Toray Toraycon Pbt Gf30 Lw 7151g40 B

Toray Toraycon® PBT+GF30%-LW 7151G40 B

    • Product Name: Toray Toraycon® PBT+GF30%-LW 7151G40 B
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 696718
    Polymer Base PBT (polybutylene terephthalate)
    Material Category Glass-fiber reinforced PBT
    Reinforcement Glass fiber
    Glass Fiber Content 30% by weight
    Special Feature Low warpage (LW) grade
    Processing Method Injection molding
    Density Approx. 1.50–1.60 g/cm³
    Tensile Strength Approx. 100–130 MPa
    Elongation At Break Approx. 2–3%
    Flexural Modulus Approx. 8–10 GPa
    Charpy Notched Impact Strength Approx. 5–10 kJ/m²
    Heat Deflection Temperature Approx. 200–210 °C at 1.82 MPa
    Molding Shrinkage Approx. 0.2–0.5%
    Water Absorption Typical <0.1%
    Flammability Rating HB (typical)

    As an accredited Toray Toraycon® PBT+GF30%-LW 7151G40 B factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toray Toraycon® PBT+GF30%-LW 7151G40 B is supplied in 25 kg moisture-barrier bags, palletized for industrial handling.
    Container Loading (20′ FCL) Toray Toraycon® PBT+GF30%-LW 7151G40 B: 25 kg bags on pallets, loaded into 20′ FCL container; cargo secured for export.
    Shipping Ship Toray Toraycon® PBT+GF30%-LW 7151G40 B as non-hazardous thermoplastic resin pellets in sealed moisture-barrier bags or containers, palletized and protected from moisture, heat, sunlight, and physical damage. Store dry and ventilated; follow the SDS and local transport regulations.
    Storage Store Toray Toraycon® PBT+GF30%-LW 7151G40 B in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep original containers tightly closed, palletized, and protected from dust, contamination, and physical damage. Use first-in, first-out stock rotation, respect the manufacturer’s shelf life, and follow the safety data sheet for additional handling and storage precautions.
    Shelf Life Shelf life is typically 12 months from manufacture when stored unopened in a cool, dry place, protected from moisture and sunlight.
    Free Quote

    Competitive Toray Toraycon® PBT+GF30%-LW 7151G40 B prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The product designation Toray Toraycon® PBT+GF30%-LW 7151G40 B identifies a black, 30 wt% glass-fibre-reinforced polybutylene terephthalate injection-moulding compound in the low-warpage family. The alphanumeric segment G40 is an internal grade code and is not a declaration of 40 wt% glass loading; the explicit reinforcement level remains 30 wt%. The suffix B denotes black colour. The compound is supplied in pellet form and is intended for thermoplastic injection moulding. PBT-based formulations of this class display a crystalline melting point near 223 °C under ISO 11357-3 and a density in the range 1.53–1.57 g/cm³ under ISO 1183-1; lot-specific certificates of analysis should be used to confirm exact values for the 7151G40 B designation. Published data for this exact configuration is limited in open sources; equivalence to class-typical PBT+GF30% behaviour should therefore be treated as a starting point rather than a substitute for supplier submission data. The low-warpage attribute is achieved through filler geometry and formulation features that reduce differential shrinkage between flow and transverse directions, not by eliminating glass reinforcement.

    The mechanical envelope expected for a 30 wt% glass-reinforced PBT low-warpage grade is characterised by tensile stress at break values of 120–140 MPa when tested according to ISO 527-2, flexural modulus values of 7.5–9.5 GPa according to ISO 178, and heat deflection temperature values of 195–215 °C at 1.80 MPa according to ISO 75-1/-2. Charpy notched impact strength class-typically falls between 8 kJ/m² and 12 kJ/m² under ISO 179-1/1eA. The unfilled PBT baseline is substantially lower in stiffness and higher in mould shrinkage: unfilled grades may show flexural modulus near 2.5 GPa and mould shrinkage of 1.5–2.0 % under ISO 294-4, while glass-reinforced low-warpage grades reduce shrinkage to 0.3–0.8 % depending on flow direction and part geometry. These ranges are derived from industrial literature for glass-filled PBT and not from a lot-specific certificate for 7151G40 B; measurement on test plaques according to the same standards is required for specification control.

    Incoming material acceptance should include ash content according to ISO 3451-1, density according to ISO 1183-1, and melt volume-flow rate according to ISO 1133-1 at 250 °C under 2.16 kg. The ash content for 30 wt% glass-filled PBT is class-typically 30 % plus the contribution of low-warpage mineral filler; the exact value should be fixed against an approved reference lot. For black grades, ash determines the total filler loading, not glass fibre loading alone, because carbon black and other inorganic processing aids may be present at 1–2 wt%. General-purpose glass-filled PBT grades commonly show MVR values of 10–20 cm³/10 min at 250 °C and 2.16 kg under ISO 1133-1; low-warpage filler systems may be at the lower end of this range due to filler geometry. Spiral-flow trials on the target moulding machine are therefore recommended before cavity layout is fixed.

    What Limits the Processing Window of Glass-Filled Low-Warpage PBT?

    The principal constraint in melt processing is hydrolytic degradation of the PBT matrix. The compound should be dried in a desiccant dryer at 120 °C for 4–6 h to a moisture content below 0.02 %, with a dew point not higher than -30 °C. Injection-moulding machines with a general-purpose screw of 20:1–25:1 L/D and a compression ratio of 2.5:1 are suitable. Start-point melt temperatures are 250–270 °C; mould temperatures should be held at 60–100 °C to control crystallisation and reduce post-moulding warpage. Back pressure of 0.3–0.7 MPa and injection pressures class-typically 80–120 MPa are used for 30% glass-filled grades; the exact gate pressure depends on flow length, wall stock, and hot-runner pressure drop. Total residence time at the upper melt temperature should not exceed 5 min to limit chain scission and colour shift. Wet material above 0.02 % moisture can generate surface splay and a measurable loss in tensile strength under ISO 527-2.

    Parameter Starting value Reference method / equipment
    Drying temperature 120 °C Desiccant dryer, dew point ≤ -30 °C
    Drying time 4–6 h Moisture ≤ 0.02 %, ISO 15512
    Melt temperature 250–270 °C Reciprocating screw injection-moulding machine
    Mould temperature 60–100 °C Water or oil mould temperature control unit
    Injection pressure 80–120 MPa Hydraulic or electric machine; cavity pressure monitored
    Screw L/D ratio 20:1–25:1 General-purpose screw, compression 2.5:1

    In compounding, the glass fibre length distribution and low-warpage filler dispersion control the balance between rigidity and warpage stability. Production-scale twin-screw extruders with 40:1–48:1 L/D and side-fed glass fibre are commonly used for this product class. Keeping the melt temperature below 280 °C during compounding is critical to prevent PBT resin degradation; the glass rovings are introduced downstream to preserve fibre length. The difference between low-warpage and standard GF30 grades is therefore partly traceable to the filler system and partly to extrusion conditions. Batch-to-batch variation in ash content under ISO 3451-1 should remain within ±1.0 wt% of nominal reinforcement.

    In production-scale injection moulding, the grade is positioned for flat, multi-cavity parts in which standard glass-reinforced PBT grades exhibit unacceptable warpage after ejection. Typical application categories include electrical connectors, relay housings, sensor bodies, motor brush carriers, and enclosed switchgear components with linear dimensions above 60 mm. The reduced shrinkage anisotropy is evaluated on edge-gated plaques according to ISO 294-4; standard glass-filled PBT often shows parallel shrinkage of 0.2–0.5 % and transverse shrinkage of 0.6–1.0 %, while the low-warpage variant narrows this difference to below 0.3 percentage points in laboratory plaques. For moulded housings, flatness measurements using a coordinate measuring machine can be used for lot acceptance. Published data for this specific configuration is limited; product validation should therefore include cavity-pressure monitoring on the target tool with clamping force appropriate to the projected area. The compound is not suitable for continuous exposure to hot water above 60 °C or for strong acidic or alkaline media unless the specific moulded component is validated under the end-use standard.

    When Standard GF30 PBT Grades Are Substituted by the Low-Warpage 7151G40 B

    The functional difference between 7151G40 B and a general-purpose PBT+GF30% grade lies primarily in mould shrinkage isotropy rather than in absolute stiffness. In standard glass-filled PBT, fibre orientation parallel to the flow path suppresses parallel shrinkage while transverse shrinkage remains high; this imbalance generates edge curl and flatness error in thin-wall parts. The low-warpage formulation reduces this imbalance. A trade-off may occur in notched impact behaviour: certain low-warpage filler systems sacrifice some ductility compared with unfilled or short-glass-only PBT. Comparative testing under ISO 179-1/1eA and ISO 527-2 is required because the direction of the measured change depends on the specific filler package and moulding conditions.

    Property Test method Unfilled PBT Standard GF30 PBT Low-warpage GF30 PBT
    Density ISO 1183-1 1.30–1.32 g/cm³ 1.52–1.56 g/cm³ 1.53–1.57 g/cm³
    Flexural modulus ISO 178 2.3–2.7 GPa 7.5–9.0 GPa 7.0–9.5 GPa
    Tensile stress at break ISO 527-2 50–60 MPa 120–140 MPa 120–140 MPa
    HDT at 1.80 MPa ISO 75-1/-2 55–65 °C 195–215 °C 195–215 °C
    Mould shrinkage parallel ISO 294-4 1.5–2.0 % 0.2–0.5 % 0.3–0.6 %
    Mould shrinkage transverse ISO 294-4 1.5–2.0 % 0.6–1.0 % 0.5–0.8 %

    These comparative ranges are class-typical values from industrial literature for glass-reinforced PBT and are not certified values for 7151G40 B; they are supplied only to establish the expected direction of property shifts. Lot-specific certificates should be referenced for pass/fail limits. Dimensional audit should be conducted after conditioning for 24 h at 23 °C and 50 % relative humidity according to ISO 291; inspection immediately after moulding may understate subsequent shrinkage due to crystallisation.

    For dimensional and material tracking, moulded parts should be marked according to ISO 11469; the polymer-filler marking would be PBT-GF30 or an equivalent recycling-marking convention. Supplier documentation should be checked for RoHS and REACH status; the black pigmentation may involve carbon black, and the glass-fibre reinforcement is E-glass class-typical. The material should be stored in closed containers at ambient temperature and not exposed to high-humidity environments above 60 % RH before drying. When regrind is used, a maximum addition of 20 wt% is common for glass-reinforced PBT; property retention should be verified on each lot using ISO 527-2 and ISO 179-1/1eA. Failure to dry regrind separately can cause inconsistent melt viscosity and moulding weight variation. For electrical connectors, surface leakage and tracking resistance should be evaluated under IEC 60112 if the component is used in voltage-bearing insulation. Low-warpage mineral fillers can alter the comparative tracking index relative to unfilled PBT; published values for this exact grade are limited in open sources, so supplier data should be requested for CTI, dielectric strength under IEC 60243-1, and volume resistivity under IEC 62631-3-1.

    Top