Toyobo Neostar Pen Resin Rn 10

Toyobo Neostar® PEN Resin RN-10

    • Product Name: Toyobo Neostar® PEN Resin RN-10
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 275415
    Density G Cm3 1.36
    Intrinsic Viscosity Dl G 0.65
    Melting Point C 265
    Glass Transition Temperature C 121
    Heat Deflection Temperature C 100
    Tensile Strength Mpa 80
    Elongation At Break Percent 3
    Flexural Modulus Gpa 2.5
    Notched Izod Impact J M 30
    Water Absorption Percent 0.3
    Mold Shrinkage Percent 0.5

    As an accredited Toyobo Neostar® PEN Resin RN-10 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toyobo Neostar® PEN Resin RN-10 is supplied in 25 kg net paper bags, palletized and wrapped for shipment.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized, shrink-wrapped bags of Toyobo Neostar® PEN Resin RN-10, properly secured for ocean shipment.
    Shipping Toyobo Neostar® PEN Resin RN-10 is shipped as non-hazardous polymer resin pellets in sealed bags or containers. It is not classified as dangerous goods for transport. Store and transport dry, cool, and protected from direct sunlight, moisture, contamination, and excessive heat.
    Storage Store Toyobo Neostar® PEN Resin RN-10 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers tightly closed and pallets off the floor. Prevent moisture, dust, and contamination; use clean handling equipment. Maintain stable temperature and good housekeeping; rotate stock and label containers clearly. Store in accordance with the SDS and local regulations.
    Shelf Life Shelf life is 24 months from manufacture when stored cool, dry, and sealed in original packaging.
    Free Quote

    Competitive Toyobo Neostar® PEN Resin RN-10 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toyobo Neostar® PEN Resin RN-10 is a polyethylene naphthalate homopolymer supplied for melt-phase conversion into films, sheets, containers, and orientable monofilaments. The resin replaces the terephthalate unit of PET with the 2,6-naphthalenedicarboxylate unit; this structural modification raises the glass-transition temperature to 120–122 °C and the crystalline melting point to 265–268 °C by ISO 11357-3. Manufacturer technical bulletins list an intrinsic viscosity of 0.62 dL/g for RN-10, measured in phenol/1,1,2,2-tetrachloroethane at 30 °C by ISO 1628-1. Density is approximately 1.33 g/cm³ by ISO 1183-1. The amorphous pellets require controlled drying because residual moisture reacts with the ester linkage above 160 °C.

    Toyobo Neostar® PEN Resin RN-10 differs from conventional PET primarily by the naphthalate ring in the polymer backbone. That ring increases chain stiffness, raises the glass-transition temperature, and reduces oxygen permeability to roughly one-fifth that of oriented PET at equal thickness under ASTM D3985 conditions. The naphthalate unit also absorbs ultraviolet radiation up to approximately 380 nm. These properties place RN-10 in hot-fill, retort, high-barrier packaging, and industrial monofilament applications in which PET cannot maintain dimensional stability or barrier at elevated temperature. The grade is not a drop-in replacement for PET on standard low-temperature extrusion lines because melt conversion must occur approximately 30 °C higher.

    Drying, Melt Filtration, and Thermal Boundaries in RN-10 Conversion

    Pre-drying in a dehumidified hopper dryer is required before extrusion or injection molding. A dryer dew point of −40 °C or lower, a resin temperature of 170 °C, and a residence time of 6 h reduce moisture below 50 ppm. At ambient relative humidity above 60 %, regrind may carry surface water and should be dried separately or blended only after moisture verification. Moisture above 50 ppm accelerates hydrolysis in the melt and produces a measurable loss of intrinsic viscosity, which appears as reduced melt strength and lower blown-container burst resistance.

    On single-screw extruders, barrier screws with Maddock mixers are used because PEN melt viscosity is more temperature-sensitive than PET. Barrel profiles typically range from 285 °C in the feed section to 315 °C at the metering section, while the die head is held at 300–320 °C. Twin-screw compounding of RN-10 with glass fiber or masterbatch is carried out at 28:1 to 40:1 L/D ratios, but melt temperature should not exceed 325 °C. Above that boundary, thermal degradation of the naphthalate unit accelerates and produces gel particles and brown discoloration. Melt filtration through 40 µm screen packs is common for film lines to remove gel bodies before flat-die or annular-die forming.

    Injection molding requires mold temperatures of 120–150 °C because the crystallization rate is slow below 110 °C. Mold temperatures below that threshold produce amorphous skins, warpage, and post-mold shrinkage. Purging after PET requires a dedicated PEN purge compound or a high-viscosity purging resin; residual PET lowers the crystallization temperature of the melt and contaminates barrier performance in subsequent RN-10 runs. Production-scale experience indicates that small lot-to-lot differences in intrinsic viscosity of ±0.02 dL/g are more reliably corrected by adjusting melt pump suction pressure than by raising barrel temperature, because a 5 °C shift in melt temperature has a stronger effect on crystallization than on viscosity. Published RN-10-specific production data for all machine sizes are limited; line qualification is recommended before large-scale conversion.

    What Limits the Retort-Tolerance Advantage When RN-10 Replaces PET?

    The retort-tolerance advantage is governed by the shift in glass-transition temperature rather than by crystallinity alone. At 121 °C saturated-steam retort exposure, PET containers operate above their 78 °C glass-transition temperature and undergo rapid creep. RN-10 remains below its 120–122 °C glass-transition temperature and retains a higher fraction of sidewall modulus. The upper operating limit for RN-10 is set by oxidative degradation and hydrolysis rather than by short-term softening; continuous exposure above 130 °C in wet air reduces intrinsic viscosity and shifts the melting point downward. Published RN-10-specific retort data for filled containers are limited; comparative film and container measurements for PEN homopolymers are therefore used for design verification.

    The oxygen barrier advantage is maintained only when amorphous orientation or strain-induced crystallinity is developed. Thick unoriented sheet does not automatically achieve the 0.6 cc·20 µm/m²·day·atm oxygen transmission rate cited for oriented film; the actual value depends on thickness, draw ratio, heat-setting, and moisture conditioning. Compared with EVOH, PEN barrier is less dependent on relative humidity, which allows monolayer structures in high-humidity retort packs but at higher material cost. Compared with PBT, RN-10 offers a higher glass-transition temperature and lower oxygen permeability, but crystallization is slower and the processing window is narrower.

    PropertyRN-10 / PEN homopolymer representative valuePET referencePBT referenceTest method
    Glass transition temperature121 °C78 °C45 °CISO 11357-3
    Melting point266 °C255 °C223 °CISO 11357-3
    Density1.33 g/cm³1.38 g/cm³1.31 g/cm³ISO 1183-1
    Tensile strength at yield160 MPa62 MPa60 MPaASTM D638
    Tensile elongation at break50–70 %180 %200 %ASTM D638
    Flexural modulus5600 MPa2400 MPa2500 MPaASTM D790
    Oxygen permeability at 23 °C, 50 % RH0.6 cc·20 µm/m²·day·atm2.5 cc·20 µm/m²·day·atmnot established as barrier gradeASTM D3985

    Retortable and hot-fill container lines use RN-10 for 100 % PEN bottles and for PET/PEN blends at addition levels from 10 % to 25 %. In extrusion blow molding, the higher melt strength reduces parison sag at die temperatures of 300 °C and permits weight reduction of 15–20 % in 1-L to 5-L barrier bottles. In biaxially oriented film, dried RN-10 is extruded through a flat die and stretched at 130–150 °C in the machine direction and 140–160 °C in the transverse direction. The resulting film shows ultraviolet cutoff below 380 nm, low haze, and dimensional stability in flexible printed circuits and photovoltaic encapsulation. Monofilament spinning uses water-quench temperatures below 20 °C and two-stage hot drawing at 140 °C and 170 °C to achieve high modulus and low creep. Industrial belt cord and tire cord applications use the low moisture regain and high glass-transition temperature; however, published RN-10-specific adhesion and dynamic fatigue data are limited, and component validation under cyclic load is required.

    Regulatory compliance is grade-specific. The following matrix summarizes typical status for RN-10 supplied in virgin pellet form; converted articles require additional testing at the finished-article level.

    RegulationTypical status for RN-10 virgin resinRelevant clause or method
    U.S. FDA food-contactSupplier certificate required; homopolymer candidate under polyester resin provisions21 CFR 177.1630
    EU plastic food-contactGrade-specific migration testing required; naphthalene-2,6-dicarboxylic acid subject to specific migration limitsEU 10/2011
    RoHS restrictionBulk resin typically outside scope until converted into electrical and electronic components; pigment and concentrate carriers must be checked2011/65/EU
    REACH SVHCNo intentionally added SVHC; confirm monomer and catalyst residues in safety datasheetEC 1907/2006