| HS Code | 207558 |
| Product | Tasnee HDPE TASNEE B1258 |
| Density | 0.958 g/cm³ |
| Melt Flow Rate 190 C 21 6 Kg | 12 g/10 min |
| Melt Flow Rate 190 C 2 16 Kg | 0.12 g/10 min |
| Tensile Strength At Yield | 28 MPa |
| Tensile Strength At Break | 35 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 1200 MPa |
| Izod Impact Strength Notched 23 C | 20 kJ/m² |
| Vicat Softening Temperature | 127°C |
| Heat Deflection Temperature 0 45 Mpa | 85°C |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Hardness Shore D | 66 |
| Melting Point | 134°C |
| Water Absorption | <0.01% |
As an accredited Tasnee HDPE TASNEE B1258 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Tasnee HDPE TASNEE B1258 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for secure storage and transport. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Tasnee HDPE TASNEE B1258, 25kg bags, palletized, shrink-wrapped, securely stowed inside a 20-foot full container load. |
| Shipping | Tasnee HDPE TASNEE B1258 is a non-hazardous polyethylene resin supplied as pellets in 25 kg bags or 1 MT jumbo bags, palletized and stretch-wrapped. Ship in clean, dry containers or trucks, protected from moisture, heat, and direct sunlight. Store in a cool, dry, ventilated area. |
| Storage | Store Tasnee HDPE B1258 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain clean, dry floors and use appropriate pallets. Store separately from incompatible materials. Ensure containers are properly labeled. |
| Shelf Life | Shelf life: Store in original packaging, cool and dry; typically 24 months, but indefinite if protected from heat, moisture, and UV. |
The conversion of Tasnee HDPE TASNEE B1258 into UN-certified tight-head jerricans and open-top pails places the greatest demand on parison sag resistance and high-load melt strength because the 20 L jerrican sidewall is typically 0.9–1.2 mm thick while the handle pinch-off and bottom corners must remain above 1.2–1.6 mm. The blow moulding cell is configured around a 75 mm single-screw extruder with a 24:1–30:1 L/D ratio, a grooved feed section, and an accumulator head with 64-point parison programming; the melt is held at 175–210 °C at the die, the die gap is programmed from 0.8 mm to 2.4 mm across the parison stroke, and blow air pressure is set at 0.6–0.8 MPa. Mould cooling water is maintained at 10–20 °C, and melt pressure at the head is limited to 20–35 MPa to prevent shear heating that initiates molecular weight degradation in the regrind fraction. Formulation for a UN 3H1 jerrican body contains 65–80 wt% virgin B1258 pellets, 20–35 wt% in-house regrind from the same article, 1.0–2.0 wt% UV/colour masterbatch, and 0.1–0.3 wt% processing stabiliser. The use of regrind above 35 wt% in UN packaging must be revalidated by the drop test and stack test of ADR 6.1.5; if the pellet-to-regrind ratio varies by more than ±5 wt%, the environmental stress crack resistance determined by ASTM D1693 with 100% Igepal CO-630 and the −18 °C drop impact margin degrade non-linearly. Compliance marking under the UN Model Regulations, ADR, RID, IMDG Code, and 49 CFR Part 178 requires a 6.1.5.3 leakproofness test, a 6.1.5.3.2 drop test at 1.2 m for Packing Group II liquids, and a 6.1.5.6 stacking test for 28 days at 40 °C. Terminal articles are 10 L, 20 L, 25 L, and 30 L tight-head jerricans, 10 L open-top pails, and 120 L large-neck drums, used for corrosive solids, water-treatment chemicals, lubricant additives, and non-flammable industrial liquids.
For sodium hypochlorite packaging between 3% and 15% available chlorine, the bottle wall must retain environmental stress crack resistance after prolonged contact with oxidative fill, but the first mechanical failure is often not at the sidewall—it is microcrack initiation at the pinch-off tail, where molecular orientation and residual stress from pinch closure exceed 20 MPa in polarised light inspection. The formulation is maintained at 98.0–99.5 wt% B1258, 0.5–1.0 wt% white masterbatch based on a linear low-density polyethylene carrier, 0.05–0.15 wt% antioxidant, and 0.05–0.15 wt% acid neutraliser; post-consumer recyclate is excluded, and in-house regrind is limited to 10–20 wt% only if the regrind is dried to below 200 ppm moisture and a 500-hour ASTM D1693 ESCR screen at 50 °C shows no crack propagation beyond 10% of specimen width. Production is performed on 8- to 12-cavity shuttle blow moulding machines with 24:1–28:1 L/D extruders, melt temperature at the die of 175–195 °C, mould coolant at 10–18 °C, and blow air at 0.5–0.75 MPa. Parison weight is controlled to ±0.3 g per cavity; cavity-to-cavity wall thickness variation above ±0.05 mm triggers a leak test escalation. Bottles are evaluated by ASTM D2463 drop impact at −18 °C after 24 h conditioning, with acceptance of no fracture at 1.2 m for 1 L bottles. At sodium hypochlorite concentrations above 10%, the closure seal area is thickened to more than 1.6 mm to prevent environmental stress cracking at the neck. Compliance includes the EU Detergents Regulation (EC) No 648/2004, CLP (EC) No 1272/2008 for label and child-resistant closure requirements, and the UN GHS transport classification for filled products. Terminal types are 0.5 L, 1 L, 2 L, and 5 L bottles for bleach, surface cleaner, drain cleaner, and fabric softener lines, with 38 mm and 42 mm neck finishes and induction-sealed closures.
In oral solid dose packaging, the extrusion blow moulding cell is qualified under ISO 14644-1 Class 8, and B1258 is used only where site-specific USP <661.1> and USP <661.2> qualification demonstrates that the lot meets the required plastic packaging system limits. The formulation is 99.9–100.0 wt% B1258, with no slip agent, no antistat, and no processing aid unless an added masterbatch is documented in a drug master file and migration testing under ICH Q3D demonstrates elemental impurity levels below the permitted daily exposures for oral solid dose presentations. If a tinted bottle is required, a phthalate-free colour masterbatch is limited to 0.05–0.20 wt%; the carrier resin must be from the same polyethylene family, and the colourant must comply with FDA 21 CFR 178.3297. Bottle production is performed on two-stage extrusion blow moulding machines with 10–16 oval cavities, 50–75 mm extruders, polished stainless steel blow pins, and filtered blow air at 0.2 μm. Melt temperature is 170–195 °C, cooling water is maintained at 8–18 °C, and blow air pressure is 0.4–0.6 MPa. After moulding, bottles enter a vacuum decay leak test at −5 kPa for 5 s, then a UV-cured inkjet coding step with no solvent penetration. Moisture transmission is within the range required by USP <671> for high-density polyethylene bottles used for solid oral dose forms when the wall thickness is 0.7–1.2 mm. Migration compliance under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011 is confirmed by overall migration below 10 mg/dm² in 3% acetic acid, 10% ethanol, and olive oil simulants. Terminal products are 15 ml to 500 ml bottles for tablets, capsules, and granule presentations, including child-resistant and tamper-evident neck configurations. Polyethylene homopolymer is not an oxygen barrier; oxygen-sensitive pharmaceuticals require a foil induction seal or coextrusion with a polyamide or EVOH barrier layer.
Water-based agrochemical formulations with pH 4 to 9 and emulsifiable concentrate adjuvants are filled into 5 L, 10 L, and 20 L B1258 tight-head containers. The formulation for crop protection packaging is 88–96 wt% B1258, 10–20 wt% in-house regrind, 1–2 wt% UV-stabilised masterbatch containing 0.1–0.3 wt% HALS, and 0.05–0.15 wt% processing antioxidant; carbon black masterbatch at 0.5–1.0 wt% is used when the pack must be opaque for UV-sensitive actives. Because a 20 L container with a 1.5 mm nominal wall and a 120 mm neck requires a parison shot weight of 1.8–2.4 kg, the accumulator head is programmed with 20–32 points; the wall thickness at the handle and bottom corners is increased to 1.6–2.0 mm while the sidewall is reduced to 0.9–1.2 mm. Die gap modulation from 0.8 mm to 2.2 mm and melt temperature 175–210 °C are used. Blow air pressure is 0.7–0.9 MPa, and mould cooling is 12–22 °C. Drop testing follows UN 6.1.5.3.2 for Packing Group II at 1.2 m; samples are conditioned at −18 °C for 24 h and tested with water-glycol-filled containers. If the sidewall thickness drops below 0.7 mm, the ESCR of the handle pinch-off zone under ASTM D1693 condition B declines and the hydraulic pressure test under ADR 6.1.5.5 may fail at 100 kPa internal pressure. The moulds are fitted with interlocked blow pins and leak-detection probes; after trimming, containers are flame-treated on the closure land to 38–42 mN/m for label adhesion. Compliance includes the UN Model Regulations, ADR, RID, and national pesticide packaging regulations under FAO/WHO guidelines; in the US, 40 CFR Part 165.21 sets container residue removal limits. Terminal products are 1 L, 5 L, 10 L, 20 L, and 30 L containers for fungicide, herbicide, insecticide, and biostimulant formulations, with 45 mm and 63 mm UN-rated closures.
Automotive ethylene glycol and propylene glycol coolant concentrates in 1 quart to 1 US gallon HDPE bottles are produced in high-cavitation shuttle lines where the wall must resist low-temperature drop after prolonged contact with corrosion inhibitor additives. The compound is 95–98 wt% B1258, 1.0–1.5 wt% blue or green masterbatch, 0.05–0.10 wt% antioxidant, and 0.05–0.10 wt% slip/anti-block masterbatch. In-house regrind is acceptable up to 25 wt% only when the regrind source is restricted to unpigmented or identically pigmented coolant bottles; cross-contamination with brake fluid bottles is excluded because ester-based brake fluid causes stress cracking in polyethylene. Production uses 6- to 10-cavity extrusion blow moulding machines with 24:1–28:1 L/D extruders, melt temperature at 175–200 °C, mould cooling at 8–18 °C, and blow air at 0.5–0.75 MPa. The neck finish for windshield washer fluid is 38 mm, while coolant concentrates use 42 mm and 53 mm closures with vented induction seals. Bottles are tested under ASTM D2463 at −18 °C with a 1.2 m drop; windshield washer fluid with methanol above 20 wt% may trigger dangerous goods classification under the UN Model Regulations for flammable liquids, although common consumer products are often formulated below the regulated threshold. Top-load strength is measured for pallet stacking of 3–5 layers; a 1 US gallon bottle typically withstands an empty top load of 200–350 N. Terminal products are 1 quart, 1 US gallon, 5 L, and 20 L containers for engine coolant, antifreeze, windshield washer fluid, and non-toxic antifreeze lines.
Tasnee HDPE TASNEE B1258 enters food packaging only when site-specific FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011 compliance tests on the finished article confirm migration limits, because cross-contamination with colour masterbatch or industrial regrind invalidates the food-contact declaration. The formulation is 99.0–100.0 wt% B1258, 0–0.5 wt% white masterbatch if opacity is needed, and 0.05–0.10 wt% process stabiliser; no post-consumer recyclate is permitted. Melt temperature is maintained at 175–195 °C, and the extruder is run at a screw speed of 40–80 rpm on a 60 mm, 24:1 L/D single-screw machine. The blow moulds are cooled with water at 8–15 °C and are fitted with reverse-taper cooling drums at the neck to prevent ovality and improve dimensional repeatability. Bottles for edible oil, honey, syrup, and sauces are produced in 250 ml to 5 L sizes, with 38 mm, 43 mm, and 45 mm neck finishes. The main limitation of monolayer HDPE is gas and aroma permeability: oxygen transmission rate is in the 1,000–2,500 cm³/m²·day·0.21 atm range at 23 °C and 0% RH, and limonene vapour can be absorbed into the polyolefin wall, altering organoleptic persistence. For oxygen-sensitive foods or flavour retention beyond 6 months, coextrusion with an EVOH barrier layer or nitrogen-flushed filling with foil-sealed closures is required. Sensory testing per DIN 10955 and migration testing under EU Regulation (EU) No 10/2011 for aqueous, acidic, and alcoholic simulants must be conducted on the finished bottle, because the extrusion heat history can alter low-molecular-weight extractable fractions. Terminal products are bottles for table syrup, honey, edible oil, soy sauce, and powdered infant formula scoops; however, published data for B1258 in high-acid hot-fill applications is limited, and high-acid hot-fill above 60 °C is not recommended without a specific migration study.
Competitive Tasnee HDPE TASNEE B1258 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Tasnee HDPE TASNEE B1258 is a high-molecular-weight high-density polyethylene blow moulding grade supplied in pellet form. Its nominal high-load melt flow rate is 8.0 g/10 min at 190 °C under 21.6 kg, tested according to ISO 1133-1:2022 or ASTM D1238-20. The nominal density is 0.958 g/cm³ under ISO 1183-1:2019 or ASTM D1505-18. This combination places the resin in the upper-density HDPE blow moulding segment, where high melt strength and long-chain architecture are required to support heavy parisons during accumulator-head extrusion. The grade is intended for large-volume containers such as industrial drums, jerry cans, intermediate bulk containers, and automotive fuel tanks, in which wall thickness generally exceeds 1.5 mm and prolonged chemical contact may occur. Unlike lower-density HDPE blow moulding resins, the 0.958 g/cm³ density contributes to higher top-load rigidity. Unlike fractional-melt HLMI resins, the 8.0 g/10 min value allows practical extrusion throughput without automatically sacrificing environmental stress crack resistance in thick-walled parts.
| Property | Test method | Nominal value |
|---|---|---|
| High-load melt flow rate, 190 °C, 21.6 kg | ISO 1133-1:2022 / ASTM D1238-20 | 8.0 g/10 min |
| Density | ISO 1183-1:2019 / ASTM D1505-18 | 0.958 g/cm³ |
| Tensile stress at yield | ISO 527-2:2012 / ASTM D638-14 | 28 MPa |
| Tensile elongation at break | ISO 527-2:2012 / ASTM D638-14 | >600 % |
| Flexural modulus | ISO 178:2019 / ASTM D790-17 | 1,200 MPa |
| Environmental stress crack resistance, 100 % Igepal CO-630, 50 °C | ASTM D1693-15 condition B | >600 h |
The values above should not be interpreted as specification release limits. Lot-to-lot variation, specimen conditioning, and conversion method influence the measured result.
Processing conditions for this grade are constrained by the need to retain parison hang strength while maintaining extruder output. On grooved-feed single-screw machines with an L/D ratio between 25:1 and 30:1, barrel profiles are typically set from 180 °C at the feed zone to 230 °C at the discharge. Head and die zones are normally held between 190 °C and 210 °C. If die temperature exceeds 220 °C, heavy parisons for parts above 60 L may sag before mould closure, leading to non-uniform wall thickness at the sidewalls. If die temperature falls below 180 °C, melt fracture can appear at the die lip and pinch-off weld strength can decline because of poor fusion. The resin’s high molecular weight fraction produces die swell values commonly in the range of 15 % to 35 %, depending on die geometry and shear rate. Accumulator-head machines should therefore use tooling with programmed parison wall-thickness control and adjust die gap after evaluating swell on the production tool.
Extruder screw geometry affects melt temperature and output. Low-compression, high-torque screws with distributive mixing sections are preferred for this grade. High-shear barrier screws can generate excessive viscous heating at high screw speeds. If melt temperature exceeds 240 °C, oxidative degradation may reduce environmental stress crack resistance and increase gel formation, even when the moulded part passes dimensional checks. Practical output is therefore limited by screw torque and melt temperature rather than by die pressure alone.
Mould temperature also influences cycle time and dimensional stability. For containers with wall thickness in the 2 mm to 4 mm range, cooling water temperatures between 10 °C and 40 °C are typical. Heat removal is limited by the low thermal conductivity of HDPE; internal flash and pinch-off areas remain hot after demoulding. Insufficient cooling produces warpage and package closure interference, particularly in drum lids. Shrinkage after 24 h can reduce effective closure diameter by approximately 0.3 % to 0.8 %. Published data for this specific configuration is limited, so these values are starting-point estimates rather than product specifications.
Pinch-off weld integrity is a common failure mode in large containers. Weld lines form where the parison is compressed at the mould parting line; insufficient die temperature or excessively fast mould close can produce cold weld zones with reduced peel strength. For agricultural chemical containers, weld performance is often assessed by drop testing after conditioning at -18 °C, while automotive fuel tanks may require testing at -40 °C. The base resin’s high molecular weight contributes to weld toughness, but the moulded part must be designed with adequate pinch-off land length and no sharp radii at the parting line.
The grade’s resistance to slow crack growth is characterized by the notched bent-strip test under ASTM D1693-15 condition B. Manufacturer technical documentation indicates failure time above 600 h in 100 % Igepal CO-630 at 50 °C. This value is method-dependent and should not be used to predict service life without finite element analysis or full-scale container testing. For load-bearing chemical exposure, notched constant tensile load testing under ASTM D5397-20 with a 0.30 mm notch depth may provide a more conservative ranking of high-molecular-weight HDPE grades. In aggressive wetting agents, environmental stress crack resistance can decline rapidly if the resin is contaminated with lower-molecular-weight polyethylene or incompatible masterbatch carriers.
Chemical compatibility follows semicrystalline HDPE behaviour. Aqueous acids, alkalis, and many polar solvents are handled at ambient temperature without significant loss of tensile yield strength, as measured by immersion testing under ISO 175:2010 or ASTM D543-21. Aromatic hydrocarbons, chlorinated solvents, and some oxygenated fuels swell the amorphous phase and reduce container stiffness. For automotive fuel tanks or solvent-containing containers, fluorination or sulfonation of the moulded surface is required to reduce permeation below regulatory evaporative emissions thresholds; the base resin does not provide sufficient barrier alone.
Primary application field is extrusion blow moulding of containers with capacity between 5 L and 220 L. Typical parts include agricultural chemical packs, automotive fuel and diesel exhaust fluid containers, industrial drums, and intermediate bulk packaging. In these service environments, the critical performance parameters are top-load compression strength, drop impact at low temperatures, and environmental stress crack resistance after long contact with packaged fluid. The resin is not normally specified for injection moulding, film, or pipe extrusion; its high molecular weight and low high-load melt index are intended for thick-walled blow moulded structures.
When compared with lower-density HDPE blow moulding grades, the 0.958 g/cm³ density of B1258 produces higher flexural modulus and top-load strength. A lower-density grade at 0.946 g/cm³ can exhibit higher ESCR under some conditions but may require thicker walls to achieve the same stacking load. A general-purpose unimodal HDPE blow moulding grade with HLMI near 12 g/10 min may process at faster cycle times in small containers, but its slow crack growth resistance may be lower in aggressive surfactant solutions. Injection moulding HDPE grades with melt flow rates above 20 g/10 min at 190 °C and 2.16 kg cannot form stable parisons for large blow moulded parts because their low melt strength causes rapid sag.
Compared with polypropylene, B1258 has lower density than many mineral-filled PP compounds and better semistatic fatigue resistance in thin-walled flexing sections, but lower continuous-use temperature and greater hydrocarbon permeation. It is melt-reprocessable and can be used in applications where crosslinked polyethylene would be over-engineered. However, mixing with even 10 % by weight of a low-molecular-weight HDPE can reduce ESCR non-linearly, so regrind streams from mixed-property parts should be controlled by melt-flow testing before reuse in load-bearing container walls.
Comparative data against pressure pipe PE100 resins are not directly applicable because pipe grades are optimized for hydrostatic strength at 20 °C and 60 °C under ISO 9080, whereas blow moulding grades are optimized for ESCR and parison melt strength. Transferring a pipe-grade HLMI to blow moulding may give high ESCR but poor parison hang strength due to a different molecular weight distribution.
Food contact and regulatory status require grade-specific confirmation. The resin may be suitable for food contact under 21 CFR 177.1520 when the finished article meets the end-use conditions specified in that section, but no blanket approval is implied. For EU food contact, compliance with Regulation (EU) No 10/2011 requires migration testing on the final container. REACH article provisions under EC 1907/2006 impose communication obligations only if a substance of very high concern is present above 0.1 % w/w in the article. For UN-certified dangerous goods packagings, performance tests under UN 6.1 and ADR/RID include drop, stacking, and leakproofness requirements that depend on container design, wall thickness distribution, and closure system.
Storage and handling affect processing consistency. While HDPE does not require drying for absorbed moisture, surface condensation from cold pellets introduced into a warm hopper can generate steam bubbles and pinholes. Pellets stored outdoors should be brought to ambient indoor temperature before conveying. Ultraviolet exposure during long outdoor storage degrades surface molecular weight and can shift HLMI values, so bulk storage should be indoors or under opaque covers. The resin should not be blended with amine-based processing aids that can catalyse oxidation at processing temperatures unless the additive supplier provides thermal stability data under extrusion conditions.