| HS Code | 450590 |
| Density | 1.36 g/cm3 |
| Water Absorption | 0.30 % |
| Linear Mold Shrinkage | 0.0020-0.0050 cm/cm |
| Tensile Strength Ultimate | 75.0 MPa |
| Elongation At Break | 90 % |
| Tensile Modulus | 2.20 GPa |
| Flexural Modulus | 2.30 GPa |
| Izod Impact Notched | 0.0500 J/cm |
| Melting Point | 265 °C |
| Glass Transition Temperature | 121 °C |
| Deflection Temperature At 1 8 Mpa | 90.0 °C |
| Dielectric Constant | 3.20 |
| Dissipation Factor | 0.0020 |
| Volume Resistivity | 1.00e+16 ohm-cm |
| Dielectric Strength | 20.0 kV/mm |
As an accredited Toyobo PEN Resin Generic PEN factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Toyobo PEN Resin Generic PEN is packaged in 25 kg moisture-proof, sealed bags within protective fiber drums. |
| Container Loading (20′ FCL) | Toyobo PEN Resin Generic PEN is loaded in a 20-foot FCL container, palletized, secured, and prepared for ocean shipment. |
| Shipping | Toyobo PEN Resin Generic PEN is shipped as a non-hazardous solid polymer in sealed bags or drums, palletized and protected from moisture and direct sunlight. No UN number or hazard class applies. Transport as general cargo; store in a cool, dry, well-ventilated area. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed and protect from moisture; use moisture-barrier packaging and avoid humid conditions to prevent resin absorption. Maintain good housekeeping to control dust, segregate from incompatible materials, and follow first-in, first-out stock rotation. Store only in original, labeled containers. |
| Shelf Life | Toyobo PEN Resin Generic PEN typically has a shelf life of about 12 months when stored cool, dry, and away from direct sunlight. |
Competitive Toyobo PEN Resin Generic PEN prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Toyobo PEN Resin Generic PEN is an unfilled polyethylene naphthalate pellet grade supplied for injection molding, extrusion, film orientation, and blow molding. The resin designation “Generic PEN” denotes a base polymer without impact modifiers, reinforcing fillers, or flame-retardant additives; specific end-use formulations are not implied by this product name. Chemically, the repeat unit incorporates 2,6-naphthalenedicarboxylate in place of the terephthalate group used in conventional PET, and the fused aromatic structure is responsible for the elevation of the glass transition temperature to 118–125 °C under ISO 11357-2 and the crystalline melting temperature to 262–272 °C under ISO 11357-3. Density is reported between 1.33 g/cm³ and 1.38 g/cm³ under ISO 1183-1. The resin is hydrolytically sensitive at melt temperatures, so drying is treated as a release-critical step rather than an optional preparation. Because no single published melt flow rate applies to all lots, processors should use the supplier certificate of analysis and monitor melt viscosity at the hopper rather than transferring generic MFR values from other PEN grades.
The naphthalene ring restricts segmental motion more than the para-disubstituted benzene ring of PET, producing a higher glass transition and a slower spherulite growth rate. Differential scanning calorimetry on quenched amorphous samples reveals a cold crystallization exotherm between 170 °C and 200 °C when heated at 10 °C/min under ISO 11357-3; for PET the corresponding exotherm is typically located at least 40 °C lower. Crystallization from the melt is slow enough that cold mold walls below 100 °C produce predominantly amorphous parts, while molds held above 120 °C allow the development of a semicrystalline morphology with higher modulus above the glass transition and better solvent resistance. Published polymer literature estimates the equilibrium melting point of PEN near 300 °C, but practical melt processing occurs at 290–310 °C because the thermodynamic melting point is approached only under very low heating rates. Intrinsic viscosity is measured by polymer-adapted methods derived from ISO 1628-5; commercial PEN grades are commonly found between 0.55 dL/g and 0.80 dL/g in 60/40 phenol/tetrachloroethane at 30 °C, though lot-specific Toyobo data must be obtained from the certificate of analysis.
Before melt processing, the pellets require desiccant drying with a supply air dew point no higher than −40 °C, preferably below −50 °C at the hopper inlet. Drying temperature is normally set between 150 °C and 170 °C for 4–6 h to achieve a residual moisture level below 50 ppm; excursions above 80 ppm have been associated with visible splay on preforms, molecular weight loss, and screw torque drift in production-scale injection molding. Melt temperature should be maintained between 290 °C and 310 °C, with rear barrel zones near 280 °C and the nozzle near 305 °C as a starting profile; actual settings depend on shot size, residence time, and hot-runner design. Screw geometries designed for PET are generally acceptable, though the higher melting point requires higher barrel settings; a shutoff nozzle is preferred to prevent drool and thermal degradation in the nozzle body. Capillary rheometry data for unfilled PEN at 300 °C indicate shear-thinning behavior with an apparent viscosity of about 200–400 Pa·s at 1,000 s⁻¹ and a power-law index between 0.5 and 0.7. Injection molds are typically held at 120–160 °C to induce crystallinity and reduce post-mold shrinkage; tools below 100 °C yield amorphous components with lower elevated-temperature stiffness. Desiccant-bed audits show that temperature recovery after hopper refill is a recurring bottleneck: if return air falls below 140 °C, the drying cycle should be restarted, not merely extended.
The fused naphthalene ring imposes a higher aromatic content per repeat unit than the six-carbon terephthalate ring, increasing chain stiffness, gas barrier, and ultraviolet absorption. The naphthalene ring imparts a UV absorption edge near 380 nm, providing intrinsic screening of UV-A and UV-B in films. Oxygen transmission measurements on biaxially oriented PEN typically fall between 0.6 mL·mm/(m²·day·atm) and 1.0 mL·mm/(m²·day·atm) at 23 °C and 0% relative humidity under ASTM D3985, whereas PET under equivalent conditions is generally reported between 2.5 mL·mm/(m²·day·atm) and 4.0 mL·mm/(m²·day·atm). Water vapor transmission is similarly lower: PEN films are reported near 2.0 g·mm/(m²·day) at 38 °C and 90% relative humidity under ASTM F1249, while uncoated PET is more commonly 4.0–6.0 g·mm/(m²·day). Tensile modulus of oriented PEN is typically 5.0–6.0 GPa under ISO 527-3, approximately double PET and PBT. The trade-off is a narrower stretch-processing window and higher raw-material cost; PBT retains faster crystallization and better low-temperature impact in thin-wall connectors, while PET remains preferred where low cost and high productivity dominate.
| Property | Test standard | Generic PEN | PET | PBT |
|---|---|---|---|---|
| Density | ISO 1183-1 | 1.33–1.38 g/cm³ | 1.34–1.40 g/cm³ | 1.31–1.35 g/cm³ |
| Glass transition temperature | ISO 11357-2 | 118–125 °C | 75–80 °C | 45–60 °C |
| Crystalline melting temperature | ISO 11357-3 | 262–272 °C | 250–260 °C | 220–230 °C |
| Tensile modulus | ISO 527-1/-2 | 5.0–6.0 GPa | 2.8–3.5 GPa | 2.5–3.0 GPa |
| Heat deflection temperature at 1.82 MPa | ISO 75-2/A | 150 °C | 70 °C | 60 °C |
| Oxygen permeability | ASTM D3985 | 0.6–1.0 mL·mm/(m²·day·atm) | 2.5–4.0 mL·mm/(m²·day·atm) | Not normally specified for unfilled PBT |
In hot-fill and returnable bottle applications, the resin is injection molded into preforms and stretch blow molded at preform temperatures between 130 °C and 145 °C. Axial stretch ratios are typically limited to 2.5–3.0 and radial ratios to 3.5–4.0, slightly lower than PET because the naphthalene backbone generates higher orientation stress. The higher glass transition permits hot-fill contact at 90–95 °C without the same degree of paneling or post-fill shrinkage observed in standard PET at equivalent wall thickness. Electrical and electronic film applications use sequential or simultaneous biaxial stretching, and PEN has been selected where short-term solder-float or soldering-iron contact temperatures near 230 °C must not produce extensive shrinkage. In monofilament and industrial fiber spinning, reported spinning temperatures are near 300 °C, with draw ratios above 5 in published fiber-processing literature. The resulting filaments retain a higher fraction of room-temperature tensile strength at 150 °C than PET monofilament, but the slower quench and higher spinline orientation require longer cooling chimneys and more precise godet temperature control.
Heat deflection temperature measured under ISO 75-2/A at 1.82 MPa provides a standardized indication of the temperature at which a defined flexural deflection occurs. Annealed unfilled PEN specimens typically show HDT values near 150 °C at 1.82 MPa and 155 °C at 0.45 MPa under ISO 75-2/B. This is approximately 70–80 °C higher than annealed PET and 85–95 °C higher than PBT at equivalent stress. The difference arises from the higher glass transition and from the slower cooperative motion of naphthalate segments. However, the HDT value is not a material constant: amorphous moldings or insufficiently crystallized parts will show lower values, and the measured result depends on specimen thickness, mold-in stress, and annealing history. Post-mold annealing at 180 °C for 30–60 min is frequently used to stabilize dimensions and increase crystallinity before precise metrology, but dimensional change during annealing can reach 0.5–1.0% depending on residual orientation. For parts requiring tight tolerances above 150 °C, the tool cooling circuit should be designed to maintain mold surface uniformity within ±5 °C because asymmetric crystallization produces differential shrinkage and measurable warpage.
Food-contact status for the final article must be established through the specific fabrication route and end-use simulant. In the United States, a supplier Food Contact Notification or equivalent regulatory clearance is typically required; processors should not assume that 21 CFR 177.1630 automatically covers polyethylene naphthalate, since that section defines polyethylene phthalate polymers and may require supplementary migration data for naphthalate repeat units. European food-contact compliance is evaluated under Regulation (EU) No 10/2011, with overall migration measured according to the EN 1186 series and specific migration of naphthalene-2,6-dicarboxylic acid as a starting substance if applicable. Electrical and electronic applications are supported by declarations of conformity to RoHS Directive 2011/65/EU and, where relevant, verification of registration status under REACH Regulation (EC) No 1907/2006. No claim of medical-grade or USP Class VI performance should be inferred for the generic resin without a separate validation package.
The principal operational boundary is hydrolytic chain scission at the ester linkage. Processing above 320 °C or cumulative residence time beyond 5–10 min can produce a measurable drop in intrinsic viscosity and an increase in carboxylic acid end-group concentration. Strong alkaline solutions, particularly at pH above 13, saponify the polyester backbone and should not be used for cleaning or service exposure. Concentrated oxidizing acids and certain chlorinated solvents may induce environmental stress cracking in molded parts carrying high molded-in stress; the part geometry and gate region are typically the first locations to show microcracks. Continuous dry-heat exposure above 180 °C can cause oxidative yellowing unless an antioxidant package is included. Published data for prolonged outdoor weathering of Toyobo-specific thick-section PEN moldings is limited; for external applications, UV-stabilized or protected constructions should be evaluated rather than assuming the naphthalene UV absorption alone confers weatherability. Purge compounds and shutdown procedures should be adapted to the higher melting point because residual PEN left in a cold barrel can freeze and require high-torque restart or barrel disassembly.