Sumitomo Chemical Hdpe F0554

Sumitomo Chemical HDPE F0554

    • Product Name: Sumitomo Chemical HDPE F0554
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 566531
    Density 0.954 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 0.50 g/10 min
    Tensile Strength At Yield 25.0 MPa
    Tensile Strength At Break 30.0 MPa
    Elongation At Break 800%
    Flexural Modulus 1100 MPa
    Notched Izod Impact Strength 23 C 100 J/m
    Vicat Softening Temperature 124°C
    Heat Deflection Temperature 0 45 Mpa 75°C
    Shore D Hardness 65
    Molding Shrinkage 1.5-3.0%
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Thermal Conductivity 0.40 W/m-K
    Water Absorption 0.01%
    Volume Resistivity 1.0E+16 ohm-cm
    Dielectric Constant 2.3
    Dissipation Factor 0.0002
    Melting Point 135°C
    Specific Heat Capacity 2.0 J/g-°C
    Brittleness Temperature -70°C

    As an accredited Sumitomo Chemical HDPE F0554 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sumitomo Chemical HDPE F0554 is typically supplied in 25 kg paper bags or 1,000 kg jumbo bags, palletized.
    Container Loading (20′ FCL) Container loading (20′ FCL): Sumitomo Chemical HDPE F0554 in 25 kg bags, palletized, about 16–18 metric tons net.
    Shipping Sumitomo Chemical HDPE F0554 is a non-hazardous high-density polyethylene resin shipped as solid pellets in 25 kg bags, big bags, or bulk containers. Store in a cool, dry, clean area away from direct sunlight and ignition sources. No special UN classification; transport as general industrial cargo.
    Storage Store Sumitomo Chemical HDPE F0554 in its original, closed packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, strong oxidizers, and incompatible substances. Stack pallets securely without excessive load, and follow first-in, first-out stock rotation. Do not expose to ultraviolet radiation or temperatures above recommended limits.
    Shelf Life Stored in original unopened packaging in a cool, dry place, Sumitomo Chemical HDPE F0554 typically has a 24-month shelf life.
    Application of Sumitomo Chemical HDPE F0554

    Blown-film conversion of Sumitomo Chemical HDPE F0554 for thin-gauge retail carrier sacks is specified where a nominal melt mass-flow rate of 0.05 g/10 min (ISO 1133-1:2022) and a density of 0.955 g/cm³ (ISO 1183-1:2019) provide the high melt strength required for stalk-bubble stability at gauge targets between 8 µm and 15 µm. The extruder configuration is typically a grooved-feed single-screw unit with 25:1–30:1 L/D and a barrier mixing section; barrel temperatures are profiled from 160 °C at the feed throat to 190–210 °C at the adapter, with die lips held at 200–220 °C. Die gap is set at 0.8–1.2 mm, and operation with a blow-up ratio of 4:1–5:1 and frost line height of 6–8 die diameters maintains the high-stalk bubble architecture required to suppress melt resonance and gauge bands. On production-scale lines, the primary failure mode is not melt fracture but bubble sag at the lower frost line limit, which produces thickness variation beyond ±8% of nominal gauge; elevated frost lines above 9 die diameters reduce throughput because the HDPE melt relaxation path lengthens without equivalent bubble cooling. Production-scale data from blown-film lines running high-stalk HMW-HDPE indicate that gauge uniformity is more sensitive to frost line height than to die gap once the stalk is stable. Operators maintain thickness variation below ±5% when the differential air temperature between the exterior air ring and internal bubble cooling is held within 10–20 °C; deviations outside this band create localised thinning at the bubble transition. Because the density of 0.955 g/cm³ raises film stiffness, the resulting carrier sacks exhibit higher top-load resistance at lower gauge than LLDPE-rich formulations, but the trade-off is reduced Elmendorf tear in the machine direction, requiring the 15–25 wt% LLDPE addition to restore tear strength. This is a process conflict: insufficient LLDPE leaves punched handle zones vulnerable to split tears, while excessive LLDPE lowers stiffness and increases die lip buildup, leading to surface defects. The optimum is therefore maintained by line-specific measurement of ASTM D1922-15 Elmendorf tear and ASTM D882-18 modulus; the typical F0554 proportion is 72–85 wt%, but it is adjusted within that range according to bag width and handle cut configuration. The formulation for this segment is nominally 72–85 wt% F0554, 15–25 wt% LLDPE or LDPE to modify dart impact and heat-seal response, and 2–4 wt% colour masterbatch; anti-block masterbatch is introduced at 1,000–2,500 ppm active silica and erucamide slip at 500–1,200 ppm when downstream bag-making requires consistent coefficient of friction. Compliance for this non-food packaging sector is evaluated under ASTM D1709-16a Method A for dart drop impact, ASTM D882-18 for tensile yield and break properties, and the EU Packaging and Packaging Waste Directive 94/62/EC for heavy-metal concentration limits; production thickness verification is performed under ISO 4593:1993. Downstream conversion includes bag-on-roll production, T-shirt bag side-seal welding, and die-cut handle punching. Finished articles include retail T-shirt carriers, produce roll bags, garment bags, and small waste bin liners in the 8–20 µm gauge range.

    What Changes When HDPE F0554 Is Upgauged into 50–150 µm Industrial Liners?

    Upgauging the same resin from thin-gauge carrier bags to 50–150 µm liner stock moves the line from drawdown-limited operation to cooling-limited operation. At thicknesses above 80 µm, a dual-lip air ring and internal bubble cooling are required to hold gauge uniformity on a grooved-feed extruder with 30:1 L/D; otherwise the bubble temperature rises and output becomes unstable. Die gap is widened to 1.2–1.8 mm, and blow-up ratio is reduced to 2.5:1–3.5:1 to balance machine-direction and transverse-direction tear. Melt temperature remains 190–220 °C, but screw cooling is engaged to limit the feed-zone temperature and to preserve solids conveying in the grooved barrel. Extruder pressure in the grooved feed section typically reaches 20–35 MPa before the screen changer; screen packs are specified at 60/100/60 mesh for heavy film to manage back pressure. The low melt flow rate also increases shear heating, so water-cooled screw cores are used on longer lines. A further process conflict arises with regrind: because heavy-gauge film often contains carbon black and anti-fibrillation additives, regrind above 20 wt% raises melt pressure and accelerates screen choke, so inline melt filtration with automatic screen changers is required. The formulation for heavy-duty liners contains 50–70 wt% F0554, 30–50 wt% LLDPE or mLLDPE for dart-impact and slow-puncture resistance, and 2–4 wt% carbon black masterbatch where UV resistance is specified; processing stabilizer is added at 0.05–0.15 wt% when significant post-industrial regrind is present. In waste-containment and construction-film specifications, compliance is typically assessed under ISO 527-3:2018 for tensile properties, ASTM D1709-16a Method B for high-gauge dart impact, ISO 4593:1993 for thickness tolerance, and EN 13592:2009 where the film is marketed as a refuse sack. The operational boundary is the high torque required by the 0.05 g/10 min melt flow rate: barrel wear at the grooved feed section accelerates if regrind contains abrasive filler, and melt temperatures above 230 °C should be avoided to prevent oxidative degradation. Finished articles include industrial container liners, construction dust barriers, demolition sheeting, heavy-gauge rubble sacks, and temporary containment liner for controlled waste streams.

    Specific Migration Limits in Dry-Food Contact Film for Cereal and Bakery Overwrap

    Film structures intended for dry-food contact are specified with F0554 primarily for moisture resistance and stiffness at 10–30 µm gauge. The production line is configured with polished stainless-steel surfaces, a 80/120/80 mesh screen pack to remove gel particles, and melt temperatures of 190–220 °C. The film is blown at a blow-up ratio of 3:1–4:1 and a frost line height of 5–7 die diameters, then collapsed onto a wooden or fibreboard core that meets direct-food packaging hygiene requirements. Formulation is restricted by the migration status of additives: 65–80 wt% F0554 is compounded with 15–30 wt% LDPE or LLDPE, erucamide slip at 500–1,000 ppm, and high-purity synthetic silica anti-block at 1,000–2,500 ppm; colour masterbatch is limited to food-approved pigments only. Migration kinetics in non-fatty dry-food contact are governed by additive molecular weight and temperature; erucamide slip migrates to the film surface within 24–72 h after extrusion, and the resulting coefficient of friction stabilises between 0.15–0.30. For organic food-contact films, surface migration is constrained by the overall migration test rather than by additive volatility; inline monitoring of film surface energy and haze is used to ensure that anti-block dispersion does not exceed 8% haze for transparent cereal liners. Compliance for the film layer is referenced to EU Regulation 10/2011 with an overall migration limit of 10 mg/dm² under the intended contact conditions, and to 21 CFR §177.1520 for olefin polymers under FDA food-contact classifications; declarations are typically issued against REACH EC 1907/2006 for substances of very high concern. The limitation of HDPE F0554 in this application is oxygen transmission: the film is suitable for moisture-sensitive dry goods but not for oxygen-sensitive products unless laminated to a barrier layer. Finished product types include cereal liners, biscuit tray overwrap, bread bags, dry pet food liners, and institutional rice sachets.

    Comparative formulation and process ranges by downstream segment
    Downstream segmentF0554 loadingCo-resin or additive loadingCharacteristic gauge or process variable
    Thin-gauge retail carrier sacks72–85 wt%LLDPE/LDPE 15–25 wt%; anti-block 1,000–2,500 ppm; slip 500–1,200 ppm8–15 µm; BUR 4:1–5:1
    Heavy-duty industrial liners50–70 wt%LLDPE/mLLDPE 30–50 wt%; carbon black 2–4 wt%80–150 µm; die gap 1.2–1.8 mm
    Dry-food contact film65–80 wt%LDPE/LLDPE 15–30 wt%; erucamide 500–1,000 ppm; silica 1,000–2,500 ppm10–30 µm; screen pack 80/120/80 mesh
    Woven sack lamination film60–80 wt%LDPE/LLDPE 15–25 wt%; TiO₂ masterbatch 5–8 wt%15–30 µm; corona 38–42 dyn/cm
    Three-layer coextruded core film50–70 wt% total; core 70–100 wt%Skin LLDPE/mLLDPE 30–50 wt%; PPA 200–500 ppmLayer ratio 20/60/20 to 25/50/25

    Lamination of woven polypropylene sacks with HDPE film uses F0554 in the 15–30 µm gauge range to reduce moisture ingress and improve printability after corona treatment. The extrusion process is blown-film rather than cast, with die gap 0.9–1.1 mm, blow-up ratio 2.8:1–3.5:1, and a take-off speed selected to produce flat film for subsequent lamination; surface energy after inline or offline corona treatment is maintained at 38–42 dyn/cm for solvent-based and water-based ink adhesion. Pre-lamination annealing at 60–80 °C for 5–10 min reduces shrinkage during hot-nip lamination and stabilises the film web. Formulation typically comprises 60–80 wt% F0554, 15–25 wt% LDPE or LLDPE for seal response, and 5–8 wt% titanium dioxide masterbatch when opacity is required; slip and anti-block additives are reduced to 300–800 ppm because downstream lamination adhesives and liquid inks are sensitive to surface migration. Lamination to woven PP is performed either by extrusion coating with a low-density tie resin at 290–320 °C melt temperature or by solventless adhesive lamination with a coating weight of 1.5–2.5 g/m², followed by nipping at 60–80 °C. Compliance is assessed through ISO 527-3:2018 film tensile properties, ISO 4593:1993 gauge verification, and T-peel adhesion under ISO 8510-1:2001 for laminate integrity; when used for food-contact bulk grain bags, the film layer must also meet EU Regulation 10/2011 and 21 CFR §177.1520 where local law applies. Finished articles include fertiliser sacks, polymer pellet bags, salt and grain packaging, and FIBC liner webs in which the HDPE layer forms a moisture-resistant inner ply.

    When Three-Layer Coextrusion Positions HDPE F0554 as the Structural Core

    Three-layer blown-film lines running this grade as a core layer are configured with separate extruders for the skin and core, with the core extruder maintained at 190–220 °C and the skin extruders at 170–200 °C. The die gap is widened to 1.0–1.8 mm, and the layer distribution is typically 20/60/20 or 25/50/25, placing F0554 as the central stiffness and moisture-resistance component while LLDPE or mLLDPE skins provide low seal-initiation temperature and tear resistance. Total F0554 content in the structure is 50–70 wt%, with the core layer itself formulated at 70–100 wt% F0554 and up to 20 wt% reclaimed edge trim where appearance specifications allow; polymer processing aid is added to the core at 200–500 ppm to manage shear at the die lips. HDPE skins would raise the minimum seal temperature, so the resin is not recommended for an all-HDPE structure where a low seal-initiation temperature is required. If the skin layers are below 15% of total thickness, flexural stress whitening can occur in overwrap films, and the coefficient of friction may become unstable at high packaging line speeds. Compliance for hygiene and tissue overwrap is generally anchored to ISO 527-3:2018 for tensile properties, ASTM F1249-20 for water-vapour transmission rate, and relevant company-specific sensory requirements; published data for this specific configuration is limited, so WVTR targets are established by end-use specification rather than by a single resin datasheet value. This configuration supplies overwrap for tissue bundles, external packaging for cotton and hygiene products, stationery overwrap, and thin protective film for paper reams.

    Free Quote

    Competitive Sumitomo Chemical HDPE F0554 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sumitomo Chemical HDPE F0554 is a high-molecular-weight high-density polyethylene grade supplied in pellet form for blown film extrusion. The resin is characterized by a nominal density of 0.955 g/cm³ measured under ISO 1183-1:2019 and a melt flow rate of 0.05 g/10 min determined at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. The polyethylene backbone carries CAS 9002-88-4. Commercial technical literature identifies the grade for thin-gauge merchandise bags, industrial liners, carrier bags, and coextruded film structures where elevated stiffness, moisture barrier, and bubble stability are required. The material is normally supplied as a natural pellet; slip, antiblock, and processing aids are introduced by the converter through masterbatch blending rather than being incorporated at the reactor.

    What Converts the High Melt Viscosity of F0554 into Stable Bubble Geometry on Standard Film Towers?

    Blown film conversion of F0554 relies on high melt strength to stabilize bubble geometry at blow-up ratios from 3:1 to 5:1. Single-screw extruders with smooth-bore barrels and screw L/D ratios of 24:1 to 30:1 are commonly used for this viscosity class. A typical barrel temperature profile begins near 180 °C at the feed throat and increases to 210 °C in the metering section; adapter and die temperatures are held between 200 °C and 220 °C. Die gaps of 0.8 mm to 1.2 mm are preferred because the high melt viscosity generates elevated die pressure, and narrower gaps can exceed barrel or clamp pressure limits. Melt pressure at the screen pack should be monitored continuously; sudden increases indicate gel accumulation or additive dispersion failure. Bubble stability is improved when the frost line height is maintained between 4 and 8 die diameters, and dual-lip air rings with chilled airflow are used. Processing above 230 °C should be minimized to limit oxidative degradation, particularly in regrind-intensive operations.

    Film Property Profile and Corresponding Test Designations

    Typical mechanical property data reported for F0554 include tensile yield stress near 29 MPa, tensile stress at break near 39 MPa, and elongation at break near 800% when tested under ISO 527-2:2012. Flexural modulus is approximately 1,300 MPa under ISO 178:2019. Vicat softening temperature is reported at 126 °C using ISO 306:2022 method A50. These values are typical characterization data, not specification release limits, and lot-to-lot variation occurs within the supplier’s published control ranges.

    Typical property data for Sumitomo Chemical HDPE F0554
    PropertyTest methodTypical value
    Melt flow rate at 190 °C, 2.16 kgISO 1133-1:20220.05 g/10 min
    DensityISO 1183-1:20190.955 g/cm³
    Tensile yield stressISO 527-2:201229 MPa
    Tensile stress at breakISO 527-2:201239 MPa
    Elongation at breakISO 527-2:2012800%
    Flexural modulusISO 178:20191,300 MPa
    Vicat softening temperature, method A50ISO 306:2022126 °C

    In film form, converter-generated data are strongly influenced by gauge, blow-up ratio, frost line height, and additive loading. For monolayer structures at 10 μm to 25 μm, the density class of 0.955 g/cm³ provides lower moisture vapour transmission than butene LLDPE of equivalent gauge when measured under ISO 15106-1. The grade is not designed for oxygen or aroma barrier applications requiring metallization or oriented structures. Surface printing requires corona treatment to a wetting tension of at least 38 mN/m measured in accordance with ASTM D2578-23. Slip and antiblock masterbatches are typically added at 2,000 ppm to 5,000 ppm to control film blocking without excessive haze. Sealing on bag-making equipment generally requires seal initiation temperatures from 120 °C to 135 °C, although actual settings depend on jaw pressure, dwell time, and film thickness.

    In coextruded structures, F0554 is used as a high-stiffness core layer between LLDPE skins. Layer distributions of 10/80/10 and 20/60/20 are common in industrial liner and heavy-duty sack constructions. The high melt strength permits stable encapsulation of the core by lower-viscosity skin layers, but skin-layer extruder temperatures should be matched to avoid interfacial instability. Cast film conversion is not an optimized application for F0554 because the high melt viscosity can produce edge instability and die-lip build-up on cast film lines.

    When F0554 Replaces a Lower-Molecular-Weight HDPE Grade in Form-Fill-Seal Equipment

    Substitution of F0554 for a conventional HDPE film or sheet grade with a melt flow rate of 0.2 g/10 min changes extrusion and sealing behaviour. The higher molecular weight of F0554 raises melt pressure at the die by 15–30% under identical screw speed and temperature settings. Retrofits may require higher-torque drives, wider die gaps, or increased barrel heating capacity. Output per revolution can be lower unless the screw is designed with barrier or Maddock mixing sections. Film produced from F0554 typically exhibits higher tensile stress at break and greater elongation than film from a 0.2 g/10 min HDPE, while the density of 0.955 g/cm³ maintains stiffness. The low melt flow rate can limit minimum gauge on high-speed lines to approximately 12 μm when melt fracture or die-lip build-up becomes process-limiting. Seal strength and hot-tack performance must be validated on the packaging line using ASTM F88/F88M-21 and ASTM F1921-18, because sealing response depends on comonomer content, additive package, and film gauge.

    Comparative positioning of F0554 against adjacent polyethylene film and extrusion grades
    PropertySumitomo Chemical HDPE F0554Conventional HDPE extrusion gradeButene LLDPE film grade
    Melt flow rate, ISO 1133-1:20220.05 g/10 min0.2–0.5 g/10 min0.8–1.0 g/10 min
    Density, ISO 1183-1:20190.955 g/cm³0.958–0.962 g/cm³0.918–0.920 g/cm³
    Flexural modulus1,300 MPa1,400–1,600 MPa250–350 MPa
    Tensile yield stress29 MPa30–32 MPa10–14 MPa
    Relative moisture barrierBetter than LLDPEHighest within HDPE density classLower than HDPE
    Bubble stability on film towersHighModerateLower

    Compliance for food-contact applications is assessed under 21 CFR 177.1520 for olefin polymers and EU Regulation No 10/2011 as amended. Conformity depends on residual monomer content, additive package, migration testing, and the finished film structure; converters must obtain a supplier compliance statement for the specific film formulation. Storage should be in dry, clean conditions below 60% RH. Although HDPE is not hygroscopic, condensation on cold pellets can introduce surface moisture and create bubble defects during extrusion. Regrind levels up to 20 wt% are common in non-food film production, but higher regrind levels may reduce dart impact resistance and increase gel counts. F0554 has lower environmental stress crack resistance than medium-density polyethylene copolymers; continuous contact with polar surfactants, alcohols, or aggressive wetting agents in stressed liner applications can reduce service life. Where long-term chemical compatibility is uncertain, converters should evaluate specimens under ASTM D1693-21 for environmental stress crack resistance and under ISO 16770-2019 for full-notch creep testing.