| HS Code | 917719 |
| Polymer Type | Polybutylene terephthalate (PBT) |
| Glass Fiber Content | 30% |
| Flame Retardant | Yes |
| Ul94 Flammability Rating | V-0 |
| Density | 1.58 g/cm3 |
| Tensile Strength | 120 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 9.0 GPa |
| Notched Izod Impact | 70 J/m |
| Hdt At 1 82 Mpa | 205 °C |
| Melting Point | 225 °C |
| Water Absorption | 0.08% |
| Mold Shrinkage | 0.2-0.8% |
| Volume Resistivity | 1e16 ohm·cm |
| Dielectric Strength | 20 kV/mm |
As an accredited Toray Toraycon® PBT+GF30%-FR 1184G-A15 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Toray Toraycon® PBT+GF30%-FR 1184G-A15 is supplied in 25 kg moisture-proof bags, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Toray Toraycon® PBT+GF30%-FR 1184G-A15 palletized in moisture-proof bags, dry, secure, compliant stowage. |
| Shipping | Toray Toraycon® PBT+GF30%-FR 1184G-A15 is shipped as non-hazardous, flame-retardant, glass-fiber-reinforced PBT pellets in moisture-proof bags or containers. It is not classified as dangerous goods for transport. Store dry, away from direct sunlight, heat, and contamination; use sealed packaging and normal industrial cargo conditions. |
| Storage | Store Toray Toraycon® PBT+GF30%-FR 1184G-A15 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Keep in original sealed, labeled containers/bags; avoid dust and static buildup. Separate from strong oxidizers, acids, and bases. Do not expose to high temperatures or prolonged humidity. Use FIFO and observe shelf-life. |
| Shelf Life | Typical shelf life is 24 months in original unopened packaging, stored dry below 30°C, away from moisture and sunlight. |
Competitive Toray Toraycon® PBT+GF30%-FR 1184G-A15 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Toraycon® PBT+GF30%-FR 1184G-A15 is classified as a glass-fiber-reinforced, flame-retardant polybutylene terephthalate injection-molding compound. The grade designation signals a polybutylene terephthalate matrix, 30% by weight glass fiber reinforcement, and a flame-retardant package intended for electrical and electronic part approval under UL 94 V-0. The semi-crystalline PBT matrix has a crystalline melting point near 223–225 °C, while the glass-filled compound exhibits a density of approximately 1.63–1.68 g/cm³ when measured according to ISO 1183-1:2019. Typical tensile strength reported for this compound class is 110–125 MPa under ISO 527-1/2, with tensile strain at break below 3%. Flexural modulus is usually in the 8,000–9,500 MPa range under ISO 178. The melt volume-flow rate typically lies between 10 and 20 cm³/10 min at 250 °C and 2.16 kg load under ISO 1133-1:2022. Heat deflection temperature under 1.8 MPa by ISO 75-1/-2 commonly remains in the 195–210 °C range for this material class. The exact flame-retardant chemistry is not specified in this introductory summary; the manufacturer safety data sheet and UL yellow card are the controlling documents for substance disclosure and end-product certification.
Flexural modulus is the primary differentiator between 30% glass-filled PBT and unfilled or 15% glass-filled alternatives. Mold shrinkage measured by ISO 294-4 typically falls in the 0.2–0.6% flow-direction range and 0.5–1.0% transverse-direction range for the GF30 flame-retardant class. The anisotropic shrinkage arises because fiber orientation follows the flow field; snap-fit geometries and press-fit pins should be gated so that the main load path aligns with the fiber-orientation direction. Weld lines formed downstream of multi-gate flow fronts may retain only 60–80% of the in-flow tensile strength, a known limitation in glass-reinforced semi-crystalline polyesters. Charpy notched impact strength under ISO 179-1/1eA is typically 6–9 kJ/m², lower than a non-flame-retardant GF30 PBT because flame-retardant additives can act as stress concentrators and reduce matrix ductility. Water absorption after 24 h immersion at 23 °C is usually 0.05–0.10% by ISO 62; although low, PBT remains susceptible to hydrolysis above 80 °C in water. Published data for the exact 1184G-A15 configuration is limited for weld-line-strength retention and should be confirmed for structural-bearing designs.
The property shift from unfilled PBT to a 30% glass-reinforced flame-retardant compound is not linear. Table 1 summarizes representative property contrasts across the unfilled flame-retardant PBT class, a 15% glass-fiber flame-retardant class, and the 30% glass-fiber flame-retardant class to which 1184G-A15 belongs. The data are not lot-specific certificate-of-analysis values but ranges assembled from published PBT compound technical data.
| Property | Test method | Unfilled FR PBT | GF15 FR PBT class | GF30 FR PBT class |
|---|---|---|---|---|
| Density | ISO 1183-1 | 1.30–1.35 g/cm³ | 1.50–1.56 g/cm³ | 1.63–1.68 g/cm³ |
| Tensile strength | ISO 527-1/2 | 50–60 MPa | 85–100 MPa | 110–125 MPa |
| Flexural modulus | ISO 178 | 2,400–2,800 MPa | 5,000–6,000 MPa | 8,000–9,500 MPa |
| Charpy notched impact | ISO 179-1/1eA | 3–5 kJ/m² | 5–7 kJ/m² | 6–9 kJ/m² |
| Heat deflection temperature | ISO 75-1/-2 at 1.8 MPa | 55–65 °C | 195–205 °C | 195–210 °C |
| Flammability | UL 94 | V-0 at 1.6 mm | V-0 at 1.6 mm | V-0 at 0.8 mm grade-specific |
The practical difference is visible in thin-wall connectors. Unfilled FR PBT can fill thin sections but lacks rigidity; GF15 FR PBT raises flexural modulus to roughly 5,000–6,000 MPa; GF30 FR PBT reaches 8,000–9,500 MPa, which is often required to hold press-fit terminal pins under thermal cycling. Dielectric strength measured under IEC 60243-1 typically falls in the 16–20 kV/mm range for a 3 mm specimen, and volume resistivity under IEC 62631-3-1 is generally above 1 × 1013 Ω·m at 23 °C. These electrical property ranges are influenced by moisture uptake; conditioning at 23 °C and 50% relative humidity for 48 h changes surface resistivity and tracking performance.
Because PBT undergoes hydrolytic chain scission when residual moisture exceeds approximately 0.02% at melt temperature, pre-drying is mandatory for 1184G-A15. A desiccant-bed dryer with a dew point of −30 °C or lower is operated at 120 °C for 4–6 h; storage at relative humidity above 60% may require 130 °C for 5–8 h. Moisture above the threshold reduces molecular weight and produces surface splay, lower weld-line strength, and dimensional drift in molded parts. Melt temperature measured at the nozzle is maintained between 250 °C and 270 °C; barrel zones are typically set in the 240–270 °C range from rear to front. Mold temperature should be held between 60 °C and 100 °C. Total melt residence time in the barrel is kept below 10 min because prolonged exposure promotes thermal degradation of the flame-retardant package and may liberate acidic species. For a production-scale hydraulic machine with a 32 mm screw and 120 t clamp force, back pressure is normally set at 2–5 bar and screw decompression at 2–5 mm to prevent drool at the nozzle. Check-ring wear and screw/barrel corrosion should be monitored more closely when processing flame-retardant PBT than when processing unfilled PBT. Runner systems should use full-round or trapezoidal cross-sections; for glass-filled PBT, cold sprue and runner diameters should not be below 3 mm if glass-fiber separation is to be avoided. Valve-gate hot runner systems are permitted, but dead zones in manifold channels can retain molten polymer and degrade the flame-retardant system; color change and purging after flame-retardant PBT is more material-intensive than with unfilled PBT.
Polybutylene terephthalate crystallizes rapidly, but the cooling rate imposed on the part surface determines the thickness of the low-crystallinity skin and the subsequent dimensional stability at elevated temperature. At mold temperatures below 60 °C, the skin freezes before spherulitic growth reaches the level obtained at 80–100 °C; post-mold shrinkage may increase, and glass-fiber orientation at the surface can lock in residual stress. The effect is most relevant for flat connector headers and relay bobbins where pin-to-pin pitch is controlled to ±0.05 mm. Increasing mold temperature from 60 °C to 90 °C typically improves mold shrinkage uniformity but extends cycle time. If the mold is held above 100 °C, crystallization rate is high, but ejection may become difficult for deep-draw parts with low draft angles and the melt may require lower injection speed to avoid flash. Cavity-pressure sensors are preferred over fixed time-based hold because glass-filled PBT freeze-off is fast. Published data for the exact 1184G-A15 crystallization kinetics is limited; processors should generate a mold-temperature study to separate filling-phase and packing-phase effects on weld-line strength and sink-mark depth.
Connectors, relay bobbins, coil formers, motor brush holders, power module housings, miniature circuit-breaker components, and switch bodies are typical usage classes for a GF30 flame-retardant PBT such as 1184G-A15. The glass reinforcement reduces creep under terminal insertion loads and maintains contact normal force after solder reflow; the flame-retardant package enables UL 94 V-0 documentation at the required final wall thickness. Electrical tracking behavior should be checked under IEC 60112, because flame-retardant additives can lower the comparative tracking index to 250–400 V; a CTI of at least 250 V is commonly required for unsupervised insulation in humid environments. Glow-wire ignition testing under IEC 60695-2-13 is typically performed at 775 °C for connectors used in unattended household appliances; the result is thickness- and color-dependent and must be confirmed with the manufacturer’s UL yellow card. Ground sprue/runner material from 1184G-A15 may be reprocessed at 20–25% addition if the regrind is dry and free of contamination, but fiber-length reduction lowers tensile and impact properties, and repeated heat histories may shift the UL 94 performance. For third-party UL-listed parts, regrind limits must follow the yellow card.
Flame-retardant chemistry of 1184G-A15 must be evaluated against the substance restrictions of REACH Annex XVII, RoHS Directive 2011/65/EU, and any customer-specific brominated flame retardant or antimony trioxide thresholds. The exact flame-retardant package is not reproduced here because published data for this specific configuration is limited. Components intended for European markets often require additional testing under IEC 62321 for restricted substances. The material is not intended for food-contact use under FDA 21 CFR or European food-contact regulations. If the flame-retardant system is halogen-containing, processing fumes may require local exhaust ventilation and corrosion-resistant tooling; if antimony-containing, end-of-life incineration and waste coding differ from halogen-free alternatives. Table 2 lists a typical electrical and regulatory compliance checklist for the GF30-FR PBT product class.
| Assessment | Standard or directive | Typical acceptance criterion |
|---|---|---|
| Flammability | UL 94 | V-0 at 0.8 mm or 1.6 mm grade-specific |
| Comparative tracking index | IEC 60112 | CTI ≥ 250 V |
| Glow-wire flammability | IEC 60695-2-13 | 775 °C pass at specified thickness |
| Ball pressure resistance | IEC 60695-10-2 | Pass at 125 °C |
| Restricted substances | RoHS 2011/65/EU | Compliant per manufacturer verification |
Compared with PBT+GF30%-FR 1184G-A15, unfilled FR PBT provides higher elongation but insufficient stiffness for pin-header applications requiring insertion retention; GF15 FR PBT reduces density and flow-direction/transverse shrinkage anisotropy but sacrifices flexural modulus and may fail snap-fit load retention. Non-flame-retardant GF30 PBT normally has higher impact strength and lower density, but it cannot satisfy UL 94 V-0 without a separate barrier or coating. Mineral-filled PBT offers lower warpage at the expense of weld-line strength and tensile strength. PBT/PET blends can improve mold surface appearance but exhibit slower crystallization and higher moisture sensitivity. The selection basis for 1184G-A15 is therefore the combination of 30% glass reinforcement for high stiffness and dimensional stability, plus a flame-retardant system for electrical ignition resistance. Operational boundaries include mandatory pre-drying, melt-temperature ceiling near 270 °C, mold-temperature minimum near 60 °C, sensitivity to hot humid environments above 80 °C due to hydrolysis, and incompatibility with contaminants such as PVC, acetal, or amine-containing masterbatches that may generate corrosive or reactive species during compounding or molding.