Toray Toraycon Pbt Gf 1184g A30

Toray Toraycon® PBT+GF 1184G-A30

    • Product Name: Toray Toraycon® PBT+GF 1184G-A30
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 699761
    Polymertype PBT
    Reinforcement Glass fiber
    Glassfibercontent 30%
    Density 1.53 g/cm³
    Tensilestrength 140 MPa
    Tensileelongationatbreak 2.5–3.0%
    Flexuralstrength 210 MPa
    Flexuralmodulus 9.0 GPa
    Heatdeflectiontemperatureat1 82mpa 205 °C
    Meltingpoint 225 °C
    Waterabsorption24h 0.07%
    Moldshrinkage 0.2–0.5%
    Volumeresistivity 1×10^16 Ω·cm
    Dielectricconstantat1mhz 3.6
    Ul94flammabilityrating HB
    Rockwellhardnessm 90
    Arcresistance 120 s
    Coefficientoflinearthermalexpansion 3×10^-5 /°C

    As an accredited Toray Toraycon® PBT+GF 1184G-A30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toray Toraycon PBT+GF 1184G-A30 is packaged in 25 kg moisture-resistant bags, 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) Standard 20′ FCL dry container: Toray Toraycon® PBT+GF 1184G-A30 in 25 kg bags, palletized, shrink-wrapped, loaded, and secured for export.
    Shipping Toray Toraycon® PBT+GF 1184G-A30 is shipped as non-hazardous polybutylene terephthalate resin pellets (30% glass fiber) in moisture-barrier bags or boxes. It is not regulated for transport; keep dry and away from heat and direct sunlight under normal industrial handling precautions.
    Storage Store Toray Toraycon® PBT+GF 1184G-A30 resin pellets in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep original bags sealed and protect from rain, dust, and contamination. Avoid contact with strong acids, bases, and solvents. Use first-in-first-out stock rotation; if moisture uptake is suspected, dry according to supplier recommendations before processing.
    Shelf Life Shelf life is typically indefinite when stored dry and cool; use within 12 months for optimal processing.
    Free Quote

    Competitive Toray Toraycon® PBT+GF 1184G-A30 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toray Toraycon® PBT+GF 1184G-A30 is a 30% glass-fiber reinforced polybutylene terephthalate injection-molding compound supplied by Toray Industries, Inc. The grade is specified for insulating components in electrical distribution, electric vehicle charge interfaces, and industrial controls where flame resistance, dimensional stability, and resistance to surface tracking are evaluated together. Representative datasheet values determined on injection-molded specimens include density 1.65 g/cm³ under ISO 1183, tensile strength 135 MPa under ISO 527-1/2, flexural modulus 10,000 MPa under ISO 178, and heat deflection temperature 205°C at 1.80 MPa under ISO 75-1/2. Flammability classification is UL 94 V-0 at 0.8 mm nominal thickness; comparative tracking index is reported at 600 V under IEC 60112. The material belongs to the 1184 series but differs from standard 1184G-30 chiefly in tracking resistance and is intended for high-density electrical isolation where IEC 60664-1 Material Group I performance permits shorter creepage distances than conventional V-0 PBT grades.

    What Drying and Melt-Temperature Limits Govern the 1184G-A30 Processing Window?

    Moisture control is the primary processing constraint. PBT hydrolyzes in the melt phase when residual moisture exceeds 200 ppm; the equilibrium target before molding is below 50 ppm. Pre-drying in a desiccant hopper dryer with a supply air dew point of -30°C to -40°C is required. The resin is dried at 120°C to 130°C for 4 h to 6 h when ambient relative humidity exceeds 60% RH. Material left in open bins for more than 2 h after drying should be sealed or re-dried. If drying is omitted, melt viscosity decreases, silver streaking appears, and tensile strength loss may exceed 10% of the dry-material value. The recommended melt temperature measured at the nozzle is 250°C to 270°C. Barrel profile from rear to front should rise from 230°C to 260°C. Mold temperature is maintained between 60°C and 100°C; mold temperatures below 60°C suppress crystallization and produce post-shrinkage in elevated-temperature service, while temperatures above 100°C extend cooling time without proportional dimensional benefit. Injection pressure for small-to-medium components is commonly 60 MPa to 120 MPa, with holding pressure 40 MPa to 80 MPa. Back pressure is kept at 0.3 MPa to 0.5 MPa to limit fiber attrition. Screw L/D ratio of 20:1 to 22:1 with a low-compression ratio and a hardened non-return valve specified for glass-filled PBT is used. Residence time at melt temperature should not exceed 10 min to 12 min; longer exposure causes discoloration and molecular weight reduction. On production-scale toggle clamp machines, shot size should occupy 25% to 75% of barrel capacity to avoid excessive residence time and poor melt homogeneity. Clamp force requirement is approximately 4.5 kN/cm² to 6.0 kN/cm² of projected area. Venting depth on the parting line is limited to 0.01 mm to 0.02 mm; vent depths above 0.03 mm produce flash because the low melt viscosity at 270°C fills thin gaps. Gate diameter for pin gates should be at least 1.5 mm; hot-tip gates smaller than 1.0 mm cause gate blush and glass fiber breakup.

    Because the 30% glass fiber content raises elastic modulus and heat deflection temperature, dimensional stability is significantly higher than unfilled PBT and short-glass compounds below 15% loading. Fiber orientation, however, creates anisotropy in shrinkage: typical mold shrinkage values range from 0.3% to 0.7% in the flow direction and 0.7% to 1.2% in the transverse direction under ISO 294-4. Ribs, boss bases, and gate locations exhibit differential shrinkage; cavity sizing corrections are applied before steel cutting. Weld line tensile strength in multi-gate configurations is governed by melt-front angle and fiber orientation. Published data for the A30 grade at specific weld-line angles were not available in the examined datasheet, so weld-line performance should be measured on prototype tools using ISO 527-2 or ASTM D638 specimens cut from representative gate configurations. Notched Charpy impact strength is typically reported near 8.0 kJ/m² under ISO 179/1eA; the material is notch-sensitive compared with unfilled PBT, and sharp internal radii below 0.5 mm should be avoided in load-bearing features. Water absorption after 24 h immersion at 23°C is approximately 0.07% under ISO 62; moisture uptake is not a dimensional concern in short-term testing but hydrolytic stability under hot aqueous service remains a constraint.

    Electrical Tracking Resistance and Flammability Classification in IEC 60664-1 Creepage Design

    The A30 modification is relevant to components where conductive deposits on insulator surfaces can establish a tracking path and create a short circuit. Under IEC 60112, the comparative tracking index of 1184G-A30 is reported as 600 V. This value places the material in IEC 60664-1 Material Group I, which permits smaller creepage distances than Material Group IIIb polymers when pollution degree and working voltage are held constant. The exact distance must be calculated according to IEC 60664-1 clause 6.2 and tabulated for the relevant pollution degree and working voltage. Flammability classification is UL 94 V-0 at 0.8 mm. Volume resistivity is typically above 1×1016 Ω·cm under IEC 62631-3-1, and dielectric strength is thickness-dependent; reported values near 15 kV/mm under IEC 60243-1 apply only to flat plaques, not complex part geometry. End-product testing at minimum wall thickness and around weld lines is required because internal glass fiber orientation can create local dielectric discontinuities.

    In electric vehicle charge couplers and power distribution modules, the grade is selected for connector housings, terminal blocks, busbar supports, and relay bases where surface contamination can initiate tracking. The material is also used in photovoltaic inverter insulators, circuit breaker arc chambers, and ignition components. For outdoor sealed housings, hydrolysis resistance must be considered: PBT service in hot, humid conditions above 60°C with residual alkaline or acidic contamination can degrade mechanical strength. Applications requiring continuous exposure to hot water or steam above 80°C are not recommended without long-term hydrolysis testing. The compound has a maximum continuous service temperature that is design-dependent; short-term thermal excursions above 200°C are possible only for low-stress components, while load-bearing applications require evaluation of creep modulus and oxidative aging under ISO 899-1 or ASTM D2990. On twin-screw compounding lines, glass fiber is fed downstream after polymer melting to limit fiber attrition; pellet length distribution and fiber length influence final mechanical properties. Injection molders report gate blush and white streaking when nozzle diameter is below 3 mm or when injection velocity is excessive at gates smaller than 1.5 mm. Mold steel should be hardened for glass-filled compounds; gate inserts and ejector bores show accelerated wear at 30% glass fiber loading.

    When 1184G-A30 Replaces Standard 1184G-30 in Low-Gas Enclosed Relays

    The critical difference between 1184G-A30 and conventional 1184G-30 is the comparative tracking index. Standard 1184G-30 is widely specified for V-0 PBT+GF30 applications but is reported with a CTI near 250 V; 1184G-A30 raises CTI to approximately 600 V, moving the material from IEC 60664-1 Material Group IIIb to Material Group I. This allows designers to reduce creepage distances on printed circuit board standoffs and high-density connector interfaces where space is limited. However, the A30 modification may exhibit slightly different flow behavior and elongation at break compared with 1184G-30. Datasheet values for tensile strength and flexural modulus are generally within 5% to 10% of each other; published data for the A30 grade's exact tensile strain at break should be confirmed against the current technical datasheet because flame-retardant packages influence ductility. For enclosed relay applications, low outgassing and contact contamination are tested under internal OEM procedures rather than a single ISO standard; the A30 designation is frequently screened for reduced volatile content in sealed electrical devices.

    Table 1. Comparative typical values of 1184G-A30 and 1184G-30.

    PropertyTest method1184G-A301184G-30
    Comparative tracking indexIEC 60112600 V250 V
    Flammability class at 0.8 mmUL 94V-0V-0
    DensityISO 11831.65 g/cm³1.65 g/cm³
    Tensile strengthISO 527-1/2135 MPa135 MPa
    Flexural modulusISO 17810,000 MPa10,000 MPa
    Heat deflection temperature at 1.80 MPaISO 75-1/2205°C205°C

    The material should not be processed in equipment previously used for polycarbonate or polyamide without thorough purging; residual polyamide can cause interfacial delamination, and polycarbonate contamination can hydrolyze at PBT processing temperatures. Avoid amine-based mold-release agents and lubricants because they can attack the PBT ester linkage at sustained melt temperatures. Hot-runner systems with dead spots should be avoided; if hot runners are used, open-pipe melt channels and nozzle tips designed for glass-filled PBT are required. Regrind usage should be limited to less than 25% by weight unless mechanical property testing confirms end-use requirements. Service above 120°C under load is not recommended; dimensional stability degrades due to thermal aging of the flame-retardant system and oxidation embrittlement. In applications requiring direct contact with hot water, strong mineral acids, or alkaline solutions above 60°C, the component must be validated under the expected chemical and thermal profile because PBT hydrolyzes and loses impact strength.

    Top