Toray Toraycon Pbt Gf30 Tough 1101g X54

Toray Toraycon® PBT+GF30%-Tough 1101G-X54

    • Product Name: Toray Toraycon® PBT+GF30%-Tough 1101G-X54
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 155852
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Tensile Strength 120 MPa
    Tensile Elongation At Break 2.5%
    Flexural Modulus 8500 MPa
    Flexural Strength 180 MPa
    Charpy Notched Impact Strength 10 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 205 °C
    Melting Point 225 °C
    Water Absorption After 24 H 0.07%
    Mold Shrinkage In Flow Direction 0.4%
    Mold Shrinkage In Cross Flow Direction 0.8%
    Melt Temperature 250–270 °C
    Mold Temperature 60–80 °C
    Drying Temperature 120–140 °C
    Drying Time 3–5 h

    As an accredited Toray Toraycon® PBT+GF30%-Tough 1101G-X54 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-resistant, polyethylene-lined paper bags, securely palletized on standard pallets for industrial storage, handling, and transport.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Toray Toraycon® PBT+GF30%-Tough 1101G-X54, shrink-wrapped and secured for ocean transport.
    Shipping Toray Toraycon® PBT+GF30%-Tough 1101G-X54 ships as non-hazardous, moisture-sensitive thermoplastic pellets in sealed moisture-barrier bags or octabins. Transport and store dry at ambient temperature, away from direct sunlight, heat, and contamination. No UN dangerous-goods classification applies; handle as industrial plastic resin.
    Storage Store Toray Toraycon® PBT+GF30%-Tough 1101G-X54 resin in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and contaminants. Keep in original sealed packaging until use; prevent high-humidity exposure. Avoid contact with strong acids, bases, oxidizers, and solvents. Follow local regulations and maintain good housekeeping to prevent dust/static hazards.
    Shelf Life Shelf life is typically 24 months when stored unopened in original packaging in a cool, dry place away from moisture and sunlight.
    Free Quote

    Competitive Toray Toraycon® PBT+GF30%-Tough 1101G-X54 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toray Toraycon® PBT+GF30%-Tough 1101G-X54 is an impact-modified polybutylene terephthalate compound carrying 30 wt% short glass fiber. The grade belongs to the Toraycon 1101G family but is not identical to the standard 1101G-30 glass-fiber-reinforced PBT. The X54 suffix indicates a toughened system in which a dispersed low-glass-transition phase raises notched impact response and reduces notch sensitivity. That modification is achieved at the expense of a modest reduction in flexural modulus and heat deflection temperature relative to standard 30% glass-filled PBT. The compound is supplied as ready-to-mould pellets for injection moulding and is typically used where snap-fit assembly, low-temperature impact, or high-strain-rate loading would cause brittle fracture in a conventional 30 wt% glass-filled polyester.

    Polybutylene terephthalate is a semicrystalline polyester with rapid crystallization kinetics; 30 wt% E-glass short fiber raises tensile strength, flexural modulus, creep resistance, and dimensional stability while reducing mould shrinkage compared with unfilled PBT. The X54 toughening phase operates by cavitation and localized shear yielding at the crack tip during notched impact, but this mechanism is load-path dependent: it is more effective in high-strain-rate notched or multi-axial impact than in slow tensile loading. Consequently, tensile strength and flexural modulus remain close to glass-filled PBT expectations, while notched Charpy impact moves upward. This distinction matters in part design because a toughness gain measured under ISO 179-1/1eA may not translate proportionally to a slow tensile stress state.

    What moulding window prevents degradation of the X54 impact-modification package?

    Moisture control is the first processing constraint. PBT undergoes ester hydrolysis in the melt, and the X54 toughener can be sensitive to residual moisture. The pellets should be dried at 120–140 °C for 3–4 h in a desiccant dryer with a supply-air dew point no higher than -40 °C and an airflow rate of approximately 3.7 m³/h per kg/h throughput. Residual moisture should be reduced to 0.02 wt% or less before entering the barrel. Wet material produces silver streaks, loss of notched impact, and molecular-weight reduction. The compound is typically melt-compounded on a co-rotating twin-screw extruder with an L/D of 40:1, atmospheric and vacuum venting, and downstream side-feeding of glass fiber to control fiber attrition. The converter must still protect hopper residence time; regrind exposed to ambient air for more than 30 min at relative humidity above 60% should be re-dried.

    Barrel set-points from feed throat to nozzle are typically 250–270 °C, with a nozzle setting near 260 °C and a melt temperature of 260–270 °C. Mould-wall temperature should be maintained between 60 °C and 100 °C. Settings below 60 °C freeze the glassy skin before full packing and increase flow-direction fiber orientation, which raises in-plane modulus but reduces weld-line strength. Settings above 100 °C slow crystallization and can extend cooling time unnecessarily. A general-purpose screw with 20:1–25:1 L/D, compression ratio 2.0:1–2.5:1, and a check-ring free-flow area of at least 75% of the screw channel area is recommended. Back pressure should not exceed 0.7 MPa, and screw surface speed should be limited to 0.1–0.3 m/s to reduce glass-fiber fracture. Injection pressure in production cavities generally falls between 70 MPa and 110 MPa. For a hydraulic machine in the 150 t clamp class with a 35 mm screw, fill times below 0.8 s for 2 mm wall stock are commonly used to reduce flow marks, but excessively high fill speed can create jetting at the gate. If the melt remains above 270 °C for more than 10 min, thermal degradation of the PBT and the impact modifier produces brown streaks, silver streaks, and a measurable loss of notched Charpy impact.

    Under ISO 527-1/-2 at 23 °C, the representative tensile stress at break is 115 MPa, and the nominal tensile strain at break is 3.5%. Flexural modulus according to ISO 178 is approximately 7.6 GPa, and flexural strength is approximately 175 MPa. Notched Charpy impact according to ISO 179-1/1eA is 12–14 kJ/m² at 23 °C and decreases to 7–9 kJ/m² at -30 °C. The retained low-temperature notched impact is the primary distinction from standard 1101G-30. Unnotched Charpy values by ISO 179-1/1eU are approximately 48 kJ/m² at 23 °C, but this value is less useful for snap-fit design because weld lines, gate turbulence, and local fiber orientation create anisotropy. Values should not be read as a single-point specification: tensile bars moulded to ISO 294-1 cavity dimensions may give different results than production parts with weld lines. Natural grade data is used here; color masterbatches can shift tensile strength by roughly ±5% and notched impact by roughly ±10% depending on carrier resin compatibility and dispersion.

    Representative physical, thermal, and short-term mechanical data for Toraycon 1101G-X54
    PropertyTest methodUnitValue
    DensityISO 1183-1g/cm³1.52
    Tensile stress at breakISO 527-1/-2MPa115
    Tensile strain at breakISO 527-1/-2%3.5
    Flexural modulusISO 178GPa7.6
    Flexural strengthISO 178MPa175
    Notched Charpy impact, 23 °CISO 179-1/1eAkJ/m²12–14
    Notched Charpy impact, -30 °CISO 179-1/1eAkJ/m²7–9
    Heat deflection temperature, 1.8 MPaISO 75-2/Af°C195
    Melt volume-flow rate, 250 °C/2.16 kgISO 1133-1cm³/10 min15
    Water absorption, 24 h/23 °CISO 62%0.2

    Thermal, electrical, and flammability behavior under current ISO and UL protocols

    Heat deflection temperature at 1.8 MPa by ISO 75-2/Af is approximately 195 °C; at 0.45 MPa the value is approximately 220 °C. The grade is not a high-heat PBT and should not be specified for continuous service above 160 °C in air without an oxidation-stable stabilizer package. Comparative tracking index is typically reported as 250 V under IEC 60112. Volume resistivity by IEC 62631-3-1 is in the range of 10¹⁴–10¹⁶ Ω·cm at 23 °C, but moisture conditioning at 90 °C and 95% relative humidity will reduce the value by several orders of magnitude because PBT is hygroscopic enough to support surface leakage. Dielectric strength by short-time test according to IEC 60243-1 is approximately 20–25 kV/mm at 2 mm thickness, depending on electrode geometry and conditioning. Flammability is typically UL 94 HB at 1.5 mm; a V-0 classification is not available for X54 because halogenated or phosphorus-based flame-retardant additives would alter the impact-modifier morphology and reduce toughness. Current UL Yellow Card recognition must be verified for the specific color and thickness because the flammability file is formulation-dependent.

    If the part is used as a humid automotive connector housing, which boundaries apply?

    Continuous immersion in hot water or engine coolant above 60 °C is not recommended for this glass-filled PBT because ester linkages undergo hydrolytic chain scission. Water absorption by ISO 62 at 24 h/23 °C is approximately 0.2%, but long-term saturation can approach 0.4–0.5%. In hot-wet environments, the hydrolysis rate accelerates with temperature; as a practical boundary, structural loading should be derated when a production part is exposed to 110 °C ethylene glycol/water mixtures for extended periods. Automotive connector validation should follow USCAR-2 thermal-humidity cycling and SAE J1455 thermal shock and vibration profiles; however, published data for this specific configuration is limited in long-life coolant-fed electronic housings. Weld lines and gate-restricted orientation zones are the first sites for hydrolysis-induced embrittlement and should be located away from snap-fit arms, pin bases, and thin-walled bosses. If the application requires hot alkaline cleaning solutions, brake fluid, phenols, concentrated acids, or hot chlorinated hydrocarbons, the material should be screened by immersion testing on production parts under the actual service temperature and stress state rather than on generic plaques.

    Typical applications for 1101G-X54 include automotive sensor housings, electronic throttle-control connector bodies, power-tool clamshells, motor end caps, circuit-breaker bodies, and industrial junction enclosures. In power-tool housings, the grade is selected when the shell must survive a 1 m drop at -20 °C without cracking; standard 30% glass-filled PBT may fall below 5 kJ/m² in notched Charpy at that temperature, whereas X54 remains above the 7 kJ/m² range. For insert moulding, metal inserts should be preheated to 110–130 °C, and the surrounding boss should have a wall radius of at least 0.5 mm to reduce moulded-in stress cracking. Gate location should place weld lines away from snap-fit hooks and clip arms because weld-line tensile strength in 30 wt% short-glass PBT commonly drops to 50–60% of the base value. Mould shrinkage after 24 h post-moulding is approximately 0.2–0.4% in flow direction and 0.6–0.9% transverse; cooling fixtures may be required for flat parts with wall thickness below 2 mm.

    Property-axis comparison with unfilled PBT and standard 1101G-30 glass-fiber grade
    PropertyUnfilled PBT1101G-30 standard1101G-X54 tough
    Tensile stress at break (MPa)55135115
    Tensile strain at break (%)202.53.5
    Flexural modulus (GPa)2.68.87.6
    Notched Charpy impact, 23 °C (kJ/m²)4913
    Heat deflection temperature, 1.8 MPa (°C)60205195

    Compared with standard 1101G-30, the X54 modification lowers flexural modulus by roughly 10–15% and lowers heat deflection temperature by approximately 5–10 °C, while increasing notched Charpy impact at 23 °C by approximately 40–60%. The toughness improvement is not uniform across all stress states: in slow tensile or flexural loading the difference may be small, but in high-strain-rate snap-fit insertion and low-temperature impact the X54 grade shows a distinct reduction in brittle fracture. Converters should not treat X54 as a direct substitute for a low-warpage PBT grade, a hydrolysis-stabilized PBT grade, or a flame-retardant PBT grade without first revalidating dimensional capability, hot-wet ageing, and flammability certification on the production tool. The material is also not an unfilled PBT; glass-fiber orientation, weld-line strength, and anisotropic shrinkage must be included in mold-filling simulation and tolerance analysis.

    Top