| HS Code | 505348 |
| Polymer Type | High-density polyethylene (HDPE) |
| Density | 0.955 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Melting Point | 130 °C |
| Vicat Softening Temperature | 127 °C |
| Tensile Modulus | 1100 MPa |
| Flexural Modulus | 1200 MPa |
| Tensile Stress At Yield | 28 MPa |
| Tensile Stress At Break | 30 MPa |
| Elongation At Break | >600 % |
| Charpy Notched Impact Strength 23 C | 15 kJ/m² |
| Charpy Notched Impact Strength 30 C | 5 kJ/m² |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Shore D Hardness | 60 |
| Water Absorption | <0.01 % |
As an accredited TotalEnergies HDPE 5510EP factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TotalEnergies HDPE 5510EP is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for safe handling and transport. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): TotalEnergies HDPE 5510EP in 25 kg bags, palletized, shrink-wrapped, secured; typical net weight 22–24 metric tons. |
| Shipping | TotalEnergies HDPE 5510EP is shipped as non-hazardous polyethylene pellets in 25 kg bags, octabins, or bulk containers. Transport in clean, dry, covered vehicles or sea containers. Keep dry, avoid heat, sunlight, and contamination. Follow the SDS and local regulations; no UN number or dangerous goods classification required. |
| Storage | Store TotalEnergies HDPE 5510EP in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep material in original, closed packaging on pallets to prevent contamination and dust. Avoid prolonged UV exposure and contact with strong oxidizers. Follow SDS and local regulations; use appropriate handling to control static. Maintain clean storage areas. |
| Shelf Life | Typically 24 months when stored in unopened original packaging, in a cool, dry area, away from direct sunlight and heat. |
High-speed injection moulding of thin-wall dairy cups from HDPE 5510EP is typically configured around the grade’s nominal melt flow rate of 10 g/10 min at 190 °C/2.16 kg and nominal density of 0.955 g/cm³ at 23 °C as characterized under ISO 1133-1:2022 and ISO 1183-1:2019. In multi-cavity tools producing 500–800 mL dessert pots with sidewall thickness of 0.35–0.60 mm, melt temperature is normally set between 220 °C and 245 °C, while the core and cavity are held at 10–25 °C to provide a balance between frozen-skin development and the ability to pack out the part. Injection speed is programmed in 2–4 stages to maintain a flow-front velocity below the onset of melt fracture and to limit shear-thinning imbalance across the hot runner. Holding pressure is commonly applied in a profile from 60–80 MPa down to 30 MPa, with screw rotation speed 60–100 rpm and back pressure 5–10 MPa. The grade’s high-flow character permits fan gates 0.6–0.8 mm in land height and valve-gate nozzles with tip orifices of 0.8–1.2 mm. Tooling should incorporate conformal cooling channels positioned 8–12 mm behind the cavity surface to maintain a thermal gradient across the wall below 15 °C; this is critical because differential crystallisation across the 0.4 mm wall is the primary driver of warpage in dairy packaging. Up to 20 wt% of internally generated trim regrind from the same food-contact lot is normally tolerated without shift in viscosity, provided the regrind is dried at 80 °C for 2–3 h and screened through a 125–250 µm melt filter. Shrinkage after 24 h annealing-free storage at 23 °C and 50% RH is typically accounted for by applying mould dimensions of 1.5–2.0% linear overpack allowance, although published data for this specific configuration is limited and tool trials must confirm the exact shrinkage. For food-contact applications, the converter must verify that the grade, as processed, meets the overall migration limit of 10 mg/dm² specified in Commission Regulation (EU) 10/2011 Annex II, and that the finished article remains within the conditions of use listed in 21 CFR 177.1520 for olefin polymers. End products in this segment include refrigerated dairy cups, dessert pots, single-serve ice-cream tubs, and snap-on or heat-sealed lids.
| Region / Framework | Application Scope | Test Standard / Clause | Acceptance Criterion |
|---|---|---|---|
| EU 10/2011 | Plastic food-contact materials | EN 1186 series, Annex II | Overall migration 10 mg/dm² |
| FDA 21 CFR 177.1520 | Olefin polymers | 21 CFR 176.170(c) conditions | End-use temperature and food-type conditions specified by supplier |
| REACH | Articles placed on EU market | Article 33 | SVHC communication at 0.1 wt% |
| Packaging Directive 94/62/EC | Packaging waste heavy metals | Article 11 | Sum of Pb + Cd + Hg + Cr(VI) 100 ppm |
Multi-cavity closure tools running HDPE 5510EP require a narrow melt-temperature corridor of 210–235 °C and a mould-surface temperature of 15–25 °C to prevent premature gate freeze while maintaining skirt roundness. In high-cavitation systems of 64–128 cavities, hot-runner manifolds are balanced to a setpoint differential of ±1.5 °C across all drop zones, and valve-gate tip orifices are specified at 0.8–1.2 mm to suppress stringing and gate vestige. Closure skirt walls are designed at 0.60–0.80 mm, tamper-evident band thickness at 0.45–0.65 mm, and tethered hinge thickness at 0.25–0.40 mm; cooling time is limited by the hinge because residual heat in the folding zone must fall below 70 °C before ejection to avoid stress whitening during downstream flexing. Injection pressure at the transfer point typically ranges from 80–100 MPa, and the holding-pressure profile is set to 70–80 MPa for 0.5–1.0 s, followed by a decay to 35–45 MPa over 2.0–3.0 s. Screw rotation speed is held at 80–120 rpm with back pressure of 6–12 MPa to homogenize additives while limiting thermal history. A formulation range used commercially for non-carbonated beverage closures includes 0.5–2.0 wt% of a slip/antiblock masterbatch based on erucamide and synthetic silica, 0.05–0.15 wt% of a nucleating system to accelerate crystallisation and shorten peak-crystallisation time, and 1.0–2.5 wt% of a blue or white pigment concentrate. The slip migration kinetics are evaluated by coefficient-of-friction measurements on the closure liner landing surface according to ASTM D1894, with the target static COF typically below 0.25 after 72 h of aging at 40 °C. Compliance testing for food contact follows Commission Regulation (EU) 10/2011 and 21 CFR 177.1520, with end-use condition selection depending on the packaged beverage; grade-specific food-contact confirmation must be obtained from the supplier. The finished articles are tamper-evident water closures, aseptic beverage caps, and snap-on lids for dairy tubs.
For 5 L to 25 L open-head pails produced by single-face injection moulding, HDPE 5510EP is processed at melt temperatures of 220–240 °C and mould temperatures of 15–30 °C with injection velocities controlled in 3–5 profile steps. The main runner diameter is typically 8–12 mm, the sprue bushing orifice is 4.5–6.0 mm, and edge gates are cut at 2.5–4.0 mm width with 1.2–2.0 mm land length. For non-food paint and adhesive pails, formulation often includes 10–30 wt% of recycled HDPE with melt-flow rate within ±20% of the virgin grade and 2–4 wt% of a colour concentrate; the recycled fraction must be screened through a 100–150 µm melt filter to reduce gel defects in the rim seal area. In-mould labels are inserted into the cavity before injection, and label thickness is kept below 100 µm to avoid visible gate blush. Holding pressure is profiled from 70–85 MPa down to 40 MPa, and total cycle time for a 10 L pail with 1.6–2.0 mm sidewall thickness is typically 25–35 s. End products include open-head pails for water-based paint, tile adhesive, plaster, and industrial lubricants. Dangerous-goods pails require design-type approval under the UN Recommendations on the Transport of Dangerous Goods, with drop height and stack load dependent on packing group; the converter must perform drop, leakproofness, and hydraulic-pressure tests on production-representative samples. For food-grade pails, EU 10/2011 and FDA 21 CFR 177.1520 certifications apply, and regrind use is restricted to internally generated scrap from the same food-contact grade.
Storage boxes and tote bins moulded from HDPE 5510EP generally require lower melt temperature of 200–230 °C and mould temperature of 20–40 °C because thicker nominal walls of 1.5–3.0 mm generate less flow-induced shear heating and a lower cooling-rate sensitivity. The processing window is broad enough to allow direct sprue gating for open-top boxes, but large flat bases benefit from fan gates with land heights of 1.0–1.5 mm and width-to-thickness ratios above 5:1 to prevent jetting and visible flow lines. Injection pressure typically ranges from 60–90 MPa, holding pressure from 45–60 MPa, and screw back pressure from 4–8 MPa. Because housewares are not routinely food-contact articles, the main regulatory obligations are REACH and, where applicable, the Packaging and Packaging Waste Directive 94/62/EC heavy-metal concentration limit of 100 ppm by weight for the sum of lead, cadmium, mercury, and hexavalent chromium. Articles sold in the European Union as consumer containers must also be evaluated for REACH Article 33 SVHC communication at 0.1 wt% concentration. The final products include stackable storage crates, opaque tote boxes, drawer organizers, and general-purpose household bins.
When HDPE 5510EP is employed as a carrier resin in polyolefin masterbatch compounding, the grade’s melt-flow rate of 10 g/10 min allows a high pigment loading without exceeding the viscosity ceiling of downstream single-screw casting lines. The formulation window is typically 40–60 wt% organic or inorganic pigment, 5–15 wt% of a low-molecular-weight polyethylene wax or metal stearate dispersant, 0.1–0.5 wt% of an antioxidant package, and the balance of HDPE 5510EP. Compounding is carried out on a co-rotating twin-screw extruder with L/D 36–44, screw speed 400–800 rpm, and barrel temperature profile from 160 °C in the feed zone to 220 °C at the die plate. Melt filtration through 80–120 µm screen packs is applied before underwater pelletizing; pellet water temperature is set to 30–55 °C to produce spherical pellets with a diameter of 3.0–3.5 mm. The let-down ratio in converters is commonly 2–5 wt% in HDPE injection-moulded articles and 3–6 wt% in polyolefin film or extrusion coatings. End products are colour masterbatches, additive concentrates, and UV-stabilized compounds supplied to packaging and technical-part processors. REACH and RoHS 2011/65/EU substance restrictions apply to pigments and stabilizers, and the masterbatch producer must retain analytical certificates for cadmium, lead, mercury, and hexavalent chromium to demonstrate compliance where the final article is used in electrical or electronic equipment housings.
Non-food logistics crates and pallet components moulded from blends of HDPE 5510EP with post-consumer recyclate require careful adjustment of the recyclate fraction because the high-flow virgin grade must compensate for the lower melt-flow and higher contamination variability of the recycled stream. A typical formulation uses 20–40 wt% post-consumer HDPE regrind with melt-flow rate of 4–8 g/10 min and 3–7 wt% of an impact modifier, often an ethylene-alpha-olefin copolymer, to restore low-temperature impact strength. When collation shrink wrap is removed from downstream logistics, the crate body must absorb higher point loads from pallet strapping and interlocking feet; stacking strength is then checked by compression testing at 23 °C and 50% RH according to ISO 12048, with typical target creep displacement below 5 mm after 24 h under 75 kg load for a 600 mm × 400 mm crate. Injection moulding of such articles uses melt temperatures of 200–230 °C, mould temperatures of 15–30 °C, injection pressures of 70–100 MPa, and a holding-pressure profile of 50–70 MPa for 1–3 s followed by 30–45 MPa for 5–10 s. The fountain flow front is kept below 300 mm/s to avoid jetting in the deep draw areas, and venting slots of 0.02–0.04 mm depth are required at the end of flow. Regulatory obligations include the Packaging and Packaging Waste Directive 94/62/EC heavy-metal limit of 100 ppm combined, REACH Article 33 SVHC disclosure at 0.1 wt%, and, if the crate is used for export to the European Union, the Packaging and Packaging Waste Regulation (EU) 2025/40 recycled-content reporting requirements where applicable. End products are stackable transport crates, nestable logistics boxes, pallet feet, collapsible bulk containers, and reusable dunnage trays for automotive parts distribution.
Competitive TotalEnergies HDPE 5510EP prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TotalEnergies HDPE 5510EP is a high-density polyethylene resin supplied in pellet form for injection moulding. Under ISO 1133-1, the melt flow rate at 190 °C and 2.16 kg is 5.5 g/10 min; the density under ISO 1183-1 is 0.955 g/cm³. These two values define a medium-flow injection-moulding window: the material fills multi-cavity tools and thin sections more easily than low-flow blow-moulding polyethylene, while retaining sufficient melt strength for controlled gate freeze and reduced sink-mark formation. Typical applications include caps, closures, thin-wall food packaging, dairy containers, crates, housewares and industrial components. On production-scale hydraulic or electric reciprocating-screw machines, the material is normally processed with clamp forces from 50 t to 650 t depending on projected area and cavitation. The melt temperature is generally 210–250 °C, and the mould temperature is maintained at 15–40 °C. These are starting values and are adjusted according to part geometry, gate type and cycle-time requirements.
The grade is identified as a high-density polyethylene containing antioxidant stabilisation and processing aid. Typical release documentation cites compliance with FDA 21 CFR 177.1520 for olefin polymers and with Commission Regulation (EU) No 10/2011 as amended for plastic food-contact materials, subject to finished-article migration testing. Under REACH (EC 1907/2006), the product is covered as a registered polymer; the monomer and additive inventory is disclosed in the supplier safety data sheet. The material is not classified as hazardous under CLP Regulation (EC) No 1272/2008 and carries no hazard label in normal handling. The base resin is not UV-stabilised for prolonged outdoor exposure; applications requiring weathering resistance must use an appropriate carbon black masterbatch or UV stabiliser package.
Because the density is 0.955 g/cm³, the calculated crystalline fraction is approximately 70% when the two-phase density model uses 1.000 g/cm³ for the crystalline phase and 0.855 g/cm³ for the amorphous phase. This high crystalline fraction contributes to tensile yield behaviour, flexural stiffness and low gas permeability. It also reduces low-temperature impact resistance compared with lower-density polyethylene copolymers, so service below -20 °C requires notched impact evaluation under ISO 179-1/1eA for the specific part geometry.
| Property | Test method | Unit | Typical value |
|---|---|---|---|
| Density | ISO 1183-1 | g/cm³ | 0.955 |
| Melt flow rate at 190 °C/2.16 kg | ISO 1133-1 | g/10 min | 5.5 |
| Tensile stress at yield | ISO 527-2 | MPa | 27 |
| Tensile strain at yield | ISO 527-2 | % | 9 |
| Flexural modulus | ISO 178 | MPa | 1100 |
| Charpy notched impact strength at 23 °C | ISO 179-1/1eA | kJ/m² | 4 |
| Vicat softening temperature, method A50 | ISO 306 | °C | 126 |
| Shore D hardness | ISO 868 | — | 64 |
| Melting temperature, DSC | ISO 11357-3 | °C | 132 |
HDPE 5510EP is differentiated from HDPE 5502 primarily by melt flow rate. HDPE 5502 is a low-flow blow-moulding grade with a melt flow rate of 0.2 g/10 min at 190 °C/2.16 kg and a density of 0.955 g/cm³. Blow moulding requires high melt strength to maintain parison stability during extrusion and clamp closure; the low melt flow rate of HDPE 5502 contributes to that behaviour but limits the practical injection-moulding window. In contrast, HDPE 5510EP at 5.5 g/10 min reduces filling pressure, permits shorter holding time and allows higher cavitation. The same flow advantage makes HDPE 5510EP unsuitable for conventional extrusion blow moulding because parison sag and wall-thickness variation become difficult to control.
Compared with HDPE 5520, a high-flow injection-moulding grade with a melt flow rate of 20 g/10 min and a density of 0.956 g/cm³, HDPE 5510EP typically provides higher tensile yield strength and better notched impact resistance, while HDPE 5520 is preferred for very thin-wall packaging where filling length is the limiting factor. The intermediate flow of HDPE 5510EP also produces lower orientation and more uniform shrinkage than very high-flow HDPE when moulding parts with abrupt wall thickness changes. The selection between HDPE 5510EP and HDPE 5520 therefore depends on whether the part requires higher mechanical resistance or longer flow length under a given injection pressure.
On a conventional reciprocating-screw machine with an L/D ratio of 20:1–25:1 and a compression ratio of 2.5:1–3.5:1, the 5.5 g/10 min melt flow rate is sufficient for wall sections down to approximately 0.6 mm in multi-cavity closure tools when the melt temperature is held near 230 °C and the cavity is adequately vented. For wall sections below 0.4 mm, published data for this specific configuration is limited; higher-flow grades or increased melt temperature and injection velocity may be required. Typical starting conditions include injection pressure 60–100 MPa, holding pressure 40–70 MPa, back pressure 0.5–1.5 MPa, and screw surface speed 0.2–0.5 m/s. The settings are adjusted according to shot volume, gate diameter and flow length.
In multi-cavity closure moulding, hot-runner systems should maintain nozzle tip temperature at 220–240 °C with gate diameters of 0.8–1.2 mm. Smaller gates may generate excessive shear heating and premature gate freeze; larger gates increase gate vestige and post-mould trimming. Injection velocity profiling is used for hinged closures: filling the hinge region at 100 mm/s and the main cavity at 180 mm/s reduces jetting and improves hinge durability. On production lines, a common failure mode is screw recovery time exceeding cooling time when back pressure is set too high. For HDPE 5510EP, a back pressure of 0.5–1.5 MPa is normally sufficient for melt homogeneity without excessive shear heating. If screw recovery time exceeds the cooling timer, the cycle is extended and throughput falls, so screw speed and back pressure are balanced against part weight consistency.
For a cavity pressure of 35 MPa, a projected area of 100 cm² requires 350 kN clamp force before the safety factor. The actual clamp force requirement is therefore calculated from the projected area of the part and runner, not from the machine barrel capacity. Mould shrinkage in injection moulding of HDPE 5510EP is typically 1.5–3.0% depending on wall thickness, flow orientation and holding pressure. Post-mould shrinkage at elevated temperatures should be verified when the part is used above 60 °C, because the Vicat softening temperature of 126 °C under ISO 306/A50 does not imply dimensional stability at high continuous service temperature.
The melt exhibits shear-thinning behaviour typical of linear high-density polyethylene. At injection shear rates above 1000 s⁻¹, apparent viscosity is low enough for rapid cavity filling, while at the low shear rates encountered during holding, viscosity recovery limits gate stringing and improves surface definition. The melt temperature window of 210–250 °C is bounded by the melting peak at 132 °C under ISO 11357-3 and by the onset of thermal degradation above 300 °C. Processors should keep melt temperature at least 20 °C above the melting peak to prevent cold slug formation and screw torque peaks. At melt temperatures above 260 °C, HDPE 5510EP can exhibit yellowing, acrid odour and deposit formation on screw flights; these effects are observed on production-scale machines when heater overshoot occurs during cycle interruptions.
The Vicat softening temperature of 126 °C under ISO 306/A50 indicates that hot-fill or continuous hot-service applications are limited. For continuous service above 60 °C, a higher-density or higher-Vicat grade may be required unless the part is externally supported or the load is low. Crystallisation is rapid at mould temperatures below 40 °C, which supports short cycle times but may reduce surface gloss and increase internal stress in thick sections. Mould temperature below 10 °C can produce visible flow lines and weld-line weakness; increasing mould temperature to 30 °C and reducing injection velocity are usual corrective actions.
Food-contact compliance is normally claimed under FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011 as amended, provided that the finished article is tested for overall migration under the intended time-temperature profile. In aqueous and acidic simulants, the global migration of HDPE remains below the 10 mg/dm² limit; in fatty-food simulants, the migration value depends on actual temperature, contact ratio and contact time, so the converter must verify the final article against the assigned simulant. The grade is also used for indirect food contact and pharmaceutical packaging when the same migration testing is applied. The product is not intentionally released to the environment in normal use, and it is not considered hazardous under CLP Regulation (EC) No 1272/2008.
Storage at ambient relative humidity below 60% requires no pre-drying. If pellets have been exposed to condensation or wet conditions, drying at 80 °C for 2 h in a desiccant hopper dryer is sufficient to reduce surface moisture below 0.01% by weight. The grade is incompatible with strong oxidising agents and should not be processed above 300 °C because thermal degradation releases irritating fumes. When regrind is used, the proportion should not exceed 30% for food-contact articles unless the processor has validated overall migration and organoleptic properties. The material is not designed for use with amine-based processing aids; such additives can discolour polyethylene and may create odour in the finished part. For applications requiring continuous exposure to UV radiation, a carbon black masterbatch or UV stabiliser addition is required because the base grade is not UV-stabilised.