| HS Code | 627658 |
| Material | Polyethylene naphthalate (PEN) |
| Grade | FN-1 |
| Tensile Strength Md Td Mpa | 250/250 |
| Elongation At Break Md Td Percent | 90/90 |
| Tensile Modulus Md Td Gpa | 6.0/6.0 |
| Heat Shrinkage 150c 30min Md Td Percent | 0.5/0.5 |
| Volume Resistivity Ohm Cm | 1e16 |
As an accredited Toyobo Neostar® PEN Film FN-1 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically supplied as one sealed pack containing 10 sheets of Toyobo Neostar® PEN Film FN-1 in protective packaging. |
| Container Loading (20′ FCL) | Toyobo Neostar® PEN Film FN-1 is palletized, securely braced, and loaded into a clean, dry 20-foot FCL container for transport. |
| Shipping | Toyobo Neostar® PEN Film FN-1 is typically shipped as non-hazardous plastic film in sealed rolls or sheets, protected from moisture, heat, and impact. Transport at ambient temperature under dry conditions; no UN hazard class or special transport label is normally required. |
| Storage | For Toyobo Neostar® PEN Film FN-1, store in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and incompatible chemicals. Keep in original packaging, protected from moisture, dust, and mechanical damage. Do not store near ignition sources. Maintain ambient temperature, avoid extreme humidity, and follow first-in, first-out. Keep containers closed and labeled. |
| Shelf Life | Shelf life is typically 12 months from manufacture when stored sealed in original packaging at ambient temperature, away from direct sunlight. |
Competitive Toyobo Neostar® PEN Film FN-1 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Toyobo Neostar® PEN Film FN-1 is a biaxially oriented polyethylene naphthalate film supplied in roll form for subsequent converting by conventional polyester slitting, sheeting, die-cutting and lamination equipment. The grade designation FN-1 identifies a specific configuration within the Neostar PEN range; however, current public documentation for FN-1 does not separately list every surface-treated or thermally stabilised variant, so incoming specifications should request the certificate of analysis for nominal thickness, roll width, core diameter, surface treatment and lot shrinkage. Where grade-specific data are not available, the ranges presented here refer to published values for biaxially oriented PEN homopolymer film and should not be used as acceptance limits without written confirmation from the producer.
The polymer backbone is polyethylene 2,6-naphthalate, formed from ethylene glycol and 2,6-naphthalenedicarboxylic acid. The naphthalate repeat unit increases chain stiffness relative to oriented poly(ethylene terephthalate) and shifts the glass transition into the 120–124 °C range, with a melting endotherm near 265–269 °C when measured by differential scanning calorimetry following ISO 11357-2. Biaxially oriented PEN films typically show tensile strength at break in the 200–300 MPa range and tensile modulus near 5–6 GPa under ASTM D882. FN-1 may fall within or outside these typical ranges depending on gauge, surface treatment and heat history.
Measurements by ASTM D3985 on uncoated 25 µm biaxially oriented PEN homopolymer films commonly show an oxygen transmission rate that is 4–5 times lower than that of an equivalent 25 µm PET film at 23 °C and 50 % RH. Water-vapour transmission rate, measured according to ISO 15106-3 or ASTM F1249, is similarly reduced by a factor of 3–4 under the same thickness and humidity gradient. The reduced permeation is not merely a thickness effect; the naphthalene dicarboxylate unit restricts segmental motion and lowers the fractional free volume available for gas diffusion. This same chain rigidity also slows oxidative and thermal degradation reactions that require backbone mobility, but it does not eliminate the need for thermal stabilisation in prolonged service above 150 °C.
In adhesiveless flexible printed circuit construction, the barrier improvement relative to PET reduces copper oxidation at the film–copper interface during humidity aging. However, the film surface must be plasma-treated, corona-treated or chemically primed to achieve peel strength values above 8 N/cm when tested by IPC-TM-650 Method 2.4.8. Untreated PEN surfaces generally fall below 4 N/cm against rolled copper foil. Laminators using heated platen presses can run above 160 °C without the severe shrinkage observed with unannealed PET, but extended dwell above 180 °C can generate oligomer bloom and increase haze. The exact upper dwell time depends on gauge, line speed and roll pressure, and must be established by production trials.
The comparative values below are typical for transparent uncoated films; they are not grade-specific acceptance limits for FN-1.
| Property | Test basis | Biaxially oriented PEN typical range | Biaxially oriented PET typical range |
|---|---|---|---|
| Glass transition temperature | ISO 11357-2 | 120–124 °C | 78–80 °C |
| Melting endotherm peak | ISO 11357-2 | 265–269 °C | 250–255 °C |
| Tensile strength at break | ASTM D882 | 200–300 MPa | 150–250 MPa |
| Oxygen transmission rate relative to 25 µm PET | ASTM D3985 | 0.20–0.25 relative | 1.0 reference |
| Water-vapour transmission rate relative to 25 µm PET | ISO 15106-3 | 0.25–0.33 relative | 1.0 reference |
Thickness uniformity in roll stock should be checked by ASTM D374 or equivalent beta-transmission gauge; lot data for biaxially oriented PEN typically show a thickness tolerance near ±5 %, but tighter values may require slit-to-width selection. The coefficient of thermal expansion for PEN film is commonly reported in the 20–25 ppm/°C range in the transverse direction, which is lower than that of many cast polymer films but higher than that of copper foil; in multilayer circuits, this mismatch produces curl after thermal lamination. The curl direction and magnitude depend on the lamination temperature, web tension and copper thickness, and should be measured after 24 h at 23 °C and 50 % RH.
During roll-to-roll laser cutting of 50 µm FN-1 film on a reel-to-reel CO₂ laser system operating at 9.3 µm or 10.6 µm, the dominant processing variables are beam fluence, scan speed and nitrogen purge flow. Excessive fluence creates edge carbonization and local crystalline melting that can later initiate crack growth under dynamic flexing. A nitrogen-assisted purge at 2–4 bar is commonly used to reduce char formation, but the nozzle-to-web distance must be held within the laser manufacturer’s prescribed depth of focus. After cutting, debris and residual edge stress can be reduced by a plasma or solvent cleaning step; however, strongly alkaline cleaning baths above 40 °C should be avoided because ester bond hydrolysis will reduce molecular weight and embrittle the film. Web tension during slitting and lamination should be controlled at the lowest value that prevents lateral drift, since excessive tension creates curl and may shift the film’s thermal shrinkage behaviour after ageing.
Before magnetron sputtering of indium tin oxide or silicon oxide barrier layers, rolls should be pre-dried at 80–100 °C for 12–24 h under vacuum or dry air to remove surface moisture. In batch coaters with base pressure below 5×10⁻⁶ mbar, outgassing from polyester films can extend pump-down; PEN’s lower moisture uptake relative to PET reduces this effect. Deposited layer adhesion is sensitive to surface activation; inline plasma treatment with argon-oxygen mixtures at power densities of 2–5 W/cm² is common but should be verified for FN-1 because excessive plasma exposure may reduce molecular weight at the surface.
In high-voltage slot liner and motor insulation testing, uncoated biaxially oriented PEN film is commonly characterised by a dielectric strength of 180–220 kV/mm at 25 µm thickness under IEC 60243-1. Relative permittivity is typically 3.0–3.4 and the dissipation factor is below 0.005 at 1 kHz when measured by IEC 62631-2-1. These values are thickness- and frequency-dependent; dielectric strength decreases as gauge increases, and partial discharge inception voltage depends on electrode geometry and void content. For inverter-fed motor insulation, partial discharge testing under impulsive voltage conditions is required because low-frequency dielectric strength alone does not qualify the film for high dv/dt environments. The lower moisture absorption of PEN relative to PET contributes to more stable capacitance and insulation resistance under high-humidity storage, but FN-1 should be evaluated for corona resistance if used in direct-contact winding applications. Published data for FN-1-specific partial discharge endurance are limited; qualification must be performed on the assembled insulation system rather than on unstressed film alone.
Substitution of FN-1 for biaxially oriented polyethylene terephthalate film in flexible printed circuit coverlay applications becomes technically advantageous when the assembly process exposes the coverlay to repeated thermal excursions above 120 °C. Standard PET grades begin to soften near 78 °C and show progressive shrinkage above 100 °C; heat-stabilised PEN grades typically retain useful dimensional stability up to approximately 150 °C for continuous exposure and can tolerate short excursions near 180 °C. The lower shrinkage is measurable by ISO 11501 or equivalent supplier methods after 30 min at 150 °C; values for heat-set PEN are often below 1.0 % in the machine direction and below 0.5 % in the transverse direction. In multilayer coverlay lamination, this dimensional stability reduces registration error and prevents adhesive squeeze-out at the coverlay edges. However, FN-1 is not a direct substitute for polyimide in continuous service above 200 °C; polyimide films retain better thermal-oxidative stability, but they absorb more moisture and may require higher-temperature lamination or curing conditions than PEN. The choice among PET, PEN and polyimide therefore depends on the upper service temperature, the humidity exposure, the required dielectric performance and the available lamination equipment.
Unlike aromatic polyimide film, Toyobo Neostar® PEN Film FN-1 can be processed on conventional polyester film slitting and hot-stamping lines without the high imidization and solvent-removal steps used in cast polyimide production. This results in lower converting cost and simpler lamination sequences, but it also defines a narrower upper-use thermal window. Chemical compatibility testing under ISO 175 indicates that biaxially oriented PEN films resist dilute mineral acids and many aliphatic hydrocarbons at room temperature, but prolonged contact with strongly alkaline electrolytes, concentrated amines or hot aromatic solvents is not recommended. In applications such as printed electronics and membrane touch switch insulation, traces may be printed with silver-palladium pastes and cured at temperatures that standard PET cannot sustain without distortion. FN-1 can provide the thermal headroom for these cure cycles, provided that solvent-borne conductive inks are tested for adhesion and surface wetting. For printed traces, final adhesion and circuit resistance should be checked by ASTM F1683 or equivalent flexible-circuit electrical continuity test protocols; surface energy and roughness are not sufficient predictors of ink adhesion.
Published product differentiation for Toyobo Neostar® PEN Film FN-1 is limited in open literature; therefore, FN-1 should not be assumed to carry the same surface treatment, shrinkage class or optical haze level as heat-stabilised, adhesion-promoted or ultra-clean PEN grades offered by the same producer or by converters. Differences among polyester film grades are typically expressed through nominal thickness tolerance, tensile strength ratios between machine and transverse directions, shrinkage at defined temperatures, haze, gel count, surface roughness and dyne level. When comparing FN-1 with biaxially oriented PET, the primary measurable differences are the higher glass transition, the lower oxygen and water-vapour transmission rates, and the higher UV-absorbing character of the naphthalate backbone. The UV-absorbing character can reduce photodegradation of underlying layers but also gives the film a light amber tint, which may be undesirable in display or optical applications that require neutral colour. When comparing FN-1 with polyimide, the primary differences are lower continuous-use temperature and lower solvent-processing resistance, balanced by lower moisture absorption and easier roll-to-roll handling. The exact operating limits for FN-1 should be obtained from the supplier, including the maximum recommended roll-storage temperature, pre-drying requirements before vacuum sputtering, and any restriction on amine-based photoresists that may attack polyester surfaces.