    Specifications
    HS Code 781926
    Material Type PBT
    Reinforcement None
    Density 1.42 g/cm³
    Melting Point 225 °C
    Glass Transition Temperature 45 °C
    Tensile Strength 50 MPa
    Elongation At Break 20%
    Flexural Modulus 2400 MPa
    Flexural Strength 85 MPa
    Notched Izod Impact Strength 3 kJ/m²
    Heat Deflection Temperature At 0 45 Mpa 150 °C
    Heat Deflection Temperature At 1 82 Mpa 70 °C
    Water Absorption 24 H 0.08%
    Molding Shrinkage 1.4–1.8%
    Ul94 Flammability Rating V-0
    Volume Resistivity 1×10^16 Ω·cm
    Dielectric Strength 20 kV/mm
    Dielectric Constant At 1 Mhz 3.2

    As an accredited Toray Toraycon® Unreinforced PBT 4284X01 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toray Toraycon® Unreinforced PBT 4284X01 is supplied in 25 kg moisture-barrier sealed bags, 40 bags per pallet.
    Container Loading (20′ FCL) Toray Toraycon® Unreinforced PBT 4284X01 is loaded in 20′ FCL containers, typically palletized in moisture-proof bags for safe transport.
    Shipping Shipping description: Toray Toraycon® Unreinforced PBT 4284X01 is a non-hazardous polybutylene terephthalate resin, not regulated for transport. Ship in clean, dry, sealed containers at ambient temperature; protect from moisture, heat, sunlight, contamination, and punctures. Avoid prolonged outdoor storage.
    Storage Store Toray Toraycon® Unreinforced PBT 4284X01 in a cool, dry, well-ventilated area, preferably in tightly sealed original packaging. Protect from moisture, direct sunlight, heat, sparks, and oxidizing agents. Avoid dust generation and keep away from ignition sources. Use first-in, first-out stock rotation, follow the manufacturer’s SDS and local regulations, and do not store near food or drink.
    Shelf Life Shelf life is typically indefinite when stored sealed in a cool, dry place, protected from moisture, heat, and contamination.
    Free Quote

    Competitive Toray Toraycon® Unreinforced PBT 4284X01 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toray Toraycon® Unreinforced PBT 4284X01 is an unfilled polybutylene terephthalate injection-molding grade supplied under the Toraycon trade name. The grade is most frequently specified for thin-wall electrical connector housings, relay bobbins, switch components, sensor housings, and precision motor parts in which melt filling, dimensional reproducibility, and electrical insulation are evaluated together. The unfilled composition distinguishes 4284X01 from glass-fiber-reinforced Toraycon grades: the absence of short-glass reinforcement lowers modulus and creep resistance but reduces mold shrinkage anisotropy. Grade-specific values for melt volume-flow rate, tensile stress at yield, notched Charpy impact strength, and comparative tracking index are reported on the supplier certificate of analysis and are measured according to ISO 1133-1:2022, ISO 527-2:2012, ISO 179-1/1eA, and IEC 60112:2020. Published data for this specific configuration is limited in open literature; processing limits should therefore be confirmed against the Toray technical data sheet for the exact color and additive package.

    Material Classification and Regulatory Position

    The polymer is classified as PBT according to ISO 1043-1 and belongs to the thermoplastic polyester family. The material is semicrystalline; a melting peak is typically detected between 220 °C and 225 °C when measured by differential scanning calorimetry under ISO 11357-3 at 10 °C/min. Regulatory documentation for 4284X01 is normally maintained under REACH Regulation (EC) No 1907/2006, with SVHC disclosure at the 0.1% weight threshold, and under RoHS Directive 2011/65/EU annex II. Flame-retardant performance is characterized by the vertical burn test of UL 94; thin-wall connector applications commonly require a rating at 0.75 mm or 1.5 mm thickness. The UL Yellow Card for the as-molded color should be reviewed because pigmentation and regrind content can alter burn performance. Halogen-free status is not automatic for every color lot and must be verified against IEC 61249-2-21 if required by the end-use specification.

    Injection molding of 4284X01 for terminal-retaining connectors requires a reciprocating-screw machine with barrel temperatures profiled from 230 °C in the rear feed zone to 250 °C or 260 °C at the metering zone and nozzle. The melt temperature measured after five consecutive air shots should not exceed 260 °C. Mold surface temperature is held between 60 °C and 80 °C with a circulating thermolator; this range controls the quench rate and stabilizes the semicrystalline morphology at the part surface. Desiccant drying at 120 °C to 130 °C for 4 h is required, with a hopper outlet moisture content below 0.02% by weight. Moisture above this level hydrolyzes the ester linkage during melt processing, producing a measurable reduction in melt viscosity under ISO 1133-1:2022 and a loss of notched Charpy impact under ISO 179-1/1eA. A general-purpose screw with a compression ratio of 2.5:1 to 3.5:1 and a shut-off nozzle or check-ring valve is used in practice to maintain a 3–6 mm cushion and to prevent aerated material from entering the cavity.

    Tool design for 4284X01 in thin-wall applications uses hardened P20 or H13 tool steel with 48–52 HRC surfaces at the gate and runner. Runner diameters are typically 3.0–4.0 mm for cold runner systems with sub-gates of 0.8–1.2 mm. The gate land is kept below 1.0 mm to reduce jetting, and the gate location is placed away from the terminal pocket weld lines. Because unfilled PBT has a higher solidification rate than glass-filled PBT, the packing pressure must be transferred to the cavity within 0.5–1.0 s after fill to avoid sink marks at bosses. Injection speed is set in the 80–150 mm/s range at the screw, adjusted to avoid gas traps; gas venting is provided with 0.02–0.04 mm deep vents on the parting line and ejector pins. Process capability studies for a 0.75 mm wall connector typically monitor a cavity pressure integral of 600–900 bar·s, although the exact limit is tool-specific and must be derived from the mold-flow study.

    The dryer hopper capacity is selected to match the shot weight and cycle time so that granulate residence in the drying hopper does not exceed 8 h at 120 °C; longer exposure can oxidize the surface and shift the yellowness index. A desiccant bed with a dew point of -40 °C or lower is used, and the return air temperature is monitored at the hopper inlet. The moisture level is verified with a Karl Fischer coulometric titrator or a loss-on-drying analyzer calibrated against ISO 15512:2019 method A. The granulate is not returned to the drying hopper after the machine throat has been opened, because ambient humidity above 60% can reintroduce moisture within 30 min in an unsealed hopper.

    Why Does Unreinforced 4284X01 Exhibit Lower Post-Mold Warpage than Glass-Reinforced PBT?

    Short-glass fiber reinforcement induces flow-direction orientation during the filling and packing phases. In 30% by weight glass-fiber-reinforced PBT, this orientation creates a difference between flow-direction and transverse mold shrinkage of 0.4% or more when measured according to ISO 294-4. Unreinforced PBT, by contrast, commonly shows less than 0.2% shrinkage difference between the flow and transverse axes, with total mold shrinkage in the 1.5% to 2.0% range. The reduced anisotropy of 4284X01 limits warpage in flat connector housings and coil bobbins. The trade-off is mechanical: unfilled PBT flexural modulus is typically 2.5–2.8 GPa under ISO 178, while a 30% glass-reinforced PBT reaches 9.0–10.5 GPa. Tensile stress at yield is correspondingly lower for the unfilled product. The comparative directions are listed in the table below; the ranges are typical published values for unfilled and 30% glass-reinforced PBT classes and are not a substitute for the 4284X01 certificate.

    ParameterTest methodUnreinforced PBT class30% glass-reinforced PBT class
    DensityISO 1183-11.30–1.43 g/cm³1.50–1.55 g/cm³
    Tensile stress at yieldISO 527-250–60 MPa130–140 MPa
    Flexural modulusISO 1782.5–2.8 GPa9.0–10.5 GPa
    Notched Charpy impactISO 179-1/1eA3–5 kJ/m²8–12 kJ/m²
    Flow/transverse shrinkage differenceISO 294-4< 0.2%> 0.4%

    The table is for specification-selection purposes only and does not represent lot-specific data.

    When Shutdown Purge Procedures Are Not Followed at Melt Temperatures Above 250 °C

    Thermal decomposition of unfilled PBT advances through ester cleavage and formation of tetrahydrofuran and carboxyl end groups; the rate becomes practically significant above 250 °C. A hold-up time of 10 min at 260 °C in the compression zone or check-ring channel can degrade the molecular weight distribution. Parts molded from heat-damaged material may exhibit a 10–20% reduction in notched Charpy impact under ISO 179-1/1eA and a melt viscosity reduction above 15% under ISO 1133-1:2022. During production interruptions longer than 10 min, the barrel is purged with a high-viscosity olefinic purge compound until the nozzle discharge is clear of black specks and the melt temperature is reduced to 180 °C or lower. Recrystallization of carbonized residue in the gate and runner is not reversible by continued purging; the hot runner manifold must be disassembled if black streaks persist. Regrind generated during a thermally abusive shutdown is restricted to 15% by weight after drying to below 0.02% moisture, unless the supplier certificate imposes a lower limit.

    Electrical use of 4284X01 in a 0.75 mm wall thickness is specified with reference to IEC 60112:2020 for comparative tracking index, IEC 60243-1 for dielectric strength, and IEC 62631-3-1 for volume resistivity. Comparative tracking index values for unfilled flame-retardant PBT are commonly 500–600 V; the exact value depends on the flame-retardant package, colorant, and gloss. Dielectric strength on 2.0 mm plaques is typically 15–20 kV/mm under IEC 60243-1 with 50 mm or 25 mm electrodes; the result is thickness-dependent and should not be extrapolated to thin-wall sections without testing. Volume resistivity after 24 h at 23 °C and 50% relative humidity is usually in the 1015–1017 Ω·cm range. The material is not recommended for continuous exposure to hot water above 80 °C, strong alkaline solutions, or amine-containing coolants because polyester hydrolysis can reduce tensile strength and promote surface erosion under ISO 527-2 and ISO 175 immersion testing.

    Compared with a non-flame-retardant unfilled PBT, 4284X01 has a higher density and a lower elongation at break due to the flame-retardant synergist; the density difference is often 0.10–0.15 g/cm³ under ISO 1183-1. The grade also differs from impact-modified PBT, which raises notched Charpy impact at the expense of heat deflection temperature and creep resistance. These differences make 4284X01 a separate selection from general-purpose unfilled PBT and from glass-reinforced PBT: the product is specified where a thin-wall flame-retardant polyester with high flow and lower anisotropic shrinkage is required, provided that the mechanical load is within unfilled polyester limits. The final selection must be confirmed by mold-flow simulation using grade-specific PVT data and by physical parts tested under the end-use standard.

    In an engine-control unit connector designed for a 0.75 mm wall and terminal retention force above 30 N per terminal, 4284X01 is processed with a mold-filling analysis using measured viscosity data from ISO 11403-2 and pressure-volume-temperature data from ISO 17744. The tool is gated with a sub-gate 0.8–1.2 mm in diameter, and short-shot studies are used to confirm that the melt reaches all terminal pockets at 95–98% of the full shot weight before the switch-over position. Terminal retention is measured according to the OEM terminal retention test, not by generic tensile data, because the retention force is governed by the plastic boss geometry and post-mold crystallization. Parts are conditioned at 23 °C and 50% relative humidity for 48 h before electrical tests under IEC 60664-1 creepage and clearance constraints.