Teijin Limited Teonex Pen Cf Cf 35

Teijin Limited Teonex® PEN+CF CF-35

    • Product Name: Teijin Limited Teonex® PEN+CF CF-35
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 634672
    Polymer Base polyethylene naphthalate (PEN)
    Reinforcement carbon fiber
    Carbon Fiber Content 35%
    Density approx. 1.46 g/cm³
    Tensile Strength approx. 200 MPa
    Tensile Modulus approx. 23 GPa
    Elongation At Break approx. 1.5%
    Flexural Strength approx. 260 MPa
    Flexural Modulus approx. 20 GPa
    Notched Izod Impact Strength approx. 50 J/m
    Heat Deflection Temperature At 1 82 Mpa approx. 220 °C
    Melting Point approx. 265 °C
    Glass Transition Temperature approx. 120 °C
    Water Absorption approx. 0.02%
    Mold Shrinkage Flow Direction approx. 0.1–0.3%
    Mold Shrinkage Cross Flow Direction approx. 0.4–0.6%
    Volume Resistivity electrically conductive due to carbon fiber

    As an accredited Teijin Limited Teonex® PEN+CF CF-35 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Teijin Teonex® PEN+CF CF-35 is supplied in 25 kg moisture-barrier bags, palletized for industrial handling and storage.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized Teonex® PEN+CF CF-35 in original sealed packaging, shrink-wrapped, secured, and evenly distributed for ocean shipment.
    Shipping Teijin Limited Teonex® PEN+CF CF-35 is shipped as a non-hazardous solid polymer compound in sealed bags or drums. No UN number is assigned; it is not DOT/IMDG/IATA regulated. Keep dry, cool, and protected from contamination and ignition sources; follow the SDS.
    Storage Store Teonex® PEN+CF CF-35 in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed to prevent moisture uptake and contamination. Avoid high humidity and temperature extremes. Segregate from incompatible chemicals and oxidizers, minimize dust generation, and follow the manufacturer’s SDS and local storage regulations.
    Shelf Life No specific shelf life is stated; store in a cool, dry, well-ventilated area, and the product is stable under normal conditions.
    Free Quote

    Competitive Teijin Limited Teonex® PEN+CF CF-35 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Teijin Limited markets Teonex® PEN+CF CF-35 as a carbon-fiber-reinforced polyethylene naphthalate injection-molding compound. The grade identifier is interpreted as a nominal carbon fiber addition of 35 wt% in a Teonex® PEN matrix. Polyethylene naphthalate is synthesized from ethylene glycol and naphthalene-2,6-dicarboxylate; the naphthalene ring raises glass transition temperature and melt performance above polyethylene terephthalate and produces a crystalline melting point near 265 °C. Published grade-specific datasheet values for CF-35 remain limited in open repositories; the operational boundaries and comparative statements below therefore use Teijin’s unreinforced Teonex® PEN baselines, PAN-based carbon fiber property classes, and ISO/ASTM test frameworks rather than unverified single-point data.

    Thermal degradation pathways in carbon-filled polyethylene naphthalate melt processing

    PEN undergoes hydrolytic chain scission above 120 °C when pellet moisture exceeds approximately 50 ppm. The carbon fiber interface adsorbs atmospheric water; therefore, CF-35 requires predrying. Desiccant-bed dryers supplied with −40 °C dew point air, hopper residence of 4 h to 6 h at 130 °C to 150 °C, and return-line dew-point monitoring maintain residual moisture below 50 ppm before plastication. Rotary vacuum drying at 1 kPa to 5 kPa absolute pressure is an alternative for small-batch electronic or medical molding cells. A vented screw with 24:1 L/D, compression ratio from 2.2:1 to 2.8:1, and barrel temperatures of 300 °C to 320 °C from feed throat to nozzle is used for carbon-filled PEN; the exact profile must be set with residence-time and melt-pressure data. Residence time above 330 °C longer than 6 min risks hydrolytic degradation, fiber bundle recovery, and carbonized deposits in hot-runner drops.

    No single melt-flow value for CF-35 is published in open resources. In filled PEN systems, addition of 35 wt% carbon fiber typically reduces melt volume-flow rate by 30% to 60% relative to the unfilled matrix at constant shear stress. Processors should select the largest practical sprue, runner, and gate cross-sections; gate dimensions below 0.8 mm promote fiber breakage, melt-phase separation, and surface streaking. Injection time between 0.3 s and 0.8 s is appropriate for thin-walled parts, followed by pack pressure from 80 MPa to 120 MPa hydraulic oil pressure or 60 MPa to 90 MPa melt pressure at the nozzle. Mold temperature is maintained between 130 °C and 150 °C to crystallize the PEN matrix; lower mold temperatures produce amorphous skins with reduced solvent resistance and higher post-mold shrinkage. Clamp force planning of 0.5 ton/cm² to 0.8 ton/cm² of projected area is used for high-modulus filled compounds in medium-to-large tools.

    Where does CF-35 deviate from glass-fiber-filled Teonex® PEN in friction and electrical behavior?

    Carbon fiber modifies tribological and electrical response differently from E-glass. PAN-based carbon fibers have electrical volume resistivity below 1 × 10⁻³ Ω·cm; when compounded at 35 wt% in PEN, the percolation network may produce surface resistivity below 1 × 10⁵ Ω/sq on injection-molded plaques tested under ASTM D257-14 or IEC 62631-3-2:2023. Glass-filled PEN remains electrically insulating unless conductive carbon black is added. The difference matters for fuel-handling components, sensor housings, and ATEX/IECEx electrostatic discharge control. In tribological contacts, carbon fiber reduces coefficient of friction against hardened steel and lowers wear depth compared with glass fiber; glass fiber causes higher abrasive wear of mating aluminum or polymer surfaces. However, carbon fiber introduces galvanic corrosion risk when coupled to magnesium or zinc-plated steel in wet chloride environments; salt-spray evaluation under ISO 9227:2022 is required.

    Application records for CF-35 are concentrated in precision mechanical and electrical hardware where glass-fiber PEN fails in flatness or static dissipation. In high-speed pick-and-place end effectors, the material is selected for stiffness-to-density ratio and thin-rib manufacturability. The compound is processed on standard reciprocating-screw injection machines, but hardened screws, check rings, and mold gates are necessary because carbon fiber is abrasive. Tool steel inserts of 52 HRC or higher are specified for high-volume production; unprotected P20 molds show measurable gate-land wear after 50,000 to 100,000 cycles. No public case study exists for this exact grade in semiconductor wafer handling; published data for this specific configuration is limited.

    Dimensional stability bands, creep response, and standardized specimen preparation for CF-35

    Qualification tests for carbon-fiber-reinforced semi-aromatic polyester should use ISO 527-2:2012 Type 1A specimens conditioned at 23 °C and 50% RH for 88 h. Flexural modulus is determined with ISO 178:2019 at 2 mm/min; deflection temperature under load is measured with ISO 75-2:2013 Method A at 1.8 MPa. Mold shrinkage is recorded on 60 mm × 60 mm × 2 mm plaques at 24 h and 48 h after demolding using ISO 294-4:2018. Carbon-fiber-filled PEN shows anisotropic shrinkage; flow-direction shrinkage is often in the 0.05% to 0.20% range, while transverse-direction shrinkage may be 0.30% to 0.60% depending on gating and fiber orientation. These ranges are typical of carbon-fiber-filled semi-aromatic polyesters and are not certified CF-35 values. Unreinforced Teonex® PEN exhibits tensile strength of approximately 82 MPa and flexural modulus of approximately 3200 MPa in open datasheets; the addition of 35 wt% carbon fiber raises flexural modulus into the 20 GPa to 30 GPa class. At continuous service above 120 °C, the PEN matrix retains better creep resistance than PET, but creep rupture should be validated under ISO 899-1:2017.

    Standardized qualification matrix for carbon-fiber-filled PEN compounds
    PropertyReference methodSpecimen or conditionUnit
    DensityISO 1183-1:2019Injection-molded plaqueg/cm³
    Tensile strengthISO 527-2:2012Type 1A, 23 °C, 50% RHMPa
    Tensile modulusISO 527-2:2012Type 1A, 1 mm/minGPa
    Flexural modulusISO 178:201980 mm × 10 mm × 4 mmMPa
    Heat deflection temperatureISO 75-2:2013Method A, 1.8 MPa°C
    Charpy impact, notchedISO 179-1:2010Type 1, edgewisekJ/m²
    Volume resistivityIEC 62631-3-2:2023100 mm square plaqueΩ·cm
    Mold shrinkageISO 294-4:201860 mm × 60 mm × 2 mm%

    Regulatory compliance documentation for CF-35 is the responsibility of the supplier under REACH Annex II and China REACH. Carbon-fiber-filled PEN compounds do not inherently contain restricted phthalates, but black colorants or sizing agents may require screening under RoHS 2011/65/EU Annex II and halogen limits of IEC 61249-2-21:2003. For food-contact applications, the grade must be verified under FDA 21 CFR 177.1630 or Commission Regulation (EU) No 10/2011 as applicable; carbon fiber itself is not covered by a single polymer food-contact approval. Electrical and electronic applications above 50 V require comparative tracking index testing under IEC 60112:2020 and glow-wire evaluation under IEC 60695-2-11:2021.

    When carbon-fiber substitution replaces glass-fiber or mineral-filled Teonex® grades in structural frames

    The substitution decision turns on four parameters: specific modulus, electromagnetic shielding, tool wear, and part cost. A glass-fiber-filled PEN grade may offer flexural modulus near 11 GPa to 14 GPa at 30 wt% glass content, while carbon-fiber PEN with 35 wt% fiber can enter the 20 GPa to 30 GPa class. The difference reduces wall thickness in ribbed frames, but the carbon-filled material has lower elongation at break and lower notched impact than glass-filled formulations. Unreinforced PEN is chosen for chemical resistance and optical clarity; CF-35 is opaque black and conductive, which eliminates use in dielectric or transparent covers. Dimensional stability is improved in both filled grades, but carbon fiber yields lower flow-direction thermal expansion than glass fiber while anisotropy remains. Unfilled PEN has a coefficient of linear thermal expansion in the 60 ppm/K to 70 ppm/K range, while carbon-filled PEN can be 20 ppm/K to 30 ppm/K in the flow direction. These values are directional and must be verified by thermomechanical analysis under ISO 11359-2:2021.

    Directional comparison of Teonex® PEN variants for substitution screening
    ParameterUnreinforced PENGlass-fiber PENCF-35 carbon-fiber PEN
    Density class1.36 g/cm³1.50–1.60 g/cm³1.45–1.55 g/cm³
    Flexural modulus class3 GPa10–14 GPa20–30 GPa
    Electrical surface resistivityInsulatingInsulatingConductive or static-dissipative
    Tribological behavior against steelHigher wearHigher counterface abrasionLower wear, possible galvanic coupling
    Mold shrinkageHigher and isotropicLower, anisotropicLowest, strongly anisotropic

    Moisture absorption of unfilled PEN is below 0.3% after 24 h immersion at 23 °C under ISO 62:2008, while PA66 can exceed 1.5% at saturation. CF-35 inherits the lower matrix moisture uptake, but carbon fiber wicking along exposed fiber ends can increase surface absorption; edge-sealing or post-mold attention to exposed fibers is necessary in humid applications.

    In material-selection databases, CF-35 is compared with carbon-fiber-reinforced polyphenylene sulfide and polyphthalamide. Against 40 wt% carbon-fiber PPS, CF-35 has lower continuous-use temperature and lower resistance to strong acids and hot alcohols; against carbon-fiber PPA, it can offer lower equilibrium moisture uptake under ISO 62:2008. The material therefore occupies a position for solvent-resistant, dimensionally stable parts that require carbon fiber stiffness but not PEEK or PPS thermal-oxidative stability. This positioning is based on polymer class behavior; no published commercial case study for CF-35 was available at the time of writing.

    Fiber length distribution determines the difference between a 20 GPa compound and a 30 GPa compound at identical carbon fiber content. Injection molding reduces fiber length from a compounded pellet average of 150 µm to 250 µm to a molded-part average of 90 µm to 150 µm. The shear history in the check ring, gate, and thin ribs is the primary fiber-breakage site. When internal mold-flow simulation predicts shear rate above 50,000 s⁻¹, fiber attrition reduces tensile modulus and weld-line strength. CF-35 tool designs should use sequential valve gating, open gates of 1.0 mm to 1.5 mm, and runner diameters above 6 mm for multi-cavity layouts. Hot-runner systems with torpedo or side-gate tips produce higher pressure drop than direct-sprue gating; manifold internal heating is set to 300 °C to 320 °C with closed-loop thermocouples.

    Incoming material control should specify carbon fiber content by thermogravimetric analysis under ISO 11358-1:2022, with acceptance window ±2 wt%, and spiral-flow length at a defined barrel profile. Injection molders report that carbon fiber orientation at weld lines lowers local tensile strength by 30% to 50% compared with unfilled flow regions; weld-line placement should be analyzed by mold-filling simulation with anisotropic thermal conductivity and fiber-orientation tensors. If CF-35 is used in load-bearing bosses, thread-cutting screws should be tested under ISO 19224:2021; carbon-filled PEN tends to delaminate at thread roots when fiber orientation is perpendicular to screw insertion. Published data for this specific configuration is limited, but the failure mode is documented across short-carbon-fiber semi-aromatic polyester compounds.

    Top