Toray Toraycon Pbt Gf30 Lw Hs 7164g 30

Toray Toraycon® PBT+GF30%-LW-HS 7164G-30

    • Product Name: Toray Toraycon® PBT+GF30%-LW-HS 7164G-30
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 490505
    Density 1.53 g/cm³
    Glass Fiber Content 30 wt%
    Water Absorption 24h 0.07%
    Molding Shrinkage Flow 0.2%
    Molding Shrinkage Cross Flow 0.8%
    Tensile Strength 120 MPa
    Elongation At Break 2.0%
    Flexural Modulus 8500 MPa
    Flexural Strength 180 MPa
    Notched Charpy Impact 7 kJ/m²
    Notched Izod Impact 60 J/m
    Hdt 0 45mpa 220 °C
    Hdt 1 82mpa 205 °C
    Melting Point 225 °C
    Volume Resistivity 1E16 Ω·cm
    Dielectric Strength 20 kV/mm
    Flammability Ul94 HB
    Arc Resistance 120 s

    As an accredited Toray Toraycon® PBT+GF30%-LW-HS 7164G-30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-barrier bags; Toray Toraycon® PBT+GF30%-LW-HS 7164G-30 supplied as pelletized resin.
    Container Loading (20′ FCL) 20′ FCL loaded with Toray Toraycon® PBT+GF30%-LW-HS 7164G-30 in 25 kg moisture-proof bags on pallets, securely stowed for safe ocean transport.
    Shipping Toray Toraycon® PBT+GF30%-LW-HS 7164G-30 is shipped as non-hazardous polybutylene terephthalate resin pellets containing 30% glass fiber, in moisture-protected bags or containers. It is not classified as dangerous goods for transport and should be kept dry and cool.
    Storage Store Toray Toraycon® PBT+GF30%-LW-HS 7164G-30 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and incompatible materials such as strong oxidizers. Keep containers tightly closed and protected from moisture, contamination, and physical damage. Avoid temperature extremes; use first-in, first-out rotation. Follow the manufacturer’s safety data sheet and applicable local regulations.
    Shelf Life Typical shelf life is 12 months from manufacture when stored dry, below 30°C, in original unopened packaging, avoiding moisture and direct sunlight.
    Free Quote

    Competitive Toray Toraycon® PBT+GF30%-LW-HS 7164G-30 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toraycon® PBT+GF30%-LW-HS 7164G-30 is a 30 wt% glass-fiber-reinforced polybutylene terephthalate injection-molding compound in the Toraycon 7164 series. The resin is designated under ISO 11469:2016 as PBT-GF30; the LW-HS suffix identifies a low-warpage, high-stiffness formulation that retains the glass reinforcement of a conventional 7164G-30 grade. Under ISO 291:2021 conditioning at 23 °C and 50% RH, representative lot averages are density 1.51–1.55 g/cm³, tensile stress at break 125–140 MPa, flexural modulus 8500–9500 MPa, flexural strength 185–205 MPa, and heat deflection temperature 200–210 °C at 1.82 MPa. The material is supplied for injection molding of thin-wall housings, connectors, and brackets in which anisotropic shrinkage of standard glass-filled PBT produces unacceptable flatness deviation.

    Typical physical, mechanical, and thermal values for material selection; not contractual specification limits.
    PropertyUnitValueTest method
    Densityg/cm³1.51–1.55ISO 1183-1:2019
    Melt volume-flow rate, 250 °C/2.16 kgcm³/10 min10–20ISO 1133-1:2022
    Tensile stress at breakMPa125–140ISO 527-2:2012
    Tensile strain at break%2.0–3.0ISO 527-2:2012
    Flexural modulusMPa8500–9500ISO 178:2019
    Flexural strengthMPa185–205ISO 178:2019
    Charpy notched impact, 23 °CkJ/m²7–10ISO 179-1/1eA:2010
    Heat deflection temperature, 1.82 MPa°C200–210ISO 75-2/Af:2013
    Melting temperature, DSC°C220–228ISO 11357-3:2018
    Water absorption, 23 °C/24 h%0.06–0.08ISO 62:2008
    Mold shrinkage, flow / transverse%0.20–0.40 / 0.60–1.00ISO 294-4:2018
    UL 94, 1.5 mm—HBUL 94

    The values above are typical dry-as-molded lot averages. Color concentrates, regrind levels above 25 wt%, and non-standard processing conditions can shift tensile and impact properties by 5–10%. The 7164 series is a non-flame-retardant PBT; if a molded part requires V-0, a flame-retardant PBT grade must be specified.

    What distinguishes the LW-HS variant from standard 7164G-30 in anisotropic shrinkage control?

    Conventional 30 wt% glass-filled PBT develops a layered orientation structure during filling: high shear near the cavity wall aligns fibers in the flow direction, while the core may contain more transverse or random orientation. Differential cooling shrinkage between these layers is the primary source of warpage in flat parts. Standard 7164G-30 mold shrinkage is commonly reported as 0.20–0.40% in the flow direction and 0.60–1.00% transverse under ISO 294-4:2018. The LW-HS variant targets a narrower shrinkage differential while maintaining 30 wt% glass fiber, so flexural modulus and heat deflection temperature remain comparable to the standard grade. Published data for the exact flow-transverse shrinkage ratio of this LW-HS configuration is limited; flatness capability should be confirmed on production tooling with a square plaque and two-dimensional coordinate measurement.

    The low-warpage package does not function as an impact modifier. Charpy notched impact at 23 °C remains in the 7–10 kJ/m² range under ISO 179-1/1eA:2010, and tensile strain at break remains below 3.0%. Snap-fit features therefore require radii above 0.5 mm and reduced deflection to avoid brittle failure. The grade is also not a surface-improved or low-gloss grade; glass fibers can still produce visible orientation at knit lines and gate blush.

    Pre-drying in a desiccant-bed dryer with an inlet air dew point of −30 °C or lower at 120–130 °C for 4–6 h is required to reduce hydrolysis-prone moisture below 0.02%. Higher drying temperatures above 140 °C may cause thermal oxidation of additives. A hopper-mounted dryer alone is generally insufficient for this 30 wt% glass-filled PBT in humid plant conditions.

    Injection molding parameters for 30% glass-fiber PBT

    Barrel zone settings from hopper to nozzle are typically 230–240 °C, 245–255 °C, 255–265 °C, 260–270 °C, and 250–260 °C; the measured melt temperature should remain 250–270 °C. The preferred mold temperature is 60–100 °C. Cavity pressure during the packing phase should be maintained at 50–70 MPa, with hold pressure set at 50–80% of injection pressure. Gate freeze time should be established with cavity-pressure transducers; hold time is typically set 0.5–1.0 s beyond gate seal. Screw back pressure of 0.3–0.5 MPa and screw speed of 50–100 rpm are common starting points for 30 wt% glass-filled PBT, though screw diameter and compression ratio modify these values.

    For production-scale equipment, a barrier screw with a cermet-coated check ring is preferred. A worn check ring with axial clearance above 0.1 mm can increase fiber attrition and reduce tensile strength by 3–5%. The compound is generally produced on a co-rotating twin-screw extruder with L/D 40:1–48:1 when compounded, with glass rovings fed downstream of the melting section by a side feeder at 250–260 °C to minimize fiber breakage. This compounding route preserves the fiber aspect ratio required for the high-modulus plateau.

    When mold temperature drops below 60 °C, weld-line strength and flatness become process-sensitive

    At low mold temperatures the melt front skins over rapidly, preventing glass fibers from crossing the weld interface. Tensile specimens cut across a weld line under ISO 527-2:2012 typically retain 55–65% of the unwelded tensile stress; below 60 °C mold temperature, retention can fall below 50%. Multi-gate housings with mold temperatures below 60 °C show observable differential shrinkage in the last-filled regions. On production-scale 16-cavity connector tools, raising mold temperature from 50 °C to 80 °C reduces warpage variation by 25–40%, although published data for this specific grade is limited. The effect is more severe in sections thinner than 1.0 mm.

    The mold-temperature increase should be balanced against cycle-time requirements. The upper mold-temperature range above 100 °C is not required for this grade and can increase cooling time without further flatness benefit. Turbulent flow in mold channels with a Reynolds number above 10,000 is recommended to maintain a uniform cavity surface temperature.

    Dimensional stability after elevated-temperature exposure

    Post-mold annealing at 120 °C for 2 h in air is a standard method to complete secondary crystallization and release molded-in orientation. This can reduce subsequent shrinkage after exposure to 150 °C by 30–50%, depending on gate location and wall thickness. However, continuous air aging above 150 °C can oxidize the PBT matrix unless a heat-stabilized variant is specified. Heat deflection temperature at 1.82 MPa under ISO 75-2/Af:2013 remains 200–210 °C, but that value indicates short-term mechanical deflection, not long-term oxidative stability.

    The coefficient of linear thermal expansion for 30 wt% glass-filled PBT is typically 25×10⁻⁶ K⁻¹ in the flow direction and 60×10⁻⁶ K⁻¹ transverse under ISO 11359-2:2021. This anisotropy contributes to warpage when parts are exposed to temperature gradients. Annealing at 140 °C for 4 h can further stabilize dimensions, but molders should verify that the additional thermal exposure does not degrade impact strength before release to production.

    Chemical compatibility and hydrolysis boundaries

    The ester backbone of PBT hydrolyzes under hot aqueous conditions. Continuous immersion in water or water-glycol coolants above 80 °C can reduce molecular weight and tensile strength by more than 15% within 1000 h; phosphate-ester and amine-containing additive packages can accelerate this degradation. The grade should not be specified for continuous coolant immersion or steam sterilization unless a hydrolysis-resistant PBT is selected. Dry-as-molded water absorption after 24 h at 23 °C is only 0.06–0.08% under ISO 62:2008, so short-term ambient humidity has limited plasticizing effect.

    Strong bases and certain chlorinated organic solvents can stress-crack PBT. Molded parts should be tested for stress-cracking under the actual chemical contact and applied strain. For electrical connector applications, the comparative tracking index is lot-specific and must be verified under IEC 60112:2003; glass reinforcement can reduce tracking resistance relative to unfilled PBT unless the additive package compensates.

    Automotive electrical connectors, fuse boxes, relay housings, sensor brackets, and power-tool motor housings are typical applications where the flatness and modulus of this grade are relevant. In these uses, the material is normally classified UL 94 HB at 1.5 mm; if the application requires V-0, a flame-retardant PBT grade is required because the 7164 series is not flame-retardant. The low-warpage behavior reduces post-mold distortion in multi-pin connectors with pin pitches of 2.54 mm or finer, but pin-retention force should be validated after thermal cycling from −40 °C to 120 °C because the glass-filled matrix has a low elongation-to-break.

    Glass content is held at 30% precisely to avoid the property cliff-edge of unfilled PBT

    Unfilled PBT has a flexural modulus of approximately 2300–2500 MPa and an HDT at 1.82 MPa of 55–65 °C. At 30 wt% glass reinforcement, the flexural modulus rises to 8500–9500 MPa and the HDT to 200–210 °C. The LW-HS formulation retains that reinforcement, so the change from standard 7164G-30 is not a reduction in glass content. Compared with a 30% glass/mineral hybrid PBT, this grade may have lower melt viscosity and better weld-line behavior, but published direct comparison data for the LW-HS configuration is limited. Hybrid grades can exceed 1.60 g/cm³ density, while this grade remains at 1.51–1.55 g/cm³.

    The density difference is relevant when molded part weight is constrained. A shift from unfilled PBT to this grade increases weight by roughly 20–25% at equal wall thickness, so thin-wall design must consider that the higher modulus may allow thickness reduction. Any thickness reduction below 1.0 mm can reduce weld-line strength and mold filling, especially in multi-cavity tools with long flow paths. Spiral-flow length should be established with the specified hot-runner layout because it is gate-dependent and wall-thickness-dependent.

    Typical compliance position for base resin and standard colorants
    Regulatory standard or codeStatus
    RoHS Directive 2011/65/EU as amended by (EU) 2015/863Conformant for typical non-flame-retardant color packages
    REACH regulation (EC) No 1907/2006, SVHC listNo SVHC above 0.1% w/w based on supplier declaration; confirm per color lot
    UL 94, 1.5 mmHB for non-flame-retardant 7164 series
    ISO 11469:2016PBT-GF30
    FDA 21 CFR 177.1660Not generally cited for glass-reinforced PBT; verify for food-contact use

    When this grade is substituted into an existing standard 7164G-30 mold, gate and venting dimensions often remain unchanged, but a cavity-pressure validation run is recommended because the low-warpage package can slightly alter solidification shrinkage and packing behavior. Molded parts should be measured after 48 h at 23 °C and 50% RH, not immediately after demolding, because post-mold crystallization continues during the first hours. Flatness inspections should use a granite surface plate and dial indicator or a coordinate measuring machine with a locating datum system, not simple caliper spot checks. This approach separates material-induced warpage from tooling and process-induced distortion.