| HS Code | 527764 |
| Density | 1.31 g/cm³ |
| Water Absorption | 0.08 % |
| Tensile Strength | 50 MPa |
| Tensile Elongation At Break | 50 % |
| Flexural Strength | 80 MPa |
| Flexural Modulus | 2200 MPa |
| Charpy Notched Impact Strength | 6 kJ/m² |
| Rockwell Hardness | R115 |
| Heat Deflection Temperature At 0 45 Mpa | 150 °C |
| Heat Deflection Temperature At 1 82 Mpa | 60 °C |
| Melting Point | 225 °C |
| Mold Shrinkage | 1.5-2.0 % |
| Volume Resistivity | 1×10^16 Ω·cm |
| Dielectric Constant At 1 Mhz | 3.2 |
| Dissipation Factor At 1 Mhz | 0.002 |
| Arc Resistance | 120 s |
| Ul94 Flammability Rating | HB |
As an accredited Toray Toraycon® Tough Unreinforced PBT 5201X11 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-barrier bags, Toray Toraycon Tough Unreinforced PBT 5201X11 pellets are packed on pallets for industrial delivery. |
| Container Loading (20′ FCL) | Standard 20′ FCL container loaded with palletized, shrink-wrapped Toray Toraycon® Tough Unreinforced PBT 5201X11 resin, secured for export shipment. |
| Shipping | Toray Toraycon® Tough Unreinforced PBT 5201X11 ships as non-hazardous thermoplastic polyester resin pellets, typically in 25 kg moisture-barrier bags on pallets. Keep dry, avoid direct sunlight and moisture during transport and storage. Normal freight; not regulated for transport. |
| Storage | Store Toray Toraycon® Tough Unreinforced PBT 5201X11 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep in original sealed packaging; reseal opened bags or use dry containers with desiccant. Prevent contamination, observe shelf-life/FIFO, and follow the supplier SDS and local regulations. |
| Shelf Life | Toray Toraycon® Tough Unreinforced PBT 5201X11 typically has a two-year shelf life when stored unopened, cool, dry, and protected from moisture and sunlight. |
Competitive Toray Toraycon® Tough Unreinforced PBT 5201X11 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Toray Toraycon® Tough Unreinforced PBT 5201X11 is a polybutylene terephthalate injection-molding compound with an elastomer-modified, non-reinforced formulation. The model designation places it within the Toraycon PBT family while indicating a toughened grade free of glass fiber, carbon fiber, or mineral filler. The unfilled composition reduces anisotropic warpage associated with fiber orientation and produces lower tool abrasion than glass-reinforced materials. The trade-off is lower flexural and tensile modulus and lower heat deflection under load. Initial design properties should be evaluated under ISO 527-2 tensile testing, ISO 178 flexural testing, and ISO 180/A notched Izod impact testing, using specimens molded and conditioned according to ISO 294-1 and ISO 291. The as-molded density of this class is typically below 1.30 g/cm³ under ISO 1183-1.
The principal difference is notched impact response. In published class-level data, impact-modified unfilled PBT shows notched Izod values at 23 °C of 15 kJ/m² to 35 kJ/m², whereas general-purpose unfilled PBT often falls below 6 kJ/m². The improvement arises from dispersed elastomer domains that cavitate under triaxial stress and blunt crack propagation. The associated trade-off is stiffness. Unreinforced tough PBT typically exhibits tensile modulus from 1.6 GPa to 2.2 GPa, compared with 2.5 GPa to 2.8 GPa for unmodified PBT. Glass-fiber reinforced Toraycon grades reach tensile modulus values of 9 GPa to 11 GPa and can sustain 1.80 MPa load at heat deflection temperatures above 200 °C under ISO 75-2. The 5201X11 unfilled class remains below 60 °C under 1.80 MPa. The material is therefore selected where ductile failure, crack resistance after assembly, or quasi-isotropic shrinkage outweighs structural stiffness at elevated temperature.
The table classifies the 5201X11 grade within typical unfilled and glass-filled PBT property windows. The values are not product-specific batch limits and must be confirmed against the supplier certificate.
| Property class | Unreinforced tough PBT (5201X11 class) | General-purpose unreinforced PBT | 30% glass-fiber reinforced PBT |
|---|---|---|---|
| Density under ISO 1183-1 | 1.25–1.30 g/cm³ | 1.30–1.32 g/cm³ | 1.50–1.56 g/cm³ |
| Tensile strength under ISO 527-2 | 35–45 MPa | 55–65 MPa | 130–150 MPa |
| Tensile modulus under ISO 527-2 | 1.6–2.2 GPa | 2.5–2.8 GPa | 9.0–11.0 GPa |
| Notched Izod at 23 °C, ISO 180/A | 15–35 kJ/m² or partial no-break | 4–6 kJ/m² | 8–12 kJ/m² |
| Heat deflection temperature at 1.80 MPa, ISO 75-2 | 50–60 °C | 50–60 °C | 200–215 °C |
| Mold shrinkage, flow direction, ISO 294-4 | 1.2–2.0% | 1.5–2.0% | 0.3–0.8% |
Impact modification also changes melt viscoelasticity. Capillary rheometry on impact-modified unfilled PBT may show greater shear sensitivity than general-purpose PBT and lower die swell. Incoming inspection should track melt volume-flow rate under ISO 1133-1 at 250 °C and 2.16 kg, but acceptance limits must be taken from the product certificate of analysis rather than generic PBT literature.
Pre-drying is the first process-control point. The pellets are dried in a desiccant dryer at 120 °C for 4 h to 6 h, with a supply dew point below -40 °C. Target residual moisture before molding is below 0.02 wt% because hydrolytic chain scission at melt temperature reduces molecular weight and notched impact. On hydraulic injection molding machines with clamp forces between 80 t and 150 t, the unfilled melt has low shear heating; barrel-temperature uniformity therefore has greater influence than screw speed. A three-zone screw with a compression ratio around 2.5:1 and a free-flow check ring is commonly used. Extended residence time in the hot barrel can generate black specks in light-colored parts. If black specks appear, purging with an acrylic-based purge compound is more effective than raising the melt temperature. Silo storage should be sealed against atmospheric moisture, and open pellet containers should be returned to dry storage after shutdown.
Barrel settings should be controlled within ±5 °C of set point to reduce shot-weight drift and viscosity variation. The working melt-temperature window is 245 °C to 270 °C. The lower limit protects the elastomer phase from thermal degradation; the upper limit improves filling in thin sections. Mold surface temperatures should be maintained from 40 °C to 80 °C. Mold temperatures below 30 °C suppress crystallinity and can increase toughness but reduce modulus and dimensional stability after service heating. For wall thicknesses from 1.0 mm to 1.6 mm, fill times of 0.3 s to 1.5 s reduce gate-freeze risk and flow marks. Peak cavity pressures in multi-cavity tools are commonly observed between 60 MPa and 90 MPa. Holding pressure is typically set at 60% to 80% of peak cavity pressure, with transfer at approximately 95% fill volume. Hot-runner manifold temperatures are maintained from 250 °C to 265 °C. Gate diameter should be at least 60% of local wall thickness, and vent depths below 0.025 mm prevent flash. Screw cushion should remain stable within 2 mm to 3 mm; inconsistent cushion transfer is a common source of impact deviation.
Electrical connectors, sensor housings, relay bobbins, and automotive door-lock housings are representative application classes. The absence of glass fiber reduces differential dielectric heating and anisotropic warpage in multi-pin connectors. The comparative tracking index of unfilled PBT is commonly reported in the 500 V to 600 V range according to IEC 60112, though the exact value for 5201X11 should be confirmed by the supplier. Flammability class is typically UL 94 HB at 1.6 mm; if a V-0 rating is required, a flame-retardant Toraycon grade should be selected. Snap-fit designs benefit from the material’s ductility, but the low modulus means that cantilever arms should be short or tapered to limit deflection under load. Mold shrinkage in the flow direction is class-level 1.2% to 2.0% under ISO 294-4; transverse shrinkage may exceed this by 0.1% to 0.3%. Connector pin pitch must account for post-mold shrinkage before annealing.
Applications subjected to cold-start impacts in cold climates or occasional high-speed insertion force benefit from the toughened unfilled PBT class. General-purpose PBT can transition to brittle fracture near 0 °C, especially at sharp notches, molded-in stress, or elevated moisture. The 5201X11 modifier shifts the ductile-to-brittle transition downward, but the shift is thickness-dependent. In sections above 4 mm, spherulitic development in the thermal center can reduce impact toughness. Therefore, thick-walled parts should be prototyped with actual wall thickness and evaluated by drop-weight puncture according to ISO 6603-2. Knit lines constitute another limitation. Impact strength at a knit line may be 40% to 60% of the bulk value in unreinforced modified PBT. Raising melt temperature can improve knit-line strength but reduces residence-time safety margin. Published data for this specific configuration is limited, and end-use testing remains necessary.
Regulatory compliance cannot be assumed from the polymer family alone. For food-contact use, poly(tetramethylene terephthalate) may be covered by FDA 21 CFR 177.1660, but the impact modifier and processing aids require independent migration review. In the European Union, Regulation (EU) No 10/2011 sets overall and specific migration limits. RoHS Directive 2011/65/EU as amended by (EU) 2015/863 restricts lead, mercury, cadmium, hexavalent chromium, PBB, PBDE, and phthalates in homogeneous materials; certification for this grade must be obtained from the supplier. REACH Regulation EC 1907/2006 SVHC declarations should be requested for each production batch.
Hydrolysis is the dominant moisture-related degradation pathway. PBT is a polyester and undergoes ester-chain scission in hot water, humid air, and exposure to strong bases. The impact-modified unfilled grade should not be used for continuous hot-water immersion above 60 °C without validation. Moisture uptake in the elastomer phase may increase the time to saturation but can also increase hydrolysis at the phase boundary. Under weathering, surface chalking and loss of gloss can occur, and UV-induced embrittlement may reduce notched impact. Formulations may contain UV stabilizers, but their presence must be confirmed on the supplier datasheet. Chemical resistance testing for automotive fluids should follow ISO 1817 or ASTM D543. Hydrocarbon oils are often less aggressive than hot glycol/water mixtures, but specific additives and oxidized fuel blends can extract or swell the impact modifier. Amine-based processing aids or color concentrates should not be used without supplier verification because they can accelerate ester-chain scission.
Post-industrial regrind from sprues and runners can be incorporated at levels below 15 wt% to 20 wt%. Higher regrind fractions reduce viscosity and notched impact. Regrind should be dried before blending with virgin pellets. Tooling should use generous draft angles, typically above 0.5° per side, and textured cavity surfaces to prevent sticking. Ejection pins should be large and well-distributed because the unfilled material is softer than glass-filled PBT. Vent depths are usually below 0.025 mm to avoid flash; insufficient venting can produce burn marks at the end of fill and reduce knit-line strength.
Short-term thermal excursions up to 120 °C in dry air can be tolerated by PBT, but continuous exposure at that temperature accelerates oxidative degradation of the impact modifier. Long-term continuous use is better limited to approximately 80 °C to 100 °C unless supported by endurance testing. Differential scanning calorimetry under ISO 11357-3 typically shows the PBT melting peak at approximately 225 °C at 10 K/min. The material should not remain at temperatures above 280 °C during processing or service. Contact with automotive transmission fluids and engine oils is often acceptable in short-term tests, but the specific fluid and additive package must be validated. The combination of hot glycol and water is more damaging than most hydrocarbon fluids. Parts requiring continuous underhood structural load at high temperature are usually better served by glass-filled Toraycon grades.