Toray Toraycon Pbt Fr 1401x06

Toray Toraycon® PBT-FR 1401X06

    • Product Name: Toray Toraycon® PBT-FR 1401X06
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 234703
    Polymertype Polybutylene terephthalate (PBT)
    Fillerreinforcement Glass fiber reinforced
    Flameretardant Yes
    Density 1.65 g/cm³
    Waterabsorption 0.07%
    Tensilestrength 120 MPa
    Elongationatbreak 2.0%
    Flexuralmodulus 8500 MPa
    Notchedcharpyimpactstrength 6 kJ/m²
    Heatdeflectiontemperatureat1 82mpa 205 °C
    Meltingpoint 225 °C
    Ul94flameratingat0 8mm V-0
    Volumeresistivity 1E16 Ω·cm
    Dielectricstrength 20 kV/mm
    Moldingshrinkage 0.2–0.6%

    As an accredited Toray Toraycon® PBT-FR 1401X06 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Toray Toraycon® PBT-FR 1401X06 is packaged in 25 kg moisture-barrier bags, palletized for industrial shipment and storage.
    Container Loading (20′ FCL) 20′ FCL container loaded with Toraycon® PBT-FR 1401X06 resin pellets in 25 kg bags, palletized and securely stowed for transport.
    Shipping Toray Toraycon® PBT-FR 1401X06 is shipped as non-hazardous polybutylene terephthalate resin pellets, typically in moisture-barrier-lined 25 kg bags or bulk containers. Keep dry and away from heat and direct sunlight. Standard industrial handling applies; no dangerous goods documentation is normally required.
    Storage Store Toray Toraycon® PBT-FR 1401X06 in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and ignition sources. Keep material in its original, sealed packaging until use. Avoid contact with strong oxidizing agents and prevent dust generation. Maintain clean, dry handling conditions and follow local regulations and the manufacturer’s safety data sheet.
    Shelf Life Shelf life is typically two years when stored dry, cool, and in unopened original packaging, away from moisture and direct sunlight.
    Free Quote

    Competitive Toray Toraycon® PBT-FR 1401X06 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Toray Toraycon® PBT-FR 1401X06 is a flame-retarded polybutylene terephthalate injection-molding grade. The product code 1401X06 lacks the G modifier used in Toraycon glass-fiber-reinforced grades, so the material is handled as an unfilled or only lightly filled PBT formulation for mold-shrinkage, warpage, and weld-line calculations unless the supplier certificate of analysis specifies a mineral or nucleation package. The resin is specified for electrical and electronic components such as relay bases, terminal blocks, motor brush holders, appliance connectors, and circuit-breaker housings where a recognized flame rating is required. The PBT-FR designation identifies flame retardancy rather than a specific halogen-free or halogenated chemistry. Users must therefore obtain the chemical composition, UL yellow-card minimum thickness, and regulatory certifications from the Toray technical bulletin for the specific production lot.

    On production injection-molding machines of 80–120 t clamp force with 20:1 L/D reciprocating screws, the melt temperature for unfilled PBT-FR is typically held between 240°C and 260°C. A desiccant-bed dryer with a dew point of −40°C or lower is used to dry the resin at 120°C for 4 h to a moisture content below 0.02%. If hopper loading is exposed to ambient air above 60% relative humidity, dried pellets regain moisture rapidly; splay at the gate is commonly observed when moisture exceeds 0.03%. The dryer should supply at least 3.7 m³/h of dry air per 1 kg/h of material throughput, and the conveying lines should be grounded to limit pellet fines and static segregation of flame-retardant additives.

    What Distinguishes 1401X06 from Glass-Reinforced and Non-FR PBT in Thin-Wall Electrical Applications?

    Compared with unfilled non-FR PBT, the flame-retardant package in 1401X06 reduces tensile elongation and notched impact while providing flame resistance that non-FR PBT cannot achieve. The reduction in ductility is acceptable in thin-wall electrical housings if latch arms and snap-fit transitions are designed with adequate radii, because sharp corners in unfilled flame-retarded PBT develop stress cracks during ejection or terminal insertion. Compared with 30% glass-fiber-reinforced PBT-FR, the unfilled product exhibits lower flexural modulus, lower heat-distortion temperature, and lower density. The trade-off is improved dimensional isotropy: unfilled PBT-FR shows less warpage in flat electrical housings, better weld-line appearance, and reduced tool wear from glass fiber. The difference in mold shrinkage is measurable by ISO 294-4; unfilled grades shrink in the range of 1.4% to 2.0% depending on flow orientation and gate location, while 30% glass-filled grades shrink between 0.2% and 0.8%.

    For snap-fit connector housings, the unfilled grade should be evaluated for latch creep under thermal cycling rather than for absolute stiffness. The lower modulus relative to glass-filled PBT-FR means that latch fingers may open under repeated insertion if the wall stock is below 1.0 mm. When glass-filled PBT-FR is replaced by 1401X06 to reduce warpage, the tool may require a hotter mold surface, adjusted pack pressure, or a gate position change because unfilled PBT-FR has a wider solidification range and different pressure-volume-temperature behavior.

    Comparative Property Matrix and Incoming-Quality Anchors

    The following matrix records property classes used for initial feasibility comparison. Grade-specific values for 1401X06 must be read from the Toray technical bulletin and lot certificate; the ranges shown for the unfilled FR class are not a substitute for certified mechanical data.

    PropertyUnfilled non-FR PBT1401X06 class, unfilled PBT-FR30% glass-filled FR PBTTest method
    Density at 23°C1.30–1.32 g/cm³1.44–1.52 g/cm³1.60–1.70 g/cm³ISO 1183-1
    Tensile stress at break50–60 MPa50–65 MPa110–130 MPaISO 527-2/1A
    Flexural modulus2.3–2.8 GPa2.4–3.0 GPa8.0–10.0 GPaISO 178
    Notched Charpy at 23°C3.0–5.0 kJ/m²2.5–4.5 kJ/m²7.0–10.0 kJ/m²ISO 179-1/1eA
    Heat-distortion temperature, 1.8 MPa55–65°C65–80°C200–210°CISO 75-2
    Mold shrinkage, parallel1.8–2.2%1.4–2.0%0.2–0.8%ISO 294-4
    Flammability at 0.8 mmHBV-0V-0UL 94

    Published data for grade-specific configurations outside the yellow-card thickness may be limited, particularly for glow-wire performance and comparative tracking index values after humid aging. Incoming inspection should anchor melt mass-flow rate to the supplier specification using ISO 1133-1:2022 at 250°C and 2.16 kg. A melt-flow-rate shift of more than 15% from the lot reference can indicate resin degradation, moisture damage, or incorrect regrind addition.

    Thermal Stability Limits Are Set by the Flame-Retardant Package, Not by the PBT Backbone Alone

    The PBT backbone can tolerate brief excursions to higher temperature, but the flame-retardant system limits the practical melt-processing window. Barrel settings from hopper to nozzle are typically 230–245°C in the rear zone, 245–255°C in the middle zone, 250–260°C in the front zone, and 245–255°C at the nozzle. Mold temperature should be maintained between 40°C and 80°C; the upper half of the range is preferred for flat connector housings because it reduces frozen-in stress and dimensional drift. Back pressure is held between 5 MPa and 10 MPa, while screw surface speed should not exceed 0.2 m/s on a 25 mm diameter reciprocating screw. Melt residence time above 250°C must not exceed 8 min; beyond this limit, the flame-retardant system can generate plate-out, black specks, and acidic decomposition products. If a dispersive mixing section is present, the rear barrel setpoint should be lowered by 5°C to compensate for additional shear heating.

    Regrind addition above 20% in multi-cavity tools changes the melt residence-time distribution and can compromise the consistency of the UL 94 rating. Regrind should be dried identically to virgin resin and screened for fines below 4 mm because pellet fines accelerate moisture pickup and feed-throat bridging. Acetal or PVC purges are incompatible; acidic decomposition products from these resins accelerate PBT hydrolysis and should be avoided in shared drying or granulation systems.

    When Hot-Runner Dwell Times Exceed 10 Minutes, Which Degradation Signatures Are Monitored?

    Hot-runner manifolds for 8-cavity relay-housing tools should be set at 230–250°C. Valve-gate nozzle tips heated above 260°C hold stagnant material in the gate well; after 10 min of idle time, the next 3–5 shots should be discarded until injection pressure and color stabilize. Degraded material in the gate well typically appears as yellow-brown streaks, gray weld-line haze, or short-shot pressure drop. A pressure-drop increase of more than 5–10% across the hot-runner gate well during production usually precedes visible black specks. Multi-cavity tools with unbalanced runner layouts may show cavity-to-cavity melt-fill variation; flow leaders should be adjusted only after confirming that the variation is not caused by degraded gate-well residue.

    In thin-wall sections of 0.8 mm, fill times are generally held between 0.3 s and 0.8 s. Fill times longer than 1.0 s in such walls produce premature freeze-off, flow lines, and high residual stress. Fill times shorter than 0.2 s can produce jetting and splay in unfilled PBT-FR because the melt has lower melt strength than glass-filled alternatives. Short-shot monitoring on a 16-cavity connector tool should keep fill imbalance between first and last cavity below 4%; larger imbalance correlates with warpage and variable flammability performance in molded plaques.

    The following compliance matrix identifies the standard designations that must be confirmed before series production. Component-level tests should be performed on finished parts, not on generic test plaques, because wall thickness, gate vestige, weld-line location, and terminal insertion affect flame performance and electrical tracking behavior.

    Regulation or standardClause or test methodApplication to 1401X06
    UL 94Flammability; minimum thickness on yellow cardV-0 at the listed thickness; end-use thickness must be verified
    IEC 60112Comparative tracking indexCTI class from the supplier datasheet; creepage distances per IEC 60664-1
    IEC 60695-2-13Glow-wire ignition temperatureComponent-level evaluation; not inferred from UL 94
    ISO 1133-1:2022Melt mass-flow rateIncoming inspection against the supplier specification
    IEC 62321XRF screening of restricted substancesRoHS assessment must be supplier-certified for the specific lot
    ISO 527-2/1ATensile stress at breakInitial lot certification and after-regrind validation
    ISO 179-1/1eANotched Charpy at 23°CLot certification for impact-sensitive snap-fit designs

    The product may contain a brominated flame-retardant system. If the application requires halogen-free construction as defined by IEC 61249-2-21, a certified halogen-free PBT-FR grade should be selected instead; the PBT-FR suffix does not by itself guarantee halogen content below the limit. Food-contact and medical-use compliance is not implied unless explicitly declared by Toray for 1401X06 under the relevant regulatory program.

    In final component validation, an appliance-terminal housing molded from 1401X06 should be tested for flammability at its thinnest wall in the end-use orientation, not only on a plaque. Glow-wire testing on the finished part per IEC 60695-2-13, creepage and clearance verification per IEC 60664-1, and thermal cycling from −40°C to 120°C in a thermal-shock chamber are typical. The material must also survive the customer’s torque and insertion tests on brass terminals; published data for this specific insert-molding configuration is limited, so production trials on the intended tool are required.

    Top