| HS Code | 680014 |
| Density | 1.36 g/cm³ |
| Melting Point | 265 °C |
| Glass Transition Temperature | 120 °C |
| Tensile Strength | 80 MPa |
| Tensile Elongation At Break | 15% |
| Flexural Modulus | 2.6 GPa |
| Heat Deflection Temperature At 1 8 Mpa | 85 °C |
| Water Absorption | 0.2% |
| Mold Shrinkage | 0.2–0.5% |
| Volume Resistivity | 1e16 Ω·cm |
| Dielectric Constant At 1 Mhz | 3.0 |
| Dissipation Factor At 1 Mhz | 0.002 |
| Flammability Rating | UL94 HB |
As an accredited Teijin Limited Teonex® PEN Resin TN8050SC factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Teijin Limited Teonex® PEN Resin TN8050SC is supplied in 25 kg net bags, palletized for shipment. |
| Container Loading (20′ FCL) | Teonex® PEN Resin TN8050SC is palletized and securely loaded into a dry 20-foot FCL container for ocean shipment. |
| Shipping | Non-hazardous polyethylene naphthalate (PEN) resin pellets, packaged in moisture-barrier bags/boxes and palletized. Ship in a dry, cool, well-ventilated area away from direct sunlight, heat, and moisture. No special DOT/IMDG/IATA hazardous transport classification is expected. |
| Storage | Store Teijin Limited Teonex® PEN Resin TN8050SC in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep containers tightly closed in original or compatible packaging to prevent moisture absorption and contamination. Avoid prolonged high-temperature or humid exposure; use first-in/first-out rotation and follow the supplier’s SDS and local regulations. |
| Shelf Life | Store sealed in a cool, dry place; typical shelf life is 24 months from manufacture, subject to supplier confirmation. |
Competitive Teijin Limited Teonex® PEN Resin TN8050SC prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Teijin Limited Teonex® PEN Resin TN8050SC is a naphthalate-based polyester supplied as transparent amorphous pellets for injection molding and extrusion processes in which cyclic oligomer deposition, vent fouling, and melt-aging variability are the principal yield constraints. The repeat unit is poly(ethylene naphthalene-2,6-dicarboxylate), a structure that replaces the benzene ring of PET with a fused naphthalene ring. The consequent chain stiffening is measured as a glass transition temperature of 118–124 °C under ISO 11357-2:2020 and a crystalline melting endotherm of 265–270 °C under ISO 11357-3:2018. The nominal solid density is 1.36 g/cm³ when conditioned and tested according to ISO 1183-1:2019. Lot-specific intrinsic viscosity should be confirmed from the certificate of analysis; published data for this specific configuration is limited, but injection-molding PEN grades of this class are commonly released between 0.50 dL/g and 0.62 dL/g when measured by ISO 1628-5:2020. The SC designation is associated with super-clean grade attributes, including reduced low-molecular-weight extractables and reduced oligomeric deposits in hot-runner manifolds and cavity vents relative to conventional Teonex injection-molding resin.
The differentiation from commodity PET is generated by the naphthalene ring rather than by filler loading or additive modification. The following comparative matrix lists typical unfilled resin values; the TN8050SC certificate of analysis controls lot-specific release.
| Property | TN8050SC-class PEN | Conventional bottle-grade PET | Test standard |
|---|---|---|---|
| Glass transition temperature | 118–124 °C | 74–80 °C | ISO 11357-2:2020 |
| Melting endotherm | 265–270 °C | 245–255 °C | ISO 11357-3:2018 |
| Relative oxygen permeability | 0.20–0.25 | 1.0 | ASTM D3985-17 |
| Relative carbon dioxide permeability | 0.25–0.30 | 1.0 | ASTM D1434-23 |
| Relative water vapour transmission rate | 0.30–0.40 | 1.0 | ASTM F1249-20 |
| Tensile modulus | 2,800–3,200 MPa | 2,200–2,800 MPa | ASTM D638-14 |
Compared with bottle-grade PET, the naphthalate ring in TN8050SC increases the glass transition temperature from approximately 74–80 °C to 118–124 °C. The practical consequence is that parts molded from PEN and crystallized at 140–150 °C maintain dimensional stability in hot-water and hot-air environments where PET parts undergo progressive crystallization, shrinkage, and embrittlement. Oxygen permeability of PEN is typically 0.20–0.25 relative to PET at 23 °C and 0 % relative humidity when tested under ASTM D3985-17. Carbon dioxide permeability is approximately 0.25–0.30 relative to PET, and water vapour transmission rate is approximately 0.30–0.40 relative to PET under ASTM F1249-20. The reduction in oxygen transport is the result of lower free volume and restricted segmental mobility from the fused naphthalene ring. Moisture absorption at 23 °C for 24 h is in the range 0.2–0.3 % when tested according to ISO 62:2008, which is lower than many glass-fiber-reinforced polyesters and contributes to more stable dielectric and mechanical performance in humid environments.
Against PBT, the TN8050SC grade provides a substantially higher glass transition temperature and lower gas permeability, but it also requires a narrower processing window and higher mold temperature to develop crystallinity. Against polycarbonate, TN8050SC offers lower melt viscosity at typical polyester processing temperatures but has lower notched impact strength and is not suitable for applications requiring room-temperature ductile behaviour in thick sections without impact modification. Against high-IV Teonex grades used for film and blow molding, TN8050SC is formulated for injection-moldable melt flow and controlled oligomer release; using a high-IV film grade in the same thin-wall injection tool would generally require higher barrel temperatures and longer residence times, increasing acetaldehyde regeneration and deposit formation.
Desiccant drying is mandatory before melt processing. At 60 % relative humidity and above, pellets can re-absorb surface moisture within 15–30 min of hopper residence; the recommended dry-air dryer set point is 140–160 °C with a dew point below -40 °C and residence time of 4–6 h to achieve <50 ppm residual moisture measured by ISO 15512:2019. On production-scale hot-runner injection cells with oil-heated cavity plates maintained at 140–150 °C, failures traced to incomplete drying are typically observed as silver streaks, gate blush, and loss of tensile strength at weld lines. The cylinder temperature profile from feed throat to nozzle should be stepped from approximately 270 °C to 300–310 °C for a general-purpose screw with L/D 20:1 and compression ratio 2.5:1. Flat-temperature profiles below 280 °C increase melt viscosity and cause short shots in thin-wall connector bodies. Residence time at melt temperature should not exceed 5 min, and hold pressure in the range 60–80 MPa is sufficient for semi-crystalline parts when gates are not frozen prematurely.
Mold temperature is the principal variable controlling crystallinity. At 120–150 °C the part develops sufficient crystallinity for dimensional stability and heat resistance; at 80–100 °C the part remains largely amorphous, with lower heat deflection temperature and greater warpage after post-mold annealing. At 300 °C and 1.20 kg load under ISO 1133-1:2022, melt flow rate for low-IV injection grades of this class is typically 10–16 g/10 min; the TN8050SC lot-specific value should be confirmed. Use of nucleating agents or amine-based colorants should be avoided because polyester aminolysis can accelerate chain scission and acetaldehyde regeneration. The hot-runner manifold should be purged with a high-viscosity polyolefin, not PVC or acetal purge compounds, because acidic decomposition products from PVC purge can hydrolyze the PEN backbone. For thin-wall parts below 1.0 mm, injection velocity should be 150–300 mm/s at transfer, with a short hold-pressure ramp. Back pressure of 0.5–1.0 MPa and screw rotation of 50–100 rpm limit shear heating and uncontrolled viscosity loss.
High-heat electrical and automotive parts represent the most direct injection-molding opportunities for TN8050SC. Surface-mount connector bodies, relay bases, and coil bobbins require a melting endotherm above lead-free solder reflow peaks of 255–265 °C; the TN8050SC melting range of 265–270 °C permits short-term reflow exposure when the part is crystallized and dried below 50 ppm moisture. The heat deflection temperature of crystallized PEN at 1.80 MPa is typically 118–125 °C under ASTM D648-18, which is above the continuous service requirement for many underhood sensor housings but below the requirement for high-load power electronics. Unfilled TN8050SC should not be specified for continuous service above 130 °C under mechanical stress; reinforced PPS or PA46 should be considered in those conditions. Fuel vapour barrier components benefit from the low hydrocarbon permeability of the naphthalate backbone, but long-term exposure to aggressive fuel blends containing strong amines or caustic additives requires compatibility testing because polyester hydrolysis and aminolysis are accelerated at elevated temperature.
In high-barrier packaging components, the oxygen permeability advantage of PEN allows wall-thickness reduction or extended shelf life relative to PET at comparable geometry. TN8050SC is not a film-extrusion grade; it is used where injection-molded closures, preforms, or barrier liners must be produced with less gas transmission than PET and with higher heat resistance than standard polyolefins. Electrical insulation applications benefit from the low moisture uptake and stable dissipation factor of PEN, but specific dielectric strength and comparative tracking index values must be confirmed on the final part because electrode geometry and mold-induced crystallinity change surface properties. The SC designation becomes operationally relevant in these applications because cavity vent deposits and hot-runner degradation can interrupt high-volume electronic component production lines before dimensional or electrical performance limits are reached.
Steam sterilization at 121 °C is within the thermal capability of crystallized PEN for short cycles, but repeated autoclave exposure can progressively hydrolyze the ester backbone; the hydrolysis rate is lower than that of PET but is not zero. Dried and crystallized parts exposed to 50 kGy gamma irradiation generally retain useful mechanical properties, although published data for this specific grade configuration is limited and lot-specific validation should be performed. Food-contact status must be confirmed with Teijin for the exact TN8050SC formulation. Compliance may be based on 21 CFR 177.1630 or EU Regulation 10/2011 when the finished article meets composition and migration limits; the resin is not supplied with an unconditional food-contact clearance. The grade is not inherently flame-retardant, and applications requiring UL 94 V-0 at 1.5 mm require an approved flame-retardant compounded variant or additional testing. TN8050SC should not be blended with PET regrind if the oxygen barrier or heat deflection temperature of the final part is critical, because even small PET fractions can reduce the naphthalate-order contribution and reduce the barrier property more than would be predicted by simple linear mixing.
Incompatibility with amine-based additives, strong alkaline cleaning solutions, and high-acid process residues must be managed. The polymer backbone is susceptible to aminolysis and alkaline hydrolysis at elevated temperature, and production equipment that previously processed PVC or flame-retardant concentrates containing zinc borate or antimony trioxide should be purged with a neutral polyolefin before PEN is introduced. Drying conditions should not exceed 170 °C for extended periods because prolonged exposure to high hopper temperatures can cause pellet fusion, yellowing, and loss of intrinsic viscosity before melting. For operations at relative humidity above 60 %, closed-loop desiccant drying with a hopper-loading inert atmosphere is recommended rather than open hot-air drying, because moisture re-adsorption during loading can reverse the drying effect within minutes. Processors who do not control hot-runner residence time and mold temperature will observe higher variance in cyclic oligomer deposits and crystallinity-related shrinkage than in PET, despite the lower equilibrium moisture absorption of PEN.