| HS Code | 338987 |
| Product | Tasnee HDPE TASNEE 100 BK |
| Material | High-Density Polyethylene (HDPE) |
| Color | Black |
| Density | 0.959 g/cm³ |
| Melt Flow Rate 190 C 5 Kg | 0.20 g/10 min |
| Carbon Black Content | 2.0-2.5% |
| Tensile Strength At Yield | 23 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 1000 MPa |
| Vicat Softening Temperature | 125°C |
| Environmental Stress Crack Resistance Escr | >5000 h |
| Oxidation Induction Time Oit | >20 min at 200°C |
| Hydrostatic Strength | 12.4 MPa |
| Water Absorption | <0.01% |
| Thermal Conductivity | 0.40 W/m·K |
As an accredited Tasnee HDPE TASNEE TASNEE 100 BK factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Tasnee HDPE TASNEE 100 BK is supplied in 25 kg poly-lined bags, palletized and stretch-wrapped for secure industrial transport. |
| Container Loading (20′ FCL) | 20′ FCL container loading Tasnee HDPE TASNEE 100 BK in 25 kg bags, palletized, shrink-wrapped, and securely stowed for export. |
| Shipping | Tasnee HDPE TASNEE 100 BK is shipped as black high-density polyethylene pellets in 25 kg bags or 1,000 kg jumbo bags on pallets, inside dry, clean containers. It is generally non-hazardous for transport, with no UN number or hazard class; avoid moisture, heat, direct sunlight, and packaging damage. |
| Storage | Store Tasnee HDPE TASNEE TASNEE 100 BK in its original packaging in a cool, dry, well-ventilated area. Keep away from direct sunlight, heat, flames, and strong oxidizing agents. Prevent moisture, dust, and contamination. Stack pallets safely to avoid deformation or bag rupture. Use first-in, first-out stock rotation and follow the manufacturer’s safety data sheet and local regulations. |
| Shelf Life | Tasnee HDPE TASNEE TASNEE 100 BK shelf life: 24 months in original packaging, protected from direct sunlight, heat, and moisture. |
Under ISO 12162, TASNEE 100 BK is classified as PE 100 with a minimum required strength of 10 MPa at 20°C for 50 years when assessed through ISO 9080 regression analysis. The melt flow rate determined at 190°C under 5 kg load typically falls between 0.20 g/10 min and 0.30 g/10 min per ISO 1133-1, while density measured by ISO 1183-1 generally lies in the 0.958–0.961 g/cm³ band. Carbon black content in this UV-stabilized pressure pipe compound is commonly controlled to 2.0–2.5 wt% by ISO 6964, and dispersion must not exceed rating 3 under ISO 18553. In single-screw grooved barrel extruders with L/D 30:1 to 36:1, barrel zones are set from 190°C in the feed throat to 220°C at the metering section, while the die head and mandrel are held between 200°C and 220°C to reduce melt oxidation. Because the high molecular weight fraction raises melt pressure at the screen pack, breaker plates are commonly fitted with 60/80/100 mesh screens. A clogged or oversized screen pack can elevate melt temperature above 230°C, at which uncontrolled thermo-oxidative chain scission may reduce hydrostatic rupture times. After the die lips, vacuum calibration tanks set the external diameter and wall thickness, with vacuum typically maintained at −0.2 to −0.6 bar relative to atmosphere and cooling water staged from 20°C to 5°C to limit residual stress. Production pipe must meet hydrostatic strength criteria under ISO 4427-2 or EN 12201-2, including sustained pressure testing at 20°C and 80°C without premature ductile or brittle failure. The terminal components are potable water mains, gas distribution pipes, and industrial effluent lines. Because the resin is black, optical inspection of butt weld surfaces requires a clean skived face and removal of any oxidized melt bead. This grade is not recommended for continuous service above 60°C in pressure applications, and outer surface exposure should always retain the compounded carbon black to avoid UV degradation of unshielded polymer. If sacks are stored in high-humidity environments, surface condensation is removed by pre-drying at 80°C for 1–2 h; otherwise moisture entrapped in the melt can create micro-voids that reduce slow crack growth resistance.
Injection moulding of PE 100 black fittings from TASNEE 100 BK runs at melt temperatures of 220°C to 240°C and mould temperatures of 15°C to 30°C. The low melt flow rate increases the hold-pressure requirement; injection pressure is typically set to 600–1000 bar on machines with shut-off nozzle lengths above 240 mm to prevent drool between cycles. Because carbon black particles in the compound act as nucleating and stress-concentration sites, agglomerates larger than 30 µm are not permitted in the dispersion assessment. Poor dispersion above rating 3 under ISO 18553 can localize stress in the weld-line zone of socket and butt fusion fittings, reducing the short-term tensile weld factor below the 0.9 threshold referenced in some project specifications. Fittings are produced for PE 100 pipe networks under ISO 4427-3 or EN 12201-3, and destructive testing follows ISO 13953 for tensile strength of fusion joints and ISO 1167-1 for pressure resistance. Gate freeze time for thick sections in 40 mm to 63 mm walls is longer than unfilled HDPE; holding pressure must remain active until gate seal is complete, or sink marks near the injection point can act as crack initiation sites in pressure cycling. The terminal articles include electrofusion sockets, spigot fittings, mechanical couplers, and branch saddles for water and gas distribution. Hot runner systems are generally avoided because extended residence time at 240°C increases gel formation; cold runners with multiple gates create knit lines that must be placed away from high hoop stress zones. Dimensional stability after demoulding is influenced by post-mould shrinkage of 2.5–3.0% across the flow direction. Annealing is not normally required if end-gated tools are used and cooling is uniform, but published data for this specific configuration is limited, and tool trials should confirm gate sealing time and weld-line placement.
On twin-wall corrugator lines, TASNEE 100 BK is extruded through annular corrugator mould blocks with vacuum slots. Melt temperature at the die is held between 195°C and 215°C; higher setpoints close to 230°C reduce melt strength and cause inner-wall sagging before the vacuum forming station locks the corrugation geometry. The external corrugated wall provides ring stiffness, while the smooth inner wall minimizes flow resistance. Products are classified under EN 13476-2 or AASHTO M294 for stormwater management; ring stiffness is measured by ISO 9969 at SN4 to SN8 levels depending on wall structure and corrugation pitch. The carbon black level in the pipe compound, typically 2.0–2.5 wt% per ISO 6964, permits above-ground storage of pipe stocks without severe UV embrittlement. During forming, the melt is stretched by vacuum at −0.3 to −0.8 bar; too aggressive vacuum can thin the corrugation tips and reduce local slow crack growth resistance, while insufficient vacuum produces uneven inner-wall fusion at the crown. The main processing bottleneck on production lines is the mismatch between corrugator speed and extruder output. The high molecular weight of the PE 100 base generates elevated screw torque, and extruder amperage may limit line speed before the melt cools. Jointing uses socketed spigots with EPDM seals. Terminal products include stormwater culverts, retention systems, agricultural field drains, and cable protection ducts. The material is not intended for long-term continuous immersion in strong oxidizing acids or aromatic hydrocarbon solvents; chemical compatibility must be checked for contaminated runoff applications.
For geomembrane sheet production, the flat die width may exceed 3 m and thickness ranges from 1.0 mm to 3.0 mm. Barrel and die temperatures are controlled between 200°C and 220°C, while the polishing roll stack is maintained at 70°C to 90°C to control surface gloss and reduce internal frozen-in stress. Carbon black content is measured in accordance with ISO 6964 and dispersion under ISO 18553; for geomembrane service, many project specifications require carbon black content of 2.0–2.5 wt% and a dispersion rating of 1 or 2 because undispersed carbon black agglomerates can reduce stress crack resistance in exposed liner applications. The flat sheet is welded on site using hot wedge or extrusion welding. Wedge welding temperatures are adjusted to produce a melt bead with visible shear deformation; destructive peel and shear tests follow ASTM D6392 for wedge welds or ASTM D4437 for field seam evaluation. The main failure mode observed on landfill and mining liner installations is not sheet yield but slow crack growth from notches or scratches created during deployment; the high-density PE 100 base provides a notch resistance that is evaluated by ASTM D5397 notched constant tensile load testing. Because the sheet is black and exposed to UV, surface oxidation may occur over months of outdoor stockpiling; oxidative induction time measured by ASTM D3895 at 200°C is used as a quality gate for incoming sheet. Terminal applications are landfill basal liners, mining heap leach pads, brine evaporation ponds, and secondary containment basins. The compound is not recommended for direct contact with highly concentrated nitric acid or halogens, and designers must verify chemical resistance against the specific leachate composition.
Sheet and pipe sections made from TASNEE 100 BK are butt welded with hot plates at surface temperatures between 200°C and 220°C for chemical storage tanks, scrubbers, and ventilation ducting. The flat plate must be clean and non-stick coated; repeated heating of the same melt surface raises the gel content and reduces the oxidative induction time measured by ASTM D3895. Fabricators following DVS 2207-1 or national welding standards control plate temperature, change-over time, and joining pressure. Change-over times above 6 s allow the melt surface to cool below the crystalline melting range, producing a weak fusion line; change-over times below 3 s can entrap air and carbonized dust at the interface. The black compound provides consistent fusion pressure because carbon black increases thermal conductivity and reduces melt surface stickiness compared with unfilled HDPE. After welding, tensile testing of the joint is performed per ISO 13953 for butt-fused specimens; the failure mode should be ductile in the parent material outside the weld. Terminal fabrications include rectangular tanks for pickling acids, caustic soda storage up to 40% concentration at ambient temperature, and ductwork for corrosive vapours. The resin is not suitable for continuous storage of concentrated oxidizing acids, chlorinated solvents, or aromatic hydrocarbons without a chemical resistance review; swelling and environmental stress cracking are the dominant life-limiting mechanisms. Because the welded structure contains residual stress from sheet extrusion and weld bead removal, annealing is sometimes applied in sections thicker than 30 mm to reduce stress cracking in service.
In direct-buried cable conduit extrusion, the black HDPE compound runs at lower line speeds because the same high-molecular-weight backbone that meets pressure-pipe requirements also increases head pressure in grooved barrels. Melt temperature is kept at 200–215°C and vacuum sizing pressure is held at −0.2 to −0.4 bar to maintain outer diameter within ±0.3 mm on small-bore conduits. The carbon black loading of 2.0–2.5 wt% under ISO 6964 provides the UV resistance required by outdoor exposure specifications such as IEC 61386-24 for buried conduit systems and ASTM D3350 cell classification. Products are tested for crush resistance, low-temperature impact, and longitudinal reversion; excessive melt temperature or insufficient cooling can leave frozen-in orientation that shows reversion above 3% in hot-oil tests under ISO 2505 for pipe reversion. Because the black compound resists UV effectively, conduit can be stored outdoors for installation campaigns, but surface chalking may occur after extended exposure without affecting the internal cable environment. The low melt flow rate also helps maintain dimensional stability during vacuum sizing of ribbed conduit and multi-duct bundles. Terminal products are single-wall corrugated conduits, smooth-wall ducts, and multi-bore cable ducts for buried power and fiber-optic networks. This grade is not recommended for conduit exposed to continuous indoor high-temperature cable loads above 60°C, where heat distortion may reduce bore clearance.
Competitive Tasnee HDPE TASNEE TASNEE 100 BK prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Tasnee HDPE TASNEE TASNEE 100 BK is a bimodal high-density polyethylene pipe compound supplied as a black pellet. The grade carries a PE 100 designation under ISO 12162, corresponding to a minimum required strength of 10 MPa at 20 °C after 50 years in water. Carbon black is incorporated at a nominal 2.0–2.5 % m/m, giving the extruded pipe resistance to ultraviolet exposure during storage and above-ground service. The compound is intended for solid-wall pressure pipe extrusion; it is not formulated for rotomoulding, blown film, or injection-moulded fittings unless the converter performs independent qualification on those processes. The melt rheology, stabilizer package, and carbon-black dispersion are balanced for thick-wall pipe applications, not for thin-film or low-viscosity processing.
The grade differs from conventional unimodal HDPE in molecular architecture. A bimodal molecular weight distribution combines a high-molecular-weight fraction that raises slow crack growth resistance with a lower-molecular-weight fraction that controls shear viscosity during extrusion. In practice this permits a melt flow rate under ISO 1133-1 at 190 °C and 5 kg of 0.20–0.30 g/10 min while retaining pipe toughness; a unimodal HDPE at the same melt flow rate typically has lower resistance to slow crack growth and notched pipe failure under ISO 13479.
Compared with PE 80 black compounds, TASNEE 100 BK has a hydrostatic design basis of 10 MPa instead of 8 MPa. Under a service coefficient C = 1.25, the resulting design stress for water at 20 °C is 8.0 MPa, whereas PE 80 materials are limited to 6.3 MPa. For a fixed internal pressure and outside diameter the wall thickness reduction is approximately 21–25 %, based on the ratio of allowable design stresses. The thinner wall reduces feedstock consumption and installed pipe weight, but also raises the requirement for pipe dimensional control during calibration.
Relative to natural or coloured PE 100 compounds, the black grade relies on carbon black rather than synthetic UV absorbers for weathering resistance. The carbon black content is controlled by ISO 6964, and dispersion quality in the finished pipe is assessed by ISO 18553 or equivalent national standards. Natural PE 100 grades may offer easier colouring for blue or yellow pipe identification, while the black grade is normally used as solid black or with co-extruded identification stripes.
| Property | Method | Unit | Typical value or limit |
|---|---|---|---|
| Density | ISO 1183-1 | g/cm³ | 0.958–0.962 |
| Melt flow rate, 190 °C/5 kg | ISO 1133-1 | g/10 min | 0.20–0.30 |
| Carbon black content | ISO 6964 | % m/m | 2.0–2.5 |
| Tensile stress at yield | ISO 527-2 | MPa | 23–26 |
| Elongation at break | ISO 527-2 | % | >600 |
| Flexural modulus | ISO 178 | MPa | 800–1000 |
| Oxidative induction time at 210 °C | ISO 11357-6 | min | >20 |
| Minimum required strength, MRS | ISO 12162/ISO 9080 | MPa | 10 |
| Design stress, water at 20 °C, C = 1.25 | ISO 12162 | MPa | 8.0 |
Lot-specific certificates should be consulted before tooling design or pressure-rating calculations, because the values shown above are representative of industrial PE 100 black pipe compounds and may not match every production lot.
Long-term hydrostatic strength is validated through creep rupture data under ISO 1167 and extrapolation according to ISO 9080. Minimum required strength is 10 MPa. The resulting PE 100 classification under ISO 12162 permits a design stress of 8.0 MPa at 20 °C for water service using C = 1.25. At 40 °C, the conventional derating coefficient for PE 100 water service is approximately 0.74, reducing the effective design stress from 8.0 MPa to about 5.9 MPa. Continuous operation above 60 °C is outside the normal design envelope for pressure-rated HDPE pipe.
Slow crack growth resistance is a central requirement for buried pipe. PE 100 pipe compounds are characteristically evaluated in notched pipe tests under ISO 13479 at 80 °C. Published lot-specific times for TASNEE 100 BK should be obtained from the manufacturer certificate; the broad PE 100 classification requires the material to satisfy applicable hydrostatic and slow crack growth thresholds. Environmental stress crack resistance values for bimodal HDPE pipe grades commonly exceed 1,000 h under ASTM D1693 condition B, but the result is test-dependent and published data for this specific grade is limited.
Rapid crack propagation resistance is assessed by ISO 13477, the small-scale steady-state test at 0 °C. In field terms, a pipe with insufficient rapid crack propagation resistance can sustain axial crack propagation over long distances. The bimodal architecture of PE 100 grades is intended to suppress this failure mode at pressures above the maximum operating pressure of the installed pipe. Carbon black dispersion is not cosmetic; agglomerates larger than acceptable under ISO 18553 can act as stress concentrators and reduce slow crack growth performance.
On production-scale grooved-feed single-screw lines with L/D 30:1–36:1, the melt temperature for TASNEE 100 BK is held between 200 °C and 230 °C. The barrel profile from feed to adapter is typically 30–50 °C, 180–190 °C, 200–215 °C, 210–220 °C, and 210–220 °C. Die head and spider temperatures are usually maintained at 210–220 °C. At these settings the melt pressure at the die inlet commonly falls between 15 MPa and 25 MPa for medium-diameter pipe. Sustained die pressure above 30 MPa should be corrected by screen-pack adjustment or die sizing because it indicates excessive shear work and can raise melt temperature beyond specification.
Vacuum degassing at −0.08 MPa is used to remove volatiles and avoid surface porosity. Pre-drying is not normally required because the polymer is hydrophobic; if pellets have been stored in cold outdoor silos and then moved to a warm plant, condensed surface moisture can be removed at 80 °C for 1–2 h in a desiccant dryer. Drying above 100 °C can accelerate additive loss and should be avoided.
Residence time at melt temperature should be kept below 15 min. When line stoppages occur, the barrel should be purged with a low-density polyethylene or dedicated polyethylene purge compound to prevent carbon black deposits on screw roots and die lips. Carbon black deposits from HDPE black grades can score the screw if not purged before shutdown. Field data from long-diameter runs indicates that pressure fluctuations wider than ±1.5 MPa across a screw revolution suggest screw wear or unstable feed section temperature; the cause should be corrected before pipe wall thickness variation exceeds ±2 %.
Pipe calibration uses a vacuum calibration tank at −0.02 to −0.05 MPa; the first cooling spray or water bath is maintained at 30–40 °C, with subsequent bath at 20–30 °C. Higher first-tank water temperatures are used for thick-wall pipe to reduce residual stress and shrink-back. Low first-tank temperatures below 20 °C can increase axial orientation and reduce low-temperature impact resistance. The low melt flow rate of this grade requires high torque and head pressure; extruder motor load may become limiting with low L/D or worn screws.
The primary conversion route is solid-wall pressure pipe for municipal water distribution and transmission. Finished pipe is evaluated to the ISO 4427 series or regional equivalents such as EN 12201. At 20 °C water service the PE 100 design stress of 8.0 MPa supports standard dimension ratios from SDR 11 to SDR 26 depending on pressure class. Butt fusion welding is generally carried out under ISO 21307 procedures; electrofusion sockets are governed by ISO 12176 compatibility requirements.
For gas distribution, the compound may be used when the finished pipe conforms to ISO 4437 or EN 1555. Solid black pipe is acceptable in many national gas codes, with yellow identification stripes added by co-extrusion or marking. Design stress and temperature derating follow gas-specific standards; sustained operating pressure must be below the calculated maximum operating pressure.
Industrial pressure applications include seawater cooling lines, mining tailings, dredge discharge, and chemical transfer. The pipe wall must be selected after chemical resistance testing, commonly ISO 4433 or ISO 175 immersion data. Aromatic hydrocarbons, strong oxidizers, and some chlorinated solvents can reduce allowable stress or cause environmental stress cracking; specific service compatibility should be confirmed through immersion testing of the finished pipe.
| Attribute | TASNEE 100 BK | PE 100 natural/coloured | PE 80 black |
|---|---|---|---|
| Minimum required strength | 10 MPa | 10 MPa | 8 MPa |
| Carbon black content | 2.0–2.5 % m/m | 0 % m/m | 2.0–2.5 % m/m |
| Design stress, water at 20 °C | 8.0 MPa | 8.0 MPa | 6.3 MPa |
| UV stabilisation | Carbon black | Synthetic UV stabiliser | Carbon black |
| Relative wall thickness at equal pressure | Baseline | Same as baseline | 21–25 % thicker |
| Typical molecular architecture | Bimodal | Bimodal | Bimodal or unimodal |
The operational boundaries for this compound are defined by processing temperature and service temperature as much as by pressure. The pellets should be kept in sealed packaging and protected from prolonged weathering. Carbon black provides ultraviolet resistance, but surface oxidation of unstabilised pellet surfaces can still occur when bags are left open for extended periods. Silo and hopper temperatures should remain below 50 °C to prevent pellet agglomeration. The product is not formulated for direct food-contact use unless the final article meets the applicable migration test programme.
Final pipe certification for potable water may require NSF/ANSI 61, AS/NZS 4020, or national positive-list compliance; these certifications are completed by the pipe manufacturer, not the resin supplier. Under European regulation, the compound and its additives are subject to REACH registration and must be used within the conditions of the safety data sheet. RoHS heavy-metal restrictions generally apply to carbon black formulations only where electronic scrap or recycled feedstocks are introduced; converters should verify lot-specific certificates.
Melt blending with other polyethylene grades that have markedly lower melt viscosity or with unknown recycled HDPE containing high levels of unbound carbon black, calcium carbonate, or incompatible catalysts can reduce hydrostatic strength and create surface defects in the pipe bore. For colour changes from black to natural on the same extrusion line, a documented purge procedure with at least 5–10 barrel capacities of natural PE purge compound is required to remove carbon black carryover. Published data for this specific compound under every possible field configuration is limited; values in this document are representative of industrial PE 100 black pipe compounds and should be checked against the manufacturer’s lot certificate.