Sstpc Sinopec Sabic Tianjin Hdpe Pn049

SSTPC (Sinopec SABIC Tianjin) HDPE PN049

    • Product Name: SSTPC (Sinopec SABIC Tianjin) HDPE PN049
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 142247
    Product Name SSTPC (Sinopec SABIC Tianjin) HDPE PN049
    Polymer Type High Density Polyethylene (HDPE)
    Grade PN049
    Pe Classification PE100
    Mrs 10.0 MPa
    Density 0.959 g/cm³
    Melt Flow Rate 190 C 5 Kg 0.22 g/10 min
    Tensile Yield Strength 25 MPa
    Elongation At Break >600%
    Flexural Modulus 1000 MPa
    Vicat Softening Temperature 125 °C
    Oxidation Induction Time 200 C >20 min
    Carbon Black Content 2.0-2.5%
    Moisture Content <0.1%
    Bulk Density 0.55 g/cm³
    Color Black
    Form Pellets

    As an accredited SSTPC (Sinopec SABIC Tianjin) HDPE PN049 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SSTPC (Sinopec SABIC Tianjin) HDPE PN049 comes in 25 kg bags; 1,000 kg jumbo bags available.
    Container Loading (20′ FCL) 20′ FCL container loading of SSTPC (Sinopec SABIC Tianjin) HDPE PN049: 25 kg bags, palletized, shrink-wrapped, and secured for sea freight.
    Shipping Sinopec SABIC Tianjin HDPE PN049 ships as non-hazardous polyethylene pellets in 25 kg bags, palletized and shrink-wrapped. Use clean, dry containers or trucks. Protect from moisture, direct sunlight, heat, and contamination. Secure loads against shifting. Standard commercial documents apply; no UN dangerous goods classification or special placarding required.
    Storage Store SSTPC (Sinopec SABIC Tianjin) HDPE PN049 in a cool, dry, well-ventilated warehouse. Keep original bags sealed and palletized off the floor. Protect from direct sunlight, moisture, heat, ignition sources, and contamination. Avoid prolonged UV exposure and strong oxidizing agents. Maintain clean handling and follow the supplier SDS and local regulations.
    Shelf Life Shelf life is typically 24 months when stored unopened in a cool, dry, well-ventilated area, away from sunlight and moisture.
    Application of SSTPC (Sinopec SABIC Tianjin) HDPE PN049

    SSTPC HDPE PN049 is processed as a bimodal high-density polyethylene pipe resin in potable water distribution systems where the primary qualification route is ISO 4427-2 / EN 12201-2 for PE100. The natural resin’s density is approximately 0.949 g/cm³ per ISO 1183, and the melt mass-flow rate is near 0.30 g/10 min at 190 °C under 5 kg load per ISO 1133-1; these values place the grade in the high-molecular-weight pipe extrusion window where shear thinning is critical for output stability. The minimum required strength is evaluated under ISO 9080 and classified under ISO 12162; a PE100 designation corresponds to an MRS of 10.0 MPa and permits a design stress of 8.0 MPa at 20 °C with a service coefficient of 1.25 for water applications. Conversion on grooved-feed single-screw extruders uses L/D ratios between 30:1 and 36:1, barrel set temperatures from 180 °C to 210 °C, and die-head set temperatures from 200 °C to 220 °C; melt temperature at the die entry is maintained within 210 °C to 230 °C because lower melt temperatures produce insufficient homogenization of the high-molecular-weight fraction and higher temperatures accelerate thermo-oxidative degradation. Although the resin is not hygroscopic, surface condensation on pellets stored at high humidity should be removed with a dry-air hopper dryer at 60 °C for 1 h when ambient RH exceeds 60 %; otherwise moisture can generate surface voids at the die exit. For black pressure pipe, a carbon black masterbatch is dosed to achieve 2.0 wt% to 2.5 wt% carbon black content by mass in the pipe wall, and carbon black dispersion is assessed by ISO 18553 with a maximum rating of 3. Hydrostatic type tests are performed on finished pipe according to ISO 1167, typically at 20 °C, 12.4 MPa for 100 h, and at 80 °C, 5.4 MPa for 165 h, with additional long-term tests applied for PE100 qualification; slow crack growth is assessed by the notched pipe test of ISO 13479 at 80 °C under a hoop stress of 4.0 MPa, and no brittle failure is permitted within the specified period. Shared silo handling must exclude polyethylene-compound contamination with polypropylene or polyamide, as immiscible contaminants reduce slow crack growth resistance and can create weld-line defects in butt fusion joints. End products include buried water mains, service laterals, and district water distribution lines where butt fusion and electrofusion joints are used to assemble the polymer network.

    Gas Distribution Networks Under EN 1555: Melt Homogeneity and Rapid Crack Propagation Controls

    The same PE100 classification supports gas distribution piping when the compound is qualified under ISO 4437-2 / EN 1555-2; the design coefficient for natural gas systems is commonly 2.0, producing a design stress of 5.0 MPa at 20 °C for an MRS of 10.0 MPa. Gas pipe processors must control melt homogeneity more tightly than water pipe producers because localized high-molecular-weight gel particles created during poor plastication act as initiation sites for rapid crack propagation; extruders are therefore equipped with barrier screws, Maddock mixing sections, and melt-pressure transducers at the screen changer. A melt temperature ceiling of 230 °C is applied with barrel profiles of 180 °C to 210 °C to avoid molecular weight reduction that would shift the ISO 9080 regression curve and compromise the 50-year service life. Rapid crack propagation is evaluated by the small-scale steady-state test of ISO 13477; a pipe batch is rejected if the critical pressure falls below the minimum required for the installed operating pressure at the specified minimum wall temperature. Gas pipe is color-coded yellow or black with yellow longitudinal co-extruded stripes according to EN 1555; when black pipe is produced, the carbon black content is maintained at 2.0 wt% to 2.5 wt% and dispersion is checked to ISO 18553. The terminal products are SDR 11 and SDR 17 mains and service lines for natural gas distribution grids, where butt fusion welding is performed under ISO 21307 parameters with interfacial bead geometry used as a field weld acceptance indicator.

    Application segmentGoverning standard codePN049-relevant test methodCritical numerical acceptance or design value
    Potable water pressure pipeISO 4427-2, EN 12201-2ISO 9080, ISO 12162MRS 10.0 MPa; design stress 8.0 MPa at 20 °C
    Natural gas distribution pipeISO 4437-2, EN 1555-2ISO 13477Design stress 5.0 MPa at 20 °C
    Gravity sewer solid-wall pipeEN 12666-1ISO 9969Ring stiffness SN4 or SN8
    Cable conduitASTM F2160, NEMA TC 7ISO 18553Carbon black dispersion rating ≤ 3
    Mining slurry and dredge lineProject-specific, ASTM D3350 for cell classificationASTM D1693F50 > 1,000 h in 10 % Igepal
    Agricultural irrigation pressure pipeISO 4427-2, EN 12201-2ISO 11357-6OIT at 210 °C ≥ 20 min

    For mining slurry and dredge line service, PN049 is selected less for pressure containment than for resistance to slow crack growth and erosive particle impingement. Slurry lines are extruded as solid-wall HDPE pipe with wall thicknesses increased from pressure requirements to provide sacrificial wear allowance; typical SDR classes range from 9 to 13.5, and the outermost layer is formulated with 2.0 wt% to 2.5 wt% carbon black when the line is stored outdoors or floated on water. The bimodal molecular weight distribution of PN049 contributes to high environmental stress crack resistance, and the relevant material property is measured by ASTM D1693 at 50 °C in 10 % Igepal CO-630 solution with F50 failure times exceeding 1,000 h for qualified pipe compounds. In abrasive service, the processing constraint is torque management on the extruder: the resin’s melt viscosity at low shear is higher than unimodal HDPE grades, so screw speed must be reduced or barrel heating adjusted to maintain a melt temperature between 210 °C and 230 °C without exceeding the screw torque limit of the extrusion line. Production-scale lines often use a 33:1 L/D grooved-feed extruder with a static mixer at the die adapter to equalize melt temperature before the pipe die. Published abrasion test data for PN049 under standard slurry abrasion configurations is limited; wall wear allowance should therefore be validated by field slurry tests using the actual particle size distribution and solids loading rather than resin pellet data alone. End-use configurations include tailings transport from mineral concentrators, dredge discharge lines, and ash slurry disposal systems where flanged connections and wear-resistant elastomer couplings absorb axial movement and pump pulsation.

    When Is HDPE PN049 Extruded Into Solid-Wall Gravity Sewer Pipe?

    Solid-wall gravity sewer pipe is manufactured from PN049 under non-pressure drainage specifications where the governing performance criterion is ring stiffness rather than hydrostatic design stress. The material is processed on the same grooved-feed single-screw extruders used for pressure pipe, but downstream calibration and cooling equipment is configured for larger diameters and lower wall stresses. Ring stiffness is determined by pipe geometry and the flexural modulus of the compound; PN049-based pipe with a density of approximately 0.949 g/cm³ in natural form and a flexural modulus near 900 MPa can be dimensioned to meet SN4 or SN8 classifications under ISO 9969. The relevant product standard for buried gravity drainage and sewerage is EN 12666-1, while North American projects may reference ASTM F2306 for corrugated or profile-wall HDPE pipe; when PN049 is used in solid-wall pipe, the extrusion line’s pipe die and vacuum calibration sleeves must be matched to the outer diameter and wall thickness required for the specified ring stiffness. Carbon black content is maintained at 2.0 wt% to 2.5 wt% for ultraviolet resistance, and butt fusion joints are executed under ISO 21307 procedures to produce leak-free gravity lines. Terminal products include municipal storm sewers, combined sewer outfalls, and industrial drainage collectors where chemical resistance to dilute acids and soil loads is required over a design life of 50 years.

    Extrusion variableIndicative rangeMeasurement or control point
    Single-screw extruder L/D ratio30:1–36:1Machine specification
    Barrel zone set temperature180 °C–210 °CPID thermocouples on cylinder
    Adapter and die head set temperature200 °C–220 °CBand and probe controllers
    Melt temperature at die entry210 °C–230 °CMelt pyrometer immersion probe
    Carbon black content in pipe wall2.0 wt%–2.5 wt%Muffle furnace or TGA follow-up
    Die-head melt pressure20 MPa–40 MPaMelt-pressure transducer before screen changer
    Carbon black dispersionRating ≤ 3ISO 18553 microtome specimen

    If Cable Protection Conduit Requires Crush Resistance Without Internal Pressure Classification

    Cable protection conduit and telecom duct made from PN049 are non-pressure extrusions in which the resin’s melt strength and slow crack growth resistance support solid-wall designs specified under ASTM F2160 or smooth-wall coilable duct under NEMA TC 7. The processing window differs from pressure pipe because wall thickness is lower and haul-off speed is higher; vacuum calibration tanks apply controlled negative pressure to fix the outer diameter while the inner surface is air-cooled. Crush resistance and low-temperature impact requirements are geometry-dependent and are measured on finished conduit rather than on resin pellets; PN049-based conduit can be tested under ASTM F2160 for outside diameter, wall thickness, ovality, and tensile strength parameters. The pipe is produced in black with 2.0 wt% to 2.5 wt% carbon black, and the dispersion of the carbon black is checked by ISO 18553 to avoid localized embrittlement in cold-weather cable pulls. Terminal products are buried duct banks for fiber-optic trunk lines, high-voltage power cable sleeves, and railway signal conduits where the pipe must withstand compression from soil loads and construction equipment.

    Agricultural Irrigation Mainline and Sub-main Pressure Systems

    Agricultural irrigation mainlines and sub-mains consume PN049 in PE100 pipe designed for intermittent flow, seasonal temperature swings, and disinfectant or fertilizer residuals. The governing documents are ISO 4427-2 and EN 12201-2 for pressure pipe; the design stress is selected from the same 10.0 MPa MRS classification with service coefficients adjusted by the system designer. Chlorine-containing water can cause oxidative attack, so the pipe compound’s stabilizer package is evaluated by oxidative induction time at 210 °C per ISO 11357-6, with a common minimum OIT of 20 min for qualified PE100 pipe materials; resistance to chlorine-induced slow crack growth may be assessed by ASTM F2263 where potable or treated irrigation water is transported. The extrusion process for smaller-diameter irrigation pipe uses a 33:1 L/D grooved-feed extruder and die-head pressure between 20 MPa and 40 MPa, depending on the SDR and tooling diameter; the melt is filtered through screen packs of 60/80/120 mesh to remove gels before the die. Fittings are typically injection molded from a PE100-compatible fitting compound, or machined from thick-walled pipe, and joined by butt fusion or electrofusion. Terminal end products include solid-wall above-ground pump discharge lines, buried mainlines for drip and micro-sprinkler systems, and sub-main pipes that reduce the number of riser connections in large-field layouts.

    Free Quote

    Competitive SSTPC (Sinopec SABIC Tianjin) HDPE PN049 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SSTPC (Sinopec SABIC Tianjin Petrochemical Co., Ltd.) HDPE PN049 is a bimodal high-density polyethylene pipe extrusion compound supplied as black pellets. The material is designated for long-term pressure-pipe service and is classified within the PE100 stress category under ISO 12162, with an extrapolated minimum required strength of 10 MPa at 20 °C for 50 years per ISO 9080. The grade is distinguished from injection and blow moulding HDPE resins by its low melt flow rate, published at 0.40 g/10 min under 5 kg load at 190 °C. Representative datasheet values include a base resin density of 0.949 g/cm³, tensile yield stress of 22 MPa, elongation at break greater than 600%, and flexural modulus near 900 MPa. These values position PN049 among high-molecular-weight bimodal PE100 pipe compounds used for pressure water, industrial fluid, and gaseous fuel distribution systems where long-term creep rupture resistance and slow crack growth resistance are governing design factors.

    The bimodal molecular weight distribution of PN049 combines a low-molecular-weight fraction that reduces melt viscosity during extrusion with a high-molecular-weight fraction that increases tie-molecule density in the crystalline network. This architecture shifts the long-term failure mode under sustained hoop stress from brittle crack propagation toward ductile yielding over long test periods. Unlike conventional unimodal HDPE grades, PN049 is formulated to maintain hydrostatic design basis after notched-pipe exposure and pipe surface damage. However, the resin itself does not confer final product certification; pipe manufacturers must qualify the converted pipe according to the relevant system standards.

    What separates PN049 from unimodal PE80 and first-generation PE100 compounds?

    Unimodal PE80 pipe resins are classified with an MRS of 8 MPa, whereas PN049 carries an MRS of 10 MPa. Under ISO 4427 and EN 1555, this difference permits higher design stress at the same service temperature or a reduced wall thickness at a given pressure rating. A PE80 pipe at SDR 11 has a lower pressure rating than a PE100 pipe at SDR 11; conversely, PN049 can achieve the same rating at higher SDR, reducing mass per metre. Compared with first-generation unimodal PE100 grades, PN049’s bimodal architecture provides a broader molar mass distribution. The high-molecular-weight tail increases entanglement density and slow crack growth resistance, while the low-molecular-weight tail maintains shear thinning. This reduces the processing torque penalty that would otherwise accompany a fully high-molecular-weight resin. The distinction is observed in notched pipe tests such as ISO 13479 and in creep rupture testing under ISO 9080, where bimodal PE100 compounds generally withstand higher crack-initiation times at a given stress intensity.

    Within the SSTPC HDPE portfolio, PN049 differs from injection moulding grades with melt flow rates commonly in the range of 5 g/10 min to 20 g/10 min. Those products are intended for thin-wall moulded components and closures. PN049 also differs from high-flow pipe coating and film grades because its melt strength is tuned for sag resistance in thick-wall pipe extrusion. The difference in melt elasticity is visible on a capillary rheometer as higher entrance pressure loss and longer relaxation time; these features are intentional for large-diameter pipe dimensional stability.

    Representative datasheet profile and test method matrix

    The following table consolidates representative values from public technical literature and typical PE100 black compound datasheets. Actual certificate-of-analysis values may vary by production lot and should be obtained from SSTPC.

    PropertyTest methodTypical valueUnit
    Density (base resin)ISO 1183-10.949g/cm³
    Melt flow rate at 190 °C / 5 kgISO 1133-10.40g/10 min
    Tensile stress at yieldISO 527-222MPa
    Elongation at breakISO 527-2>600%
    Flexural modulusISO 178900MPa
    Oxidation induction time at 210 °CISO 11357-6≥20min
    Carbon black contentISO 69642.0–2.5%
    Moisture contentISO 15512≤0.05%

    These properties are determined on compression-moulded or injection-moulded test specimens, not directly on pipe. For pipe-specific design, the hydrostatic strength of the converted pipe must be evaluated under ISO 4427 and ISO 9080. The carbon black content range of 2.0% to 2.5% provides ultraviolet stabilization. Dispersion quality is evaluated by ISO 18553; poor dispersion can create local stress concentrations at pipe surfaces.

    Project specifications usually require the following compliance matrix:

    Standard / test designationScopeRelevance to PN049 pipe manufacture
    ISO 12162Classification of thermoplastic pipe materialsPE100 MRS 10 MPa designation
    ISO 9080Long-term hydrostatic strength extrapolation50-year strength basis at 20 °C
    ISO 4427PE pressure pipe systems for waterPipe dimensional and pressure rating basis
    EN 1555PE piping for gaseous fuelsGas distribution pipe qualification
    ISO 13479Notched pipe test for slow crack growthSCG resistance evaluation
    ISO 21307Butt fusion welding of PE pipesJointing procedure for PN049 pipes
    NSF/ANSI/CAN 61 or equivalentHealth effects of potable water componentsRequires pipe manufacturer verification

    When PN049 is processed on grooved-feed single-screw extrusion lines

    Extrusion of PN049 is typically performed on single-screw extruders with grooved-feed sections and screw lengths of L/D 30:1 to L/D 37:1. Barrel set temperatures commonly range from 180 °C to 220 °C, with adapter and die head temperatures maintained between 200 °C and 210 °C. Melt temperatures should not exceed 230 °C to 240 °C because thermo-oxidative degradation of the high-molecular-weight fraction can generate crosslinked gels, reduce oxidation induction time, and produce surface roughness. At the opposite boundary, melt temperatures below 180 °C reduce carbon black dispersion and may cause shark-skin melt fracture, especially at high shear rates through pipe dies. Screw torque is higher than for unimodal PE80 resins. Extruder drives operating near torque limits should be derated by 10% to 15% when changing from PE80 to PN049. Melt pump inlet pressure on a 75 mm grooved-feed extruder at approximately 400 kg/h is often observed in the range of 25 MPa to 35 MPa, though line-specific pressure loss depends on die land length and pipe diameter.

    Virgin pellets stored in dry sealed containers do not require routine pre-drying. Regrind exposed to relative humidity above 60% should be dried at 80 °C for 2 hours to reach moisture content below 0.05%. In thick-wall pipes, the residual stress generated by rapid external cooling can be controlled by increasing calibrator length and reducing cooling-water temperature differential. Pipe dimensions, wall thickness, and pressure ratings are governed by ISO 4427 for water and EN 1555 for gas. The selected SDR must match the design pressure and service temperature.

    Slow crack growth resistance does not automatically confer chemical compatibility

    The high tie-molecule density of PN049 improves slow crack growth resistance under sustained stress, but this mechanical property does not prevent oxidative attack by disinfectants, strong acids, or hydrocarbon permeation. The oxidation induction time at 210 °C is typically ≥20 min per ISO 11357-6, reflecting the antioxidant package. In potable-water service with free chlorine concentrations above 1 mg/L at elevated temperatures, antioxidant depletion can occur at the pipe wall; design codes apply chlorine reduction factors and temperature derating. Contact with copper ions, manganese-based catalysts, or amine-based fire-retardant additives can antagonize the stabilizer package and should be avoided unless validated by long-term hydrostatic exposure. For buried gas distribution, hydrocarbon permeation is low but not zero; odorant compatibility should be assessed with the specific mercaptan or sulfur-free odorant used by the network operator.

    For potable-water contact, pipe manufacturers must verify compliance with national health-effect standards such as NSF/ANSI/CAN 61, EU 10/2011, or corresponding local approvals. The PN049 pellet grade alone does not provide these approvals; certification applies to the finished pipe system. Regrind addition above 10% by mass can alter melt flow rate, antioxidant concentration, and carbon black dispersion, and should be qualified by retained tensile, OIT, and hydrostatic tests.

    PN049 is used in extruded pressure pipe for drinking water, irrigation, sewage pressure mains, and natural gas distribution. Pipe manufactured from PN049 is typically butt-fusion welded using procedures defined in ISO 21307; fusion temperature, bead rollover size, and cooling time must be adjusted for wall thickness and ambient conditions. Electrofusion joining of PN049 pipe should use fittings designed for PE100, with heating cycles validated under the fitting manufacturer’s procedure. The low melt flow rate of PN049 is not optimized for injection-moulded fittings; many fitting producers select PE100 grades with higher MFR or use injection-compression moulding with higher barrel temperatures. Published data for this specific configuration—SSTPC PN049 processed into large-diameter fittings—is limited; trials should define the processing window.

    In pressure rating calculations for PE100 water pipe, the design stress is derived from 10 MPa MRS and an overall service coefficient of 1.25, yielding 8 MPa. Under this basis, SDR 11 corresponds to PN16, SDR 13.6 to PN12.5, SDR 17 to PN10, and SDR 21 to PN8 at 20 °C. In comparison with MDPE and lower-density HDPE pipe resins, PN049’s higher density of 0.949 g/cm³ as a base resin increases modulus and hoop strength but slightly reduces stress-crack resistance relative to lower-density copolymers. The black compound is suitable for above-ground storage and installation due to carbon black ultraviolet screening; however, long-term outdoor exposure beyond 5 years without pressure derating should consider surface oxidation and coating if required by project specification. The product is not intended for use with strong oxidizing acids at elevated temperatures, aromatic hydrocarbon distribution, or continuous service above 60 °C unless explicitly qualified by the pipe manufacturer.