Toyobo Neostar Pen Film Fn 2

Toyobo Neostar® PEN Film FN-2

    • Product Name: Toyobo Neostar® PEN Film FN-2
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 859290
    Material Polyethylene naphthalate (PEN)
    Grade FN-2
    Film Type Biaxially oriented film
    Thickness Range 25–250 µm
    Density 1.36 g/cm³
    Melting Point 265 °C
    Glass Transition Temperature 121 °C
    Tensile Strength Md 250 MPa
    Tensile Strength Td 250 MPa
    Elongation At Break Md 110%
    Elongation At Break Td 110%
    Youngs Modulus Md 6.0 GPa
    Youngs Modulus Td 6.0 GPa
    Heat Shrinkage 150c 30min Md 0.3%
    Heat Shrinkage 150c 30min Td 0.3%
    Coefficient Of Thermal Expansion 15 ppm/°C
    Refractive Index 1.65
    Haze 1.0%
    Total Light Transmittance 87%
    Water Absorption 0.4%
    Dielectric Constant 1mhz 3.0
    Dielectric Loss Tangent 1mhz 0.005
    Breakdown Voltage 300 kV/mm
    Surface Roughness Ra 0.01 µm
    Continuous Service Temperature 150 °C

    As an accredited Toyobo Neostar® PEN Film FN-2 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toyobo Neostar® PEN Film FN-2 is supplied as one roll per cardboard box, individually wrapped and protected for shipment.
    Container Loading (20′ FCL) Toyobo Neostar® PEN Film FN-2 is safely loaded, palletized, secured, and moisture-protected in a 20′ FCL container for transport.
    Shipping Toyobo Neostar® PEN Film FN-2 is shipped as a non-hazardous, non-regulated solid film in sealed, moisture-resistant packaging. Transport at ambient temperature, away from direct sunlight, heat, and physical damage. Avoid punctures, compression, and contamination; handle with clean gloves and keep original labels intact.
    Storage Store Toyobo Neostar® PEN Film FN-2 in its original packaging in a clean, cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, moisture, dust, and strong oxidizers. Keep rolls or sheets supported/flat to prevent warping or mechanical damage. Maintain stable ambient conditions and follow the manufacturer’s shelf-life and handling recommendations.
    Shelf Life Shelf life is 12 months from manufacture when stored in original packaging under normal temperature and humidity, away from direct sunlight.
    Free Quote

    Competitive Toyobo Neostar® PEN Film FN-2 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toyobo Neostar® PEN Film FN-2 is a biaxially oriented polyethylene naphthalate film supplied by Toyobo Co., Ltd. The model designation places FN-2 within the Neostar PEN film range; the suffix identifies a two-side surfaced grade in the manufacturer’s nomenclature, while the base resin remains polyethylene naphthalate as defined under ISO 1043-1. Molecular orientation is developed through controlled stretching after melt casting, producing a balance of tensile, thermal, and dielectric properties that differs from conventional poly(ethylene terephthalate) film. Published gauge availability for the Neostar PEN family extends from 2 µm to 250 µm; however, lot-specific thickness capability for FN-2 is not fixed in publicly available technical literature and should be confirmed against the current Toyobo specification sheet.

    The glass transition temperature of PEN, measured by differential scanning calorimetry according to ISO 11357-2, is approximately 155 °C; the crystalline melting peak occurs near 265 °C. For oriented PET, the corresponding glass transition is roughly 78 °C to 80 °C, which limits PET in high-temperature converting and end-use conditions. In PEN, the naphthalene-2,6-dicarboxylate unit increases chain stiffness and thermal transition temperatures compared with the terephthalate unit used in PET. The result is a film that can tolerate short thermal excursions above PET’s practical service range while retaining polyester-like electrical properties.

    Which Physical, Thermal, and Electrical Benchmarks Define the FN-2 Grade?

    Because FN-2-specific guaranteed values are found on the manufacturer’s certificate of analysis, the following table records class-typical values for biaxially oriented PEN film in the Neostar family. The values are engineering references and are not to be read as release limits for any specific lot. Dimensional, surface-treatment, and electrical acceptance criteria are controlled by the Toyobo product specification for the ordered caliper.

    Property Test method Class-typical value Reference note
    Thickness range ISO 4593 2 µm to 250 µm Neostar family range
    Density ISO 1183-1 1.36 g/cm³ 23 °C
    Tensile strength, MD ASTM D882-18 275 MPa Balanced orientation may vary by ±10%
    Tensile strength, TD ASTM D882-18 275 MPa Lot-dependent
    Elongation at break, MD/TD ASTM D882-18 60% / 60% Class-typical
    Tensile modulus, MD/TD ASTM D882-18 6.0 GPa / 6.0 GPa Class-typical
    Thermal shrinkage, 30 min at 150 °C, MD/TD ASTM D1204 0.5% / 0.3% Lower than PET under same exposure
    Total light transmittance ASTM D1003 87% Visible-region value
    Haze ISO 14782 3% Class-typical
    Dielectric strength at 25 µm IEC 60243-1 200 kV/mm Short-term test
    Dielectric constant at 1 MHz IEC 60250 3.0 Similar to PET
    Dissipation factor at 1 MHz IEC 60250 0.004 Class-typical
    Volume resistivity IEC 62631-3-1 1 × 1017 Ω·cm 23 °C, 50% RH
    Water absorption, 24 h at 23 °C ISO 62 0.4% Lower than polyimide
    Linear thermal expansion coefficient ISO 11359-2 20 × 10⁻⁶ K⁻¹ MD/TD class-typical

    The property pattern places FN-2 between PET and polyimide in thermal capability. The dielectric constant of 3.0 at 1 MHz matches standard PET and is lower than typical polyimide values of 3.4 to 3.5. Water uptake of 0.4% under ISO 62 is similar to PET but well below polyimide films that often absorb more than 2% moisture by mass. Dimensional stability at 150 °C is substantially better than PET; oriented PET under the same thermal exposure commonly exceeds 1.5% machine-direction shrinkage. The two-side treatment is intended for converting processes using waterborne, solventborne, or UV-curable coatings. Converters may specify wetting tension of 50 mN/m or higher under ISO 8296, but the actual acceptance value is lot-specific.

    When Roll-to-Roll Coating and Lamination Lines Process the Treated Web

    Web handling on high-speed converting lines is governed by caliper, tension, and oven residence. For a 25 µm treated PEN web, typical unwind tensions of 80 N/m to 150 N/m and a rewind taper from 20% to 40% are used on air-float dryers operating at 150 °C. Pre-drying is not generally required for slitting, but exposure to ambient moisture above 60% relative humidity before an oven process above 180 °C can contribute to hydrolysis-induced strength loss. When film has been stored in opened packaging, rack drying at 120 °C for 2 h to 4 h with a dew point below -30 °C reduces surface defects on coated webs.

    Slitting PEN generates higher edge wear than PET. Hardened steel or carbide shear knives are specified; blade depth is normally set at 2 to 3 times the film caliper. On a center-wound slitter with closed-loop tension control, excessive rewind pressure can produce blocking because the two-side treatment raises surface energy. A lay-on roller with contact pressure of 30 N to 60 N can prevent trapped air without inducing blocking. At line speeds near 100 m/min, web wander measured at the steering guide should be kept below 2 mm; edge misalignment beyond 5 mm at the coater can create baggy edges that are difficult to rewet or laminate evenly. UV-curable coatings applied over FN-2 may require higher dose when cure is attempted through the film, because PEN absorbs UV below 380 nm.

    In flexible printed circuit applications, FN-2 is evaluated as a base substrate or cover film where lead-free solder float temperatures reach 260 °C for 3 s to 5 s. PET-based films are generally not specified for this brief excursion because their glass transition is below 80 °C and shrinkage can exceed 1.5% at 150 °C. PEN’s melting point of 265 °C permits short solder exposure, but the operational boundary is explicit: continuous service above 180 °C or solder dwell beyond 10 s at 260 °C is better assigned to polyimide. Qualification should include solder-float testing according to IPC-TM-650 2.4.13.1 on the final laminated construction rather than on raw film alone.

    In wound capacitor production, FN-2 is used in thin gauges where PET dielectric temperature margins are insufficient. The dielectric strength of 200 kV/mm at 25 µm and dissipation factor of 0.004 at 1 MHz support pulse-rated and high-temperature capacitor designs. On capacitor winders, wrinkle control requires sheet-tension uniformity better than ±5% across the web, and film with cross-web caliper variation above ±2% is generally rejected for capacitor duty. Published performance data for FN-2 in specific capacitor configurations are limited; qualification is generally conducted by the converter using internal constant-current charge-discharge and thermal-endurance programs.

    Technical Comparison of PET, PEN FN-2, and Polyimide for High-Temperature Circuit Insulation

    Substitution of FN-2 for PET or polyimide involves trade-offs in thermal class, dimensional stability, and moisture sensitivity. The following comparative table is a design guide rather than a guarantee for any specific grade. The FN-2 certificate of analysis and the converter’s qualification program control final acceptance.

    Property Test method PET, oriented PEN FN-2 class-typical Polyimide, typical
    Glass transition ISO 11357-2 78–80 °C 155 °C 300 °C or greater
    Melting or decomposition ISO 11357-3 255 °C 265 °C No melt; decomposition above 500 °C
    Shrinkage at 150 °C, 30 min ASTM D1204 1.5–2.5% 0.3–0.5% <0.1%
    Water absorption, 24 h at 23 °C ISO 62 0.5% 0.4% 2.8%
    Dielectric constant at 1 MHz IEC 60250 3.0 3.0 3.4
    Dissipation factor at 1 MHz IEC 60250 0.005 0.004 0.010
    Solder float response IPC-TM-650 2.4.13.1 Not generally specified at 260 °C Limited to 3–5 s duration Suitable for extended dwell above 10 s
    Continuous electrical service class IEC 60085 Class 130 or lower Class 155 depending on UL file Class 240 or higher

    This comparison shows that FN-2 retains PET-like electrical properties while extending the thermal window toward polyimide. The principal limitation is not dielectric strength but upper service temperature. Polyimide remains the appropriate selection when continuous electrical service exceeds 155 °C or when dimensional change below 0.1% at 150 °C is mandatory. The two-side treatment of FN-2 may also permit lower lamination temperatures than untreated PEN, but published data for this specific configuration are limited.

    In high-temperature label and release-liner applications, FN-2 is exposed to thermal-transfer print heads near 200 °C and short oven dwells. PET labels can distort under these conditions, while FN-2 maintains legibility when oven dwell is held below 30 s at 180 °C. The treated surfaces accept waterborne and UV-curable topcoats; coating adhesion should be evaluated under ASTM D3359-17 cross-cut tape testing after 24 h post-cure. Hydrolysis resistance of PEN is advantageous in automotive underhood label applications where humidity and thermal cycling are present. In membrane switch or circuit-overlay use, the film is selected for dimensional stability after repeated actuation, but no generic flex-cycle life statement should be made without device-specific testing.

    Operational boundaries include avoidance of strong oxidizing acids, hot concentrated alkaline baths, and phenolic solvents because prolonged exposure can attack the polyester backbone. The higher glass transition of PEN compared with PET also means that heat-sealing and ultrasonic welding windows shift to higher temperatures or longer dwell. Where dimensional change below 0.1% at 150 °C is mandatory, polyimide or high-temperature thermoset films should be specified rather than FN-2. Flame-retardant classification such as UL 94 VTM-0 is caliper-dependent and must be confirmed from the Toyobo UL file for the exact FN-2 thickness and construction.