    • Product Name: Sumitomo Chemical HDPE F0554T
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 968271
    Product Name Sumitomo Chemical HDPE F0554T
    Manufacturer Sumitomo Chemical
    Polymer Type High Density Polyethylene (HDPE)
    Grade F0554T
    Density 0.954 g/cm³
    Melt Flow Rate Mfr 5.0 g/10 min (190°C, 2.16 kg)
    Tensile Strength At Yield 29 MPa
    Tensile Elongation At Break >500%
    Flexural Modulus 1,200 MPa
    Notched Izod Impact Strength 50 J/m
    Vicat Softening Point 127°C
    Heat Deflection Temperature 110°C at 0.45 MPa
    Melting Point 134°C
    Shore D Hardness 66
    Mold Shrinkage 2.0%
    Water Absorption <0.01%
    Dielectric Constant 2.3 at 1 MHz
    Volume Resistivity >10^16 Ω·cm

    As an accredited Sumitomo Chemical HDPE F0554T factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sumitomo Chemical HDPE F0554T comes in 25 kg polyethylene-lined bags, stacked on pallets for transport and storage.
    Container Loading (20′ FCL) 20′ FCL loaded with Sumitomo Chemical HDPE F0554T high-density polyethylene resin, palletized, shrink-wrapped, and secured for ocean shipment.
    Shipping Sumitomo Chemical HDPE F0554T is a non-hazardous high-density polyethylene resin, shipped as pellets in 25 kg bags or 1,000 kg jumbo bags on pallets. Transport in clean, dry containers or trucks at ambient temperature. Keep dry and away from heat, direct sunlight, and contamination. Not regulated for dangerous goods transport.
    Storage Store Sumitomo Chemical HDPE F0554T in a cool, dry, well-ventilated warehouse, preferably below 40°C. Keep original sealed bags or containers on pallets, away from direct sunlight, rain, moisture, heat, flames, and oxidizing agents. Avoid dust buildup, physical damage, and static discharge. Use FIFO rotation, keep area clean, and consult the SDS.
    Shelf Life Sumitomo Chemical HDPE F0554T has a shelf life of about 24 months when stored in original, unopened packaging, cool, dry, away from direct sunlight.
    Application of Sumitomo Chemical HDPE F0554T

    Sumitomo Chemical HDPE F0554T enters T-shirt carrier bag production as a blown-film extrusion grade with nominal melt flow rate 0.05 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022 and nominal density 0.955 g/cm³ per ISO 1183-1:2019. On a grooved-feed single-screw extruder with 30:1 L/D and forced feed-zone cooling, the resin is melt-homogenized across a barrel profile of 180–230 °C, then metered through a die gap of 1.2–1.8 mm at a blow-up ratio of 3:1–5:1. The fractional-melt viscosity stabilizes a stalk height of 6–10 die diameters before frost-line crystallization; stalk length above 10D increases machine-direction/transverse-direction tensile imbalance and bubble wander when winder tension exceeds 2–4 N/cm of film width. Terminal film gauge is normally 15–25 µm, with inline slit widths matched to bag length and die-cut handle geometry. For printable white T-shirt bags, 1–3 wt% titanium dioxide masterbatch is combined with 500–1500 ppm erucamide slip and 1000–3000 ppm synthetic silica antiblock; the slip package reduces coefficient of friction below 0.25 under ISO 8295:1995, while antiblock above 3000 ppm raises screen-pack pressure and lowers dart impact. Heat sealing uses heated serrated or flat jaws at 125–140 °C, dwell 0.5–1.0 s, and jaw pressure 0.3–0.6 MPa; seal strength is evaluated by ASTM F88/F88M-21 on 25 mm strip specimens. Regulatory compliance for non-food T-shirt bags is governed by REACH Annex XVII and EU Directive 94/62/EC packaging heavy-metal limits; food-contact printed bags require compliance with FDA 21 CFR 177.1520 for olefin polymers and organoleptic qualification of the titanium dioxide concentrate under EU 10/2011.

    What Limits Blow-Up Ratio Above 4:1 in Heavy-Duty Sack Film?

    In heavy-duty sack and industrial liner extrusion, HDPE F0554T is modified with linear low-density polyethylene at 10–30 wt% to increase dart impact and machine-direction tear resistance; below 10 wt% LLDPE, film at 50–80 µm gauge exhibits brittle puncture propagation, while above 30 wt% bubble stability declines because the lower-viscosity LLDPE phase concentrates at the bubble surface and reduces melt strength. Carbon black masterbatch is added at 2–6 wt% for UV-stabilized construction sacks, and hindered-amine light stabilizer concentrations of 0.1–0.3 wt% are used for outdoor storage exposure. Extruders are specified with 25:1–30:1 L/D, grooved feed bushings, and barrier screws; melt temperature is held at 200–230 °C to avoid over-oxidation of the fractional-melt HDPE. Die gap is kept at 1.2–1.8 mm, and blow-up ratio is bounded at 3:1–5:1. Above 5:1, the high-density bubble shows frost-line flutter because local cooling rate around the bubble circumference becomes non-uniform; this instability is amplified when ambient air velocity exceeds 3 m/s. Table 1 records process variables monitored on a 600 mm die line.

    Process variableOperating rangeObserved instability threshold
    Blow-up ratio3:1–5:1Bubble flutter above 5:1
    Frost line height6–10DMD/TD tear imbalance below 6D
    Melt temperature200–230 °CGel formation above 230 °C after 45 min residence
    Die gap1.2–1.8 mmMelt fracture below 1.0 mm at output above 150 kg/h

    Terminal heavy-duty sacks are fabricated by bottom sealing and side gusseting with film thickness from 60–120 µm; compliance is limited to non-food industrial packaging under REACH SVHC screening, RoHS 2011/65/EU for electrical product outer packaging, and UN Model Regulations for outer packaging of hazardous fill. Tensile properties are measured by ISO 527-3:2018, tear resistance by ASTM D1922-15, and puncture resistance by ASTM D5748-19.

    Direct food-contact cereal liners and frozen food bags use HDPE F0554T in a 100% virgin formulation; the resin falls under FDA 21 CFR 177.1520(c) as an olefin polymer intended for food contact, and EU 10/2011 requires overall migration below 10 mg/dm² in food simulants. The extrusion line is run with low-shear screw geometry at 180–210 °C to keep melt temperature below the threshold where oxidative chain scission generates aldehydes and ketones that alter organoleptic profile. White masterbatch at 1–2 wt% uses titanium dioxide pigment with low extractable heavy metals; slip and antiblock additions are restricted to 400–1200 ppm because higher erucamide loadings can bloom during frozen storage and create visible surface haze. Film is fabricated at 20–50 µm, with bubble cooling by chilled air at 8–12 °C to accelerate crystallization and reduce blocking. End products include cereal box liners, frozen vegetable bags, and bread bags. For acidic or fatty food simulants, migration testing is performed under EU 10/2011 Annex III conditions with simulant B and simulant D2 at 40 °C for 10 days. Published data for this specific grade in low-temperature migration is limited; converters qualify each film structure by total migration and sensory evaluation under ISO 13302:2003.

    RequirementStandard or regulationValue or condition
    Food-contact olefin polymerFDA 21 CFR 177.1520Monomers and adjuvants meet extractive limits
    Overall migrationEU 10/2011<10 mg/dm²
    Organoleptic panelISO 13302:2003No off-odor at 40 °C for 24 h
    Heavy metals in packagingEU 94/62/ECSum Pb/Cd/Hg/Cr VI <100 mg/kg

    Thermal and Shear History Effects in Down-Gauged Produce Bags

    Down-gauging HDPE F0554T to 7–15 µm for roll produce bags depends on the fractional-melt viscosity to maintain bubble stability at high stalk height; the extruder is run with a die gap of 1.0–1.5 mm, blow-up ratio of 4:1–6:1, and frost line height of 8–12D. At film thickness below 10 µm, transverse-direction tear resistance becomes the controlling defect mode because high blow-up ratios orient crystalline lamellae perpendicular to machine direction; the resulting transverse-direction tear values under ASTM D1922-15 are typically 30–50% lower than machine-direction tear values. To counter this imbalance, converters reduce frost line height to 6–8D and increase melt temperature to 210–225 °C, but melt temperature above 225 °C lowers melt strength and induces gauge bands of ±2 µm across the web. The additive package contains 0.5–1.0 wt% slip masterbatch and 0.2–0.5 wt% antiblock; higher slip reduces coefficient of friction but causes blocking on wound rolls if roll tension exceeds 0.1 N/mm. Terminal products are perforated produce bags with film gauge 8–15 µm, heat-sealed at 120–135 °C. Compliance for produce bags sold in EU markets is under EU 10/2011 for food contact and FDA 21 CFR 177.1520 for US distribution; finished rolls are also tested for unwind force at 500 mm/min under ISO 527-3:2018 to confirm dispensability.

    If HDPE F0554T Is Coextruded with LLDPE Seal Layers, What Changes in Heat Seal Strength?

    Three-layer coextruded film with an HDPE F0554T core and metallocene LLDPE skins is used for frozen food pouches and coffee overwrap where seal initiation must occur below 105 °C. The HDPE core supplies stiffness and moisture barrier, while the LLDPE skins contribute hot-tack strength and seal-through-contamination resistance. The layer ratio is typically 20:60:20 or 30:40:30; at core fractions above 60%, the heat seal curve shifts upward because the HDPE melt crystallization domain begins at 118–122 °C and the seal jaw cannot uniformly displace the skin layer. Viscosity mismatch is managed by selecting metallocene LLDPE with melt index 1.0 g/10 min at 190 °C/2.16 kg, and by raising coextrusion melt temperature to 210–230 °C. Seal initiation temperature is measured by ASTM F88/F88M-21 with 25 mm strips, 0.5 s dwell, and 0.4 MPa jaw pressure; seal strength at 110 °C is typically 8–12 N/25 mm for film thickness 60 µm. Hot-tack performance under ASTM F1921-18 shows a peak hot-tack range of 100–115 °C; above 120 °C, the HDPE core begins to flow and the film web fails at the seal root. Terminal products include frozen food pouches, side-gusseted stand-up pouches, and lamination base films. Compliance is with FDA 21 CFR 177.1520 for all layers, EU 10/2011 with simulant D2 at 40 °C for 10 days, and California Proposition 65 screening for printing inks applied to the outer skin. Published data for this specific coextruded configuration is limited; converters determine seal plateaus by differential scanning calorimetry at 10 °C/min under ISO 11357-1:2016 to correlate skin melting endotherm with jaw temperature.

    Free Quote

    Competitive Sumitomo Chemical HDPE F0554T prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sumitomo Chemical HDPE F0554T is a high-molecular-mass high-density polyethylene resin engineered for blown-film extrusion. The grade designation F0554T identifies a film-class material with nominal density 0.955 g/cm³ measured under ISO 1183-1:2019 and melt mass-flow rate 0.05 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2011. It is not interchangeable with medium-molecular-weight HDPE film grades, nor with injection-moulding or blow-moulding HDPE, because high molecular mass elevates zero-shear viscosity and melt relaxation time. In blown-film conversion, the resin maintains bubble stability at thin gauge and resists draw resonance; in injection moulding, the same viscosity reduces screw recovery and increases shear heating in the plasticating unit.

    Representative published property values for Sumitomo Chemical HDPE F0554T
    Property Test method Typical value
    Melt mass-flow rate, 190 °C/2.16 kg ISO 1133-1:2011 0.05 g/10 min
    Density ISO 1183-1:2019 0.955 g/cm³
    Tensile yield stress ISO 527-2:2012 29 MPa
    Tensile elongation at break ISO 527-2:2012 ≥600%
    Flexural modulus ISO 178:2010 1.20 GPa
    Vicat softening temperature, A50 ISO 306:2013 127 °C

    What Distinguishes the F0554T Melt Architecture From Standard HDPE Film Resins?

    Molecular weight distribution controls the balance between bubble strength and extruder load. F0554T exhibits a melt mass-flow rate near 0.05 g/10 min, approximately one order of magnitude below the 0.5–1.0 g/10 min range common for medium-molecular-weight HDPE film grades. The high-load melt flow index at 190 °C/21.6 kg is correspondingly low; however, the producer may report the flow rate ratio as a marker of shear sensitivity. The practical result is higher extensional viscosity during bubble inflation and reduced tendency for melt fracture at high draw ratios. The limitation is higher melt pressure and lower output per screw revolution on smooth-bore extruders. Grooved-feed barrels with L/D 25:1–30:1 are required to maintain stable solids conveying, and drive motors sized for 0.18–0.25 kWh/kg specific energy are typical on commercial lines running F0554T.

    By comparison, a high-flow HDPE injection-moulding grade with MFR 4–8 g/10 min would exhibit lower minimum cycle time but cannot sustain a stable blown-film bubble because melt strength is insufficient to resist sag and draw resonance at thickness below 20 µm. F0554T therefore occupies a film-specific high-viscosity position in the Sumitomo Chemical HDPE portfolio. It is also not a direct substitute for bimodal HDPE grades designed for very high dart impact at low temperature; those grades may combine higher molecular weight fractions with higher side-branch content, producing different puncture and slow crack growth profiles.

    Extrusion of F0554T on a 65 mm grooved-feed blown-film line with a 180 mm spiral mandrel die and 1.6 mm die gap is normally conducted with barrel settings 180–210 °C, adapter 210 °C, and die zones 210–220 °C. A blow-up ratio of 3.5:1–5.0:1 and frost-line height 700–1000 mm suppress excessive transverse orientation and reduce gauge scatter. The high melt viscosity can reduce die-lip deposition relative to lower-viscosity HDPE film grades when the die is cleaned after each 100–150 h run; oxidized material accumulating in the spiral channels can generate melt fracture streaks that appear as unintended gauge bands. If melt temperature exceeds 230 °C, chain scission and gel formation accelerate, especially when oxygen is not excluded from the hopper. Published data for maximum specific output are line-specific and should not be extrapolated from torque rheometry alone.

    Head pressure at 150 kg/h output on a 65 mm grooved-feed extruder is commonly between 450 bar and 650 bar; the actual value depends on melt temperature, die gap, and motor speed. The screen changer bypass is not used as a routine pressure-control device. Production lines commonly use 80/120/80 mesh screen packs to trap crosslinked gels; pressure build-up across the screen should be monitored, with a pack change initiated when differential pressure rises by 30–40 bar above baseline.

    Predrying is not typically required at ambient storage below 60% RH, but pellets stored in silos or sea containers with large temperature swings can accumulate condensation. A dry-air purge at 70 °C for 1–2 h is applied when surface moisture is detected, because water fed to a grooved-feed section reduces solids conveying efficiency and increases melt temperature variability.

    Dimensional Stability and Tear Anisotropy in Blown Film

    At nominal 20 µm film thickness, tensile yield stress measured under ISO 527-3:2018 is typically near 29 MPa, and elongation at break exceeds 600%. Elmendorf tear strength measured under ISO 6383-2 displays machine-direction values roughly half transverse-direction values, reflecting the preferential orientation of lamellae and not an anomalous weakness of F0554T. Flexural modulus near 1.20 GPa under ISO 178:2010 and Vicat softening temperature near 127 °C under ISO 306:2013 support stack-load retention in warm storage. These values are typical and do not replace lot-specific certification.

    When film is down-gauged below 12 µm, absolute tear force decreases with caliper, and the coefficient of variation for dart-drop measurements can exceed 10–15% unless the collapsing frame is aligned to within ±1° and ambient draft is controlled. Static pinning of the bubble above the air ring is not normally required for F0554T, but alternating current corona treatment at 38–42 mN/m is specified for water-based lamination and flexographic ink adhesion. Dyne decay after 30–45 days is accelerated by high-slip additive levels above 800 ppm and by exposure to direct sunlight.

    A direct comparison with a 0.949 g/cm³ medium-molecular-weight HDPE film resin illustrates the trade-off. The lower-density grade processes with less motor torque and lower melt temperature, but top-load stiffness and warm creep resistance are inferior. F0554T is selected when a film must hold a pallet load without excessive deformation at 40–50 °C warehouse temperatures. In high-speed form-fill-seal packaging, however, lower-viscosity grades may be preferred because F0554T can increase backpressure and lengthen screw recovery on undersized extruders with L/D below 25:1.

    Environmental stress-crack resistance is enhanced relative to medium-molecular-weight HDPE because high molecular mass slows crack propagation. Testing under ASTM D1693, condition B, 10% Igepal, can substantiate the difference, but published data for F0554T-specific configuration is limited and should be obtained for each campaign. The standard grade does not include UV stabilizer; outdoor service life is therefore limited unless carbon black or hindered amine light stabilizer is added by the converter.

    Directional comparison with a conventional medium-molecular-weight HDPE film resin
    Parameter F0554T MMW-HDPE reference Processing consequence
    Melt mass-flow rate, 190 °C/2.16 kg 0.05 g/10 min 0.7–1.0 g/10 min Higher head pressure; reduced pumping capacity per screw revolution
    Density 0.955 g/cm³ 0.948–0.952 g/cm³ Higher film stiffness and top-load resistance
    Flexural modulus 1.20 GPa 0.80–1.00 GPa Increased machine-direction stiffness; may require wider collapsing frame
    Vicat softening temperature 127 °C 120–124 °C Better shape retention under warm load
    Tear anisotropy MD less than TD MD less than TD Similar directional bias; downgauging amplifies absolute values

    When Downstream Converting Demands Gauge Uniformity Below 12 µm

    Bag-making heat sealing on F0554T film is typically set to 135–155 °C jaw temperature with 0.3–0.5 s dwell and 0.4–0.6 MPa seal pressure. At line speeds above 45 m/min, seal strength is governed by jaw temperature uniformity and dwell geometry rather than by the resin melting point, because the polymer has a broad molecular weight distribution that widens the sealing window. Pinhole formation during star-seal conversion is observed when the film is drawn over misaligned forming collars or when melt fracture streaks are present from an unclean die. Lubricant systems containing erucamide at 500–1000 ppm can reduce coefficient of friction but can also increase organoleptic risk in sensitive food packaging; migration testing under EU Regulation 10/2011 may be required.

    Compliance Status Is Conditional on End-Use Migration Testing

    Food-contact status is not automatically assigned to F0554T. Under EU Regulation 10/2011, the film must show overall migration below 10 mg/dm² under the intended time and temperature conditions; test method selection follows the food simulant matrix for aqueous, acidic, alcoholic, or fatty contact. For the United States, compliance with 21 CFR 177.1520 applies to olefin polymers provided the specified density and extractable fractions are met. The grade is not marketed as a medical-grade material, and cytotoxicity or hemocompatibility data are outside the standard release documentation. Under REACH, the polymer itself is exempt from registration as a substance; residual monomers and additives remain subject to downstream article obligations. RoHS Directive 2011/65/EU restrictions on lead, mercury, cadmium, hexavalent chromium, PBBs, and PBDEs are met by formulation control, but the user must verify compliance of any masterbatch or post-print applied to the film.

    In heavy-duty shipping sacks produced on a tandem blown-film line with a 75 mm grooved-feed extruder and 200 mm annular die at 2.1 blow-up ratio, F0554T is typically run at 190–205 °C melt temperature to produce 80–100 µm film. The resin’s high melt strength allows stable operation at neck heights of 5–7 die diameters, but the limiting factor on output is usually tower height and air-ring chilling capacity, not the resin itself. Published data for maximum stable line speed with this specific grade are limited; validation on the target line is necessary because screw cooling capacity, die geometry, and winder tension act together to determine gauge spread and final roll quality.

    Top