parison length variation more effectively than raising blow pressure. No single processing recipe can replace melt-temperature profiling at the die because heat history and regrind content change melt viscosity independent of barrel setpoints.
Published data for this specific configuration of TPC (Japan) HDPE KB158Z under every commercial blow-moulding platform is limited. The processing ranges above are therefore derived from established behaviour of high-density polyethylene blow-moulding resins in the same density and high-load melt-flow class, and they should be validated on target equipment. Resin certification should be requested from TPC Japan when the application involves wall thickness below 1.5 mm, because thin-wall moulding with this molecular weight class can require die-gap adjustment above 1.5 mm and higher blow pressure to achieve acceptable surface replication.
The inclusion of regrind in KB158Z processing changes not only melt viscosity but also environmental stress-crack resistance and odour profile. Production lines using closed-loop regrind at 20–30 wt% typically maintain acceptable ESCR and impact properties, provided the regrind is ground from clean post-industrial scrap and processed without thermal degradation. Regrind levels above 30 wt% can narrow the melt-temperature window by increasing low-shear melt viscosity and reducing parison extensibility. The onset of surface melt fracture may then appear at die temperatures that were previously stable, requiring a reduction in screw speed rather than an increase in temperature. Batch-to-batch variation in regrind particle size also influences bulk density in the feed throat; a maximum particle size of 8 mm is recommended for grooved-feed single-screw extruders to avoid feed bridging and output fluctuation.
Pre-drying is required when pellets or regrind have been stored in ambient relative humidity above 60 % or moved from cold storage into a warm processing hall. Surface moisture on HDPE feed can produce splay, internal bubbles, and inconsistent parison welding. A desiccant dryer set to 70–80 °C for 2–4 h is usually adequate for pellet surface moisture. Drying at temperatures above 90 °C should be avoided for extended periods because oxidative exposure in a hot-air hopper can initiate surface yellowing and build-up of oxidised gel layers on the screw. For applications requiring low odour and low extractables, such as pharmaceutical intermediate containers, the use of certified pellet lots without post-blending of unknown regrind sources is advised.
In compatibility terms, KB158Z-class HDPE should not be melt-blended with amine-based processing additives without prior evaluation, because amine stabiliser packages can interact with acid scavenger chemistry and shift colour during extended processing. Colour change is measured after multiple heat histories using CIELAB delta E against a control plaque prepared at 200 °C. A delta E above 1.5 after 5 extrusion cycles indicates additive incompatibility or thermal degradation. For colour-critical containers, concentrate systems based on polyethylene carriers with no amine slip agents are preferred. When fluoropolymer processing aids are used to delay melt fracture, addition levels should be limited to 300–600 ppm and should be precompounded rather than dusted onto the pellets, because undispersed processing aid can produce optical defects in the container surface.
Regulatory verification for food-contact containers in the target jurisdiction must be based on the supplier’s food-contact statement. High-density polyethylene resins in this class are commonly assessed under FDA 21 CFR 177.1520 for US applications, EU Regulation No 10/2011 for European Union compliance, and additional national migration limits where applicable. Industrial packaging applications may also require conformance to REACH and RoHS Recast 2011/65/EU when the finished article is exported. The processor is responsible for verifying that additives, masterbatches, and regrind do not invalidate the resin supplier’s compliance position. Because published regulatory documentation for this specific TPC grade may not cover every application condition, end-use migration testing under specified temperature and simulant conditions is required for fatty or aqueous food contact at elevated fill temperatures.
In automated blow-moulding cells with in-line leak testing and post-mould deflashing, the grade’s high melt strength supports consistent pinch-off welds at the parting line. Pinch-off design should provide a knife angle of 30–45° and a land width of 0.5–1.0 mm for containers with wall thickness from 2 mm to 5 mm. Narrower pinch-off land widths can generate excessive shear and weaken the bottom weld, while wider land widths may leave excessive flash and require secondary trimming. The observed production issue of bottom-weld cracking in large drums has been correlated with low melt temperature at the pinch-off, excessive regrind fines, and inadequate mould cooling. Raising die temperature by 5 °C without exceeding the 220 °C melt threshold improves weld consolidation without sacrificing impact strength.