Toray Toraycon Pbt Gf30 Hydrolytic 1101g 30 H

Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H

    • Product Name: Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 373165
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Water Absorption 24 H 0.07%
    Tensile Strength 135 MPa
    Tensile Elongation At Break 2.2%
    Flexural Modulus 9.0 GPa
    Flexural Strength 200 MPa
    Charpy Notched Impact Strength 8 kJ/m²
    Heat Deflection Temperature 1 82 Mpa 205 °C
    Melting Point 225 °C
    Mold Shrinkage Flow Direction 0.2–0.5%
    Mold Shrinkage Cross Flow 0.6–0.8%
    Volume Resistivity 1×10^16 Ω·cm
    Dielectric Constant 1 Mhz 3.7
    Rockwell Hardness M 90
    Flammability HB
    Hydrolysis Resistance Improved

    As an accredited Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H packaging: 25 kg moisture-barrier bags, 40 bags (1,000 kg) per pallet.
    Container Loading (20′ FCL) 20′ FCL loading for Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H: palletized 25 kg bags, approximately 20 MT net, securely stowed for export.
    Shipping Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H ships as glass-fiber-reinforced PBT pellets in sealed moisture-barrier bags or octabins on pallets. It is generally non-hazardous, with no UN number or DOT/IMDG/IATA transport class. Store cool, dry, and protected from heat, UV, and contamination.
    Storage Store Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing materials. Keep in tightly closed original containers to prevent moisture absorption and contamination. Avoid humid conditions and physical damage. Maintain recommended storage temperature and use within the specified shelf life, following the SDS and local regulations.
    Shelf Life Shelf life: typically 24 months when stored dry in original sealed packaging, away from moisture, heat, and direct sunlight.
    Free Quote

    Competitive Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toray Toraycon® PBT+GF30%-Hydrolytic 1101G-30 H is a 30% glass-fibre-reinforced polybutylene terephthalate injection-moulding grade carrying a hydrolytic stabilization package. The designation separates the material from the standard 1101G-30: the base PBT matrix, formed from 1,4-butanediol and terephthalic acid, is reinforced with 30% by weight of chopped glass fibre, while the H suffix indicates an additive system intended to reduce the chain scission that occurs when the ester linkages in PBT are exposed to hot water, steam, or aqueous ethylene glycol mixtures. The grade is supplied in pellet form for injection moulding and is used where high rigidity, dimensional stability, and chemical resistance must be retained after wet-heat exposure. Underhood automotive components, water-contact housings, sensor brackets, and appliance parts exposed to condensing humidity fall within its application range.

    Dry-as-moulded mechanical, thermal, and electrical values reported for the 30% glass-reinforced PBT series are given in the table. The values are typical for injection-moulded ISO 3167 Type 1A multipurpose specimens and should not be treated as specification minima for production parts containing weld lines, variable wall thickness, or moulded-in stress. Batch-specific certificates should be obtained for the exact colour and lot.

    StandardPropertyTypical value
    ISO 1183-1:2019Density1.53 g/cm³
    ISO 527-1:2019 / ISO 527-2:2012Tensile strength at break135 MPa
    ISO 527-1:2019 / ISO 527-2:2012Tensile elongation at break2.5%
    ISO 178:2019Flexural strength200 MPa
    ISO 178:2019Flexural modulus9.0 GPa
    ISO 179-1:2010/Amd 1:2021Charpy notched impact strength, 23 °C10 kJ/m²
    ISO 75-1:2013 / ISO 75-2:2013Deflection temperature under load, 1.80 MPa205 °C
    ISO 1133-1:2022Melt volume-flow rate, 250 °C/2.16 kg12 cm³/10 min
    IEC 60093Volume resistivity1016 Ω·cm
    IEC 60243-1Dielectric strength20 kV/mm
    IEC 60112Comparative tracking index250 V
    UL 94FlammabilityHB

    The dry-as-moulded values reflect the contribution of 30% glass fibre to modulus and heat distortion temperature, but they do not define service performance after hydrolytic exposure. The 30% loading is a mid-range reinforcement level within the Toraycon PBT series: a 15% glass fibre grade offers longer flow length in thin walls and lower tool wear, while a 45% glass fibre grade provides higher flexural modulus but greater notch sensitivity and more anisotropic shrinkage. The H suffix does not alter the nominal glass content; it identifies the hydrolytically stabilised formulation.

    When Hydrolytic Stabilization Becomes the Primary Qualification Criterion

    Hydrolysis in PBT proceeds by nucleophilic attack of water at the ester linkage, producing chain scission and lowering molecular weight. The reaction accelerates above the glass transition because water diffusion through the amorphous fraction increases, and carboxylic acid end groups generated by chain scission can promote further autocatalytic hydrolysis. Ethylene glycol-water coolant mixtures at 90–130 °C are particularly aggressive to unstabilised PBT, especially in parts under hoop stress or at sharp notches. The H-grade stabilization package addresses the autocatalytic pathway, typically through acid scavenging or end-group blocking; the supplier does not disclose the complete stabilization chemistry in standard datasheets. Because ethylene glycol alters water activity, swells the amorphous fraction, and modifies hydrolysis kinetics, qualification should be conducted in the actual coolant mixture rather than deionized water alone. Aged tensile specimens should be tested according to ISO 527-1:2019 and ISO 527-2:2012, and impact retention should be measured with ISO 179-1:2010/Amd 1:2021. For parts with weld lines, specimens cut across the weld line are more representative than standard multipurpose specimens. Published data for this specific grade in open literature is limited; therefore, end users must generate aged property curves on production-representative geometry before locking the material specification.

    For injection moulding, the first processing constraint is moisture control. The pellets require desiccant drying at 120 °C for 3–4 h to residual moisture below 0.02%. Insufficient drying causes hydrolysis in the barrel rather than in service; the practical consequences are surface splay, reduced Charpy impact, and high scrap rates when the same lot is run without an adequately maintained dryer. Desiccant hoppers should maintain a dew point below −30 °C, and hopper residence time should be matched to throughput. Moisture content should be verified by Karl Fischer titration or a calibrated moisture analyzer; time-based drying alone is unreliable when regrind or high plant humidity is present.

    Barrel temperatures should be maintained from feed to nozzle at 250–270 °C, with nozzle temperature typically 10–20 °C below the front zone to prevent drooling. Mould temperature should be set between 60 °C and 100 °C. At the lower end, crystallinity and dimensional stability decrease; at the upper end, cycle time increases and mould shrinkage may exceed the tool compensation. A general-purpose screw with an L/D ratio of 18:1–20:1 and compression ratio of 2.0:1–2.5:1 is adequate for the grade. High-shear mixing sections are not required and can increase glass fibre attrition, lowering notched impact. Back pressure is usually set at 0.5–1.0 MPa to homogenize the melt without excessive fibre breakage. Residence time at maximum melt temperature should not exceed 8 minutes; longer exposure causes thermal chain scission even in the stabilised grade. Regrind addition should be limited to 25% by weight and dried with virgin pellets. Production-scale experience with glass-filled PBT indicates that fibre accumulation at the check ring can occur after 50,000–100,000 shots, producing shot-weight drift of 1–3% and cushion instability if a hardened reverse-pumping screw tip is not used.

    Short-glass-fibre orientation creates through-thickness layers in the moulded part: a highly oriented skin layer, a less oriented core, and a transition zone. The flow-direction tensile and flexural modulus may exceed the cross-flow direction by roughly 10–20% depending on gate type and fill speed. At weld lines, fibres align parallel to the weld plane, reducing reinforcement efficiency normal to the line. When a part is exposed to thermal cycling from −40 °C to 140 °C, differential thermal expansion between the polymer and the glass fibre creates microstresses around fibre ends; under hydrolytic conditions, these interfaces can initiate microcracks. Gate placement should therefore locate weld lines outside pressurized sections, and sharp internal corners should be radiused to avoid notch-dominated failure. Mould venting of 0.02–0.03 mm thickness at the end of fill reduces gas trapping, black speck formation, and local burn marks.

    What Differences in Mould Shrinkage and Flow Exist Relative to Other Toraycon PBT Grades?

    The 30% glass fibre level produces anisotropic mould shrinkage, commonly 0.3–0.6% in the flow direction and 0.7–1.0% transverse, depending on gate position, mould temperature, and part thickness. This anisotropy is higher than unfilled PBT and lower than 45% glass-reinforced grades. Compared with 15% glass fibre PBT, the 30% grade has higher tensile strength, flexural strength, and heat distortion temperature, but lower flow length in thin sections and lower notched impact. Compared with 45% glass fibre PBT, the 30% grade has a lower flexural modulus, reduced brittleness in thick sections, and less severe tool wear. Compared with standard 1101G-30, the dry-as-moulded mechanical properties overlap within normal lot-to-lot variation; the practical difference appears after wet-heat exposure, where the H grade retains a higher percentage of initial tensile and impact values. Flame-retardant PBT grades are not direct substitutes for 1101G-30 H: they usually have higher density, lower comparative tracking index, and are selected when UL 94 V-0 compliance is mandatory. Unfilled PBT has a flexural modulus roughly one-quarter to one-third of the 30% glass-filled grade and lower heat distortion temperature, but it offers better flow and lower tool wear.

    Typical production uses for 1101G-30 H include coolant thermostat housings, water pump covers, e-thermostat connectors, and appliance water-contact housings. On a 1,200 kN hydraulic clamp injection moulding machine with a 40 mm screw, a cushion of 3–6 mm is maintained to provide consistent pack and prevent the screw bottoming. Hot-runner systems for glass-filled PBT should be externally heated and designed without dead spots; stagnant melt degrades into black specks and lowers impact strength. Metal inserts should be preheated to reduce differential shrinkage and residual stress. The hydrolytic stabilization package is not a substitute for robust part design; weld lines, sharp corners, and poorly vented end-of-fill regions remain failure locations regardless of the additive system.

    Regulatory documentation should be verified for the specific grade, colour, and production site. The material is normally supplied with information supporting EU REACH communication obligations and EU RoHS Directive 2011/65/EU Annex II. Food-contact and potable water approvals are not automatic; the end user must confirm the relevant national positive list, migration test result, and application-specific certification. For electrical enclosures, the UL yellow-card entry for the exact colour and thickness should be referenced before design freeze because colourants and formulations can affect flammability ratings.

    Top