| HS Code | 925844 |
| Density G Cm3 | 1.20 |
| Water Absorption 24h Percent | 0.08 |
| Linear Mold Shrinkage Percent | 1.5-2.0 |
| Tensile Strength Mpa | 45 |
| Elongation At Break Percent | >100 |
| Flexural Strength Mpa | 65 |
| Flexural Modulus Mpa | 1800 |
| Notched Izod Impact Kj M2 | 40 |
| Heat Deflection Temperature 1 82 Mpa C | 60 |
| Melting Point C | 225 |
| Volume Resistivity Ohm Cm | 1E16 |
| Dielectric Constant 1 Mhz | 3.2 |
| Dielectric Strength Kv Mm | 20 |
| Flammability Ul94 | HB |
As an accredited Toray Toraycon® Tough Unreinforced PBT 5201X10 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-proof, polyethylene-lined bags, Toray Toraycon® Tough Unreinforced PBT 5201X10, palletized for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL loading for Toray Toraycon® Tough Unreinforced PBT 5201X10: palletized bags in dry container, ambient conditions, secured stowage. |
| Shipping | Shipping description: Toray Toraycon® Tough Unreinforced PBT 5201X10, polybutylene terephthalate resin pellets, non-hazardous, not regulated for transport (no UN number, class, or packing group). Packaged in moisture-barrier bags/containers; keep dry, cool, away from direct sunlight. Use standard industrial handling and confirm local regulations/SDS before shipment. |
| Storage | Store Toray Toraycon® Tough Unreinforced PBT 5201X10 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, moisture, and incompatible chemicals. Keep original packaging sealed and palletized; protect from physical damage and contamination. Use first-in, first-out stock rotation. If packaging is opened, reseal promptly and dry the resin according to Toray’s processing recommendations before use. |
| Shelf Life | Toraycon PBT 5201X10 typically has a 12-month shelf life in original unopened packaging stored cool, dry, and moisture-protected; confirm with Toray. |
Competitive Toray Toraycon® Tough Unreinforced PBT 5201X10 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Toray Toraycon® Tough Unreinforced PBT 5201X10 is an unfilled polybutylene terephthalate grade whose designation identifies a toughness-modified material within the broader Toraycon PBT portfolio. The formulation is intended for injection-moulded components in which notch sensitivity and multiaxial impact failure are the primary mechanical risks, but where glass-fibre reinforcement is excluded to preserve wall-thickness uniformity and eliminate abrasive tool wear. Under ISO 527-2 tensile testing, unfilled toughness-modified PBT of this class typically exhibits yield stress in the 50–55 MPa band and elongation at yield or break exceeding 30%; the exact lot-specific values for 5201X10 are governed by the supplier’s certificate of analysis rather than by generic datasheet ranges. Relative to a standard unreinforced PBT, the grade sacrifices some tensile modulus for higher notched impact energy. Relative to a 30% glass-fibre-reinforced Toraycon grade, it provides lower stiffness but substantially more uniform shrinkage and reduced warpage in flat connectors, sensor housings, and snap-fit latch bodies. Because the elastomeric modifier is present as a discrete dispersed phase, the material retains the rapid crystallisation and chemical resistance associated with the PBT backbone rather than behaving as a fully miscible blend.
In processing, the product requires closed-loop moisture control. PBT is subject to hydrolytic chain scission at melt temperature, and the toughness-modified grade is particularly sensitive because molar mass retention is directly linked to impact performance. Before injection moulding, pellets are dried in a dehumidifying hopper dryer at 120–130 °C for 4–6 h, with inlet air dew point below −30 °C. A residual moisture content below 0.02 wt% is required for sustained impact performance; lots exposed to 60% relative humidity without closed packaging can reabsorb surface moisture within 30–60 min. The melt is maintained at 245–260 °C measured at the nozzle, and barrel residence time should not exceed 8 min for natural or light-coloured material because thermally initiated ester cleavage reduces molecular weight and creates volatile degradation products. These limits are derived from production-scale injection moulding behaviour of unfilled toughness-modified PBT and should be confirmed against the current Toray processing guide for 5201X10.
The melt volume-flow rate of 5201X10 under ISO 1133-1 at 250 °C and 2.16 kg is lower than that of general-purpose unreinforced Toraycon PBT grades, reflecting the high-molecular-weight polyester backbone and the presence of the elastomeric phase. Capillary rheometry performed at 260 °C on the dry pellet typically shows apparent viscosity of the product class decaying from 300–500 Pa·s at 100 s⁻¹ to less than 100 Pa·s above 1000 s⁻¹; however, published capillary data for grade 5201X10 specifically should be checked against the latest Toray technical datasheet. For mould-filling analysis, the material can be treated as a pseudoplastic polymer with a melt density near 1.15 g/cm³ and a no-flow temperature in the 210–215 °C band. Shear-thinning behaviour is sufficient to fill thin-wall sections down to 0.4 mm when adequate injection velocity is maintained, but the lower thermal diffusivity of the impact modifier slows solidification in thick sections and can extend required cooling time by 10–20% compared with standard unfilled PBT.
Injection moulding conditions for 5201X10 on a conventional reciprocating screw machine with an L/D of 18–22 and a compression ratio of 2.0–2.5:1 are typically set with a rear zone at 230–240 °C, a centre zone at 245–255 °C, and a front zone at 250–260 °C. The mould is held at 40–80 °C; the lower range improves cycle time, while the upper range improves weld-line strength and surface appearance. A hydraulic back pressure of 0.3–0.7 MPa is applied to homogenise the melt without excessive shear heating. Screw surface speed is maintained between 0.15 m/s and 0.35 m/s. The cushion distance is held at 3–6 mm to avoid cushion loss and short shots. For hot-runner systems, the manifold temperature is kept within 245–260 °C, and the thermal gate tip should not exceed 270 °C to avoid local polymer degradation. These conditions are consistent with standard unfilled PBT practice and may require adjustment when the mould contains long flow paths, thin hinges, or multi-stage injection profiles.
Substitution of a 30% glass-fibre-reinforced Toraycon PBT with 5201X10 is justified only where impact resistance and warpage control outweigh stiffness loss. Under ISO 178, the flexural modulus of the unreinforced tough grade is approximately one-third to one-quarter that of a 30% glass-filled PBT; the exact ratio depends on fibre length, fibre sizing, and processing shear. This reduction in modulus lowers the load-bearing capacity of snap-fit beams and requires an increase in beam thickness or width when deflection force must remain constant. Conversely, the unreinforced grade eliminates fibre orientation-induced differential shrinkage that causes warpage in complex parts with multiple gates. Moulded connectors show more isotropic shrinkage when measured after 48 h at 23 °C; unpacked tool-shrinkage values for this product class generally lie in the 1.2–1.8% range in the flow direction and 1.5–2.0% in the transverse direction. Published values for the specific 5201X10 formulation should be used for steel-cut tooling, because the dispersed elastomer phase reduces crystallisation rate slightly and can shift shrinkage relative to unmodified PBT.
| Property | Test method | Tough unreinforced PBT class | Standard unreinforced PBT class | 30% glass-fibre PBT class |
|---|---|---|---|---|
| Density | ISO 1183-1 | 1.30–1.32 g/cm³ | 1.31–1.33 g/cm³ | 1.52–1.55 g/cm³ |
| Tensile stress at yield | ISO 527-2 | 50–55 MPa | 55–60 MPa | 130–150 MPa |
| Flexural modulus | ISO 178 | 2.1–2.4 GPa | 2.4–2.7 GPa | 8.5–10.5 GPa |
| Notched Charpy impact | ISO 179-1/1eA | 7–10 kJ/m² | 3–5 kJ/m² | 8–11 kJ/m² |
| Heat deflection temperature at 1.8 MPa | ISO 75-2 | 55–65 °C | 60–70 °C | 200–210 °C |
The unfilled nature of 5201X10 preserves the chemical resistance of PBT to aliphatic hydrocarbons, automotive fuels at moderate temperature, and many cleaning agents, but the elastomeric modifier reduces resistance to hot water and strong acids relative to the unmodified polyester. Continuous exposure to aqueous glycol at 120 °C may hydrolyse the PBT matrix and should be validated by immersion testing under ISO 175 for the intended fluid, concentration, and temperature. The product is not recommended for prolonged contact with steam, concentrated sulfuric acid, or alkaline solutions exceeding pH 9 at elevated temperature. When used in under-hood environments, continuous load-bearing service temperature should not exceed 120 °C, with excursions to 140 °C permitted only for short-term non-load cases. These limits are based on the oxidative stability of PBT and should be confirmed with the specific stabilisation package used in the 5201X10 formulation.
For low-voltage electrical connectors, 5201X10 provides sufficient dielectric strength and arc resistance for many applications below 60 V but is not a substitute for flame-retarded Toraycon grades where regulatory ignition resistance is required. Typical unfilled PBT in this product class shows dielectric strength by IEC 60243-1 in the 15–20 kV/mm range for 2 mm plaques and a comparative tracking index by IEC 60112 in the 250–300 V band. The product is generally classified UL 94 HB at 0.8 mm thickness; if end-use standards require UL 94 V-0 at 0.8 mm, a flame-retarded grade such as Toraycon 1401X06 should be evaluated instead. The elastomer phase can lower tracking resistance relative to that of a non-toughened unfilled PBT, so application-specific tracking tests are warranted for connector spacing below 2 mm.
For parts moulded from 5201X10, knit-line strength is controlled by melt temperature at the flow front, mould temperature, and the pause time between flow fronts. When a double-gated tensile bar is moulded under ISO 527-2, the weld-line strength retention can fall to 50–70% of the virgin tensile strength if the mould temperature is below 40 °C; raising the mould to 80 °C and reducing flow-front hesitation can recover some of this loss. Published data for grade 5201X10 in this specific configuration is limited, so tooling trials are required before relying on weld-line strength in structural features. Gate location should be moved away from high-stress regions and placed to orient weld lines along low-stress paths. For multi-cavity tools, the runner system should be naturally balanced; artificially balanced runners may produce different shear heating between cavities and widen the scatter of filling behaviour because the tough grade has a lower melt-flow index than standard unfilled PBT. Direct edge gates or tab gates are preferred over pin gates in thick sections because the impact modifier increases melt elasticity and can cause gate blush or post-gate surface irregularities if the gate freezes too quickly. A gate land length of 0.5–1.0 mm and a gate thickness of 50–70% of the nominal wall thickness are typical starting values.
| Requirement | Standard or directive | Typical status for 5201X10 |
|---|---|---|
| Restriction of hazardous substances | RoHS 2011/65/EU | Below threshold levels; supplier certification required for each lot |
| SVHC communication | REACH 1907/2006, Article 33 | No listed SVHC above 0.1 wt% based on supplier documentation |
| Flammability classification | UL 94 | HB at 0.8 mm; not classified V-0 |
| Melt mass-flow or melt volume-flow rate | ISO 1133-1 | Lot-to-lot control by supplier; exact range on certificate of analysis |
| Tensile property verification | ISO 527-2 | Supplier lot testing or user incoming inspection recommended |
Storage of 5201X10 before moulding should be in sealed, moisture-barrier containers at 10–30 °C. Once the original package is opened, the remaining material should be re-dried before use if ambient humidity exceeds 50%. Regrind from sprues and runners can be added at 15–20 wt% without systematic loss of tensile properties when the regrind is dry and generated under the same thermal history; higher regrind fractions may reduce notched impact energy because the elastomeric modifier can undergo morphology changes during repeated shear. Vacuum drying is not required if the dehumidifying dryer dew point is maintained below −30 °C. In colour-critical applications, regrind should be omitted because the heat history discolours the unfilled resin slightly, and the yellowness index should be measured against the supplier’s original moulded-plaque reference under a controlled method. Parts requiring dimensional certification should be conditioned at 23 °C and 50% relative humidity for at least 48 h before metrology, because the low but non-zero moisture uptake of PBT can shift small feature dimensions by several micrometres per millimetre of wall thickness in uncontrolled ambient conditions.