| HS Code | 197605 |
| Polymer Type | PBT (polybutylene terephthalate) |
| Reinforcement | Unreinforced |
| Flame Retardancy | UL94 V-0 |
| Density | 1.31 g/cm³ |
| Tensile Strength | 55 MPa |
| Elongation At Break | 30% |
| Flexural Modulus | 2,300 MPa |
| Flexural Strength | 85 MPa |
| Notched Izod Impact Strength | 4 kJ/m² |
| Hdt At 0 45 Mpa | 150 °C |
| Hdt At 1 82 Mpa | 65 °C |
| Water Absorption | 0.08% |
| Molding Shrinkage | 1.5–2.0% |
| Volume Resistivity | 1×10^16 Ω·cm |
| Dielectric Strength | 20 kV/mm |
| Melting Point | 225 °C |
As an accredited Toray Toraycon® Unreinforced PBT 1401 F01 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Toray Toraycon® Unreinforced PBT 1401 F01 is packaged in 25 kg moisture-barrier, polyethylene-lined bags, supplied on pallets. |
| Container Loading (20′ FCL) | Toray Toraycon® Unreinforced PBT 1401 F01 is packed in bags on pallets and loaded into a dry 20′ FCL container. |
| Shipping | Toray Toraycon® Unreinforced PBT 1401 F01 is shipped as non-hazardous thermoplastic resin pellets in sealed bags or boxes. It is not regulated for transport under DOT, IATA, or IMDG. Store in a cool, dry, ventilated area; protect from moisture, contamination, and excessive heat. |
| Storage | Store Toray Toraycon® Unreinforced PBT 1401 F01 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and incompatible materials. Keep original containers tightly closed to prevent moisture pickup and contamination. Use first-in, first-out stock rotation. Follow the manufacturer’s SDS and local regulations for safe storage and handling. |
| Shelf Life | Toray Toraycon® Unreinforced PBT 1401 F01 typically has a 24-month shelf life when stored in original sealed packaging in cool, dry conditions. |
Competitive Toray Toraycon® Unreinforced PBT 1401 F01 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The Toraycon® 1401 F01 grade is an unreinforced polybutylene terephthalate (PBT) compound supplied in pellet form for injection moulding and extrusion where no glass fibre, mineral filler, or flame-retardant additive is present. The numerical designation 1401 identifies the unfilled PBT series, while the suffix F01 denotes a producer-specific melt-viscosity and additive variant within that series. Because the grade is unfilled, it is evaluated for applications in which flow length, surface quality, electrical insulation, and low mould abrasion are more critical than the elevated flexural modulus obtained from glass-reinforced PBT. Typical specification review requires confirmation of density, melt volume-flow rate, moisture content, tensile properties, and UL 94 classification against the manufacturer’s current datasheet; published data for this specific configuration is limited where colourant or nucleating packages alter crystallisation behaviour.
The short-term mechanical profile of an unreinforced PBT such as 1401 F01 is conventionally reported by tensile testing to ISO 527-2 and flexural testing to ISO 178. Representative values for unfilled PBT in this grade class fall within a density range of 1.30–1.32 g/cm³ under ISO 1183, tensile stress at yield of 50–60 MPa, tensile strain at break of 25–50%, and flexural modulus of 2.3–2.6 GPa. Notched Charpy impact strength is typically 3–6 kJ/m² under ISO 179-1/1eA, with the lower end observed at low moisture content and high test speed. These values place 1401 F01 below a 30% glass-fibre PBT in stiffness and load-bearing capacity, but above it in ductility and impact-related energy absorption in thin-wall sections. The absence of fibre also reduces orientation-induced anisotropy, but mould shrinkage remains significant at 1.7–2.3% in the flow direction and 1.5–2.0% transverse, so dimensional control depends on gate location and packing pressure rather than filler restraint.
Drying ahead of melt processing is not optional for the unfilled 1401 F01 grade because polybutylene terephthalate undergoes hydrolytic chain scission when melt moisture exceeds 0.02%. A desiccant dryer with a dew point of -40 °C or lower and an air flow of approximately 3.7 m³/h per kg/h is used to reduce pellet moisture to 0.015–0.020% after 3–5 h at 120 °C. On a 35 mm reciprocating-screw injection moulding machine with a 20:1 L/D screw, the barrel profile is usually set from 240–260 °C, with nozzle temperature held at 250–270 °C. Melt temperature should not exceed 270 °C, and total residence time above 250 °C should be kept below 5 min to limit ester cleavage and discolouration. Mould temperature is normally maintained at 40–80 °C; below 40 °C the part cools with reduced crystallinity and can exhibit post-mould dimensional drift, while above 80 °C cycle time increases without a proportional improvement in crystallinity. At wall stocks below 0.8 mm, high injection speed and vent depths of 0.02–0.03 mm are required to prevent short shots, but published spiral-flow data for this specific configuration is limited. Regrind fractions up to 30% may be reincorporated only after drying, with melt volume-flow rate checked at 250 °C/2.16 kg to ISO 1133-1 to detect batch-to-batch viscosity drift.
Short-term thermal resistance is defined by heat deflection temperature rather than crystalline melting point. At 1.80 MPa, unreinforced PBT typically exhibits a heat deflection temperature of 55–65 °C to ISO 75-2, while at 0.45 MPa the value rises to 150–160 °C. Continuous-use temperature is application-dependent and must be validated by thermal ageing; non-load-bearing electrical insulation commonly uses a provisional limit of 120–130 °C, but this is not an ISO continuous-use rating. Electrical insulation data for unfilled PBT include volume resistivity of 10^14 Ω·cm or higher to IEC 62631-3-1, dielectric strength of 20–25 kV/mm to IEC 60243-1, and comparative tracking index in the range of 400–600 V to IEC 60112, with the lower end associated with certain colourant or release-agent packages. Because unfilled PBT can absorb moisture, electrical values are measured at room temperature after standard conditioning; high-humidity exposure above 60% RH can reduce surface resistivity if condensation or ionic contamination is present.
In a substitution from a 30% glass-fibre PBT to the unreinforced 1401 F01, flexural modulus falls from approximately 9 GPa to 2.4 GPa, and tensile stress at yield declines from roughly 135 MPa to 55 MPa. Snap-fit arms, ribs, and gear teeth therefore require increased section height or revised geometry to avoid permanent set or brittle overload. At the same time, melt viscosity is lower, flow length improves, mould shrinkage becomes more isotropic, and the risk of warpage in flat rectangular parts is reduced. Glass-fibre scoring on unhardened tool steel gates, runners, and ejector pins is largely eliminated, which lowers tool maintenance frequency in long production runs. The trade-off is that unfilled PBT exhibits higher mould shrinkage and greater moisture sensitivity after moulding, so dimensional inspection must be delayed until the part reaches equilibrium moisture content. The table below summarises the comparative property envelope used for preliminary material selection; exact values must be confirmed from the producer’s current datasheet for the specific grade and test specimen type.
| Property | Test method | Toraycon® 1401 F01 unfilled PBT | 30% glass-fibre PBT reference |
|---|---|---|---|
| Density | ISO 1183 | 1.30–1.32 g/cm³ | 1.53–1.56 g/cm³ |
| Tensile stress at yield | ISO 527-2 | 50–60 MPa | 130–145 MPa |
| Tensile strain at break | ISO 527-2 | 25–50% | 2–3% |
| Flexural modulus | ISO 178 | 2.3–2.6 GPa | 8.5–9.5 GPa |
| Charpy notched impact | ISO 179-1/1eA | 3–6 kJ/m² | 7–10 kJ/m² |
| Heat deflection temperature at 1.80 MPa | ISO 75-2 | 55–65 °C | 200–215 °C |
| Mould shrinkage, flow direction | producer data | 1.7–2.3% | 0.2–0.5% |
Compliance documentation for the 1401 F01 grade must be requested from the producer for each production lot because regulatory status can change with colourants, stabilisers, and regional formulations. The base resin is generally assessed against RoHS Directive 2011/65/EU Annex II restrictions and REACH Regulation (EC) No 1907/2006 SVHC reporting at the article level. UL 94 classification is commonly HB at 0.8 mm and 1.5 mm; a V-0 requirement calls for a flame-retardant PBT grade rather than unfilled 1401 F01. For food-contact use, confirmation under the relevant 21 CFR section is required because published data specific to 1401 F01 in food simulants is limited. The grade is not recommended for continuous exposure to hot water above 60 °C, alkaline cleaning media above pH 9, or ethylene glycol coolants at elevated temperature, because ester linkages in the PBT backbone hydrolyse under such service conditions. Pre-drying is required when ambient relative humidity exceeds 60%, and sealed aluminium-lined bags should be opened only at the processing line to limit moisture uptake.