Toray Toraycon Unreinforced Pbt 1401x70

Toray Toraycon® Unreinforced PBT 1401X70

    • Product Name: Toray Toraycon® Unreinforced PBT 1401X70
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 875886
    Density 1.31 g/cm³
    Water Absorption 0.08 %
    Mold Shrinkage 1.5–2.0 %
    Tensile Strength 55 MPa
    Elongation At Break 40 %
    Flexural Strength 85 MPa
    Flexural Modulus 2.4 GPa
    Charpy Notched Impact Strength 3.5 kJ/m²
    Heat Deflection Temperature 1 82 Mpa 60 °C
    Melting Point 224 °C
    Rockwell Hardness R118
    Volume Resistivity 1×10^16 Ω·cm

    As an accredited Toray Toraycon® Unreinforced PBT 1401X70 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toray Toraycon® Unreinforced PBT 1401X70 is typically supplied in 25 kg moisture-proof bags, palletized and shrink-wrapped for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL dry container loaded with palletized 25 kg bags of Toray Toraycon® Unreinforced PBT 1401X70, approx. 20 MT net.
    Shipping Shipping description: Toraycon® Unreinforced PBT 1401X70 is solid polybutylene terephthalate resin pellets. It is non-hazardous and not regulated as dangerous goods under DOT, IMDG, or IATA; no UN number assigned. Ship in sealed moisture-barrier bags or boxes, store cool and dry, and protect from moisture, heat, and contamination.
    Storage Store Toray Toraycon® Unreinforced PBT 1401X70 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep containers tightly closed to prevent contamination and humidity ingress. Avoid prolonged high-temperature or humid exposure. Store at ambient temperature unless the SDS specifies otherwise. Follow the manufacturer’s SDS, local regulations, and first-in/first-out inventory practices. Use clean handling equipment.
    Shelf Life Toray Toraycon® Unreinforced PBT 1401X70 has an approximately two-year shelf life when stored dry in its unopened original packaging.
    Free Quote

    Competitive Toray Toraycon® Unreinforced PBT 1401X70 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toray Toraycon® 1401X70 is an unreinforced polybutylene terephthalate (PBT) injection-molding grade belonging to the unfilled 1401 series. The suffix X70 designates a controlled melt-viscosity variant intended for high-flow filling of thin-wall electrical and automotive components. No glass fiber, mineral filler, or impact modifier is present in the base-grade composition. Because peer-reviewed or supplier-published data for this exact suffix are limited in English-language technical literature, the property data below are presented as the ISO-conditioned envelope for the 1401 series and for general-purpose unreinforced PBT; lot-specific values should be confirmed against the supplier certificate of analysis.

    The nominal material envelope for this unfilled PBT class is density 1.30–1.32 g/cm³ per ISO 1183-1, tensile strength 55–65 MPa and tensile modulus 2500–2800 MPa per ISO 527-2, flexural strength 80–90 MPa per ISO 178, notched Charpy impact 3–5 kJ/m² per ISO 179-1/1eA, and heat deflection temperature under 1.8 MPa load 50–60 °C per ISO 75-1/-2. The melt volume-flow rate of a high-flow unfilled PBT typically falls between 20 cm³/10 min and 35 cm³/10 min at 250 °C/2.16 kg per ISO 1133-1. Linear mold shrinkage for unfilled PBT generally ranges from 1.5% to 2.0% in the flow direction and 1.4% to 1.8% transverse when measured on a 60 mm × 60 mm × 2 mm plaque per ISO 294-4. These values distinguish the unfilled grade from glass-filled and mineral-filled Toraycon types, which have higher modulus and lower shrinkage.

    The controlling pre-processing variable is moisture. PBT ester linkages hydrolyze at melt temperatures when pellet moisture exceeds 0.03 wt%. In production, pellets are dried at 120 °C for 4–6 h in a desiccant dryer with air dew point no higher than -30 °C; residual moisture below 0.02 wt% is confirmed by Karl Fischer titration before restarting the barrel. A barrel profile from 240 °C to 260 °C, nozzle temperature 250–260 °C, and mold wall temperature 40–80 °C provide a crystallization window that balances cycle time and dimensional stability. On toggle-clamp machines of 80–120 t, general-purpose screws with L/D 20:1–25:1 and compression ratio 2:1–3:1 are used; back pressure is maintained at 0.3–0.7 MPa and screw surface speed at 0.1–0.3 m/s to avoid excessive shear heating. When mold temperature drops below 40 °C, the low crystallization rate increases post-mold shrinkage and can produce tight-hole dimensional drift in connectors. When mold temperature exceeds 80 °C, cycle time increases without proportionally higher crystallinity.

    How Does the Glass-Filled PBT Grade Differ from the Unreinforced 1401X70 Type?

    Glass reinforcement changes the mechanical and failure behavior of PBT in three directions. The addition of 30% by weight short glass fiber raises tensile strength from the 55–65 MPa range to approximately 120–140 MPa and tensile modulus from 2500–2800 MPa to 9500–11000 MPa, but reduces elongation at break from 20–30% for unfilled PBT to 2–3%. The practical consequence is that the unfilled 1401X70 is selected for thin-wall connector housings and relay bases where high flow and low warpage are more important than load-bearing capacity. Glass-filled grades are reserved for structural brackets and motor end caps where creep resistance at high temperature is required.

    PropertyTest methodUnreinforced PBT 1401 seriesGF30 PBTImpact-modified unfilled PBT
    DensityISO 1183-11.30–1.32 g/cm³1.52–1.55 g/cm³1.27–1.30 g/cm³
    Tensile strengthISO 527-255–65 MPa120–140 MPa40–50 MPa
    Tensile modulusISO 527-22500–2800 MPa9500–11000 MPa2000–2300 MPa
    Flexural strengthISO 17880–90 MPa180–210 MPa65–75 MPa
    Notched Charpy impactISO 179-1/1eA3–5 kJ/m²8–11 kJ/m²10–20 kJ/m²
    Heat deflection temperature at 1.8 MPaISO 75-1/-250–60 °C200–210 °C45–55 °C
    Melt volume-flow rate at 250 °C/2.16 kgISO 1133-120–35 cm³/10 min8–15 cm³/10 min10–20 cm³/10 min
    Mold shrinkage, flow directionISO 294-41.5–2.0 %0.2–0.4 %1.4–1.8 %

    The comparison is illustrative for unfilled, glass-reinforced, and impact-modified PBT classes. Published data for 1401X70 specifically may fall outside the listed envelope; supplier certification prevails.

    When wall thickness falls below 0.8 mm in multi-pin connector housings

    Multi-pin connector bodies with wall stock between 0.3 mm and 0.8 mm impose a flow-length-to-thickness ratio that standard unfilled PBT grades may not fill within the machine pressure limit. A high-flow unfilled grade such as 1401X70 reduces melt pressure loss in the runner and gate so that cavity pressure at end-of-fill remains above the minimum required for packing. On hot-runner molds with valve-gate drops, cavity pressure transducers are typically set to trigger transfer at 80–120 MPa in the cavity; insufficient cavity pressure in thin sections produces sink marks and weak weld lines. The trade-off is that raising melt flow by reducing molecular weight tends to lower notched impact; therefore the part design should avoid sharp notches, and gate locations should move weld lines away from snap-fit roots. When flow-length-to-wall-thickness ratio exceeds 100:1, mold-filling simulation and short-shot studies on the production tool are required before process release.

    Unreinforced PBT is selected for electrical and electronic components because it absorbs less moisture than polyamide 66 and therefore maintains dimensions and dielectric properties across seasonal humidity changes. At 23 °C and 50% RH, water absorption is approximately 0.2% per ISO 62, compared with 2.5% for PA66 under the same conditions. Typical electrical values for unfilled PBT are comparative tracking index 400–600 V per IEC 60112, dielectric strength 15–25 kV/mm at 2.0 mm per IEC 60243-1, volume resistivity 1015 Ω·cm per IEC 60093, and relative permittivity 3.0–3.3 at 1 MHz per IEC 60250. These characteristics support use in relay bases, switch bodies, terminal blocks, motor brush holders, sensor housings, bobbins, and automotive electrical distribution housings. For connectors requiring UL 94 V-0 at wall thickness below 0.75 mm, the unreinforced non-flame-retardant 1401X70 is typically not suitable; a flame-retardant Toraycon series or a mineral-filled FR grade should be evaluated.

    Moisture uptake, dimensional change, and relative tracking index differences

    When benchmarked against other unfilled engineering thermoplastics, the 1401X70 grade occupies a narrow position between PA66, POM, and PET. The table below provides class-level values for dry-as-molded or conditioned specimens; they are not lot-specific for 1401X70 but identify the selection boundaries.

    PropertyTest methodUnreinforced PBT 1401 seriesPA66 dry-as-moldedPOM copolymerPET unreinforced
    Water absorption at 23 °C/50% RHISO 620.2%2.5%0.2%0.2%
    Heat deflection temperature at 1.8 MPaISO 75-1/-250–60 °C65–85 °C95–110 °C65–75 °C
    Comparative tracking indexIEC 60112400–600 V500–600 V600 V500 V
    Dielectric strength at 2.0 mmIEC 60243-115–25 kV/mm20–30 kV/mm20–25 kV/mm20–30 kV/mm
    Notched Charpy impactISO 179-1/1eA3–5 kJ/m²3–5 kJ/m²6–8 kJ/m²2–3 kJ/m²

    PA66 gains moisture and loses stiffness and glass transition temperature; PBT retains dimensional stability in humid environments but has lower HDT than POM. POM offers higher fatigue resistance but is sensitive to acidic hydrolysis and has narrower processing-temperature control. PET offers higher continuous-use potential but generally lower impact and poorer long-term alkaline resistance. These boundaries explain why an unfilled PBT such as 1401X70 is chosen for electrical and electronic parts that require stable dimensions and good electrical tracking behavior but do not require the high HDT of POM or glass-filled PBT.

    Thermal ageing limits in continuous-use electrical enclosures

    Unreinforced PBT under continuous thermal load is governed by oxidative degradation and eventual embrittlement. Under UL 746B long-term thermal ageing, unfilled PBT grades commonly show electrical relative temperature indices near 120 °C and mechanical relative temperature indices from 85 °C to 105 °C at 0.75 mm thickness; grade-specific RTI values for 1401X70 must be taken from the UL yellow card or supplier certification. In dry-heat applications below the HDT, dimensional changes are small after initial annealing. Above 60 °C in water or water-glycol mixtures, hydrolytic degradation accelerates; therefore 1401X70 is not appropriate for sustained exposure to pressurized hot water, steam sterilization, or engine coolant immersion. Photochemical degradation limits outdoor use unless UV-stabilized grades are specified. Strong bases, hot concentrated acids, and some amines attack PBT and should be excluded from the application environment. If a part requires both high CTI and V-0 combustion resistance, an FR-unfilled PBT or a mineral-filled FR grade should be evaluated instead of 1401X70.