Toyobo Neostar Pen Bottles Bn 3

Toyobo Neostar® PEN Bottles BN-3

    • Product Name: Toyobo Neostar® PEN Bottles BN-3
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 262444
    Product Name Toyobo Neostar® PEN Bottle BN-3
    Brand Toyobo
    Series Neostar
    Model BN-3
    Material Polyethylene naphthalate (PEN)
    Bottle Type Narrow-mouth screw-cap bottle
    Capacity 3 L
    Color Transparent
    Closure Type Screw cap
    Heat Resistance High heat resistance
    Gas Barrier High gas barrier
    Chemical Resistance Good chemical resistance
    Extractables Low extractables

    As an accredited Toyobo Neostar® PEN Bottles BN-3 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in a carton containing 50 Toyobo Neostar® PEN Bottles BN-3, securely cushioned for safe transport and storage.
    Container Loading (20′ FCL) Toyobo Neostar® PEN Bottles BN-3 are loaded into a 20′ FCL container in palletized cartons, secured for safe ocean transport.
    Shipping Toyobo Neostar® PEN Bottles BN-3 are non-hazardous laboratory consumables and are not classified as dangerous goods for transport. No UN number, hazard class, or packing group applies. Ship at ambient temperature in secure, dry packaging, protected from impact and contamination.
    Storage Store Toyobo Neostar® PEN Bottles BN-3 in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and incompatible substances. Keep containers tightly closed and properly labeled. Protect from physical damage and moisture. Follow local regulations and the supplier’s safety data sheet for segregation and secondary containment.
    Shelf Life Recommended shelf life: 24 months from manufacture when stored sealed in original packaging at room temperature, avoiding moisture and direct sunlight.
    Free Quote

    Competitive Toyobo Neostar® PEN Bottles BN-3 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toyobo Neostar® PEN Bottles BN-3 is an injection stretch blow molding grade of polyethylene naphthalate homopolymer. The BN-3 grade controls intrinsic viscosity, crystallinity behavior, and melt stability for single-stage and two-stage bottle conversion. Published representative values for BN-3-class PEN bottle resin include an intrinsic viscosity of 0.62 dL/g determined by ISO 1628-1:2009, a density of 1.36 g/cm³ per ISO 1183-1:2019, a glass transition temperature of 121 °C and melting peak 265 °C per ISO 11357-2:2020 and ISO 11357-3:2018. These values are not specification limits; lot-specific certificates of analysis must be used for release testing.

    The polymer backbone uses ethylene glycol and naphthalene-2,6-dicarboxylic acid. The fused naphthalene ring increases chain stiffness, giving BN-3 a glass transition approximately 45–50 °C higher than bottle-grade PET and a melting point approximately 18–20 °C higher. The main processing consequence is that BN-3 cannot be run on a standard PET preform injection machine without a higher-temperature barrel and hot runner capability. Applications for BN-3 include hot-fill containers, returnable bottles that require alkaline washing, barrier-sensitive beverage bottles, and rigid pharmaceutical or cosmetic packages that benefit from ultraviolet screening below 380 nm.

    What Are the Processing Limits That Govern BN-3 Preform and Bottle Production?

    Predrying is the first critical limit. PEN hydrolyzes rapidly when residual moisture in the pellet exceeds 50 ppm at melt temperatures near 300 °C. The hopper dryer must deliver dehumidified process air with a dew point at or below −40 °C. Typical BN-3 drying conditions are 170 °C for 5–6 h. On single-stage ISBM lines with reciprocating screw L/D ratios of 20:1 to 24:1, insufficient drying has been observed as gate crystallinity, screw torque fluctuation, and unstable preform wall distribution because hydrolysis lowers melt viscosity. Batch-to-batch moisture variation is highest when pellets are stored at relative humidity above 60%; opened gaylords should therefore be resealed and dried before use.

    Injection melt temperature is typically controlled at 295–305 °C. Hot runner and nozzle zones may require 300–310 °C depending on throughput and gate size. Melt residence time should be kept below 5–7 min to limit thermal oxidation and yellowing. Preform mold cooling water is usually maintained at 8–12 °C. The narrow processing window is the major difference from PET: overheating above 310 °C accelerates degradation, while underheating produces preform stress-whitening and poor stretch uniformity. BN-3 should not be blended with amine-based oxygen scavengers or polyamide-containing additives without testing; amine end groups can catalyze ester cleavage and generate color bodies.

    Table 1. Representative processing window for BN-3/PEN bottle resins.

    Processing variableRecommended BN-3 / PEN bottle-grade range
    Predrying temperature170 °C
    Predrying time5–6 h
    Drying air dew point≤ −40 °C
    Residual moisture after drying≤ 50 ppm
    Injection melt temperature295–305 °C
    Preform mold cooling water8–12 °C
    Stretch blow mold temperature130–150 °C

    The table is a starting point for machine setup. Barrel temperature profiles must be adjusted to the specific injection unit, and the actual preform surface temperature must be measured with an infrared pyrometer rather than inferred from barrel settings. Mold filling of BN-3 preforms differs from PET because the melt viscosity at 300 °C is higher than that of bottle-grade PET at 280 °C. The injection holding pressure, gate diameter, and hot runner channel size therefore require adjustment. Preforms with wall thickness above 4 mm are more likely to develop gate crystallinity unless the mold cooling circuit maintains the gate insert surface below 15 °C. Multi-cavity tooling with 72 to 96 cavities is common on two-stage ISBM lines; cavity-to-cavity fill balance must be verified because the higher viscosity magnifies short-shot variation.

    In returnable bottle systems where caustic washing is integrated between filling cycles, BN-3 is used for its hydrolytic stability at elevated temperature. The glass transition of 121 °C permits hot-fill exposure up to 95 °C without the sidewall paneling that occurs in unheat-set PET at similar fill temperatures. Alkaline washing with 1.5–2.0% sodium hydroxide at 60 °C is a standard returnable-bottle cleaning condition; PET bottle resin loses intrinsic viscosity and barrier performance more rapidly under repeated wash cycles, whereas PEN homopolymer retains molecular weight longer because the naphthalene-containing backbone is more resistant to hydrolysis. However, the number of return trips must be validated by line trials including drop impact testing per ASTM D2463-15 and oxygen transmission testing per ASTM D3985-17. Published data for BN-3 under specific caustic wash cycle counts is limited; laboratory barrier panels cannot be used as absolute cycle-life guarantees.

    Barrier Data and Ultraviolet Screening Performance

    The naphthalene ring in BN-3 lowers gas solubility and diffusivity relative to PET. Comparative data for PEN bottle resins show an oxygen transmission coefficient reduction factor of 4–5 relative to PET at 23 °C and 50% relative humidity under ASTM D3985-17. Carbon dioxide retention, relevant to carbonated soft drink bottles, is improved by a factor of 5–7 relative to PET; water vapor transmission is reduced by a factor of 3–4. The reduction factors are dimensionless rankings and do not replace package-level transmission testing. UV screening is another differentiator: PEN absorbs ultraviolet light below approximately 380 nm, whereas conventional PET absorbs below approximately 310 nm. This cutoff reduces light-initiated off-flavor formation in beverages and can extend shelf life where photooxidation is a limiting mechanism.

    Table 2. Relative barrier and ultraviolet screening comparison for PEN bottle resin and PET.

    PropertyTest methodBN-3 class PEN versus PET bottle resin
    Oxygen transmission coefficientASTM D3985-17reduction factor 4–5
    Carbon dioxide transmission coefficientASTM F2476-20reduction factor 5–7
    Water vapor transmission coefficientISO 15106-2:2019reduction factor 3–4
    Ultraviolet cut-offUV-Vis spectrophotometry380 nm versus 310 nm

    The relative factors in the table are based on PEN bottle-grade film data and should not be treated as BN-3 specification values. Absolute oxygen ingress into a finished bottle is governed by wall thickness distribution, closure permeation, and storage temperature. Package-level testing on the actual container is required for shelf-life claims, and oxygen ingress through the closure may exceed wall transmission in small bottles, so the closure liner and neck finish seal must be included in shelf-life modeling.

    When BN-3 Is Compared Directly with PET, PBT, and Other Polyester Bottle Resins

    Compared with PET bottle resins, BN-3 requires higher melt temperature, higher preform reheat setting, and higher mold temperature, but it provides the thermal and barrier improvements described above. PET heat-set grades can be processed at lower cost and are sufficient for fill temperatures below 85 °C; BN-3 becomes technically relevant when the bottle must survive hot-fill above 90 °C or repeated alkaline washing. Compared with PBT, BN-3 has a much higher glass transition and lower gas permeability; PBT crystallizes rapidly and is not normally used for monolayer barrier bottles. Compared with polyolefin-based stretch blow molded containers, BN-3 offers higher rigidity and clarity but lower impact resistance at subzero temperatures. The polyester backbone also creates a recycling incompatibility: PEN must be separated from PET reclaim because melt blending of PEN and PET forms transesterified copolyesters with altered crystallinity and haze. Even small PEN residuals in PET reclaim can reduce clarity and melt stability, so sorting and label systems must prevent cross-contamination.

    BN-3 also differs from general-purpose Toyobo Neostar® PEN film grades. Bottle grade BN-3 is controlled for intrinsic viscosity and melt flow stability during preform injection, whereas film grades are formulated for extrusion and biaxial orientation in sheet or film. The difference is not merely viscosity: bottle-grade additive and copolymer controls are selected for blow molding stretch ratios and preform surface finish. No assumption should be made that a film-grade PEN resin is interchangeable with BN-3 on a bottle line. Compared with glass, BN-3 reduces container mass and breakage, but glass remains superior for oxygen-sensitive products requiring near-zero oxygen transmission. The decision to use BN-3 in a barrier bottle must therefore be based on the product’s tolerable oxygen ingress limit, not on a general assumption that high-barrier polyester equals glass.

    Food Contact Compliance and Industrial Specification Boundaries

    Food contact suitability of BN-3 must be confirmed through the manufacturer’s food contact statement and the relevant market regulation. In the European Union, the framework is Regulation (EU) No 10/2011; specific migration of naphthalene-2,6-dicarboxylic acid and ethylene glycol must be assessed for the finished container under the intended fill temperature and contact time. In the United States, converters should obtain the manufacturer’s Food Contact Notification or applicable premarket authorization, because generic 21 CFR sections for PET should not be assumed to cover PEN. REACH registration and RoHS Directive 2011/65/EU documentation should be requested from the supplier for non-food or industrial packaging where applicable.

    For all processes, moisture control is the operational boundary. If the resin is stored at RH above 60%, predrying must be repeated after storage. BN-3 is not recommended for continuous exposure to strong alkali at concentrations above 2% sodium hydroxide at temperatures above 80 °C because polyester hydrolysis accelerates. Gamma sterilization at doses above 25 kGy may shift color and reduce intrinsic viscosity; published data for BN-3 in gamma-sterilized formats above this dose is limited, so converters must validate color, molecular weight retention, and migration resistance for pharmaceutical or diagnostic packaging.