Toray Toraycon Unreinforced Pbt 1401x31

Toray Toraycon® Unreinforced PBT 1401X31

    • Product Name: Toray Toraycon® Unreinforced PBT 1401X31
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 804070
    Density 1.31 g/cm³
    Water Absorption 24h 0.08%
    Mold Shrinkage Flow Direction 1.7%
    Tensile Strength 55 MPa
    Tensile Elongation At Break 50%
    Flexural Strength 85 MPa
    Flexural Modulus 2.2 GPa
    Charpy Notched Impact Strength 4 kJ/m²
    Rockwell Hardness M70
    Melting Point 224 °C
    Deflection Temperature At 1 82 Mpa 60 °C
    Flammability Ul94 HB
    Dielectric Constant At 1 Mhz 3.1
    Volume Resistivity 1×10^16 Ω·cm
    Arc Resistance 120 s

    As an accredited Toray Toraycon® Unreinforced PBT 1401X31 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-barrier bags, Toray Toraycon® Unreinforced PBT 1401X31 resin pellets are packaged for industrial handling and storage.
    Container Loading (20′ FCL) Toray Toraycon® Unreinforced PBT 1401X31 is packed in 25 kg bags, palletized, and loaded into a 20′ FCL container for secure export shipment.
    Shipping Shipping description: Non-hazardous polybutylene terephthalate resin pellets. Supplied in sealed moisture-barrier bags, cartons, or octabins on pallets. Transport at ambient temperature in dry, clean conditions; protect from moisture, direct sunlight, and excessive heat. No UN number, hazard class, or special transport label required. Keep containers closed until use.
    Storage Store Toray Toraycon® Unreinforced PBT 1401X31 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture pickup and contamination. Maintain original packaging and labeling; avoid prolonged high humidity or excessive temperatures. Separate from incompatible chemicals and follow local regulations and SDS guidance.
    Shelf Life Shelf life is typically 24 months when stored unopened in original packaging under cool, dry conditions, protected from moisture and direct sunlight.
    Free Quote

    Competitive Toray Toraycon® Unreinforced PBT 1401X31 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toraycon® 1401X31 is an unfilled polybutylene terephthalate (PBT) injection-moulding grade manufactured by Toray Industries, Inc. The material is supplied as natural or coloured pellets for thin-wall parts in electrical, electronic, and automotive applications. Its ISO 1043-1 designation is PBT. The grade is characterised by a density of 1.31 g/cm³ under ISO 1183-1:2019 and a melt volume-flow rate of approximately 22 cm³/10 min at 250 °C and 2.16 kg under ISO 1133-1:2022. The unreinforced composition provides a UL 94 HB rating at 1.5 mm and is therefore reserved for low-voltage insulating or enclosure applications that do not require a V category.

    Because the melt contains no glass fibre or mineral filler, solidification is semi-crystalline and the mould shrinkage after 48 h is approximately 1.8 % in flow direction and 2.0 % transverse when measured on a 60×60×2 mm plaque under ISO 294-4:2018. The coefficient of linear thermal expansion is approximately 90 × 10⁻⁶ K⁻¹ in flow and 110 × 10⁻⁶ K⁻¹ transverse under ISO 11359-2:2021. These values are higher than glass-reinforced PBT; tool designers should therefore apply larger draft angles and avoid thick-to-thin transitions that amplify differential shrinkage.

    Typical data for Toraycon® 1401X31 natural-grade unreinforced PBT
    PropertyValueTest method
    Density1.31 g/cm³ISO 1183-1:2019
    Melt volume-flow rate22 cm³/10 min at 250 °C, 2.16 kgISO 1133-1:2022
    Tensile stress at yield55 MPaISO 527-1:2019, ISO 527-2:2012
    Tensile strain at break200 %ISO 527-1:2019, ISO 527-2:2012
    Flexural modulus2.3 GPaISO 178:2019
    Charpy notched impact strength, 23 °C, type 1eA3.0 kJ/m²ISO 179-1:2010
    Heat deflection temperature, 1.80 MPa60 °CISO 75-2:2013, method A
    Water absorption, 24 h, 23 °C0.08 %ISO 62:2008
    Mould shrinkage, 60×60×2 mm, flow/transverse1.8 / 2.0 %ISO 294-4:2018
    Flammability, 1.5 mmHB at 1.5 mmUL 94

    Where Does 1401X31 Sit Within the Toraycon Unreinforced PBT Portfolio?

    Within the Toraycon PBT portfolio, the X31 suffix denotes a flow-optimised unreinforced grade. Standard unfilled PBT grades often exhibit melt volume-flow rates between 10 and 15 cm³/10 min at 250 °C and 2.16 kg; 1401X31 at approximately 22 cm³/10 min is therefore intended for multi-cavity tools, thin-wall sections, and long flow-length-to-wall-thickness ratios. The higher melt volume-flow rate is achieved by molecular-weight adjustment; a consequence is lower tensile stress at yield and lower Charpy notched impact than high-viscosity or extrusion-grade PBT. Published data for exact molecular weight distributions are limited, but the mechanical and rheological shift is measurable.

    On production-scale horizontal reciprocating screw machines with clamp forces from 500 to 3500 kN, the flow-optimised grade reduces in-cavity pressure loss, but narrows the processing window because the low melt viscosity increases sensitivity to flash at parting lines if clamp force is insufficient. Experience in multi-cavity relay socket tools indicates that cavity-to-cavity mass imbalance is lower when the runner diameter is reduced by 10 % to 15 % compared with a standard-viscosity PBT, because the low-viscosity melt fills edge cavities without requiring excessive overpacking of centre cavities.

    Thermal and Mechanical Limits Encountered in Connector Applications

    At 23 °C, the tensile stress at yield is 55 MPa and tensile strain at break is 200 % under ISO 527-1:2019 and ISO 527-2:2012. Flexural modulus is 2.3 GPa under ISO 178:2019, and Charpy notched impact strength is 3.0 kJ/m² under ISO 179-1:2010 using a type 1eA specimen. The heat deflection temperature is 60 °C at 1.80 MPa under ISO 75-2:2013. These values place 1401X31 in connector housings, relay bases, switch bodies, sensor connectors, and lamp sockets where short-term excursions above 60 °C are possible but continuous structural load at that temperature is avoided.

    For press-fit and snap-fit features, the high tensile elongation permits assembly deflection, but the low notched impact strength limits sharp corners and cold-temperature installation. At -40 °C, the notched impact strength of unfilled PBT typically falls below 2.0 kJ/m²; published data for this specific grade at low temperature is limited. Therefore live-hinge designs, thick-wall bosses, and metal-thread inserts should be avoided unless validated by impact testing under ISO 179-1:2010 on production-moulded specimens.

    Regulatory conformity for the natural grade is typically declared against Directive 2011/65/EU (RoHS) including Commission Delegated Directive (EU) 2015/863, and against Regulation (EC) No 1907/2006 (REACH). The grade is not inherently flame-retardant; the UL 94 HB classification excludes use as a substitute for V-0 PBT formulations in unattended appliance electrical housings.

    Practical moulding of 1401X31 on production-scale injection lines begins with desiccant drying because residual moisture hydrolyses the ester linkages at melt temperature. The supplier recommendation for unfilled PBT is drying at 120 °C for 4 h using a desiccant-bed hopper dryer with a dew point below -30 °C; the granule moisture level should be below 0.02 % by Karl Fischer titration before entering the feed throat. In plants where ambient relative humidity exceeds 60 %, open hopper residence time beyond 2 h should be avoided or the hopper must be sealed and purged with dried air. Failure to maintain dryness appears on moulded parts as silver streaks, gate blush, and reduced Charpy notched impact; repeated processing of damp regrind decreases notched impact from 3.0 kJ/m² to below 2.0 kJ/m² after two cycles.

    Barrel temperatures should be profiled from 240 °C at the rear zone to 260 °C at the front, with the nozzle held at 260 °C to 270 °C. Mould temperature is set at 60 °C to 80 °C using turbulent water flow in conformal channels. A general-purpose screw with 20:1 to 22:1 L/D and compression ratio 2.4:1 to 2.8:1 is sufficient; high-shear barrier screws are not required because no filler dispersion is involved. Screw speed should be 100 rpm to 150 rpm, back pressure 0.3 MPa to 0.7 MPa. Injection pressure of 60 MPa to 100 MPa and holding pressure of 40 MPa to 80 MPa are typical for multi-cavity cold-runner connector tools. Shot size should remain between 30 % and 70 % of barrel capacity to limit residence-time variation; cushion is maintained at 3 mm to 5 mm to provide consistent hold pressure transfer.

    Melt residence time at 250 °C should not exceed 8 min. During production stoppages, barrel temperatures should be reduced to 200 °C or the melt should be purged with a high-viscosity polyolefin purging compound to prevent thermal degradation. The use of regrind from sprues and runners is generally limited to 20 % by weight because higher levels increase melt viscosity variation and reduce impact strength. Hot-runner systems with externally heated manifolds and needle-valve gating are preferred for thin-wall parts; internal hot-runner drops should be avoided if dead spots create hydrolytic decomposition.

    When the Specification Requires Unfilled PBT Instead of Glass-Fibre Reinforcement

    The second table compares 1401X31 with representative 30 % glass-fibre reinforced PBT. The unfilled grade is selected when lower warpage, lower melt viscosity, lower density, and lower tool wear are more important than load-bearing capacity and heat resistance. However, the property penalty is substantial.

    Comparative data for material selection: 1401X31 versus representative 30% glass-fibre PBT
    Property1401X3130% glass-fibre PBTTest method
    Density1.31 g/cm³1.53 g/cm³ISO 1183-1:2019
    Tensile stress at yield55 MPa130 MPaISO 527-1:2019, ISO 527-2:2012
    Flexural modulus2.3 GPa9.0 GPaISO 178:2019
    Heat deflection temperature, 1.80 MPa60 °C205 °CISO 75-2:2013
    Charpy notched impact strength, 23 °C3.0 kJ/m²8.0 kJ/m²ISO 179-1:2010
    Mould shrinkage, flow/transverse1.8–2.0 %0.3–0.5 %ISO 294-4:2018
    CLTE, flow direction90 × 10⁻⁶ K⁻¹30 × 10⁻⁶ K⁻¹ISO 11359-2:2021

    In electrical housings, the unfilled grade provides a better surface finish and avoids exposed glass fibres at the weld line. It also reduces mould corrosion compared with glass-filled PBT, which is significant in high-cavitation tools. However, the heat deflection temperature of 60 °C at 1.80 MPa means that any bracket or structural feature requiring dimensional stability above 55 °C must be transferred to a reinforced PBT or a polyphenylene sulphide grade.

    Compared with polyamide 66, 1401X31 absorbs 0.08 % water in 24 h at 23 °C under ISO 62:2008, whereas conditioned PA66 may absorb around 2.5 % at 23 °C and 50 % relative humidity. This gives PBT more stable electrical performance in humid automotive interiors, but PA66 has higher continuous-use temperature and better low-temperature impact. When dimensions must remain within ±0.2 mm across a 50 mm connector body, the lower moisture growth of PBT is the key material-selection factor.

    Relay sockets, sensor connectors, lamp sockets, and switch bodies are typical production parts for 1401X31. In relay sockets, the material is processed with multi-cavity cold-runner tools to achieve wall thicknesses as low as 0.4 mm; the low melt viscosity permits filling without flash at clamp force settings of 600 kN to 1500 kN for 16-cavity tools. In automotive lamp sockets, short-term bulb heat can raise the housing wall above 80 °C, so the part must be derated or metal shielded to avoid creep.

    The grade is not recommended for continuous contact with hot aqueous coolant above 75 °C, hot alkaline cleaning solutions above 60 °C, or strong acidic media because PBT undergoes ester hydrolysis. Gasoline and mineral oils show limited effect at ambient temperature, but long-term exposure data under ISO 175:2010 for the specific grade is limited and should be generated for under-bonnet components.

    Top