Tpc Japan Hdpe Kb147n

TPC (Japan) HDPE KB147N

    • Product Name: TPC (Japan) HDPE KB147N
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 189618
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Strength At Yield 30 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 700%
    Flexural Modulus 1.20 GPa
    Notched Izod Impact Strength 20 kJ/m²
    Shore D Hardness 65
    Vicat Softening Point 124 °C
    Melting Point 135 °C
    Environmental Stress Crack Resistance Escr >1000 h
    Water Absorption 0.01%
    Thermal Conductivity 0.45 W/(m·K)
    Volume Resistivity >1×10^16 Ω·cm
    Dielectric Strength 20 kV/mm

    As an accredited TPC (Japan) HDPE KB147N factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KB147N packaging: 25 kg polyethylene-lined paper bags, palletized; also supplied in 1,000 kg jumbo bags.
    Container Loading (20′ FCL) 20′ FCL loading for TPC (Japan) HDPE KB147N: palletized 25 kg bags, shrink-wrapped, securely loaded, approximately 18–20 MT per container.
    Shipping TPC (Japan) HDPE KB147N ships as non-hazardous high-density polyethylene pellets, typically in 25 kg bags or 1 MT jumbo bags, palletized and containerized. Keep dry, sealed, and away from heat, sunlight, and ignition sources. Not regulated as dangerous goods (no UN number) for sea, air, or road transport.
    Storage Store TPC (Japan) HDPE KB147N in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and ignition sources. Keep original bags sealed and palletized off the floor. Avoid moisture, contamination, and contact with oils, solvents, acids, or oxidizers. Rotate stock using FIFO and follow the manufacturer’s SDS and local regulations. Protect from UV radiation and mechanical damage.
    Shelf Life Shelf life typically 24 months when stored in original unopened packaging, cool, dry, well-ventilated, away from direct sunlight.
    Application of TPC (Japan) HDPE KB147N

    Municipal water utilities and gas distribution contractors frequently specify TPC (Japan) HDPE KB147N for pressure piping because the grade’s high molecular weight distribution permits long hydrostatic design life under sustained hoop stress. In pipe extrusion, the resin is run on single-screw extruders with screw diameters of 60–75 mm, an L/D ratio of 33:1, and a grooved feed section that stabilizes output against back-pressure fluctuations. The barrel temperature profile is typically set from 180 °C at the feed throat to 210–220 °C at the metering zone, while the die head is held at 200–210 °C; melt temperature measured at the adapter should remain between 190 °C and 220 °C. The die is a spiral mandrel or screen-basket design with a die gap of 1.8–2.5 mm. Vacuum sizing tanks with slot calibration control outer diameter and wall thickness; haul-off speed is linked to an ultrasonic wall thickness gauge to maintain tolerances under EN 12201-2:2020 for water supply and ISO 4437-2:2014 for gas distribution. For black pressure pipe, a carbon black masterbatch is metered to give a final carbon black content of 2.0–2.5 wt%, the range required for ultraviolet stabilization in ISO 4427 and ASTM D3350 cell classification; blue potable water pipe uses a cobalt blue pigment masterbatch at 2–4 wt% let-down ratio. The antioxidant and acid scavenger package is introduced as a pre-compounded masterbatch at 0.5–1.5 wt% to protect against thermo-oxidative degradation during extrusion and to prevent catalytic residue-induced discoloration. Processors must not compensate for batch-to-batch melt flow variation by raising barrel temperatures above 230 °C, because this accelerates antioxidant consumption and generates gels that reduce slow crack growth resistance. The extruded pipe is tested for hydrostatic strength under ISO 1167-1:2006; PE100 pressure-rated grades must meet an extrapolated hydrostatic design stress of 10 MPa at 20 °C for 50 years using ISO 9080:2012 regression analysis. Notched pipe test performance under ISO 13479:2009 and full-scale creep rupture testing are part of the material qualification file. Potable water contact requires compliance with EU 10/2011 and FDA 21 CFR 177.1520 migration limits on the finished pipe. Terminal product types include PE100 water distribution mains, gas distribution pipes, industrial slurry transfer lines, and mining process water piping.

    StandardParameterRequirement
    ISO 1167-1Hydrostatic strength at 20 °C, 12.4 MPa≥100 h
    ISO 1167-1Hydrostatic strength at 80 °C, 5.0 MPa≥1000 h
    ISO 13479Notched pipe test at 80 °C, 4.6 MPa≥500 h
    ASTM D3350Cell classificationPE445574C or equivalent

    What Limits Regrind Loading in UN-Certified Drum Blow Molding with HDPE KB147N?

    Accumulator-head extrusion blow molding lines running HDPE KB147N for jerrycans and tight-head drums must maintain parison melt strength during the transfer from die to mold. The resin is processed at melt temperatures of 180–210 °C; barrel zones are profiled from 170 °C at the hopper to 200 °C at the accumulator, with a mold temperature of 10–25 °C. A 30-point parison programmer is required for containers above 50 L to adjust the die gap along the parison length and compensate for swell and sag; blow air pressure is typically 0.6–1.0 MPa. Formulation for UN-certified packaging is governed by the packaging test report and the selected dangerous goods packing group. A hindered phenolic antioxidant masterbatch is metered at 0.2–0.5 wt%, a HALS UV stabilizer masterbatch at 0.1–0.3 wt% when the container is stored outdoors, and zinc stearate or calcium stearate acid scavenger at 0.05–0.15 wt%. Recycled material from the same production line is limited to ≤20 wt% in the outer layer for UN-certified dangerous goods packaging because higher regrind fractions depress the notched environmental stress crack resistance below the threshold required by ASTM D1693-15 Condition B and ISO 16770:2019 FNCT. Molded containers are subjected to hydraulic internal pressure testing at 250 kPa for 30 min under 49 CFR 178.504, stack compression, and drop impact from up to 1.8 m at −18 °C following conditioning. Permeation and compatibility for specific liquids are assessed under ADR/RID 6.1.3 and the IMDG Code Chapter 6.1; the certificate of approval must list the maximum specific gravity and vapor pressure. Terminal product types include UN 3H1 tight-head jerrycans, UN 1H1 tight-head drums, and UN 1H2 open-top drums for solvent, lubricant, agrochemical, and detergent transport.

    In geomembrane fabrication, TPC (Japan) HDPE KB147N is extruded into smooth or textured sheet on flat-die sheet lines with barrel temperatures from 210 °C to 240 °C and a die gap of 2.0–3.0 mm; the sheet is quenched on polished chrome rolls at 60–90 °C and wound under constant tension to avoid stress whitening. For landfill basal liners, the formulation includes a carbon black masterbatch to give a final carbon black concentration of 2.0–3.0 wt% to meet the carbon black dispersion requirements of ASTM D3350 and GRI-GM13, an antioxidant package at 0.3–0.8 wt% to protect against oxidative degradation during extrusion and long-term service, and no plasticizer or filler. Short-term mechanical properties are verified under ASTM D638-14, ASTM D1004-13, and ASTM D4833/D4833M-07(2018); long-term stress crack resistance is assessed by ASTM D5397-19 notched constant tensile load testing and ASTM D1693 ESCR. Field seaming uses dual-track hot-wedge welding or extrusion fillet welding; weld peel strength is tested per ASTM D6392-12, and air-channel pressure testing is performed per ASTM D7177/D7177M-05(2019). For mining applications, the sheet is exposed to sulfuric acid and cyanide solutions; chemical resistance is verified under DIN EN ISO 175 immersion testing at service temperature. Terminal products include HDPE geomembranes for municipal solid waste cells, mining heap leach pads, reservoir liners, and secondary containment basins.

    Multilayer Coextrusion Windows for Automotive Fuel System Shells with HDPE KB147N

    Coextruded automotive fuel system shells utilize HDPE KB147N as the outer and inner structural layers because of its high melt strength and resistance to environmental stress cracking in the presence of fuel vapors, road salt, and underbody mechanical stress. The six-layer blow molding process runs on a coextrusion accumulator or continuous-parison machine with layer distribution controlled by a gravimetric dosing system; typical layer percentages are HDPE outer 20–30 wt%, regrind 20–35 wt%, tie-layer 1.5–2.5 wt%, EVOH barrier 1.5–3.0 wt%, tie-layer 1.5–2.5 wt%, and HDPE inner 20–30 wt%. Melt temperatures for the HDPE layers are held at 200–220 °C, while the EVOH layer requires 190–210 °C and must be kept below 240 °C to avoid crosslinking and gel formation. Formulation for the HDPE layers includes carbon black masterbatch at 1.0–2.0 wt% when conductive grades are not specified, antioxidant package at 0.2–0.5 wt%, and no stearate above 0.1 wt% to minimize plate-out on the die lips. Permeation limits are set by ECE R34, EPA 40 CFR 86, and CARB LEV III evaporative emission requirements; material compatibility is assessed under SAE J1681 and ISO 175 immersion tests with Fuel C and aggressive ethanol blends. The finished part is subjected to burst pressure testing, drop impact at low temperature, and leak testing under OEM-specific tank test protocols. Terminal product types include multilayer fuel tanks, urea solution reservoirs, and fuel filler neck shells for passenger vehicles and commercial trucks.

    When Sheet Extruders Supply HDPE KB147N for Corrosion-Resistant Chemical Tank Lining

    Where industrial processors extrude thick HDPE sheet for fabrication of chemical storage tank linings and dual-laminate vessels, HDPE KB147N is processed on single-screw extruders with a length-to-diameter ratio of 30:1 or higher and a barrier screw to minimize residence time distribution. The sheet is extruded at melt temperatures of 210–235 °C, polished on a three-roll stack at 70–95 °C, and annealed below 100 °C to reduce frozen-in stress before welding. The formulation is adjusted for chemical service: carbon black masterbatch at 2.0–2.5 wt% for UV resistance in outdoor tanks, antioxidant package at 0.2–0.6 wt%, and no recycled material when the liner is specified under DVS 2205-1 or DVS 2205-2 for thermoplastics in chemical plant construction. Butt fusion welding of sheets is performed with a hot plate at 210–230 °C and a joining pressure of 0.10–0.15 MPa; welds are inspected visually and by bend testing according to DVS 2205-1 or ASTM E190. Chemical resistance is evaluated under DIN EN ISO 175 after immersion in sulfuric acid, sodium hydroxide, and sodium hypochlorite at service temperatures; published data for aggressive organic solvents with HDPE KB147N specific configurations is limited and exposure testing is recommended. Terminal products include HDPE tank liners for steel chemical storage tanks, dual-laminate scrubber shells, and fabricated acid neutralization vessels.

    Free Quote

    Competitive TPC (Japan) HDPE KB147N prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KB147N is identified in supplier technical documentation as a high-density polyethylene resin intended for extrusion blow molding of rigid packaging and industrial hollow articles. The grade is supplied as free-flowing pellets, with the manufacturer’s certificate of analysis and current product datasheet controlling density, melt flow rate, molecular weight distribution parameters, and additive loading. The resin belongs to the linear polyethylene family and is placed in the HDPE class under ASTM D4976-12a and ISO 17855-1:2014 because the as-molded density is above 0.940 g/cm³. Published data for this specific configuration is limited; the following technical description therefore defines the grade through the processing envelope and specification methods applicable to high-molecular-weight HDPE blow-molding resins, and through the known differences from general-purpose HDPE grades.

    The principal specification parameters are not limited to single-point melt flow. A low melt flow rate, customarily determined under ISO 1133-1:2022 at 190 °C and 2.16 kg, is expected to be paired with a broad or bimodal molecular weight distribution that provides shear sensitivity during plastication and melt strength during parison formation. Density is measured by ISO 1183-1:2019 or ASTM D1505-18 after annealing; density controls flexural stiffness, chemical permeation resistance, and top-load strength. The short-chain branching level and comonomer type influence environmental stress crack resistance and slow crack growth, so ESCR values under ASTM D1693-15 are used as lot-qualification data rather than as design constants. Tensile yield strength and elongation at break are determined under ISO 527-2:2012 or ASTM D638-14 on compression-molded sheets, but these values do not directly predict container performance because blow-molded walls are formed at much lower orientation.

    What Controls Parison Stability and Wall Thickness Distribution?

    Parison stability is governed primarily by extensional viscosity and the high-molecular-mass tail of the resin. On accumulator-head and reciprocating-screw blow molding machines, the resin is processed with barrel temperatures from 180 °C to 220 °C and die-head temperatures held between 190 °C and 210 °C to limit parison sag. Extruder length-to-diameter ratios of 24:1 to 30:1, compression ratios of 2.5:1 to 4.0:1, and screw speeds below 80 min⁻¹ are common for high-molecular-weight HDPE. A grooved-feed section or crammer may be used to suppress torque variation when regrind levels exceed 20 weight-% because high-molecular-weight HDPE has limited melt-phase thermal conductivity and can develop melt-temperature gradients.

    Die gaps between 1.5 mm and 3.0 mm are typical for articles with wall thickness from 0.4 mm to 2.0 mm. Parison swell at these gaps is controlled by shear history and land-length geometry rather than by raising melt temperature alone. A short land length increases die swell and can improve pinch-off weld strength in multi-cavity tooling, but it also widens the tolerance of the parison diameter. The resin’s melt strength is not indefinite; if the shot volume exceeds 5 L, cumulative sag before mold closing can reduce the effective bottom wall thickness by more than 0.2 mm on continuous shuttle machines.

    One process conflict occurs when die temperature is increased above 220 °C to suppress melt fracture or improve surface gloss. This reduces the extensional viscosity that supports the parison and can create a non-linear increase in sag rate on large containers. Conversely, reducing melt temperature below 180 °C raises back-pressure and may produce unmelts or flow lines at the pinch-off. Shot-to-shot melt temperature variation should be held within ±3 °C, and accumulator fill time should be kept below 4 s because residence-time dispersion broadens the local molecular weight distribution through thermal-oxidative chain scission. Published data for this specific configuration is limited.

    Dynamic oscillatory shear at 190 °C can be used to quantify crossover modulus and the high-molecular-weight tail. A high value of storage modulus at low frequency correlates with parison sag resistance. Incoming resin should also be tested by capillary rheometry at apparent shear rates from 100 s⁻¹ to 1000 s⁻¹ because these are typical of die flow. Melt fracture onset at the die is a function of wall shear stress; if die entry pressure fluctuation exceeds ±0.5 MPa, the die land should be inspected for degraded polymer deposits.

    Compared with general-purpose HDPE injection-molding grades, the KB147N designation is differentiated by a lower melt flow rate, a higher average molecular weight, and a rheology profile that favors intermittent extrusion rather than long, thin-walled injection flow. In injection molding tools with flow-length-to-thickness ratios above 200:1, this class of material may freeze off prematurely or require melt temperatures above 240 °C, which increases the risk of oxidation. The grade is also not a structural pipe or film resin: pipe grades are formulated for long-term hydrostatic strength under ISO 9080, while film grades are optimized for bubble stability and tear resistance under high-stalk extrusion.

    Against HDPE grades designed for small blow-molded bottles, the differentiation often lies in ESCR and stiffness balance. If the resin uses a higher comonomer content, ESCR improves but density and top-load stiffness decline. If the resin uses a lower comonomer content and narrower molecular weight distribution, stiffness and gloss may improve but ESCR can fall below the threshold needed for detergents and liquid concentrates. The product’s specific comonomer type and antioxidant package must be read from the supplier datasheet; a supplier compliance statement is required before the material is used in containers for aggressive surfactants, oxygenated solvents, or aqueous emulsions.

    Specification Methods and Lot-Release Data

    The following methods are relevant for incoming inspection and periodic process verification. The actual lot-release values, tolerances, and measurement conditions for TPC (Japan) HDPE KB147N are fixed by the manufacturer’s specification and certificate of analysis.

    PropertyStandardConditionUse in process control
    Melt mass-flow rateISO 1133-1:2022190 °C, 2.16 kgIncoming resin flow classification
    DensityISO 1183-1:2019 / ASTM D1505-1823 °C after annealingStiffness and classification
    Tensile yield strengthISO 527-2:2012 / ASTM D638-1450 mm/min type I specimenCompression-molded sheet quality
    Elongation at breakISO 527-2:2012 / ASTM D638-1450 mm/minDuctility indicator
    ESCRASTM D1693-15Condition B, 10 % Igepal, 50 °CDetergent and chemical resistance
    Notched Charpy impactISO 179-1:202323 °CImpact screening
    Oxidative induction timeISO 11357-6:2018 / ASTM D3895-19200 °C, O₂Stabilizer package verification

    Blow-molded containers made from this class of resin are typically qualified by top-load compression, drop impact at −20 °C, and ESCR on bottle specimens rather than by injection-molded tensile plaques. Top-load force is proportional to wall thickness, density, and section modulus; for a cylindrical bottle of 1 L capacity and 0.8 mm nominal wall, top-load is not controlled solely by resin density, because tooling, parison programming, and pinch-off geometry contribute more variability than the resin lot itself. Drop impact at sub-ambient temperatures is sensitive to pigment dispersion, regrind content, and stress concentrations at the pinch-off; visual inspection alone does not detect microcracks that propagate under stress cracking conditions.

    Food-contact and potable-water applications must be supported by a written supplier certification against FDA 21 CFR 177.1520, Commission Regulation (EU) No 10/2011 and its amendments, GB 9685-2016 for additives used in China, and the applicable Japan Food Sanitation Law specifications. The grade should not be assumed compliant for all food types; oily or alcoholic simulants require specific migration testing on the finished article. For non-food industrial applications, the resin should be covered by REACH registration and, where applicable, RoHS recast 2011/65/EU documentation for cadmium, lead, mercury, and hexavalent chromium below threshold limits.

    Regulatory boundaryRequired evidenceLimiting condition
    United States food contactFDA 21 CFR 177.1520Olefin polymer class; end test for migration
    European Union plastics contactRegulation (EU) No 10/2011Overall migration and specific migration limits
    China additive complianceGB 9685-2016Additive positive list and use level
    Japan food sanitationJapan Food Sanitation Law specificationsPolyethylene oven temperature and migration
    REACH registrationRegistration number per tonnage bandSubstance and article obligations
    RoHS recast2011/65/EU documentationThreshold limits for restricted metals

    Storage prior to processing is less sensitive than for polyamides or polycarbonate, but surface moisture from outdoor storage or condensation can produce splay in blow-molded parts. When visible moisture is present, pellets should be dried at 70 °C to 80 °C for 2 h to 3 h using a desiccant or hot-air dryer with a dew point below −20 °C. Prolonged drying above 90 °C can deplete the antioxidant package and reduce oxidative induction time. The resin should not be dry-blended with PET, PVC, polycarbonate, or filled polymers; even small fractions of these contaminants create delamination defects and can accelerate environmental stress cracking.

    Regrind from trimmed flash, defective parisons, and start-up scrap can be reincorporated at typical levels of 10–20 weight-% when the regrind is dust-free and generated from the same lot family. Higher regrind fractions may lower the swell ratio and reduce melt strength because of repeated chain scission and the loss of high-molecular-mass chains. The exact maximum regrind percentage for a given container lot must be determined by measuring parison length retention and top-load capacity after molding; a change in radial wall-thickness distribution greater than 0.05 mm indicates that the regrind fraction exceeds the process capability of the tool.

    Thermal degradation accelerates above 230 °C, and melt hold time during stoppages should not exceed 10 min at processing temperature. Oxidative degradation causes yellowing and a shift in melt flow rate that can exceed 10 % relative to the virgin pellet. If black specks, acrid odor, or fluctuating head pressure are observed, the barrel and die should be purged with a low-melt-index polyethylene purge compound, not with PVC or halogenated cleaning agents. The die and mandrel should be inspected for degraded polymer deposits at least once per 8 h of continuous operation.

    Top