| HS Code | 192669 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.955 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.25 g/10 min |
| Tensile Strength At Yield | 24 MPa |
| Tensile Strength At Break | 33 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 1.10 GPa |
| Shore D Hardness | 62 |
| Vicat Softening Temperature | 124 °C |
| Melting Temperature | 131 °C |
| Brittleness Temperature | -70 °C |
| Environmental Stress Cracking Resistance | 1000 h |
| Water Absorption | 0.01% |
| Thermal Conductivity | 0.45 W/m·K |
| Specific Heat Capacity | 1.9 J/g·°C |
| Coefficient Of Linear Thermal Expansion | 1.2E-4 1/°C |
| Dielectric Constant | 2.3 |
| Dielectric Strength | 20 kV/mm |
| Volume Resistivity | 1E16 ohm·cm |
As an accredited Sumitomo Chemical HDPE B2555 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sumitomo Chemical HDPE B2555 is supplied in 25 kg multiwall paper bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL: 18 MT net of Sumitomo Chemical HDPE B2555, packed in 25 kg bags, palletized for export shipment. |
| Shipping | Sumitomo Chemical HDPE B2555 ships as a non-hazardous, non-regulated solid polymer resin. Typically packed in 25 kg bags, palletized and stretch-wrapped, then loaded into dry containers or covered trucks. Protect from moisture, heat, and contamination. Standard shipping documents apply; no UN number or dangerous goods declaration required. |
| Storage | Store Sumitomo Chemical HDPE B2555 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original packaging sealed and off the ground on pallets to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Maintain clean handling equipment and segregate from incompatible chemicals, oxidizers, and odorous materials. |
| Shelf Life | Stable HDPE resin; store cool, dry, ventilated. Recommended shelf life is typically 24 months in unopened original packaging. |
For industrial container blow moulding, Sumitomo Chemical HDPE B2555 is processed on shuttle presses equipped with a 25:1 L/D barrier screw and a 4.5 kg accumulator head. The melt temperature is maintained between 190°C and 210°C, while the die head is held at 195°C to 205°C to limit parison sag. Blow pressure is set at 0.7 MPa to 0.9 MPa with a mould temperature of 8°C to 18°C. A 10-point axial parison programming profile is required because the high molecular weight distribution produces 35% to 45% die swell. For a 220 L open-head drum weighing 9.2 kg, the minimum formed sidewall thickness is 1.9 mm, and the cycle time typically ranges from 125 s to 150 s depending on cooling water temperature. Virgin pellets do not require desiccant drying; however, when post-wash regrind exceeds 30 wt%, a vented extruder is necessary because surface moisture above 0.05 wt% generates pinholes in the pinch-off zone. The material contributes a tensile yield stress of 29 MPa when tested to ISO 527-2, a flexural modulus of 1250 MPa when tested to ISO 178, and an environmental stress crack resistance greater than 1000 h under ASTM D1693 condition B with 10% Igepal at 50°C. These properties support revalidation of UN 1H1 drums, but the pinch-off tail must be trimmed cleanly because residual flash exceeding 2 mm at the mould parting line reduces drop-test reproducibility.
| Test | Standard | Condition | Required result |
|---|---|---|---|
| Melt flow rate | ISO 1133-1:2022 | 190°C / 2.16 kg | 0.25 g/10 min nominal |
| Density | ISO 1183-1:2019 | 23°C | 0.955 g/cm³ nominal |
| ESCR | ASTM D1693 | Condition B, 50°C, 10% Igepal | No failure before 1000 h |
| Drop test | UN Model Regulations 6.1.5.3 | -18°C, 1.2 m | No leakage |
| Hydraulic pressure | UN Model Regulations 6.1.5.4 | ≥250 kPa | No leakage |
| Stacking | UN Model Regulations 6.1.5.5 | 40°C, 28 d | No buckling |
Six-layer coextrusion lines combine B2555 skins with a central EVOH barrier layer and maleic anhydride grafted PE tie layers. The HDPE extruders run at 200°C to 220°C; the EVOH extruder is limited to 205°C to 215°C because residence above 230°C produces gel particles at the layer interface. EVOH pellets are pre-dried at 80°C for 4 h to a moisture content below 0.3%, while B2555 requires no desiccant drying. The accumulator head is held at 210°C, and the die gap is set between 1.8 mm and 2.4 mm. For a 60 L diesel tank shell weighing 8.5 kg, the parison programmer increases the thickness to 4.0 mm at the pinch-off corners and reduces it to 2.2 mm in the sidewall. Blow pressure is 0.6 MPa to 0.8 MPa. A critical process conflict is shear heating from the high-viscosity B2555 layer: an undersized extruder below 90 mm diameter can push the melt above 230°C at the screw tip even when barrel setpoints remain conservative, causing EVOH degradation and delamination. Layer adhesion should be revalidated by ISO 10365 peel testing; published data for this specific six-layer configuration using B2555 is limited, so bonding must be confirmed on the production line before serial moulding. B2555 reduces parison sag due to its 0.25 g/10 min melt flow rate, but the trade-off is higher head pressure and slower extruder recovery. The mould clamp must hold 800 kN to 1,000 kN during blowing to prevent flash at the pinch-off. Fuel permeation performance is evaluated by ECE R34 or SAE J1737; the EVOH layer, not B2555, controls hydrocarbon permeation, so the B2555 layer is selected primarily for impact toughness and environmental stress crack resistance.
When flat die extrusion over a three-roll polishing stack converts HDPE B2555 into secondary containment liners, sheet thickness is controlled between 2.0 mm and 4.0 mm, with the melt temperature held at 195°C to 210°C. The polishing roll surface temperature is set at 70°C to 85°C to limit frozen-in orientation. Heating for thermoforming uses a twin-sided quartz oven with a surface temperature of 125°C to 135°C, measured by pyrometer, before a syntactic foam plug assists pre-stretching. A draw ratio of 2:1 is typical for basin dimensions up to 1.2 m × 1.0 m × 0.4 m. High melt strength is required to avoid sheet sag during oven dwell; B2555 with its low melt flow rate maintains a sag deflection below 5 mm for a 3.0 mm sheet over a 400 mm unsupported span. The mould is maintained at 50°C to 70°C to reduce thermoforming stress. Welded corners are completed by hot-gas extrusion welding, and weld factors are validated by DVS 2207-1. Immersion testing under ASTM D543 is required for the specific acid or alkaline medium; B2555 shows broad resistance to 30% sulfuric acid, 10% sodium hydroxide, and 5% sodium chloride, but aromatic solvents and strong oxidizers are outside the continuous-use envelope. The operational boundary is 60°C; above this temperature, the flexural modulus decays sufficiently to produce creep under hydrostatic pressure, and polypropylene or engineering thermoplastics should be considered instead of HDPE.
The substitution becomes technically binding only after revalidation of the mould filling phase because the lower melt flow rate changes pinch-off wall thickness distribution. A 1,000 L composite IBC inner bottle is blow moulded on a machine with a 15 kg accumulator head and a clamp force of 1,200 kN to 1,500 kN. The melt temperature is set at 200°C to 210°C, and the die head is held at 205°C to 215°C. The bottle weight is 14 kg to 15 kg, with minimum corner wall thickness of 3.0 mm and body wall thickness of 2.5 mm. Because B2555 exhibits 35% to 45% die swell, the parison is programmed shorter than with a 0.5 g/10 min grade; failure to reduce parison length produces thick flash and extends cycle time beyond 240 s. Blow pressure is 0.8 MPa. The pinch-off weld must be tested by ASTM D638-14 on a specimen cut across the weld; a weld factor above 0.85 is required for UN 31H1 qualification. Environmental stress crack resistance is evaluated by ASTM D1693 condition C in 100% Igepal, and B2555 normally exceeds 1,000 h without failure. Regrind use is limited to 20 wt% because higher levels broaden molecular weight distribution and reduce top-load buckling resistance. Mold temperature is kept at 10°C to 20°C to control cooling shrinkage; uneven cooling of the 1,000 L bottle can cause sidewall warpage exceeding 5 mm, which complicates cage assembly. The bottle must pass hydraulic pressure testing at 100 kPa for 10 min and a drop test at -18°C from 1.2 m according to UN Model Regulations.
Cumulative damage from repeated pallet stacking is simulated by ASTM D5276 drop tests at -18°C after conditioning for 48 h. A 20 L jerrycan is blow moulded at 850 g with a minimum sidewall thickness of 2.0 mm and a top and bottom pinch-off thickness of 3.5 mm. The accumulator head is set at 200°C to 215°C, and the mould temperature is held at 8°C to 15°C. Cycle time is 55 s to 75 s per two-cavity mould. B2555 is selected because conventional 0.5 g/10 min HDPE grades fail after prolonged contact with organophosphate ester-based crop protection formulations; the high molecular weight fraction of B2555 delays crack initiation at moulded-in stress concentrations. However, low-temperature impact is sensitive to pinch-off flash, and a flash line remaining above 1.5 mm from the parting surface acts as a crack initiator. Post-moulding fluorination is used for solvent barrier improvement; the fluorine concentration must not exceed 1.0% surface atomic fluorine because higher levels create a brittle skin layer that reduces drop impact by more than 30%. The jerrycans are closed with an UN 3H1 certified closure and tested under UN Model Regulations chapter 6.1.5 for drop, leakproofness, and hydraulic pressure. Leakproofness is evaluated at 30 kPa for 5 min for packing group II; B2555 allows consistent pinch-off weld quality when the flash is removed within 2 s of mould opening, before the weld zone cools below 120°C.
Because reservoir geometries include offset fill necks and pump sockets that require curved parison placement, B2555 is processed on a 3D blow moulding line with a parison manipulator. Extrusion blow moulding of automotive washer fluid reservoirs uses B2555 for its resistance to stress cracking in methanol and ethanol blends at temperatures from -30°C to 60°C. Melt temperature is 200°C to 210°C, die head temperature 205°C, and blow pressure 0.5 MPa to 0.7 MPa. The reservoir shell weight is 600 g to 900 g, with wall thickness of 2.0 mm to 2.5 mm. A mould clamp of 500 kN to 700 kN is adequate for single-cavity tools. The material is not dried; however, reclaimed internal skeleton scrap must be dried at 80°C for 2 h if stored above 70% relative humidity to prevent internal porosity at weld lines. Resistance to washer fluid containing 30% methanol and 10% ethanol is verified by immersion at 60°C for 500 h followed by ISO 527-2 tensile retention above 85%. Burst testing is performed at 250 kPa internal pressure for 60 s without visible swelling or leakage. The main incompatibility is with concentrated brake fluid or hot engine coolant, which can exceed the 60°C continuous-use boundary and should be directed to polypropylene or polyamide reservoirs.
Competitive Sumitomo Chemical HDPE B2555 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sumitomo Chemical HDPE B2555 is a high-molecular-weight high-density polyethylene resin supplied under the Sumikathene-F designation for extrusion blow moulding of rigid containers and technical hollow parts. The product is classified as PE-HD under ISO 1043-1 and is intended for accumulator-head, continuous-extrusion, and shuttle blow moulding machines that manufacture articles from approximately 5 L to 220 L. The material enters the market as a pelletized, non-filled polyolefin with a density of 0.955 g/cm³ measured by ISO 1183-1 and a melt mass-flow rate of 0.25 g/10 min at 190 °C and 2.16 kg measured by ISO 1133-1. That combination places the grade in the high-density, low-melt-flow segment in which stiffness, top-load capacity, and environmental stress crack resistance are required at the same time. The numerical designation B2555 is supplier-specific and does not encode a standardized property set; release testing on the certificate of analysis remains the controlling specification for lot acceptance.
Within the Sumitomo Chemical HDPE portfolio, B2555 sits between softer blow moulding grades of density 0.949–0.952 g/cm³ used for squeezable or intermediate-stiffness containers and higher-density injection grades with melt mass-flow rates above 1.0 g/10 min. This positioning defines its principal difference from other products: it is selected when a container must hold aggressive detergent or agricultural chemical formulations under stacking loads and still be produced on standard extrusion blow moulding equipment. The grade is not a pressure-pipe material, a thin-gauge film resin, or a thin-wall injection resin.
The molecular design of B2555 is based on a broad or bimodal molar mass distribution rather than a conventional unimodal distribution. In extrusion blow moulding, the low molar mass fraction contributes to shear-induced viscosity reduction in the die land, while the high molar mass fraction maintains extensional viscosity in the parison. A standard unimodal HDPE with the same 0.25 g/10 min melt mass-flow rate typically exhibits lower die swell, higher parison sag, and lower melt strength under the same head pressure. The higher molar mass tail in B2555 also increases slow crack growth resistance, but it narrows the temperature window for stable extrusion because the zero-shear viscosity rises sharply with increasing high molar mass fraction. This is the central processing difference from standard blow moulding HDPE of 0.60–0.80 g/10 min used for milk bottles or thin-wall containers: B2555 is not optimized for short-cycle, thin-wall production, but for thick-wall articles in which chemical stress cracking and stacking loads dominate service conditions.
The comonomer content is low and preferentially incorporated in the high molar mass chains, which is typical of broad or tandem-reactor HDPE architecture. Because the density remains high, the amorphous fraction is limited, but short-chain branches in the high molar mass fraction interrupt crystalline lamellae and increase the energy required for slow crack propagation. This structural balance explains why the material retains stiffness while improving ESCR. It also explains why an over-stabilized or highly filled replacement would not be equivalent to B2555, even if density and MFR match.
| Property | Test method | Representative value |
|---|---|---|
| Density | ISO 1183-1 | 0.955 g/cm³ |
| Melt mass-flow rate | ISO 1133-1 (190 °C, 2.16 kg) | 0.25 g/10 min |
| Tensile yield stress | ISO 527-2 type 1B | 28 MPa |
| Tensile strain at break | ISO 527-2 type 1B | >500% |
| Flexural modulus | ISO 178 | 1350 MPa |
| Charpy notched impact at 23 °C | ISO 179-1/1eA | 25 kJ/m² |
| Shore D hardness | ISO 868 | 64 |
| Vicat softening point A50 | ISO 306 | 129 °C |
| ESCR F50, 10% Igepal CO-630 at 50 °C | ASTM D1693 Condition B | >600 h |
| Oxidation induction time at 200 °C | ISO 11357-6 | >20 min |
On accumulator-head blow moulding lines, B2555 is processed at melt temperatures from 200 °C to 220 °C; head temperatures are usually set 5–10 °C below the melt temperature to limit die drool. Grooved-feed single-screw extruders with 24:1 to 30:1 L/D and barrier screws are the standard production configuration because the grooved bushing suppresses solids bed slip and stabilises throughput at high head pressure. Motor amperage rather than melt temperature is often the more sensitive indicator of melt viscosity changes in this grade. Screw speeds must be managed so that melt temperature overshoot does not exceed 230 °C, because the high molar mass fraction is the first component to suffer thermo-oxidative chain scission. Pre-drying is not required if the resin remains in sealed, moisture-tight packaging; after storage above 60% RH, surface moisture can produce microvoids and an irregular parison, and dehumidified-air drying at 80 °C for 2–4 h is applied. Die gaps from 2.5 mm to 4.5 mm are typical depending on wall thickness; die swell in production accumulators is commonly observed at 30–50%, and parison programming must compensate for swell variation caused by barrel temperature drift.
| Parameter | Set point or range |
|---|---|
| Melt temperature | 200–220 °C |
| Head temperature | 195–210 °C |
| Die gap | 2.5–4.5 mm |
| Blow-up ratio | 1.8:1–2.5:1 |
| Screw L/D | 24:1–30:1 |
| Pre-drying | 80 °C for 2–4 h if exposed to above 60% RH |
Rheological characterization on a capillary rheometer according to ISO 11443 shows pronounced shear thinning in B2555: apparent shear viscosity at 100 s⁻¹ is approximately two orders of magnitude lower than at 0.1 s⁻¹. The high molar mass fraction increases entrance pressure loss in the die; therefore accumulator-head tooling should avoid sharp die-entry angles below 30° to prevent melt fracture at high throughput. Bagley and Rabinowitsch corrections are required for capillary data because wall slip is limited but not absent in high-density polyethylene at these shear rates. On-line rheometers are used on production lines to track lot-to-lot variation in melt viscosity; a shift of ±5% in zero-shear viscosity is observable as a change in parison length and is corrected by adjusting screw speed rather than temperature when the melt temperature is already at the upper limit.
Die and mandrel design for B2555 must account for the high die swell and low melt-flow. Divergent die lands with land lengths of 10–15 mm are used for thick-walled containers; land length is adjusted to control shear history and die swell uniformity. In accumulator-head tooling, flow channels with sharp transitions or pin-holder disruptions generate memory effects that appear later as parison weld lines. Polished surfaces and gradual transitions are more important for this grade than for lower-viscosity HDPE.
The high molar mass fraction that provides slow crack growth resistance also carries most of the zero-shear viscosity. Extended hold-up in an accumulator head above 240 °C produces random chain scission in that fraction, permanently lowering ESCR even when the melt mass-flow rate remains inside the 0.20–0.30 g/10 min range. On scale-up from laboratory torque rheometers to production machines, the observed failure mode is not a soft barrel or gross discolouration, but a loss of parison uniformity and an increase in gel-like defects caused by oxidized high molar mass material breaking away from the edges of the die land. Accumulator-head machines with long residence times should therefore carry a shutdown purge with a low-MFR LDPE or a commercial purge compound; purging after each production stop reduces stagnation in the grooved bushing, adapters, and die-lip zones. Screw and barrel wear is another operational boundary. The high viscosity at 200 °C increases motor load relative to a conventional HDPE of 0.60 g/10 min; wear in the metering section above 0.5 mm clearance loss appears as throughput oscillations and parison length drift. On lines producing 25-L detergent bottles, this wear mode is frequently misdiagnosed as a stabilizer problem until the screw is pulled and measured. Because the grade is shear-thinning, use of high-shear mixing elements in corotating twin-screw extruders is not required for direct blow moulding and can reduce the high molar mass tail if masterbatch is compounded instead of dry-blended.
The tensile yield stress of 28 MPa and flexural modulus of 1350 MPa provide stacking stiffness, but the governing design criterion in aggressive media is slow crack growth. Unimodal HDPE grades with the same 0.25 g/10 min melt mass-flow rate often exhibit ASTM D1693 F50 values below 100 h in 10% Igepal CO-630 at 50 °C, whereas B2555 is specified above 600 h under the same condition. The distinction arises from the high molar mass tail and short-chain branch placement, not from density alone. In a 200-L stack-packed drum, the sidewall must withstand compressive hoop stress without craze formation; published industrial case histories identify weld-line contamination and cap-sealing defects as more common causes of leakage than bulk resin yield. The notched Charpy value of 25 kJ/m² at 23 °C is not intended for low-temperature impact applications below −20 °C, where a lower-density butene- or hexene-comonomer HDPE may be required.
Compared with a high-molecular-weight film HDPE of density 0.949 g/cm³ and melt mass-flow rate 0.05 g/10 min, B2555 has a higher MFR and higher density, which favours shorter blow moulding cycles and higher top-load capacity but gives lower dart impact and tear resistance if extruded as thin film; the grade is not used for thin-gauge film. Compared with a PE100 pipe compound, B2555 has a molecular design optimised for parison formability and surface quality in thick-wall hollow articles, and no hydrostatic design basis under ISO 9080 is claimed. Compared with a medium-molecular-weight injection moulding HDPE of melt mass-flow rate 20 g/10 min, B2555 cannot fill thin-wall moulds because the high viscosity prevents short-cycle injection; injection moulding is outside the intended processing envelope.
In quality-assurance practice, the melt mass-flow rate and density are primary lot-release parameters, but the high molar mass fraction is not fully captured by those two numbers. Gel permeation chromatography with infrared detection is used to quantify the high molar mass tail; a modest reduction in that tail can lower ESCR disproportionately while leaving MFR nearly unchanged. Batch-to-batch variation in comonomer placement also changes the slow crack growth response. For this reason, converter qualification protocols should include an ASTM D1693 F50 determination on each significant formulation change, and should not rely solely on the melt index specification.
For containers holding detergent concentrates, emulsifiable agricultural formulations, or surfactant-laden cleaners, ESCR testing under ASTM D1693 is a screening tool rather than a direct service-life prediction. Full-scale qualification on 200-L drums usually includes stack-load creep under ISO 16495 and drop impact under ASTM D2463. The high ESCR of B2555 allows the wall thickness distribution to be adjusted to meet top-load requirements without moving to a lower-density grade that would reduce buckling strength. The operational boundary appears when the same package is used with strong oxidizers, aromatic hydrocarbons, or chlorinated solvents at sustained temperatures above 40 °C. Under those conditions, the resin’s inertness is not the limiting factor; permeation through the wall and stress cracking in the neck and handle weld zones dominate. Published data for this specific configuration is limited for cyclic exposure to xylene and methylene chloride; those fluids sit outside the intended service envelope. For outdoor storage, carbon black addition in the 2.0–2.5 wt% range or a hindered amine light stabilizer package is required because unpigmented natural HDPE will embrittle after extended UV exposure; the base grade does not carry a long-term outdoor weathering warranty.
When dry-blending colour or UV masterbatch, the low melt-flow rate of B2555 requires a carrier resin with a matched density and a similar viscosity. A mismatched LDPE carrier with a melt mass-flow rate of 0.8 g/10 min can melt earlier in the grooved feed section and produce visible streaks in the parison. Gravimetric dosing at the throat is preferred over volumetric dosing to keep let-down within ±0.5%. On accumulator-head lines running dark-coloured detergent bottles, masterbatch deviations above 3% can create local viscosity shifts at the die lips and variable parison length, which are corrected by lowering screw speed and increasing back pressure rather than by raising head temperature, because the latter may damage the high molar mass fraction.
B2555 trimmings and flash can be reground and reintroduced into the blow moulding process at up to 20% with only minor changes to die swell, provided the regrind is dry and free of paper fines or conveying dust. Higher levels can reduce ESCR and increase gel specks because the high molar mass fraction is partially degraded during each heat history. Reprocessing should avoid repeated extrusion at temperatures above 230 °C. This boundary is important in multi-layer coextrusion where an inner layer of recycled B2555 is sandwiched between virgin skins to maintain surface quality and food-contact status.
The olefin base resin is within the scope of FDA 21 CFR 177.1520 for olefin polymers intended for food contact when the additive package and finished article conditions of use are consistent with the regulation. European food-contact status is assessed under EU 10/2011; overall migration must be verified on the converted article with food simulants assigned to the intended food type, commonly OM2 or OM7. The grade falls within the registration requirements of REACH; for electrical and electronic applications, RoHS 2011/65/EU applies to the completed article rather than to the polymer alone. Conformity to ASTM D4976 cell classification should be confirmed from the certificate of analysis because the grade designation does not specify additive package, UV stabilizer, or lot-to-lot molecular weight distribution. The product is not certified for potable water pressure pipe under ISO 4427, and no pharmaceutical or medical device claim is made for the unfilled resin.
The base resin is not formulated with intentionally added phthalates, and no halogenated flame retardants are used in the standard grade. A supplier composition statement should still be obtained for food-contact or toy applications because additives such as processing stabilizers, neutralizers, and lubricants may fall outside specific user protocols. Pellet handling should include dust control to avoid explosible dust concentrations under NFPA 654 or equivalent industrial hygiene standards; this is an operational safety boundary unrelated to polymer performance.