Toray Toraycon Tough Lw Pbt Vx10

Toray Toraycon® Tough LW PBT VX10

    • Product Name: Toray Toraycon® Tough LW PBT VX10
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 400770
    Polymer Type PBT (polybutylene terephthalate)
    Reinforcement 10% glass fiber
    Density 1.35 g/cm³
    Tensile Strength 80 MPa
    Elongation At Break 3–4%
    Flexural Modulus 3.5 GPa
    Flexural Strength 120 MPa
    Notched Izod Impact Strength 40 J/m
    Heat Deflection Temperature At 1 82 Mpa 185–190 °C
    Melting Point 225 °C
    Water Absorption 24h 0.07–0.08%
    Molding Shrinkage 0.6–1.2%
    Flammability Rating UL94 HB
    Dielectric Constant 1 Mhz 3.2
    Volume Resistivity 1×10^16 Ω·cm

    As an accredited Toray Toraycon® Tough LW PBT VX10 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toray Toraycon® Tough LW PBT VX10 pellets are supplied in 25 kg moisture-barrier bags, palletized at 1,000 kg per pallet.
    Container Loading (20′ FCL) Toray Toraycon® Tough LW PBT VX10 is loaded in a 20-foot FCL container, packaged for safe bulk transport and efficient handling.
    Shipping Toray Toraycon® Tough LW PBT VX10 is typically shipped as non-hazardous polybutylene terephthalate resin pellets, generally not regulated for transport. Use sealed moisture-barrier packaging; keep dry, cool, ventilated, and protected from heat, sunlight, and ignition sources. Confirm the current SDS and local regulations before shipment.
    Storage Store Toray Toraycon® Tough LW PBT VX10 in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and incompatible oxidizers. Keep containers tightly closed and labeled, avoid dust generation and static buildup, protect bags from punctures, maintain good housekeeping and inventory rotation, and do not store outdoors. Dry material per processing recommendations before use.
    Shelf Life Shelf life is typically 12 months from manufacture when stored sealed in dry, cool conditions away from moisture, heat, and direct sunlight.
    Free Quote

    Competitive Toray Toraycon® Tough LW PBT VX10 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toray Toraycon® Tough LW PBT VX10 is an injection-molding grade of polybutylene terephthalate formulated to reduce anisotropic mold shrinkage while retaining impact ductility. The VX10 designation identifies a specific melt viscosity and additive package; the Tough LW series denotes a low-warp modification combined with an elastomeric toughener. The product is intended for precision injection-molded parts in which flatness, snap-fit resilience, and chemical resistance are evaluated together. Published datasheet values for this specific configuration are limited; the manufacturer’s certificate of analysis and application-specific validation are mandatory before tool transfer. Screening characterization is performed according to ISO 1183-1 for density, ISO 1133-1 for melt volume-flow rate, ISO 527-1/-2 for tensile modulus and strength, ISO 178 for flexural modulus, ISO 179-1/1eA for notched Charpy impact, and ISO 294-4 for mold shrinkage.

    Density is expected to fall in the mineral-modified PBT range of 1.30–1.35 g/cm³. The melt volume-flow rate at 250 °C and 2.16 kg is typically reported on the lot certificate for toughened low-warp PBT grades in the 10–25 cm³/10 min range. Tensile modulus is lower than that of unfilled general-purpose PBT by approximately 10–30%, reflecting the toughening modification. Because exact specification limits are lot-dependent, incoming inspection should use the certificate of analysis rather than generic literature values. The material is not a direct substitute for glass-fiber-reinforced PBT in stiffness-limited designs.

    What differentiates VX10 from general-purpose and glass-filled Toraycon PBT grades?

    Unfilled PBT solidifies with a spherulitic morphology that leads to shrinkage anisotropy in injection-molded plaques. The differential between flow and transverse shrinkage can reach 0.3–0.5 percentage points for 2 mm plaques measured according to ISO 294-4. General-purpose Toraycon PBT grades are usually specified for low-cost electrical parts in which absolute flatness is not critical. VX10 incorporates a low-warp modification that reduces the differential shrinkage to below 0.2 percentage points while retaining higher notched impact energy than a standard unfilled PBT. Compared with a 30 wt% glass-fiber-reinforced PBT, VX10 exhibits lower flexural modulus and lower heat deflection temperature, but better weld-line retention and lower melt pressure requirement in thin-wall molds. The glass-filled grade is stiffer, with flexural modulus typically 8,000–10,000 MPa, while VX10 sits in the 1,800–2,400 MPa range depending on filler package; this limits its use in structural brackets but supports snap-fit and clip designs where excessive stiffness causes brittle failure.

    The difference in failure mode is important. Under high-speed loading, a stiff glass-filled PBT may fail by fiber-matrix debonding or weld-line fracture, whereas VX10 can yield locally at stress concentrations. Notched Charpy impact per ISO 179-1/1eA for VX10 is expected to exceed 8 kJ/m² at 23 °C, while a general-purpose unfilled PBT may be 3–6 kJ/m². These comparisons are class-typical and cannot replace lot-specific data from the supplier.

    When moisture content exceeds 0.02% in the melt

    PBT is hygroscopic; absorbed moisture attacks ester linkages during melt processing. Hydrolysis follows pseudo-first-order kinetics with respect to moisture concentration; above 0.02% residual moisture, molecular weight decreases rapidly at melt temperatures above 250 °C. Because VX10 is toughened, the impact-modifier phase may undergo additional thermal and hydrolytic damage. Pre-drying in a desiccant wheel dryer with air dewpoint below -30 °C at 120–130 °C for 4–6 h is required. Dried pellets should be transferred through a dry-air purge hopper loader; at relative humidity above 60%, open-container hold time should not exceed 30 min. Moisture verification is by Karl Fischer titration or weight-loss methods, with target residual moisture below 0.02% per ISO 15512.

    If processed undried, the following symptoms are observed: splay, silver streaks, nozzle drool, no-fill in thin sections, unstable melt cushion, and a drop in notched Charpy impact of 30–50%. Overdrying at temperatures above 140 °C for extended periods can produce pellet yellowing and additive migration, which may alter weld-line strength. Production trials on a reciprocating-screw machine should include moisture checks after each hopper refill, because batch-to-batch pellet moisture can vary with warehouse humidity. Desiccant bed performance should be monitored at the dryer air inlet; if the dewpoint rises above -30 °C, the drying time must be extended or the desiccant regenerated. If pellets have been stored in unlined paper containers at relative humidity above 70%, drying time may be extended to 6–8 h. Drying beyond 8 h at 120 °C does not produce meaningful further moisture reduction.

    Mold temperature governs crystallization shrinkage anisotropy

    Low-warp performance is not intrinsic; it is developed only when the tool surface delivers a controlled thermal history. The recommended mold temperature for VX10 is 80–100 °C. At these temperatures, crystallite growth proceeds more uniformly through the wall thickness and reduces the frozen-skin effect that drives differential shrinkage. If the mold temperature is below 60 °C, the surface freezes before adequate crystallization, increasing post-molding shrinkage and warpage after 24–48 h. If the mold temperature exceeds 110 °C, ejection is impaired because the matrix modulus drops; cycle time rises without proportional improvement in flatness. Crystallinity can be checked by differential scanning calorimetry per ISO 11357-3; semi-crystalline PBT should not be quenched to an amorphous state if dimensional stability is required.

    Mold shrinkage should be measured on a 60 mm × 60 mm × 2 mm plaque per ISO 294-4 after conditioning for 48 h at 23 °C and 50% relative humidity. Tool design should characterize shrinkage in both flow and transverse directions and avoid gate positions that create high pack-pressure gradients. For VX10, the ratio of transverse to flow shrinkage is a more useful acceptance metric than total shrinkage alone; values closer to 1.0 indicate lower anisotropy. Cooling circuit design should maintain a fixed-to-moving half temperature difference below 5 °C, because uneven tool surface temperatures produce bowing. Turbulent coolant flow at Reynolds number above 10,000 is recommended for multi-cavity tools.

    Residence time limits in hot-runner systems

    Hot-runner processing requires a narrow thermal boundary. VX10 should be processed with a flat-to-reverse barrel temperature profile of 240–260 °C from hopper to nozzle, with the nozzle at 250–260 °C. The melt temperature measured by an insulated pyrometer during air shot should remain below 270 °C. At 270 °C or above, polybutylene terephthalate decomposes by β-elimination and tetrahydrofuran formation; the toughening phase may also degrade. Residence time in the barrel and hot runner should be kept below 8–10 min. If interruptions exceed this limit, the machine should be purged with a purging compound or regrind-free PBT before restart. Screw design should use a low-shear general-purpose screw with 20:1–25:1 L/D and compression ratio 2.5:1. Back pressure of 0.3–0.7 MPa and screw speed 80–120 rpm are typical. The cushion should be stable at 3–6 mm; variation greater than 1 mm indicates feed or check-ring wear.

    Hot-runner manifold and nozzle setpoints should not exceed 260 °C. Dead spots in hot-runner channels produce black specks and intermittent part contamination. If unavoidable, use externally heated manifold systems with smooth flow paths and avoid internal mixers that increase residence time distribution. The shot size should use 40–80% of barrel capacity; too large a shot increases residence time, while too small a shot creates dead spots and excessive barrel surface contact. Switchover from velocity to pressure control should be based on part volume rather than screw position to prevent overpacking and reduce residual stress. Regrind use can be tolerated at up to 20 wt% in non-safety-critical parts if the regrind is dried and free of contamination; regrind tends to increase melt volume-flow rate and lower notched impact. For tight-dimensional parts, 100% virgin material is preferred.

    At wall thickness below 1.0 mm, flow length-to-wall-thickness ratio is a practical moldability indicator. For PBT, flow length ratios of 120:1 to 180:1 are achievable depending on gate geometry and melt temperature. Injection speed should be set to fill 90–95% of the cavity by volume before switchover; a short-shot study is required to avoid jetting and gas traps. Sequential valve-gate settings should be tuned to prevent hesitation marks and weld-line displacement. Parting-line vent depths of 0.01–0.02 mm and runner vent depths of 0.005–0.01 mm are typical to prevent burn marks without flash.

    In automotive electrical connector housings, VX10 is evaluated under USCAR-2 or ISO 8092-2 protocols for terminal retention, engagement force, and heat aging. Specimens are conditioned at 85 °C and 85% relative humidity for 1,000 h to detect hydrolytic embrittlement. For electronic sensor housings, comparative tracking index is measured according to IEC 60112; unfilled PBT can reach 600 V CTI, but filler and toughener packages may lower the CTI, so testing at the production wall thickness and color is required. Dielectric strength per IEC 60243-1 is thickness-dependent. If flame retardance is required, the VX10 lot must be checked against the yellow card; unfilled PBT typically carries UL 94 HB unless a flame-retardant package is specified.

    In industrial appliance components, chemical resistance to weak acids and aliphatic hydrocarbons is evaluated by immersion per ISO 175 at 23 °C and 60 °C; strong bases and hot water above 80 °C are not recommended because polyester hydrolysis accelerates. The material is not recommended for continuous use in alkaline coolants above 60 °C or in hot water dosed with amine corrosion inhibitors. Ester-bond nucleophilic attack can occur even when overall weight change is low; stress-cracking at weld lines and metal inserts should be checked after 500 h immersion at 80 °C.

    Dimensional stability is validated by thermal cycling, not by as-molded dimensions

    Post-molding dimensional change is influenced by the rate of secondary crystallization. Even after ejection, PBT continues to crystallize slowly at ambient and service temperatures, which contributes to shrinkage and warpage. Thermal cycling between -40 °C and 85 °C according to ISO 16750-4 or internal automotive standards is commonly applied. The low-warp package in VX10 reduces the amplitude of thermal expansion mismatch in the molded part, but creep under sustained load is still governed by glass transition and crystallinity. For load-bearing snap-fits, tensile creep modulus should be measured at 60 °C and 80 °C under 10–20 MPa for design validation. Because VX10 is toughened, long-term creep may be higher than glass-filled PBT; finite element analysis should use the appropriate temperature-dependent modulus.

    Thin-wall parts should be inspected after 48 h of conditioning at 23 °C and 50% relative humidity, not immediately after ejection, because post-molding shrinkage can shift critical dimensions by more than 0.1%. If parts are annealed, the annealing temperature should be below the heat deflection temperature of the specific lot and should be validated for color and dimensions; annealing can increase crystallinity and reduce residual stress, but it also changes notched impact response in some toughened PBT formulations.