    Specifications
    HS Code 793237
    Density 0.955 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.04 g/10 min
    Tensile Strength At Yield 28 MPa
    Tensile Strength At Break 32 MPa
    Elongation At Break 600%
    Flexural Modulus 1100 MPa
    Notched Izod Impact Strength 23 C 100 J/m
    Vicat Softening Temperature 127°C
    Heat Deflection Temperature 0 45 Mpa 75°C
    Melting Temperature 132°C
    Hardness Shore D 65
    Environmental Stress Crack Resistance F50 >1000 h
    Water Absorption <0.01%
    Volume Resistivity >10^15 ohm·cm
    Dielectric Constant 1 Mhz 2.3
    Dissipation Factor 1 Mhz 0.0002
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C

    As an accredited Tasnee HDPE TASNEE F0455 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Tasnee HDPE TASNEE F0455 typically comes in 25 kg polywoven bags, palletized/shrink-wrapped, or 1,000 kg jumbo bags for bulk shipment.
    Container Loading (20′ FCL) Tasnee HDPE F0455, 25 kg bags palletized, securely stowed in a dry 20′ FCL, approximately 24–25 metric tons.
    Shipping Tasnee HDPE TASNEE F0455 is shipped as non-hazardous polyethylene pellets in moisture-resistant 25 kg bags or 1–1.5 MT jumbo bags, palletized and stretch-wrapped. Transport in dry, clean containers or trucks at ambient temperature, protected from sunlight, heat, moisture, and contamination. No hazardous classification; standard cargo handling applies.
    Storage Store Tasnee HDPE TASNEE F0455 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, clean, and palletized to prevent moisture, UV degradation, and contamination. Avoid excessive stacking. Do not store outdoors uncovered. Maintain good housekeeping, use FIFO stock rotation, and comply with local regulations.
    Shelf Life Shelf life is typically 24 months when stored in original packaging, dry, at ambient temperature, away from direct sunlight and heat.
    Application of Tasnee HDPE TASNEE F0455

    TASNEE HDPE F0455 is a high-molecular-weight high-density polyethylene blown film resin with nominal density 0.955 g/cm³ and melt flow rate 0.4–0.5 g/10 min under ISO 1133-1:2022 at 190°C/2.16 kg. Density is established by ISO 1183-1:2019 after conditioning at 23°C ± 2°C. The grade is selected for thin-gauge blown film segments where high modulus, low water vapour transmission, and down-gauging capacity outweigh low-speed puncture softness. Converter records from production-scale blown film lines indicate that F0455 behaves as a high-viscosity, medium-swell melt: single-screw extruders with L/D 24:1–30:1 may reach motor current limits before melt temperature exceeds 215°C, and head pressure can be 15–25% higher than with LLDPE of equivalent melt index. The following scenarios are limited to documented downstream HDPE blown film applications; the grade is not positioned for injection moulding, bottle blow moulding, or rotational moulding. Pre-drying is not required for closed-bag storage at ambient relative humidity below 60%; surface condensation should be removed by drying at 70–80°C for 1–2 h before extrusion.

    T-shirt grocery sacks are drawn to 8–25 µm on high-stalk lines

    Blown film lines producing T-shirt grocery sacks from F0455 specify the resin as the primary film-forming layer at 100 wt%; converters add 5–10 wt% LLDPE or 10–20 wt% clean post-industrial reclaim when dart impact and bubble stability must be adjusted for high-speed bag machines. The compliance boundary for grocery sacks without direct food contact is the EU Packaging and Packaging Waste Directive 94/62/EC Article 11, limiting the sum of lead, cadmium, mercury, and hexavalent chromium to 100 mg/kg, plus REACH Regulation (EC) No 1907/2006 Annex XVII substance restrictions; incidental food-contact acceptance is supported by FDA 21 CFR 177.1520(c) 3.2a for the olefin polymer. The downstream process is a high-stalk blown film line: die diameter 100–200 mm, die gap 1.2–1.8 mm, spiral mandrel die, blow-up ratio 3.5:1–5:1, melt temperature 190–215°C, and frost line height 5–8 die diameters. At frost line heights below 4 die diameters, machine-direction tear strength drops and bag handles split during automatic wicket punching; above 8 die diameters, haze increases and dart impact becomes inconsistent. In-process gauge variation is normally held to ±5% using capacitive or nuclear gauging, and automatic air ring control can reduce transverse gauge bands to ±2%. Dart drop impact on 25 µm film is measured under ASTM D1709-22 Method A; published data for this specific configuration is limited, but converter trials on F0455 should establish lot-specific values rather than relying on generic HDPE film data. Film is slit into tubing and converted by inline punching, side welding, and cutting into terminal products: shopper bags, grocery sacks, produce bags on rolls, and stack-pack consumer takeaway bags. Batch-to-batch viscosity differences are observed as screw motor amperage shifts of up to 10% at constant screw speed; this is the primary production-scale indicator of lot-to-lot melt flow rate drift.

    In waste bin liner production, the limiting failure mode is puncture and tear propagation along folded edges and heat-sealed corners, not pure tensile yield. F0455 is therefore modified with 10–25 wt% LDPE or LLDPE and, in cost-driven formulations, 5–15 wt% calcium carbonate masterbatch; the resultant reduction in flexural modulus is accepted because handle puncture and seal integrity improve at thin gauge. The compliance scope is non-food packaging under 94/62/EC Article 11 heavy metal limits and REACH SVHC communication duties under (EC) No 1907/2006; finished bin liners carrying recycled-content claims require substantiation under ISO 14021:2016 with clear post-consumer/post-industrial content percentages. Processing windows on conventional low-stalk or neutral-stalk blown film lines differ from grocery sack production: blow-up ratio is held at 2.5:1–3.5:1, die gap 1.4–2.0 mm, melt temperature 185–210°C, and film thickness ranges from 15 µm to 30 µm for household bin liners and up to 40 µm for commercial waste liners. High-shear dispersion of calcium carbonate masterbatch is required to prevent screen pack pressure rise behind 100–150 mesh screens; backpressure increases above 20% of the clean-resin baseline indicate agglomerate retention or insufficient distributive mixing. Terminal finished products include drawstring kitchen bags, household bin liners, can liners, and janitorial refuse sacks.

    What limits odour retention and WVTR in cereal liner coextrusions?

    Dry food cereal liners using F0455 in the core or external skin rely on the density-dependent reduction in water vapour transmission rate; published data for this specific configuration is limited, but HDPE blown film in the 0.950–0.960 g/cm³ range typically records WVTR between 4 g/m²·day and 8 g/m²·day at 38°C/90% RH for 25 µm film under ASTM F1249. In a three-layer coextrusion, F0455 is added at 20–35 wt% of the total structure, with LDPE or LLDPE seal skins and an optional EVA tie layer; the HDPE skin or core contributes flexural modulus and heat resistance above 115°C for downstream form-fill-seal operations. The compliance boundary is direct food contact: FDA 21 CFR 177.1520(c) 3.2a for films intended for aqueous, acidic, and low-fat dry foods, and Commission Regulation (EU) No 10/2011 Annex I with overall migration below 10 mg/dm² for the finished structure. The downstream production route is multi-layer blown film coextrusion with die gap 1.8–2.2 mm, blow-up ratio 2.8:1–3.5:1, and film thickness 35–60 µm, followed by flexo printing, lamination, slitting, and bag conversion. F0455 alone does not function as a heat-seal layer because high-speed VFFS seal jaws require seal bar temperatures above 150°C and a wider hot-tack window than the HDPE layer provides; the seal skins control seal initiation while the HDPE core supplies barrier. Terminal finished products include cereal box liners, biscuit and cracker inner packs, dry powder pouch liners, and bag-in-box liners for low-moisture foods.

    Heavy-duty sack liner conversion on wide-web blown film equipment uses F0455 as a stiffening resin in blends with 15–30 wt% LDPE or LLDPE, or as a neat high-modulus ply in 50–80 µm film. The addition ratio is governed by drop-weight performance: a neat F0455 ply increases energy-to-break but reduces low-speed puncture resistance in sub-zero handling, so converters run a three-layer structure with F0455 in the outer skins and LLDPE in the core to rebalance machine-direction tear and transverse-direction puncture. Compliance for industrial non-food sacks is restricted to REACH Annex XVII and 94/62/EC Article 11; UN dangerous goods packaging specifications under UN 6.1 or UN 6.5 apply only when the liner is part of a certified packaging combination and are tested on the finished packaging, not on the resin alone. Extrusion conditions include die diameter 250–450 mm, die gap 1.8–2.4 mm, blow-up ratio 2.0:1–2.8:1, and melt temperature 195–220°C; the lower blow-up ratio improves machine-direction tensile strength but sacrifices transverse tear resistance. Terminal finished products include liner bags for polymer granulate, carbon black, mineral fillers, corrosion inhibitors, and construction chemicals packaged inside multiwall paper sacks or rigid drums.

    When the HDPE ply replaces paper in multiwall bag moisture barriers

    Replacement of one paper ply with an F0455 high-density polyethylene film ply in multiwall bag structures occurs where the packed product requires resistance to grease, oil, or moisture ingress. The F0455 ply is typically 20–40 wt% of the total bag structure, with the remaining mass composed of kraft paper plies and a woven polypropylene outer or inner ply depending on stacking load. The film ply thickness is generally 30–50 µm, and the resin may be processed neat or with 0.5–2 wt% of a colourant or anti-block masterbatch. Standards include FDA 21 CFR 177.1520(c) 3.2a where incidental food contact with dry materials is expected, EU 10/2011 for migration compliance in the European market, and EN 13430:2004 material recovery considerations if recycling claims are made for the finished bag. The production route is flat die extrusion or blown film; flat die extrusion uses chill roll temperatures between 60°C and 90°C to control gauge bands and avoid stress whitening. Blown film processes for this application run at blow-up ratios 2.2:1–2.8:1 and melt temperatures 190–220°C. Terminal finished products include moisture-barrier liners for pet food multiwall sacks, mineral premix bags, seed bags, and bulk ingredient bags for flour or sugar where the paper plies provide mechanical abuse resistance and the HDPE ply provides the barrier.

    Wicketed produce bag conversion speed and the role of additive migration

    Retail produce bag production from F0455 runs at high line speeds, and the primary processing bottleneck is not bubble stability but coefficient-of-friction control and seal bar contamination. F0455 is typically blended with 1–3 wt% of a high-clarity LDPE carrier containing slip and anti-block concentrates; the effective erucamide addition falls below 500 ppm in the final film to avoid over-migration and bag blocking. The relevant compliance frame is food contact under FDA 21 CFR 177.1520(c) 3.2a and EU 10/2011, with the slip additive selected from the positive lists of 10/2011 Annex I or FDA 21 CFR 178.3860. Film is produced on dedicated HDPE blown film lines with die diameter 50–80 mm for narrow webs, die gap 0.8–1.4 mm, blow-up ratio 3.0:1–4.0:1, and melt temperature 180–200°C. Gauge is reduced to 7–12 µm; at this gauge, F0455 bubble stability is acceptable only when the frost line is rigidly controlled at 4–6 die diameters and ambient air turbulence around the bubble is minimised. Terminal finished products include wicketed produce bags, self-opening stack bags, mini bread bags, and thin HDPE sleeve packaging for textile and hardware retail.

    Free Quote

    Competitive Tasnee HDPE TASNEE F0455 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Tasnee HDPE TASNEE F0455 is a high-density polyethylene film extrusion resin in which the grade code carries the flow and density profile: a nominal melt flow rate of 0.45 g/10 min at 190 °C under 2.16 kg load, measured in accordance with ISO 1133-1:2022, and a nominal density of 0.955 g/cm³ determined under ISO 1183-1:2019. The resin is intended for thin-gauge blown film in high-stalk and in-pocket bubble configurations. Primary converting applications include T-shirt carrier bags, produce bags on roll, bin liners, and light industrial liners. The grade is not a blow moulding or pipe extrusion resin; its molecular weight distribution and additive package are set to balance bubble stability, drawdown, and dart impact in film rather than parison melt strength or hydrostatic pressure resistance.

    The product is marketed as a single-pellet HDPE film resin. Producer data sheets list melt flow rate under ISO 1133-1:2022 and density under ISO 1183-1:2019 as the two rheological anchors for incoming inspection. Converters frequently cross-check melt flow rate under ASTM D1238-20 condition 190/2.16 and density under ASTM D1505-18 when local laboratory equipment is configured to ASTM methods. A difference between these methods is a method-equivalence issue, not a specification change.

    What Distinguishes F0455 from Lower-Melt-Index HDPE Film Grades?

    The differentiation is primarily rheological. A lower-melt-index high-molecular-weight HDPE film grade in the 0.20–0.30 g/10 min range has higher extensional viscosity, which supports a taller bubble stalk and improves dart impact but raises head pressure and limits screw-speed capacity. F0455 at 0.45 g/10 min reduces melt pressure and permits higher throughput at the same extruder speed, but the bubble stalk is more sensitive to air turbulence and film gauge variation when the melt temperature is excessive. Against a 0.70 g/10 min medium-melt-index HDPE film grade, F0455 provides more bubble stability and better gauge uniformity in thin film, at the cost of slightly higher energy input per kilogram. These differences are observed in line behaviour rather than in simple tensile values.

    Grade reference pointMelt flow rate (ISO 1133-1:2022)Relative bubble stabilityRelative output at constant rpmTypical application bias
    Tasnee HDPE TASNEE F04550.45 g/10 minmoderate-highintermediatethin-gauge sacks, bin liners
    Representative HMW film HDPE0.25 g/10 minhighlowerheavy-duty sacks, industrial liners
    Representative medium-MFR film HDPE0.70 g/10 minmoderatehigherhigh-output thin film, less impact-critical

    Published data for F0455-specific comparative values across commercial extruders is limited; the table is a relative ranking frequently observed on grooved-feed blown film lines and should be validated on the target die geometry.

    The microstructure underlying the 0.45 g/10 min flow is not fully disclosed on public datasheets. Two HDPE film grades with the same melt index and density can differ in molecular weight distribution, comonomer type, and short-chain branch distribution. Gas-phase and slurry-loop HDPE grades may respond differently to shear and extensional deformation. Therefore, the producer’s gel permeation chromatography data should be consulted when a converter needs to predict die pressure, dart impact, or bubble behaviour on a specific line. Published data for F0455-specific molecular architecture is limited.

    On air-cooled blown film lines, F0455 is typically processed on a grooved-feed extruder with a screw L/D ratio between 24:1 and 30:1 and a spiral mandrel or radial-flow die with a die gap of 1.2 mm to 2.0 mm. Melt temperature is normally held between 190 °C and 220 °C; melt temperatures above 240 °C increase gel-particle formation risk and should be avoided. Blow-up ratios between 2.5:1 and 4.0:1 are used depending on flat width and final film balance. The HDPE high-stalk bubble process is standard: the bubble neck is extended to 6–10 die diameters above the die before transverse expansion. The frost line height is adjusted between 6 and 12 die diameters to balance optical quality and machine-direction tear resistance.

    Screen packs of 40/60/80 mesh are used on 60 mm to 90 mm extruders to trap char and increase head pressure. Opening the die gap to 2.0 mm lowers orientation and can improve tear resistance in thicker liner film; closing the die gap to 1.2 mm supports drawdown in thin-gauge sacks but increases melt fracture risk if the die land temperature falls below 180 °C. Field failures observed with this class of HDPE film include bubble flutter when specific output is raised too quickly, melt fracture in thick-gauge in-pocket operation at low die temperatures, and machine-direction tear loss when the bubble is over-stretched. These are controlled by lowering melt temperature, widening die gap, or reducing draw-down ratio, not by changing the resin alone. Incoming lots should be checked against the certificate of analysis for melt flow rate and density because lot-to-lot variation in the 0.45 g/10 min specification can alter bubble height and extruder amperage on a 90 mm line. A melt flow rate shift of 0.05 g/10 min is more significant than a density shift of 0.002 g/cm³ for most blown film lines.

    Capillary rheometry data for the grade are not always published. For a nominal melt flow rate of 0.45 g/10 min, low-shear viscosity is governed by weight-average molecular weight and polydispersity; HDPE grades generally do not rely on long-chain branching as heavily as LDPE. The shear viscosity follows the normal temperature dependence of high-density polyethylene: a shift in melt temperature from 190 °C to 220 °C reduces viscosity by approximately 15–25% depending on shear rate. This range is an engineering estimate based on published HDPE viscosity data, not an F0455 datasheet value. Die pressure on a spiral die is therefore more sensitive to melt temperature than to barrel setpoint changes. Converters adjusting melt temperature to control bubble stability should measure actual melt temperature with an immersion probe before the die rather than relying only on the first barrel zone thermocouple.

    Coextrusion Layer Structures and Reclaim Placement

    F0455 is commonly placed in the core layer of three-layer coextruded film structures, where its density contributes modulus and its film-grade melt strength supports the bubble. LLDPE skins are used for seal initiation and dart impact; layer distributions such as 20/60/20 or 30/40/30 are selected according to seal strength and stiffness targets. Post-industrial trim reclaim is introduced into the core layer, but the permissible fraction is gauge-dependent and must be validated by gel-count measurement and film tensile retention. No universal reclaim limit is available for all film lines; converters should establish a limit using ASTM D882-18 tensile retention and ASTM D1709-15a dart impact after reclaim addition.

    When F0455 is coextruded with LLDPE skins, the migration of low-molecular-weight additives into the food-contact layer must be assessed under EU 10/2011 overall migration testing and FDA 21 CFR 177.1520 end-use extraction limits. The HDPE core is not a sealant resin; seal initiation temperature is governed by the skin layer. This placement permits downgauging while maintaining tensile modulus, but the film remains limited by machine-direction tear and dart impact, not by stiffness alone.

    The Stiffness-Tear Balance Limits the Downgauging Envelope

    The density of 0.955 g/cm³ places F0455 at the upper end of the HDPE film density range. Higher density increases tensile modulus and yield stress, which supports thin-gauge stiffness, but it also reduces low-strain puncture and can amplify orientation effects in the machine direction. In mono-layer films below approximately 12 µm, the machine-direction Elmendorf tear measured by ASTM D1922-09 or ISO 6383-2 often becomes the limiting property. Dart impact is measured by ASTM D1709-15a or ISO 7765-1; the value is influenced by blow-up ratio, frost line height, and die gap, not by resin density alone. Film tensile properties are evaluated by ASTM D882-18 or ISO 527-3. Published F0455-specific mechanical specifications are limited; converters should determine the dart impact and tear values on their own line geometry because these values are geometry-dependent.

    Compared with a lower-density HDPE film grade in the 0.946–0.950 g/cm³ range, the 0.955 g/cm³ F0455 is expected to show higher tensile modulus at comparable gauge but lower tear resistance in an unbalanced film. This trade-off defines the envelope in which the grade can be used for thin sacks without a high proportion of LLDPE. Increasing blow-up ratio from 2.5:1 to 4.0:1 can improve machine-direction tear but reduces line speed and may increase dart impact variability. A design of experiments varying blow-up ratio, frost line height, and die gap is required to locate the acceptable operating window for a specific film end-use; the specification sheet alone cannot predict this window.

    When F0455 Replaces a 0.30 Melt-Index Grade on Existing Lines

    Substitution on an existing blown film line configured for a 0.30 g/10 min HMW film grade requires more than screw-speed changes. Since F0455 has a lower melt viscosity at 190 °C, the extruder head pressure across the screen changer and die decreases, and the pressure-limited output ceiling rises. Screw speed can typically be increased, but the bubble must be rebalanced because the lower extensional viscosity reduces tolerance to air turbulence. The high-stalk neck height may need to be reduced by 1–3 die diameters, and the melt temperature setpoint may need to be reduced by 5–10 °C to prevent excessive film softness and blocking on the collapsing frame. The expected change in output at constant screw speed is screw-dependent; published data for F0455-specific output gains is limited. On 70 mm and 90 mm grooved-feed extruders, the most frequently reported operational issue is machine-direction gauge wobble when the same frost line height is retained; the correction is to lower the frost line and increase blow-up ratio slightly, not to add process aids.

    If the line uses internal bubble cooling, the air flow and exhaust should be recalibrated because the lower melt strength F0455 bubble reaches its final orientation earlier than a 0.30 g/10 min grade at high throughput. Surface splay caused by surface moisture appears when resin is stored above 60% relative humidity; hopper drying at 80 °C for 2 h resolves the defect. Contamination with PVC or polyacetal regrind must be excluded because acidic degradation products at melt temperatures above 220 °C accelerate chain scission and odour.

    T-shirt bag converting lines use impulse or hot-knife sealing. Heat seal strength is tested according to ASTM F88/F88M-21; failure modes include delamination or brittle failure at the seal edge. Corona treatment is required for ink adhesion on HDPE film. Surface energy is typically raised to 38–42 mN/m and monitored according to ISO 8296:2003. Treatment decay is time-dependent and must be controlled before printing.

    Regulatory compliance for F0455-based film is application-specific and must be confirmed by the converter. The base olefin polymer falls within the scope of FDA 21 CFR 177.1520 for olefin polymers when the finished article meets extraction limits for the intended food type and use temperature. Migration into food is assessed under EU 10/2011 overall migration and specific migration limits; the result depends on film thickness, time, temperature, and the complete additive package, not on the base resin alone. Overall migration for plastic food-contact articles is limited to 10 mg/dm². REACH registration is governed by EC 1907/2006 and is a supplier/importer obligation. RoHS Directive 2011/65/EU restricts lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE in homogeneous materials; packaging for electrical and electronic equipment should be covered by a material declaration from the film producer.

    Regulatory referenceScopeF0455 applicability
    FDA 21 CFR 177.1520Olefin polymers for food contactFinished film must meet extractive limits for food type and use temperature; converter verification required
    EU 10/2011Plastic food-contact materials and articlesOverall migration and specific migration limits apply to final film, including additives and printing
    EC 1907/2006 (REACH)Registration, evaluation, authorisation of chemicalsSupplier/importer registration; SVHC article obligations if applicable
    2011/65/EU (RoHS)Restriction of hazardous substances in EEEApplies only if film is part of EEE or packaging; heavy metal limits at homogeneous material level

    Post-industrial F0455 reclaim can be reintroduced into the core layer of similar HDPE film structures. The amount is limited by gel count and film appearance. Polypropylene contamination in post-consumer recycled HDPE streams lowers dart impact and increases haze; melt filtration removes large particles but not molecular-scale contamination. Differential scanning calorimetry according to ISO 11357-3 can be used to detect polypropylene contamination by melting endotherm separation. Uncontrolled peroxide masterbatch addition should be avoided because it can shift the melt flow rate and generate gels. Acidic regrind streams and high-temperature excursions above 240 °C are the primary operational boundaries. The grade should be dried only when surface moisture is present; prolonged high-temperature drying of HDPE is not required and can increase energy consumption without benefit.