| HS Code | 347090 |
| Density | 0.956 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.05 g/10 min |
| Tensile Strength At Yield | 29 MPa |
| Tensile Strength At Break | 29 MPa |
| Elongation At Break | 800 % |
| Flexural Modulus | 1.20 GPa |
| Izod Notched Impact Strength | 0.10 J/cm |
| Vicat Softening Point | 127 °C |
| Brittleness Temperature | < -70 °C |
| Shore D Hardness | 65 |
| Coefficient Of Linear Thermal Expansion | 1.20E-4 /°C |
| Thermal Conductivity | 0.440 W/m·K |
| Dielectric Strength | 20 kV/mm |
| Volume Resistivity | 1.00E+16 ohm·cm |
| Water Absorption | < 0.010 % |
As an accredited TPC (Japan) HDPE KB148A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KB148A is supplied in 25 kg polyethylene bags, palletized at 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loads about 17 MT of TPC (Japan) HDPE KB148A in 25 kg bags; palletization may reduce capacity. |
| Shipping | TPC (Japan) HDPE KB148A is a non-hazardous high-density polyethylene resin, not regulated for transport (no UN number, class, or packing group). It ships as pellets in 25 kg bags or jumbo bags, palletized, in dry containers. Keep dry, cool, ventilated, away from ignition sources and direct sunlight. |
| Storage | Store TPC (Japan) HDPE KB148A in a cool, dry, well-ventilated place, away from direct sunlight, heat, sparks, open flames, and ignition sources. Keep original bags closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and strong oxidizers. Do not stack excessively. Use first-in, first-out rotation. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | TPC (Japan) HDPE KB148A has a shelf life of 24 months when stored unopened, dry, away from direct sunlight, heat, and moisture. |
TPC (Japan) HDPE KB148A is routed through the 20–30 L tight-head monolayer jerrican segment for industrial solvent and agrochemical distribution in a shuttle-type extrusion blow molding line where the 65–90 mm grooved-barrel extruder, operated at 24:1–30:1 L/D, must hold barrel zone temperatures between 170 °C and 195 °C and die-head temperature at 190–205 °C to prevent parison curl caused by temperature differentials exceeding 5 °C across the die circumference. Fixed addition ratios in this segment are 2.0–4.0 wt% HDPE-carrier UV masterbatch, yielding an active hindered-amine light stabiliser concentration of 0.10–0.30 wt% in the finished article, alongside 0.03–0.08 wt% active phenolic phosphite antioxidant top-up; the carrier resin melt flow index is selected within 0.3–0.5 g/10 min under ISO 1133-1:2022 to avoid melt-fracture streaks on the parison surface. Production parameters include blow air pressure at 0.8–1.0 MPa, mold temperature at 12–25 °C, and pinch-off weld cooling interval of 8–15 s depending on bottom flash thickness; insufficient mold closing speed below 150 mm/s has been observed on production-scale shuttle machines to generate bottom pinch-off seams with micro-voids that fail the leakproofness test after vacuum venting. The sector is governed by UN 3H1 designation and the 49 CFR §178.603 drop test, 49 CFR §178.604 leakproofness test, 49 CFR §178.605 hydrostatic pressure test, and 49 CFR §178.606 stacking test for dangerous goods packaging groups I, II, and III; material compliance additionally falls under FDA 21 CFR 177.1520 for indirect food-contact certification where export markets require it. Finished containers include 20 L, 25 L, and 30 L tight-head UN jerricans with calibrated venting closures and handle flash removed at 40–60 °C to avoid stress whitening. The operational boundary for the grade is set by moisture pickup: no drying is required for sealed bags stored below 60% relative humidity, but open storage above 70% RH for more than 4 h can introduce surface splay and must be corrected by a 2 h hopper-dryer pass at 70 °C before extrusion.
| Drop test | 49 CFR §178.603 | Electric hoist drop tester with solid-steel toe plate |
| Leakproofness test | 49 CFR §178.604 | Venturi vacuum leak tester, differential setpoint −20 kPa |
| Hydrostatic pressure test | 49 CFR §178.605 | Closed-circuit hydrostatic pump with calibrated gauge |
| Stacking test | 49 CFR §178.606 | Automated compression stack frame with 3 m load column |
In 200 L open-head and tight-head drum production, KB148A is processed on accumulator-head blow molders with shot capacities of 30–50 kg, where the central process variable is the sag-to-swell balance between parison extrusion and mold closing. Published data for this specific configuration is limited; however, the operating window is bracketed by die swell values of 1.8–2.2 at shear rates below 150 s⁻¹ and parison sag exceeding 12% elongation over a 2.5–4.0 s open-mold interval when melt temperature exceeds 210 °C. The formulation in this sector incorporates 10–25 wt% post-industrial regrind from trimmed flash and startup tails, with 0.05–0.15 wt% zinc stearate external lubricant to reduce die-lip deposition and 1.5–2.5 wt% carbon black masterbatch only when UV-stabilised outdoor-service drums are specified. A stabiliser top-up of 0.03–0.06 wt% active antioxidant is added per 10 wt% regrind increment to compensate for thermo-oxidative consumption during multiple heat histories. The downstream process requires parison programming with wall-thickness setpoints from 4.0 mm at the top chime to 8.0 mm at the corner radius, die gap 3.0–5.0 mm, and blow pressure 0.9–1.1 MPa; mold temperature is held at 25–40 °C to balance cycle time against top-load retention. Failure modes observed on production-scale accumulator machines include pinch-off weld pearl formation when mold closing speed drops below 120 mm/s and die-head stagnation gels when the accumulator head is held at 215 °C for more than 20 min during upstream line stoppages. Compliance is evaluated through UN 1H1 qualification for 200 L drums under 49 CFR §178.603 drop testing, stacking per 49 CFR §178.606, and environmental stress-cracking resistance per ASTM D1693-15 using 10% Igepal CO-630 at 50 °C; for food-contact drums, FDA 21 CFR 177.1520 and EU 10/2011 apply. Finished types include open-head and tight-head L-ring drums of 200 L nominal capacity, including UN-rated versions for solid and liquid dangerous goods.
For 1 L, 5 L, 10 L agrochemical containers requiring resistance to toluene and xylene, KB148A is specified as the outer and inner structural layer in a three-layer coextrusion blow molding structure with a polyamide barrier core. The process is executed on a coextrusion blow molder with a 60 mm outer HDPE extruder, 35 mm PA6 barrier extruder, and 25 mm tie-resin extruder, each with L/D from 24:1 to 30:1; melt temperatures are held at 200–220 °C for the HDPE layers, 240–260 °C for the PA6 core, and 210–230 °C for the maleic-anhydride-grafted tie layer. Fixed addition ratios in the HDPE layers are 1.5–3.0 wt% UV masterbatch, 0.5–1.0 wt% antistatic masterbatch, and 2.0–4.0 wt% tie resin in the total coextruded web, with the barrier layer making up 4.0–6.0% of total wall thickness. Interlayer adhesion failure at the HDPE/tie/PA interface is the primary process conflict; it is induced when the PA melt temperature falls below 240 °C at the die exit or when the temperature differential between adjacent layers exceeds 20 °C, producing delamination at the pinch-off weld during drop testing. Solvent permeation for the finished containers is measured by gravimetric weight loss over 28 days at 40 °C and is specified at below 0.5 g·m⁻²·d⁻¹ for xylene and 0.3 g·m⁻²·d⁻¹ for toluene in qualified packages, though published data for KB148A in this exact barrier configuration is limited and must be confirmed on the actual multi-layer tool. The compliance framework includes UN 3H1 designation for the intermediate containers, 49 CFR §178.603 drop testing at packing group II heights, ASTM D2684 residual stress evaluation for polyethylene containers, and pesticide packaging guidance under FAO/WHO practical storage requirements; the HDPE food-contact surfaces are separately covered by FDA 21 CFR 177.1520 or EU 10/2011 where dual-use certification is requested. Finished articles include 1 L, 5 L, 10 L multilayer barrier bottles with three-layer parison construction and measured PA barrier distribution centered at ±0.5% of nominal layer ratio across the bottle sidewall.
On continuous rotary blow molding lines for 500 mL–1 L household bleach and trigger-spray detergent bottles, KB148A is processed as a monolayer with 2.0–3.0 wt% white titanium dioxide masterbatch and 0.5–1.0 wt% processing aid masterbatch, the latter selected with a polyethylene wax carrier rather than an amine-based masterbatch because amine migration above 0.2 wt% causes cap seal tack and torque-loss failures in polypropylene closures within 6 weeks of ambient storage. The extrusion blow molding line is configured with a 60 mm grooved-barrel extruder, 25:1 L/D, dual parison head, and multi-cavity shuttle molds running at 12–18 s cycle time per station; melt temperature is controlled at 185–195 °C, mold temperature at 8–12 °C, and blow air at 0.7–0.9 MPa. Industry compliance for these household products includes REACH Annex XVII restrictions for the final article, European Packaging Directive 94/62/EC, and FDA 21 CFR 177.1520 or EU 10/2011 where indirect food contact is invoked for combination cleaning kits stored adjacent to food. The downstream process must also observe environmental stress-cracking limits: immersion in 10% Igepal CO-630 under ASTM D1693-15 at 50 °C is used as incoming-lot screening for bottles filled with bleach and surfactant formulations at pH 11.5–12.5. For bleach-containing products, the maximum continuous product contact temperature is 35 °C, and the bottle is not recommended for sodium hypochlorite concentrations above 8.0% active chlorine due to premature oxidative embrittlement of the pinch-off weld area. Finished product types include 500 mL, 750 mL, 1 L trigger-spray and squeeze bottles with calibrated neck finishes and closure torque requirements between 1.2–1.8 N·m for linerless polypropylene caps. The operational boundary is set by low-temperature impact: below −20 °C, axial impact cracks can occur at the bottom flash-trim area if the hot-knife trim is performed below 40 °C and leaves micro-stringers; trimming is therefore executed at 45–60 °C.
In five-layer coextrusion blow molding of 1 L and 2 L dairy milk bottles with an EVOH oxygen barrier, KB148A forms the food-contact inner layer and the outer layer, while a middle layer contains 50–70 wt% post-consumer recycled HDPE. The addition ratio for the PCR middle layer is limited to 30 wt% of total bottle mass in this structure because recovered HDPE flakes above 200 µm particle size produce melt gels that rupture the 18–25 µm EVOH layer during blow-up ratio expansion of 2.8–3.2. The process is run on a five-layer coextrusion blow molder with a 70 mm main extruder, 45 mm PCR extruder, and 20 mm EVOH/tie layer capability; melt temperatures are 190–205 °C for HDPE layers, 215–230 °C for EVOH, and 200–215 °C for tie resins. After 30 wt% PCR incorporation, top-up antioxidant masterbatch is dosed at 0.8–1.2 wt% and acid scavenger at 0.05–0.10 wt% to neutralise residual catalyst residues; without acid scavenger, top-load retention at 23 °C declines by 8–12% after 4 weeks due to hydrolytic chain degradation at the EVOH interface. Compliance for food contact requires the PCR layer to be shielded from the product by virgin HDPE layers and to meet FDA 21 CFR 177.1520 or EU 10/2011 overall migration limit of 10 mg/dm²; for dairy container organoleptic performance, fill-and-hold testing at 4 °C for 14 days is used to detect off-odour transfer from recycled content. The downstream process conflict arises when the die-head pressure fluctuates by more than 0.5 MPa during PCR feed surges, causing local thinning at the pinch-off weld and intermittent pinhole failures on vacuum leak testers set at −20 kPa. Finished articles are 1 L and 2 L EVOH barrier dairy bottles with a post-consumer recycled middle layer concentration of 30 wt% maximum and a measured oxygen transmission rate below 0.15 cm³·m⁻²·d⁻¹·bar⁻¹ at 23 °C and 50% RH. Published data for KB148A in this exact five-layer PCR configuration is limited; validation under the specific EVOH/tie-layer grades in use is required before commercial line qualification.
For 500 mL oral-dispensing pharmaceutical bottles produced by shuttle blow molding, KB148A is pre-blended with 2.0–3.0 wt% titanium dioxide masterbatch and processed at 175–190 °C melt temperature; the finished bottles are evaluated under USP 661.1 plastic packaging system requirements and EU 10/2011, with light transmission controlled by USP 671 and cap liner compatibility tested by torque removal between 0.8–1.2 N·m after 24 h ambient storage.
Competitive TPC (Japan) HDPE KB148A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KB148A is a high-density polyethylene pellet grade supplied for extrusion blow moulding, thick-walled industrial sheet, and extruded profiles where melt strength and environmental stress crack resistance dominate the selection decision. The grade sits in the TPC Japan HDPE extrusion portfolio and is differentiated from standard high-flow HDPE injection grades by its high molecular weight fraction and its narrow low-load melt flow rate. The designation KB148A identifies the polymer type, melt flow modifier, and additive package; the suffix 148A is the producer’s internal code for the extrusion-grade stabilization system. Published data for grade-specific lot variation is limited, and the values in this document should be read against the manufacturer’s certificate of analysis and the cited ISO or ASTM method. In converter trials, KB148A has been used for agricultural chemical containers, 20 L industrial pails, and large detergent bottles where top load, ESCR, and parison stability are evaluated together.
The extrusion blow moulding process window for KB148A is narrower than that of lower-viscosity HDPE because the high molecular weight fraction increases elastic memory and die swell. On a grooved-barrel single-screw extruder with an L/D ratio of 30:1 and a screw diameter of 75 mm, a barrel profile of 180–220 °C and a die head temperature of 190–210 °C are typical for stable parison formation. The practical melt-temperature band is 190–210 °C; below 185 °C the high molecular weight species are not fully relaxed and melt fracture may appear at shear stresses above 0.3 MPa, while above 225 °C thermo-oxidative chain scission accelerates and reduces parison hang time. Temperature variation at the die lip should be held within ±5 °C to avoid parison curl and wall-thickness asymmetry. A die gap of 1.5–2.5 mm and a blow-up ratio of 2:1 to 3:1 have been used in field evaluations. Published data for this specific configuration is limited, but the response is consistent with HMW-HDPE grades of similar high-load melt index.
Melt flow data for KB148A show that the low-load melt flow rate at 190 °C/2.16 kg is below 0.10 g/10 min; the high-load melt index at 190 °C/21.6 kg is therefore the primary process control value. Typical extrusion equipment uses a barrier screw with a compression ratio of 1.9:1 to 2.5:1. A grooved feed section with axial groove depths of 0.5–0.8 mm improves pellet intake and reduces screw slip. On a smooth-bore extruder of equivalent diameter, throughput may fall by 10–15 % because of the low base melt flow. Start-up after a lot change should include a shot-weight verification because high-load melt index lot-to-lot variation is commonly controlled within ±0.5 g/10 min but can shift accumulator drop time and parison length. Die swell in KB148A is higher than in HDPE with a melt flow rate of 0.3 g/10 min; a die gap reduction of 0.2–0.4 mm may be required to maintain the target final wall thickness. Parison programming should account for the longer relaxation time, and screw speed should be trimmed to maintain a constant drop time rather than to exceed the cooling capacity of the mould.
Representative typical values for TPC Japan HDPE KB148A, not to be construed as sales specifications, are given below.
| Property | Typical value | Test method |
|---|---|---|
| Density | 0.956 g/cm³ | ISO 1183-1:2019 |
| Melt flow rate at 190 °C, 2.16 kg | 0.04 g/10 min | ISO 1133-1:2022 |
| High-load melt flow rate at 190 °C, 21.6 kg | 5.0 g/10 min | ISO 1133-1:2022 |
| Tensile yield stress at 50 mm/min | 27 MPa | ISO 527-2:2012 |
| Tensile elongation at break | >600 % | ISO 527-2:2012 |
| Flexural modulus | 1,250 MPa | ISO 178:2019 |
| Charpy notched impact at 23 °C | 8 kJ/m² | ISO 179-1:2010 |
| Vicat softening temperature, A50 | 122 °C | ISO 306:2022 |
| ESCR, condition A, 10 % Igepal CO-630 | >200 h | ASTM D1693 |
When KB148A is compared with conventional HDPE injection-moulding grades, the difference in melt flow rate creates a fundamental separation in process capability. An injection-moulding HDPE with a melt flow rate at 190 °C/2.16 kg of 8–12 g/10 min fills thin-wall mould sections at lower injection pressure but lacks the extensional viscosity required to support a large parison. KB148A, by contrast, supports a 20 L container parison with less than 12 % sag over a 2.5 m hang length under described die conditions, but cannot be processed on a conventional reciprocating-screw injection machine without excessive pressure and thermal degradation. Relative to HMW-HDPE blown film grades with high-load melt indices of 7–9 g/10 min and densities near 0.944 g/cm³, KB148A typically provides higher flexural modulus and top load at equivalent section thickness, while the lower high-load melt index requires closer attention to die swell and parison programming.
The differentiation between KB148A and older single-reactor HDPE grades is kinetic in origin. In a bimodal molecular weight distribution, the high molecular weight fraction increases tie-chain density and ESCR, while the low molecular weight fraction reduces high-load melt viscosity and maintains extruder throughput. A unimodal grade at the same density and melt flow rate may show lower ESCR because the molecular weight distribution cannot simultaneously satisfy both requirements. Published data for the exact molecular weight distribution of KB148A is limited, but the processing behavior is consistent with a bimodal or broad distribution.
Property differences between KB148A and lower-density HDPE blow moulding grades become apparent in top-load testing. A container made from KB148A at a wall thickness of 1.6 mm may show a top-load increase of 10–15 % relative to a density 0.944 g/cm³ resin at the same thickness, but its drop impact at -20 °C may be lower. Converters specifying low-temperature impact should evaluate notched Charpy or instrumented dart impact on the finished part rather than relying on room-temperature flexural modulus. Published data for this specific comparison in KB148A is limited; comparative work should use ISO 6603-2 for puncture behavior. North American converters may request ASTM D638-14 tensile data. The ISO 527-2:2012 method uses a Type 1A specimen and a 50 mm/min test speed; ASTM D638-14 Type IV specimens may yield slightly different elongation values, so direct cross-method comparison should not be made without specimen geometry correction.
Within the TPC Japan HDPE line, KB148A is separated from injection-moulding grades by its high-load melt index and from pipe grades by the absence of carbon black and a different stabilization package. Pipe-grade HDPE with carbon black dispersed at 2–2.5 wt% offers UV resistance but may not meet the surface appearance requirements for blow moulded containers; KB148A is typically unpigmented or coloured by masterbatch at the converter.
ESCR in KB148A is controlled by the high molecular weight fraction and by the absence of rapid crack-propagation pathways. Under ASTM D1693 condition A with 10 % Igepal CO-630, HDPE grades in this MFR and density range typically exceed 200 h, whereas a high-flow injection grade may fail below 20 h. The ESCR advantage is not cost-free: increasing density from 0.944 g/cm³ to 0.956 g/cm³ raises stiffness but lowers intrinsic ESCR; the molecular weight distribution must therefore be broad enough to maintain tie-chain density. In agricultural chemical containers, the ESCR requirement is often combined with a top-load requirement after exposure to hydrocarbon-based actives. Published data for this specific configuration is limited, and final suitability should be established by ASTM D1693 testing on the blow moulded article, not solely on the pellet.
Additive selections in KB148A are limited to the stabilization and processing packages supplied by TPC Japan. Converters should avoid combining the resin with amine-based hindered amine light stabilizers at concentrations above those recommended by the additive supplier when processing at melt temperatures above 220 °C, because amine–peroxide interactions can produce discoloration or uncontrolled radical generation. For outdoor service, UV stabilization should be introduced as a masterbatch or pre-compounded lot; carbon black masterbatch can be used but will reduce ESCR if the dispersion is poor or the loading exceeds 2.5 wt% in the wall section. Food-contact status for HDPE homopolymers is governed by FDA 21 CFR 177.1520(c) for US applications and by Regulation (EU) No 10/2011, Annex I for European applications. Compliance is end-use dependent, and migration testing on the finished article is required for fatty food simulants under EU methods.
The compliance matrix below summarizes the standards most often requested for KB148A in converter specifications.
| Requirement | Reference |
|---|---|
| Polyethylene classification | ISO 17855-1:2014 |
| Density test method | ISO 1183-1:2019 |
| Melt flow rate test method | ISO 1133-1:2022 |
| Food-contact status, US | 21 CFR 177.1520(c) |
| Food-contact status, EU | Regulation (EU) No 10/2011 |
| RoHS directive declarable substances | 2011/65/EU |
If KB148A is substituted for a lower-viscosity HDPE on an existing sheet extrusion line, the head pressure may rise by 20–30 % at a fixed screw speed. Lines designed for a melt flow rate at 190 °C/2.16 kg of 4–6 g/10 min generally use a three-zone screw with a metering depth optimized for low viscosity; under KB148A’s low-flow melt, the metering section may run starved and generate excessive shear heating. On a 90 mm single-screw sheet line with a 32:1 L/D and a melt pump, the pressure drop across the screen changer can increase from 8 MPa to 12 MPa when switching to KB148A. A barrier screw with an L/D of at least 30:1 and a grooved feed section is preferred. If the existing screw is retained, the barrel temperature setpoints should be raised by 5–10 °C in the feed and compression zones, while the die zone should be kept at 200–210 °C. Sheet thickness variation can increase if the melt temperature entering the three-roll stack fluctuates because high-molecular-weight HDPE has a longer relaxation time; chill roll temperatures of 80–100 °C are used to reduce residual stress and edge bead. In thermoforming from KB148A sheet, uniform heating is more critical than with lower-viscosity HDPE because the sheet retains a high plateau modulus through the forming window, and cold spots can produce wall-thickness variation in deep-draw parts.
Moisture absorption of KB148A is below 0.01 % by ISO 62:2008; pre-drying is not normally required, but pellets stored at relative humidity above 60 % may be dried at 80 °C for 2 h to remove surface moisture and prevent surface streaks. Residence time in the melt phase above 220 °C should be kept below 20 min to limit oxidative chain scission and loss of high-load melt index. Published data for this specific configuration in cast film, fibre extrusion, or blow moulding of multi-layer structures with polar barrier resins is limited, and those processes fall outside the primary design space for KB148A unless validated by TPC Japan technical support. The grade should not be assumed to be a drop-in replacement for lower-viscosity HDPE without a documented process capability study.