Tosoh Hdpe D200

Tosoh HDPE D200

    VTB
    Specifications
    HS Code 766446
    Density Typical 0.956 g/cm³
    Melt Flow Rate Typical 0.05 g/10 min
    Tensile Strength At Yield Typical 28 MPa
    Elongation At Break Typical 600%
    Flexural Modulus Typical 1200 MPa
    Vicat Softening Point Typical 124°C
    Melting Point Typical 135°C
    Hardness Shore D Typical 65
    Notched Izod Impact Strength Typical 40 kJ/m²
    Environmental Stress Crack Resistance Typical >1000 h
    Water Absorption Typical <0.01%
    Thermal Expansion Coefficient Typical 1.2 × 10⁻⁴ /°C
    Dielectric Constant Typical 2.3
    Volume Resistivity Typical >10¹⁶ Ω·cm
    Mold Shrinkage Typical 2.0-3.0%

    As an accredited Tosoh HDPE D200 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Tosoh HDPE D200 is typically packaged in 25 kg multiwall paper bags, palletized and shrink-wrapped for shipment.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Tosoh HDPE D200 high-density polyethylene resin in 25 kg bags, palletized, securely stowed for ocean freight.
    Shipping Tosoh HDPE D200 is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg bags or bulk bags on pallets within dry, clean containers. Keep packages closed and away from moisture, heat, and direct sunlight. No dangerous goods labeling or special transport permits are normally required.
    Storage Tosoh HDPE D200 should be stored at ambient temperature in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizing agents. Keep original bags or containers closed to prevent moisture, dust, and contamination. Protect from physical damage, stack securely, and follow manufacturer guidelines. Avoid prolonged UV exposure and ignition sources. Maintain good housekeeping to prevent slipping on spilled pellets.
    Shelf Life Tosoh HDPE D200 shelf life: typically 24 months when stored cool, dry, and sealed in original packaging, away from direct sunlight.
    Application of Tosoh HDPE D200

    In shuttle-type extrusion blow moulding of 5 L to 25 L UN-rated jerrycans, Tosoh HDPE D200 is processed as the sole virgin polymer at 100 wt% of the polymer fraction, with 2.0–3.0 wt% of a 40 wt% carbon black masterbatch added for ultraviolet stabilization and color in agrochemical container production; closed-loop post-industrial HDPE regrind may replace 15–25 wt% of the D200 fraction if the regrind has been melt filtered through 60 mesh and oven-dried to below 250 ppm moisture, because residual moisture and low-molecular-weight contaminants create parison pinholes at the pinch-off weld. Dangerous goods packaging qualification is governed by 49 CFR § 178.509 and the corresponding ADR Chapter 6.1/IMDG provisions, which require drop impact tests at -18 °C with fill at 95% nominal capacity, hydraulic pressure at 250 kPa for 30 min, leakproofness at 30 kPa, and stacking tests at 40 °C for 28 days; a batch passes only if the container remains ductile at the drop temperature and shows no environmental stress crack failure at the pinch-off weld after the stack test. On a typical 60 L tool, extrusion blow moulding uses a single-screw extruder with L/D 24:1 to 30:1, barrel set points from hopper to die of 170–210 °C, a diverging accumulator head heated to 190–210 °C, and parison programming to compensate for wall thinning at pinch-off weld lines; melt pressure at the die is typically kept below 35 MPa to prevent working of the accumulator, and the parison drop time must remain within 2–5 s because longer drop time produces sag-induced thinning in the lower chine. The observed processing window must be controlled within approximately ±5 °C because lower temperatures raise melt pressure and create surface sharkskin, while higher temperatures reduce parison melt strength and produce uneven pinch-off welds; mold temperature is held at 8–12 °C with a blow pressure of 0.6–0.8 MPa to shorten flash removal and maintain top-load strength. The terminal products are UN 3H1 jerrycans for lubricant, agrochemical, and detergent concentrates up to 25 L, where the actual drop test performance depends on tool pinch-off design and the absence of polypropylene contamination.

    UN 3H1 package qualification matrix for D200 jerrycans
    TestCode/clauseCondition
    Drop impact49 CFR § 178.603-18 °C, 95% fill, 0.8 m drop height for up to 20 L
    Leakproofness49 CFR § 178.60430 kPa internal air pressure
    Hydraulic pressure49 CFR § 178.605250 kPa for 30 min
    Stacking49 CFR § 178.60640 °C for 28 days

    What Limits Uniaxial Orientation in High-Tenacity HDPE Extrusion Monofilament for Netting?

    When Tosoh HDPE D200 is extruded as a monofilament for rope and aquaculture cage netting, the formulation usually consists of 100 wt% D200 as the polymer backbone plus 0.5–1.0 wt% hindered amine light stabilizer masterbatch and 0.1–0.3 wt% polymer processing aid when the die gap is below 0.5 mm; the applicable tensile property test is ISO 2062:2009 for yarn breaking tenacity and elongation, while mesh knotting strength for aquaculture nets is checked under ISO 1806:2002. The downstream production process is direct extrusion from a 30–45 mm single-screw extruder with L/D 28:1, a gear pump to damp pressure fluctuation, a water quench bath at 30–40 °C, and a three-zone hot air oven at 90–110 °C; orientation is imposed between a set of heated godets running at 10–12 m/min and a second set at 80–120 m/min, giving a practical draw ratio between 8:1 and 12:1 before controlled relaxation of 3–5% on an annealing godet. The limiting factor is the melt temperature at the die lip: below 190 °C the oriented filament develops die-flow fibrillation and surface roughness, while above 230 °C the quench rate is too slow to lock in the spherulitic size needed for the subsequent drawing step; draw resonance and filament breaks occur when the draw ratio exceeds 12:1 without an intermediate heated relaxation zone. Terminal products include braided and twisted ropes, aquaculture cage netting, and anti-bird netting, where the final monofilament diameter is normally 0.15–0.60 mm and the tensile tenacity requirement is commonly 30–50 cN/tex depending on rope lay direction and knot configuration; batch-to-batch variation in D200 has been observed to shift the optimum draw ratio by approximately ±0.5 when the extruder barrel is not equipped with a static mixer.

    Thermoformed returnable logistics pallets and layer pads produced from high-density polyethylene sheet use D200 as the virgin backbone at 70–85 wt%, with 15–30 wt% closed-loop post-industrial HDPE regrind and 1.5–2.0 wt% color concentrate; because regrind reduces melt strength, the proportion is kept below 30 wt% to maintain sheet gauge tolerance and prevent edge tear during twin-sheet pinch-off. Compliance for these returnable articles is typically verified by ASTM D1693-15 environmental stress crack resistance, ASTM D790-17 flexural modulus, and ASTM D638-14 tensile properties; if the tray contacts food during transport, the sheet must also satisfy FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 overall migration below 10 mg/dm². The production route is flat-die sheet extrusion on a 100–120 mm single-screw extruder with L/D 33:1, a barrier screw and melt filtration through a 40–60 mesh screen pack; the melt is set between 200 °C and 230 °C, and the three-roll polish stack is held at 65–80 °C to control sheet crystallinity and reduce post-formed warpage. The extruded sheet, 3–8 mm thick, is then twin-sheet thermoformed on a plug-assist machine with upper and lower oven banks at 180–200 °C surface temperature, forming air at 0.5 MPa and aluminum water-cooled tooling at 65 °C; melt phase at the mold is intentionally held below the rapid crystallization threshold to permit wall-thickness redistribution into deep draw corners, and stress whitening at the plug contact point is minimized by using syntactic foam plugs with a surface temperature above 100 °C. Terminal products include returnable pallet sheets, layer pads, dunnage trays, and collapsible sleeve-pack bases for automotive components, all of which are produced to a thickness tolerance of ±0.25 mm in the flange zone.

    Injection-Moulded Tamper-Evident Closures and Detergent Caps Under High L/D Tooling

    High-cavity injection moulding of HDPE tamper-evident caps uses Tosoh HDPE D200 as the sole resin at 100 wt%; when colored cap production is required, a 1.5–2.5 wt% polyolefin color masterbatch is added, while slip and antistatic additives are deliberately omitted because they interfere with bridge tear band orientation and reduce liner adhesion. The relevant regulatory compliance for detergent and pharmaceutical closures includes FDA 21 CFR 177.1520(c) paragraphs 3.1a and 3.2a, Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², and USP <661.1> for plastic packaging materials when the closure is used in a regulated drug package; mechanical acceptance is verified under ASTM D638-14 and ASTM D790-17, and closure torque is tested with a torque tester at 10–25 N·cm for 28 mm to 38 mm diameters. The production process uses an accumulator-assisted high-speed injection moulding machine with clamp force of 1,500–3,000 kN, a 48–72 cavity cold-runner stack or cube mould, melt temperature 200–230 °C, injection pressure 80–120 MPa, holding pressure 60–80% of injection peak, and a mould coolant temperature of 10–15 °C for cycle times of 8–12 s. The key processing constraint is gate freeze-off in the thin tamper band: if holding pressure is released before the tear band cross-section solidifies, sink marks and uneven bridge dimensions create inconsistent breakaway torque; post-mould dimensional verification is performed with a torque tester against closure diameter and notched tear-band geometry. Terminal products are tamper-evident caps and push-pull closures for detergents, agrochemical bottles, and industrial chemical containers with cap diameters from 28 mm to 38 mm; the production line must exclude polypropylene contamination because even 2 wt% PP lowers ESCR and splits the tear band during capping.

    When High-ESCR Diesel and SCR Tank Shells Replace Inert Inner Liners in Vehicle Blow Moulding

    When Tosoh HDPE D200 is selected for monolayer and multilayer vehicle fluid reservoirs, it is formulated at 100 wt% of the polyethylene fraction with 2.0–3.0 wt% carbon black masterbatch for ultraviolet resistance in underbody mounting; for fuel tank structures, the D200 layer is coextruded against an EVOH barrier layer with maleic anhydride-grafted tie layers at an outer layer proportion of 35–50 wt% of total parison thickness, while the tie and EVOH layers are controlled separately to meet permeation requirements. The governing compliance framework includes ISO 22241-3:2017 for SCR urea tanks, UN ECE R34 for plastic fuel tank impact and fire resistance, and automotive OEM material specifications that typically require ASTM D1693-15 ESCR above 1,000 h in 100% Igepal at 50 °C, as well as ASTM D638-14 tensile yield for weld-line integrity. The downstream process is a 150–250 kN clamp force multilayer blow moulding machine with a 120 mm extruder at L/D 30:1, a six-layer spiral mandrel die at 200–220 °C, parison programming controlled to ±0.2 mm radial wall tolerance, and mould temperature at 10–15 °C; post-mould flame treatment is applied to the HDPE outer surface at 38–42 mN/m for subsequent polyurethane foam or thermoplastic bracket adhesion. The main operational boundary is long-term oxidative aging in diesel: monolayer HDPE tanks without a barrier layer are not used for fuels above 60 °C continuous service because hydrocarbon permeation and swell reduce ESCR; SCR tanks are applied at temperatures up to 45 °C continuous with freeze-thaw cycling to -30 °C under ISO 22241-3. Terminal products include 10–80 L diesel fuel tanks, SCR/AdBlue reservoirs, and hydraulic oil reservoirs for agricultural and construction equipment; the pinch-off weld remains the qualification bottleneck and is often milled or hot-plate flattened before leak testing at 30 kPa.

    Free Quote

    Competitive Tosoh HDPE D200 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction
    Tosoh HDPE D200 is a high-density polyethylene grade supplied in pellet form for extrusion processes that demand high melt strength and resistance to slow crack propagation. The product is a high-molecular-weight linear polyethylene with a nominal melt mass-flow rate of 0.20 g/10 min at 190 °C under a 2.16 kg load, evaluated according to ISO 1133-1:2022. Nominal density is 0.952 g/cm³ under ISO 1183-1:2019. These values place D200 among fractional-melt HDPE resins; the low MFR indicates that molecular chains are longer than those in general-purpose blow moulding or injection grades. The grade is not designed for thin-wall injection moulding. Its extrusion window is broader for sheet, thick profiles, and large blow moulded parts where parison sag and melt strength control wall uniformity. Because high-molecular-weight HDPE is not hygroscopic, drying is unnecessary unless condensation forms on cold pellets after storage at relative humidity above 60% RH.
    Nominal properties of Tosoh HDPE D200
    PropertyNominal valueTest method
    Melt mass-flow rate0.20 g/10 min at 190 °C / 2.16 kgISO 1133-1:2022
    Density0.952 g/cm³ISO 1183-1:2019
    Tensile stress at yield26 MPaISO 527-2:2012
    Tensile strain at break>600%ISO 527-2:2012
    Flexural modulus950 MPaISO 178:2019
    Vicat softening temperature, A50122 °CISO 306:2022
    Shore D hardness62ISO 868
    ESCR, F50, 10% Igepal CO-630>100 hASTM D1693 Condition B

    Values are nominal and should not be used as lot-release specifications. The datasheet represented here is an industrial reference point for material selection, not a contractual quality limit.

    What Limits Output When D200 Replaces an 0.8 g/10 min Blow Moulding Grade?

    On a single-screw extruder with 24:1 L/D and a general-purpose barrier screw with 3.0 compression ratio, substituting D200 for a blow moulding grade of 0.8 g/10 min moves the process toward torque-limited operation. The higher molecular weight increases melt viscosity at low shear rates, so head pressure at a given screw speed rises. Published data for this specific configuration is limited, but extrusion lines set for high-rate parison delivery frequently require barrel set points of 210–230 °C and die temperatures of 200–220 °C to control backpressure. Screen packs of 60/80/60 mesh are appropriate; finer screens compound the pressure rise. Melt temperature should not be allowed to exceed 240 °C to limit oxidative degradation. The output ceiling is not governed by melting capacity alone but by the onset of flow instabilities in the die land. Operators should expect to reduce screw speed relative to a 0.8 g/10 min grade until the pressure transducer reading at the breaker plate remains below the machine safety limit, commonly 350 bar. If the die gap is below 1.5 mm, shear rates can approach the critical region for sharkskin; adjusting die temperature upward by 5–10 °C may shift the defect boundary, but die gap and land length modifications are more effective.

    Slow crack growth resistance in contact with neutral aqueous media is the main reason D200 is selected over fractional-melt extrusion grades with similar density. In ASTM D1693, Condition B, 10% Igepal CO-630 at 50 °C, the nominal F50 value exceeds 100 h. This test result reflects the high tie-molecule concentration associated with a low MFR high-density backbone. In extruded sheet for chemical tank linings, the practical failure mode is not immediate tensile overload but the propagation of microcracks from notches or weld lines. The D200 balance of molecular weight and density supports ductile response at slow loading rates where a 0.952 g/cm³ density still provides stiffness without the brittleness of higher-density grades near 0.960 g/cm³. Comparative data between D200 and a 0.960 g/cm³ injection grade show lower notch sensitivity in Charpy tests under ISO 179-1/1eA at 23 °C, although published data for this specific comparison is limited.

    Rheological Boundaries on 24:1 to 30:1 Extruders

    The product exhibits a low melt flow index and high zero-shear viscosity. Under capillary rheometry at 190 °C, shear thinning becomes significant above 100 s⁻¹; below 10 s⁻¹ viscosity is high enough to support parison and sheet hang. This low-shear viscosity is measured indirectly through MFR and melt strength rather than by a single standardized method. When processing on an extruder of 30:1 L/D with a static mixer, the pressure drop across the mixer becomes a control point. Static mixers add 20–40 bar depending on number of elements and flow rate; selecting a 30:1 machine with adequate thrust capacity prevents screw speed from being limited by gearbox torque. For D200, screw cooling in the feed zone should be set to maintain stable solids conveying; overheating in the feed section can stall the screw and cause melt pressure fluctuations. The screw speed window is normally 20–60 min⁻¹ on a 90 mm single-screw sheet line, but actual settings depend on die width and downstream cooling capacity.

    At 0.952 g/cm³, D200 occupies a middle position in the HDPE density range. Tensile yield stress is approximately 26 MPa when tested per ISO 527-2:2012 on machined specimens; flexural modulus is approximately 950 MPa per ISO 178:2019. These values support structural sheet and profile applications without the warpage and brittle impact of highly crystalline injection grades. The Vicat softening temperature under ISO 306:2022, Method A50, is typically 122 °C, limiting continuous service under load to lower temperatures when long-term creep is considered. Short-term thermal stability in air can be characterized by oxidative induction time under ISO 11357-6; published data for this specific configuration is limited. The density also controls permeation; a 0.952 g/cm³ density provides a lower water-vapour transmission rate than 0.940 g/cm³ MDPE but a higher impact threshold than 0.960 g/cm³ homopolymer. This is why the grade is specified for chemical containment profiles where both stiffness and slow crack resistance are required.

    When Wall Thickness Consistency in Blow Moulded Components Becomes a Controlling Variable

    In extrusion blow moulding of containers with volume below 20 L, D200 requires higher head tooling pressure than fractional-melt grades but gives improved parison hang. On a reciprocating screw or accumulator head machine, the accumulator pressure typically reaches 250–350 bar, and the parison drop time must be matched to swell. A higher molecular weight resin reduces sag during drop, allowing more uniform wall thickness over a 1.5 m parison. The die swell of D200 is greater than that of 0.8 g/10 min HDPE, so die gap and tooling diameter need correction. Published data for this specific configuration is limited, but tooling adjustments of 10–15% in die gap are commonly made to compensate for swell. The melt temperature at the die exit should be 200–215 °C; lower temperatures increase melt fracture, higher temperatures reduce sag resistance. Cooling time is governed by wall thickness and density; at 4 mm average wall thickness, cooling time in chilled aluminium moulds is longer than for injection moulding but shorter than for solid thick sheet.

    Sheet extrusion lines using D200 operate with polished three-roll stacks at 60–80 °C to control surface finish and residual stress. The grade is used for chemical tank linings, machine guards, and structural profiles where welding and fabrication are part of the downstream process. Because the resin has a low MFR, extrusion welding and hot-gas welding consume more heat than lower-viscosity grades, but the weld retains high melt strength. Geometries with wall thickness from 2 mm to 10 mm are common; above 12 mm, cooling rate gradients can create residual stress differences through the thickness. In such cases, stack gap should be set to 95–100% of final sheet thickness to avoid overcompression of the melt. For profile lines, calibrator vacuum of 0.02–0.06 MPa is used, depending on profile complexity. These parameters are not grade-specific alone; they must be tuned to line speed and cooling water temperature.

    Comparative Position Against Injection Moulding and Pipe Extrusion Grades

    Compared with an injection moulding HDPE with MFR from 8 g/10 min to 20 g/10 min, D200 is unsuitable for thin-wall moulding because the spiral flow length is shorter and gate freeze occurs faster. Injection machines with clamp force below 1500 kN may not inject the material without excessive pressure loss. Pipe grades classified as PE100 under ISO 12162 are typically formulated with similar low MFR but are tested against hydrostatic strength at 20 °C and 80 °C. D200 is not sold as a PE100 pressure pipe compound; its performance in long-term hydrostatic loading has not been established by the manufacturer in the same published format. The grade is therefore placed between high-molecular-weight sheet resins and bimodal pipe resins in its property profile.

    Representative comparison matrix for D200 and adjacent HDPE categories
    CharacteristicTosoh HDPE D200General-purpose injection HDPEPE100 pipe compound
    Melt mass-flow rate0.20 g/10 min (190 °C, 2.16 kg)8–20 g/10 min (190 °C, 2.16 kg)0.2–0.3 g/10 min (190 °C, 5 kg)
    Density0.952 g/cm³0.958–0.965 g/cm³0.950 g/cm³
    Tensile yield stress26 MPa28–30 MPa25–27 MPa
    ESCR indication>100 h<10 h>1000 h
    Primary conversionThick sheet, profile, large blow mouldingThin-wall injection mouldingPressure pipe extrusion

    Values are representative of generic categories; they do not establish equivalency with specific commercial grades. The matrix is a selection aid, not a specification.

    Food-contact compliance must be confirmed on the commercial product, but olefin polymers of the HDPE family fall within 21 CFR 177.1520 when the additive package meets the stated extractives limits. The grade is not formulated with halogenated flame retardants; it does not offer intrinsic UV stability unless carbon black or a UV stabilizer masterbatch is added. Long-term outdoor exposure requires a minimum 2–3% carbon black addition by weight for ultraviolet screening in many profiles, with dispersion verified by optical microscopy or ISO 18553 assessment of agglomerates. Processors should avoid combining D200 with excessive levels of low-molecular-weight lubricants or organoleptic additives that can migrate under sustained service at elevated temperature.

    Operational boundaries are as follows: melt temperature should remain below 240 °C, residence time at temperature should be minimized to avoid chain scission, and screw geometries designed for high-speed high-shear mixing are not required for natural resin. When using regrind, the proportion should be limited to 20–30% in demanding applications because thermal history can reduce ESCR. The product should not be processed as a sole component in pressure-pipe applications without applicable hydrostatic design basis validation. Storage should avoid direct sunlight and prolonged temperatures above 60 °C to prevent pellet blocking.