Toray Toraycon Pbt Gf30 Heat Shock 5001g 30

Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30

    • Product Name: Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 899184
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Water Absorption 0.07%
    Mold Shrinkage Flow Direction 0.2%
    Mold Shrinkage Cross Flow Direction 0.8%
    Tensile Strength 135 MPa
    Elongation At Break 3.0%
    Flexural Modulus 8.8 GPa
    Flexural Strength 200 MPa
    Izod Notched Impact Strength 75 J/m
    Deflection Temperature Under Load 1 82 Mpa 205 °C
    Deflection Temperature Under Load 0 45 Mpa 220 °C
    Rockwell Hardness M90
    Volume Resistivity 1E16 Ω·cm
    Dielectric Strength 20 kV/mm
    Dielectric Constant 1 Mhz 3.5
    Dissipation Factor 1 Mhz 0.002
    Flammability Rating UL94 HB
    Melting Point 224 °C

    As an accredited Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30 is supplied in 25 kg bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL container loaded with Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30 in moisture-proof bags, palletized and secured for ocean transport.
    Shipping Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30 is shipped as non-hazardous, moisture-sensitive thermoplastic pellets in sealed, labeled bags/containers. Keep dry, cool, and protected from UV/contamination; avoid prolonged heat. No special dangerous-goods classification is normally required; verify SDS and local transport rules before shipment.
    Storage Store Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30 indoors in a cool, dry, well-ventilated area, protected from direct sunlight and moisture. Keep containers sealed in original packaging and away from heat sources, open flames, and incompatible chemicals. Avoid prolonged exposure to humid conditions. Maintain stable storage temperature, prevent package damage, practice good housekeeping, and use oldest stock first.
    Shelf Life Store in a dry, cool place in sealed original packaging; shelf life is typically 12 months from date of manufacture.
    Free Quote

    Competitive Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toray Toraycon® PBT+GF30%-Heat-Shock 5001G-30

    Toraycon® 5001G-30 is a 30 wt% glass-fiber-reinforced polybutylene terephthalate injection-molding grade in the Toraycon® PBT portfolio, positioned specifically for heat-shock resistance. The material is specified for underhood electrical and electronic components in which repeated temperature excursions create differential thermal strain between glass reinforcement and the semicrystalline PBT matrix. Unfilled PBT exhibits a coefficient of linear thermal expansion near 9–11 × 10−5 K−1; the 30 wt% glass reinforcement reduces the flow-direction value to roughly 2.5–4.0 × 10−5 K−1 when measured according to ISO 11359-2. That reduction stabilizes the dimensional position of molded-in terminal arrays, but it also transfers cyclic stress to the fiber–matrix interface and to weld lines. The 5001G-30 grade therefore addresses crack initiation under repeated heating and cooling rather than simply increasing filler content.

    PBT melting point for this class is approximately 223–225°C, with glass-transition temperature between 45°C and 55°C. Short-term mechanical properties are characteristic of 30 wt% glass reinforcement: tensile stress at break in the 120–140 MPa range under ISO 527-1/-2, flexural modulus from 8,500 MPa to 10,000 MPa under ISO 178, and heat deflection temperature at 1.80 MPa between 195°C and 210°C under ISO 75-1/-2. The following table reports representative property ranges for the glass-reinforced heat-shock-resistant PBT class; regional datasheet revisions, color concentrates, and production lot certificates will vary.

    Representative property ranges for Toraycon® 5001G-30-type 30 wt% glass-fiber-reinforced PBT
    Property Test method Typical range
    Density ISO 1183 1.52–1.55 g/cm³
    Tensile stress at break ISO 527-1/-2 120–140 MPa
    Tensile strain at break ISO 527-1/-2 2.0–3.0%
    Flexural modulus ISO 178 8,500–10,000 MPa
    Notched Charpy impact, 23°C ISO 179/1eA 8.0–12.0 kJ/m²
    Heat deflection temperature, 1.80 MPa ISO 75-1/-2 195–210°C
    Molding shrinkage, flow ISO 294-4 0.2–0.5%
    Molding shrinkage, transverse ISO 294-4 0.7–1.0%
    Volume resistivity IEC 60093 1 × 1015 Ω·cm or greater
    Dielectric strength, 1 mm IEC 60243-1 20–25 kV/mm
    Comparative tracking index IEC 60112 250–400 V

    Published data for the exact interfacial chemistry and modifier package in 5001G-30 is limited. The grade should therefore be qualified on molded plaques and on production-representative parts under the end user’s thermal-cycle protocols. Single-point ISO laboratory values do not fully capture retained weld-line elongation after heat-shock aging.

    What governs heat-shock behavior in a 30% glass-reinforced PBT matrix?

    Heat-shock failure in 30% glass-reinforced PBT is governed primarily by differential contraction between the glass fiber, with a coefficient of linear thermal expansion near 5 × 10−6 K−1, and the PBT matrix, which can exceed 8 × 10−5 K−1 in unreinforced regions. During rapid cooling from 125°C or 150°C to −40°C, tensile stress concentrates at fiber ends, at weld lines, and around sharp internal corners where glass bundles orient transverse to the load path. Standard 30% glass-reinforced PBT may yield acceptable Charpy notched impact at 23°C under ISO 179/1eA, but that value alone does not predict whether a thin-walled snap-fit will survive repeated thermal excursions. The heat-shock-resistant grade is formulated to retain higher weld-line elongation and lower crack-growth tendency after cycling.

    Component-level thermal-shock testing is usually performed under IEC 60068-2-14 test Na, with transfer time controlled between cold and hot zones. Automotive connector qualification commonly requires 100–300 cycles from −40°C to 150°C, followed by terminal retention and visual inspection. In snap-fit arms and boss features below 1.2 mm wall thickness, cracking generally initiates near the gate or weld line if mold temperature is too low or if the cavity is overpacked. The 5001G-30 designation is therefore specified for full-part heat-shock performance rather than only for ISO specimen values.

    Compounding of the heat-shock-resistant grade typically uses a co-rotating twin-screw extruder with an L/D ratio near 40:1, with chopped glass fed downstream of the first kneading section to limit fiber breakage. Fiber length distribution after compounding has a strong influence on notched impact and weld-line toughness. If mean fiber length falls below 250 µm, impact retention and crack deflection diminish; if it rises well above 500 µm, thin-wall flow and surface appearance can deteriorate. These are general processing relationships for 30 wt% glass-reinforced PBT rather than grade-specific pass/fail limits. Batch-to-batch variation in fiber length distribution can shift notched Charpy impact by approximately ±1 kJ/m² and should be tracked by ashing or digestion in addition to standard physical testing.

    Pre-Drying, Barrel Profiling, and Mold Temperature Control

    PBT is hydrolytically unstable in the melt. Moisture above approximately 0.02 wt% causes molecular-weight reduction, splay, low weld strength, and increased susceptibility to heat-shock cracking. The product should be dried in a desiccant dryer to 0.02 wt% or less, typically at 120°C for 3–4 h or 130°C for 2–3 h. At ambient relative humidity above 60%, dried pellets should reach the hopper within 30 min or remain in a closed hopper-fed drying circuit.

    Barrel temperature profiles for injection molding range from approximately 230°C in the rear to 250–270°C at the front, nozzle, and hot runner. Melt temperature should remain above 250°C for adequate glass wetting but below 270°C during hold. Total residence time above 260°C should stay below 8 min to avoid PBT depolymerization and tetrahydrofuran formation. Mold temperature is the most influential variable for heat-shock performance: 60–90°C is typical, and the upper portion of this range improves weld-line consolidation and reduces frozen-in stress at the cost of longer cooling time.

    On production-scale electric injection molding machines with screw L/D ratios of 20:1 to 22:1, worn check rings produce glass-rich leading melt and unreinforced trailing melt. This leads to localized warpage and reduced impact in end-gated connectors. A cushion position variation exceeding ±0.5 mm in a heat-shock-critical mold is an indicator for check-ring and screw-tip maintenance. Back pressure is generally set at 0.5–1.5 MPa hydraulic with screw speed from 60 rpm to 120 rpm. Melt flow rate for 30 wt% glass-reinforced PBT under 250°C and 2.16 kg load per ISO 1133-1 is commonly 10–25 g/10 min. A drop in apparent viscosity beyond the specified MFR range after drying indicates molecular weight loss and calls for process hold rather than higher barrel temperature.

    Gate placement and venting must account for glass-fiber anisotropy. Flow-direction shrinkage of 0.2–0.5% and transverse shrinkage of 0.7–1.0% under ISO 294-4 cause distortion if gate placement is unbalanced. Edge gating at one end of an elongated connector creates a weld line with transversely oriented glass; sequential valve gates or two end gates positioned so that the weld line lies away from snap-fit arms are preferred. For pin rows with 1.5 mm nominal wall sections, gate land length below 0.8 mm and adequate end-of-fill venting reduce gas traps that later become crack initiation sites. Flow-front temperature at the weld line should remain above 250°C for adequate chain interdiffusion; excessive injection time can cool the flow front and create a visible weld line that opens during thermal cycling. For multicavity connector molds, clamp force requirement is approximately 0.6–0.8 ton/cm² of projected area.

    Comparison with other Toraycon® products shows that 5001G-30 is not selected for maximum flow or maximum short-term impact alone. Standard 30 wt% glass-reinforced PBT grades provide similar modulus and HDT, but may exhibit lower tolerance for thermal cycling when molded at low mold temperature. Unreinforced PBT offers higher elongation but a heat deflection temperature below 60°C at 1.80 MPa and a much higher coefficient of linear thermal expansion, making it unsuitable for dimensionally stable underhood housings. High-flow GF30 grades reduce injection pressure for thin-wall parts, but the lower melt viscosity often reflects lower molecular weight and may reduce weld-line strength. The table summarizes application-relevant differences among unreinforced PBT, standard GF30, and the heat-shock-resistant GF30 class represented by 5001G-30.

    Application-related comparison of unreinforced PBT, standard GF30 PBT, and heat-shock-resistant GF30 PBT
    Characteristic Unreinforced PBT Standard GF30 Heat-shock GF30 (5001G-30)
    Tensile stress at break 55–65 MPa 120–140 MPa 120–140 MPa
    Flexural modulus 2,500–3,000 MPa 8,500–10,000 MPa 8,500–10,000 MPa
    HDT at 1.80 MPa 50–60°C 195–210°C 195–210°C
    Linear CTE, flow 9–11 × 10−5 K−1 2.5–4.0 × 10−5 K−1 2.5–4.0 × 10−5 K−1
    Weld-line cracking after −40°C/150°C cycling baseline moderate improved
    Thin-wall fill capability higher moderate moderate

    When Underhood Connector Housings Are Exposed to −40°C/150°C Cycling

    Underhood connector housings, ignition coil bobbins, sensor bodies, relay bases, and motor brush holders are primary application fields for 5001G-30. Glass reinforcement stabilizes terminal pitch during thermal soak, while the PBT matrix supplies electrical insulation and resistance to automotive fluids. In ignition coil bobbins, short-term peak temperatures near the valve cover can approach 150°C; heat deflection temperature above 195°C at 1.80 MPa provides thermal margin, but only if wall thickness and gate design avoid high packing stress. Connector pin retention after cycling is more important than initial tensile strength: a housing that passes initial terminal pull force can still crack along pin rows after 100 cycles if the material lacks sufficient retained elongation.

    Electrical properties are consistent with 30 wt% glass-reinforced PBT. Volume resistivity is generally at or above 1 × 1015 Ω·cm under IEC 60093, dielectric strength at 1 mm thickness is in the 20–25 kV/mm range under IEC 60243-1, and comparative tracking index is commonly 250–400 V under IEC 60112. These values support low-voltage moderate-pollution-degree insulation but do not automatically qualify the material for all high-energy arcing conditions. Flammability classification should be confirmed from the UL yellow card for the specific grade and color; standard 30 wt% glass-filled PBT is typically HB under UL 94 unless flame-retardant additives are specified.

    Chemical resistance is typical of semicrystalline PBT. Short-term contact with mineral oil, lithium grease, aliphatic hydrocarbon mists, and diluted salt solutions is generally acceptable. Aromatic solvents, strong acids, strong bases, brake fluid, and steam above 80°C can cause cracking or hydrolysis. Compatibility should be tested by immersion according to ISO 175 on both standard tensile bars and weld-line specimens, because molded-in glass orientation influences chemical crack resistance.

    Regrind Is Only Acceptable After Impact and Thermal-Cycle Validation

    Regrind from sprues and rejected parts can be blended with virgin 5001G-30 at 20–25 wt% for many non-appearance structural applications. Heat-shock-critical parts require separate validation because regrind has shortened glass-fiber length distribution and additional heat history. Melt flow rate can remain within specification while notched Charpy impact drops; ISO 179/1eA impact and part-level thermal cycling are therefore more reliable acceptance tools than melt flow alone. Glass content should be verified by ashing or digestion according to ISO 3451-1, with a target glass content of 30 wt% and tolerance stated in the certificate of analysis.

    Fiber accumulation in hot-runner tips and shut-off nozzles is a known production bottleneck. Hot-runner tips below 1.0 mm diameter can accumulate glass-rich melt at the gate, causing gate blush and locally reduced impact. Valve-gate systems with minimal dead spots are preferred. Residual PVC or acetal in the barrel decomposes at PBT processing temperatures to hydrogen chloride or formaldehyde and formic acid, respectively; both cause PBT depolymerization and surface splay. Purging through a low-melt-index polypropylene purge compound followed by PBT purge compound is required until no streaks or bubbles remain. Toraycon® is a registered trademark of Toray Industries, Inc.

    Top